Abstract
Chloride-induced reinforcement corrosion is a major cause of premature deterioration of reinforced concrete bridge elements exposed to cyclic wetting and de-icing agents. Visual inspection mainly records the propagation stage, whereas water-soluble chloride testing can identify hazardous conditions before widespread cracking and spalling. Chloride content, however, cannot by itself define the operational condition without considering reinforcement depth, moisture, cracking and electrochemical evidence. To generalize field measurements of water-soluble chlorides in six transportation structures in Kyiv, evaluate spatial variability and develop a practical diagnostic workflow. The study covered a bridge over the Lybid River and five overpasses near Poliarna Street, Portova Street and the Osokorky, Nyvky and Chernihivska metro stations. Visual inspection, core or local sampling, layer preparation and silver nitrate titration were used. After removing duplicate and missing records, 103 determinations expressed as percent of estimated cement mass were analyzed. Water-soluble chloride content ranged from 0.01 to 2.00 %, with a median of 0.55 %. Under the adopted limits for non-prestressed reinforcement, 23 results fell within the common range for conditions 1–3, 36 within condition 4, and 44 within condition 5; the corresponding counts for prestressed reinforcement were 19, 13, and 71. Thirty paired surface/deeper measurements confirmed a non-uniform chloride profile. Results should be interpreted using assessment levels corresponding to operational conditions 1–5, with separate limits for prestressed and non-prestressed reinforcement and samples taken at two levels. Chloride content alone does not distinguish conditions 1–3; the final condition requires visual, electrochemical, and structural evidence.