The present study investigates the development of fatigue damage in welded S460 high-strength steel specimens subjected to different corrosion exposure conditions. Four surface conditions were considered: an uncorroded reference condition, 3-day exposure, 6-day exposure and combined 6+3-day exposure, hereafter referred to as 3D, 6D and 6+3D/9D, respectively. Fatigue tests were performed at a stress ratio of . Microscopic observations were carried out before and after fatigue testing using an Olympus DSX1000 digital microscope to evaluate surface degradation, crack/fracture localization and damage development in the welded region. The uncorroded reference condition showed fatigue damage that was predominantly localized in the welded region, thereby confirming the dominant role of weld geometry and the local notch effect. As the level of corrosion exposure increased, the surface condition changed progressively. The 3D condition exhibited limited early degradation, the 6D condition revealed more distinct surface defects, and the 6+3D/9D condition showed the most pronounced corrosion-product regions and pit-like surface damage. The fatigue results indicated a non-monotonic influence of corrosion exposure. The apparent improvement observed for the 3D and 6D conditions may be related to local modification of the weld-toe surface condition and partial mitigation of the original weld-induced notch effect. After fatigue testing, all representative specimens showed crack/fracture development near the weld toe and heat-affected zone (HAZ) vicinity. The findings indicate that fatigue damage was governed by the combined effect of weld-toe geometry, the visually distinguishable HAZ vicinity and corrosion-induced surface degradation.

This publication has 12 references indexed in Scilit: