Effect of Various Veneering Techniques on Mechanical Strength of Computer‐Controlled Zirconia Framework Designs
- 13 January 2014
- journal article
- Published by Wiley in Journal of Prosthodontics
- Vol. 23 (6) , 445-455
Abstract
Purpose: The objectives of this study were to evaluate the fracture resistance (FR), flexural strength (FS), and shear bond strength (SBS) of zirconia framework material veneered with different methods and to assess the stress distributions using finite element analysis (FEA).Materials and Methods: Zirconia frameworks fabricated in the forms of crowns for FR, bars for FS, and disks for SBS (N = 90, n = 10) were veneered with either (a) file splitting (CAD‐on) (CD), (b) layering (L), or (c) overpressing (P) methods. For crown specimens, stainless steel dies (N = 30; 1 mm chamfer) were scanned using the labside contrast spray. A bilayered design was produced for CD, whereas a reduced design (1 mm) was used for L and P to support the veneer by computer‐aided design and manufacturing. For bar (1.5 × 5 × 25 mm3) and disk (2.5 mm diameter, 2.5 mm height) specimens, zirconia blocks were sectioned under water cooling with a low‐speed diamond saw and sintered. To prepare the suprastructures in the appropriate shapes for the three mechanical tests, nano‐fluorapatite ceramic was layered and fired for L, fluorapatite‐ceramic was pressed for P, and the milled lithium‐disilicate ceramics were fused with zirconia by a thixotropic glass ceramic for CD and then sintered for crystallization of veneering ceramic. Crowns were then cemented to the metal dies. All specimens were stored at 37°C, 100% humidity for 48 hours. Mechanical tests were performed, and data were statistically analyzed (ANOVA, Tukey's, α = 0.05). Stereomicroscopy and scanning electron microscopy (SEM) were used to evaluate the failure modes and surface structure. FEA modeling of the crowns was obtained.Results: Mean FR values (N ± SD) of CD (4408 ± 608) and L (4323 ± 462) were higher than P (2507 ± 594) (p < 0.05). Mean FS values (MPa ± SD) of CD (583 ± 63) and P (566 ± 54) were higher than L (428 ± 41) (p < 0.05). Mean SBS values (MPa ± SD) of CD (49 ± 6) (p < 0.05) were higher than L (28 ± 5) and P (30 ± 8). For crown restorations, while cohesive failures within ceramic and zirconia were seen in CD, cohesive failures within ceramic were found in both L and P. Results were verified by FEA.Conclusion: The file splitting technique showed higher bonding values in all mechanical tests, whereas a layering technique increased the FR when an anatomical core design was employed. Clinical significance: File splitting (CAD‐on) or layering veneering ceramic on zirconia with a reduced framework design may reduce ceramic chipping.Keywords
Funding Information
- Ege University, Scientific Research Project Department (2011-DİŞ-006)
This publication has 30 references indexed in Scilit:
- Load-bearing capacity and failure types of anterior zirconia crowns veneered with overpressing and layering techniquesDental Materials, 2011
- Experimental and FE shear-bonding strength at core/veneer interfaces in bilayered ceramicsDental Materials, 2011
- Fracture stability of anterior zirconia crowns with different core designs and veneered using the layering or the press-over techniqueEuropean Journal of Oral Sciences, 2011
- Prototyping for Surgical and Prosthetic TreatmentJournal of Craniofacial Surgery, 2011
- Performance of Dental Ceramics: Challenges for ImprovementsJournal of Dental Research, 2011
- Influence of the fabrication process on the in vitro performance of fixed dental prostheses with zirconia substructuresClinical Oral Investigations, 2010
- Fit of zirconia fixed partial denture: a systematic reviewJournal of Oral Rehabilitation, 2010
- Influence of substructure design and spacer settings on the in vitro performance of molar zirconia crownsJournal of Dentistry, 2009
- State of the art of zirconia for dental applicationsDental Materials, 2008
- Fatigue and fracture properties of yttria partially stabilized zirconia crown systemsDental Materials, 2008