High-speed scanning ablation of dental hard tissues with a λ = 9.3 μm CO2 laser: adhesion, mechanical strength, heat accumulation, and peripheral thermal damage
Authors:
- 1 January 2011
- journal article
- research article
- Published by SPIE-Intl Soc Optical Eng in Journal of Biomedical Optics
- Vol. 16 (7) , 071410-071410-9
Abstract
CO2 lasers can be operated at high laser pulse repetition rates for the rapid and precise removal of dental decay. Excessive heat accumulation and peripheral thermal damage is a concern when using high pulse repetition rates. Peripheral thermal damage can adversely impact the mechanical strength of the irradiated tissue, particularly for dentin, and reduce the adhesion characteristics of the modified surfaces. The interpulpal temperature rise was recorded using microthermocouples situated at the roof of the pulp chamber on teeth that were occlusally ablated using a rapidly-scanned CO2 laser operating at 9.3 μm with a pulse duration of 10 to 15 μs and repetition rate of 300 Hz over a 2 min time course. The adhesion strength of laser treated enamel and dentin surfaces was measured for various laser scanning parameters with and without post-ablation acid etching using the single-plane shear test. The mechanical strength of laser-ablated dentin surfaces were determined via the four-point bend test and compared to control samples prepared with 320 grit wet sand paper to simulate conventional preparations. Thermocouple measurements indicated that the temperature remained below ambient temperature if water-cooling was used. There was no discoloration of either dentin or enamel laser treated surfaces, the surfaces were uniformly ablated, and there were no cracks visible. Four-point bend tests yielded mean mechanical strengths of 18.2 N (s.d. = 4.6) for ablated dentin and 18.1 N (s.d. = 2.7) for control (p > 0.05). Shear tests yielded mean bond strengths approaching 30 MPa for both enamel and dentin under certain irradiation conditions. These values were slightly lower than nonirradiated acid-etched control samples. Additional studies are needed to determine if the slightly lower bond strength than the acid-etched control samples is clinically significant. These measurements demonstrate that enamel and dentin surfaces can be rapidly ablated by CO2 lasers with minimal peripheral thermal and mechanical damage and without excessive heat accumulation.Keywords
Funding Information
- NIH/NIDCR (R01-DE19631)
- National Institute of Dental and Craniofacial Research (R01-DE19631)
- NIH/NIDCR (T32 DE0073060)
This publication has 52 references indexed in Scilit:
- Pulpal effects of enamel ablation with a microsecond pulsed λ = 9.3‐µm CO2 laserLasers in Surgery and Medicine, 2009
- Weakening of dentin from cracks resulting from laser irradiationDental Materials, 2009
- Nondestructive assessment of dentin demineralization using polarization‐sensitive optical coherence tomography after exposure to fluoride and laser irradiationJournal of Biomedical Materials Research Part B: Applied Biomaterials, 2009
- Near-infrared image-guided laser ablation of dental decayJournal of Biomedical Optics, 2009
- Adhesion of composite to enamel and dentin surfaces irradiated by IR laser pulses of 0.5–35 μs durationJournal of Biomedical Materials Research Part B: Applied Biomaterials, 2006
- Rapid and conservative ablation and modification of enamel, dentin, and alveolar bone using a high repetition rate transverse excited atmospheric pressure CO[sub 2] laser operating at λ=9.3 μmJournal of Biomedical Optics, 2006
- Chemical analysis and surface morphology of enamel and dentin following 9.6μ CO2 laser irradiation versus high speed drillingJournal of Dentistry, 2005
- Thermal and chemical modification of dentin by 9–11‐μm CO2 laser pulses of 5–100‐μs durationLasers in Surgery and Medicine, 2002
- Histologic analysis of the effect on dental pulp of a 9.6-?m CO2 laserLasers in Surgery and Medicine, 2002
- Sealant bond strengths of CO2 laser-etched versus acid-etched bovine enamelLasers in Surgery and Medicine, 2000