500 °C high-temperature reliability of Ni/Nb ohmic contact on n-type 4H-SiC

Authors:

Abstract
The reliability of Ni/Nb ohmic contact on n-type 4H-SiC at 500 °C was investigated. The current–voltage characteristics showed that, while the Ni(50)/Nb(50)/4H-SiC sample without applying the CF 4 :O 2 etching process degraded just after 25 h and lost ohmic behavior after 50 h aging, the Ni(75)/Nb(25)/4H-SiC contact undergone CF 4 :O 2 surface treatment still showed excellent stability after aging for 100 h at 500 °C. Though X-ray diffraction results indicated that the chemical compounds remained stable during the aging process, transmission electron microscopy showed that there was a redistribution of the chemical compounds at the interface of the contact after 500 °C aging. The depth distribution of the elements and energy-dispersive X-ray analyses revealed that the contribution of carbon agglomeration at the interface accounted for the degradation of the sample without applying the etching process. Whereas the well-controlled excess carbon atoms of the contact undergone CF 4 :O 2 treatment ensured the stability of this contact when operating at a high ambient temperature.
Funding Information
  • JSPS KAKENHI (JP15KK0240)
  • JSPS KAKENHI (JP17H03253)
  • JSPS KAKENHI (JP20H00252)

This publication has 38 references indexed in Scilit: