Surface Evaluation of Polishing Techniques for New ResilientCAD/CAMRestorative Materials
- 14 July 2015
- journal article
- Published by Wiley in Journal of Esthetic and Restorative Dentistry
- Vol. 28 (1) , 56-66
Abstract
Purpose: The purpose of this study was to measure the surface roughness of milled chairside computer‐assisted design/computer assisted machining (CAD/CAM) restorations using several contouring/polishing systems as to their effectiveness for creating a clinically acceptable surface.Materials and Methods: One hundred onlays were milled from monolithicCAD/CAMblocks with anMCXLmilling chamber (SironaDental) as follows: 30 resin nano‐ceramic (LavaUltimate, 3M ESPE), 30 hybrid ceramic (Enamic,Vita) and 40 leucite‐reinforced ceramic (EmpressCAD,Ivoclar). A single group ofEmpressCADonlays was glazed‐fired in a porcelain oven (ProgramatCS2,Ivoclar). Finishing and polishing systems consisted of either an abrasive‐polish technique or a brush‐polish technique. Roughness values were measured using a three‐dimensional measuring laser microscope (OLS4000 LEXTbyOlympus).Results: There was a significant difference in the baseline surface roughness of theCAD/CAMmaterials (p ≤ 0.05), with the resin nano‐ceramic (LavaUltimate) being smoother than the hybrid ceramic (Enamic), and both being smoother than the leucite‐reinforced ceramic (EmpressCAD). All polishing techniques resulted in a smoother surface compared with the baseline surface for the leucite‐reinforced ceramic (p ≤ 0.05), with both techniques resulting in a significantly smoother surface than glazing in a porcelain oven (p ≤ 0.05). Both polishing techniques resulted in a smoother surface compared with the baseline surface for both the nano‐ceramic and hybrid ceramic materials (p ≤ 0.05).Conclusions: It is possible to create an equally smooth surface for chairsideCAD/CAMresilient materials compared with milled ceramics using several finishing and polishing techniques. In general, the polished ceramic surfaces were smoother than the glazed ceramic surfaces.Clinical Significance: The results of the study indicate that it is possible to create an equally smooth surface for chairsideCAD/CAMresilient materials compared with milled ceramics using several finishing and polishing techniques. In addition, both polishing techniques resulted in smoother ceramic surfaces when compared to glazed ceramic surfaces. The polished surface of the ceramic material was smoother than the glazed ceramic surface.Keywords
Funding Information
- VH Technology
This publication has 17 references indexed in Scilit:
- Performance of Different Polishing Techniques for Direct CAD/CAM Ceramic RestorationsOperative Dentistry, 2010
- Effects of Six Surface Treatment Methods on the Surface Roughness of a Low‐Fusing and an Ultra Low‐Fusing Feldspathic Ceramic MaterialJournal of Prosthodontics, 2009
- Wear of ceramic and antagonist—A systematic evaluation of influencing factors in vitroDental Materials, 2008
- Which mechanical and physical testing methods are relevant for predicting the clinical performance of ceramic‐based dental prostheses?Clinical Oral Implants Research, 2007
- An overview of treatment considerations for esthetic restorations: A review of the literatureThe Journal of Prosthetic Dentistry, 2006
- Effect of surface roughness of porcelain on adhesion of bacteria and their synthesizing glucansThe Journal of Prosthetic Dentistry, 2000
- An in vitro investigation into the wear effects of glazed, unglazed and refinished dental porcelain on an opposing materialJournal of Oral Rehabilitation, 1999
- Comparison of methods for measuring surface roughness of ceramicJournal of Oral Rehabilitation, 1995
- Surface roughness of two polished ceramic materialsThe Journal of Prosthetic Dentistry, 1994
- Strengthening of porcelain by ion exchange subsequent to thermal temperingDental Materials, 1992