Effect of Isochronous Annealings on the Microstructure and Mechanical Properties of the Ti49.8Ni50.2 (at.%) Alloy after abc Pressing at 573 K
Open Access
Abstract
The regularities and features of the evolution of the grain–subgrain structure, phase composition and mechanical properties in Ti49.8Ni50.2 (at.%), depending on the temperature of isochronous annealings at 573–973 K are herein studied. The state of the Ti49.8Ni50.2 (at.%) alloy samples after abc pressing at T = 573 K with the given true strain e = 9.55 was taken as the initial state. It is shown that the grain–subgrain structure of the samples after annealing for 1 h in the temperature range of 573–673 K changes slightly. In samples annealed at 673 K, regions with the microband structure similar to the microstructure of a fast-frozen turbulent liquid flow were found. It has been established that during annealing at 773 K the beginning of an active recrystallization process is realized; the size of grains does not exceed the submicrocrystalline scale (~200 nm). At 873 K, the recrystallization process occurs in the entire volume of the samples; the grains with an average size of 2 ± 0.5 µm are almost equiaxed. The microstructure of the samples after annealing at 973 K (with average grain sizes of 5 ± 0.5 µm) is qualitatively similar to the microstructure of the samples after annealing at 873 K. It was found that the phase composition of the samples as a result of isochronous annealing at 573–973 K changes from R and B19’ immediately after abc pressing to a three-phase state: B2, R and B19’ phases. It is shown that the highest values of yield stress σy, ultimate tensile strength σUTS (1043 MPa and 1232 MPa, correspondingly) and low ductility (the deformation to fracture εf = 48%) are observed in the initial samples. Increasing the temperature of post-deformation annealing and, correspondingly, the development of recrystallization, led to a decrease in σy, σUTS and an increase in εf to the values of these characteristics in the coarse-grained samples (σy = 400 MPa, σUTS = 920 MPa and εf = 90%).Keywords
Funding Information
- Government research assignment for ISPMS SB RAS (project FWRW-2021-0004)
This publication has 16 references indexed in Scilit:
- Large and Severe Plastic Deformation of Metals: Similarities and Differences in Flow Mechanics and Structure FormationAdvanced Engineering Materials, 2021
- Effect of Quasi-Continuous Equal-Channel Angular Pressing on Structure and Properties of Ti-Ni Shape Memory AlloysJournal of Materials Engineering and Performance, 2021
- Structural evolutions of metallic materials processed by severe plastic deformationMaterials Science and Engineering: R: Reports, 2018
- An overview on severe plastic deformation: research status, techniques classification, microstructure evolution, and applicationsThe International Journal of Advanced Manufacturing Technology, 2018
- Effect of the quasi-continuous equal-channel angular pressing on the structure and functional properties of Ti–Ni-based shape-memory alloysPhysics of Metals and Metallography, 2017
- Grain size effect on stress hysteresis of nanocrystalline NiTi alloysJournal of Alloys and Compounds, 2016
- Mechanisms of Microstructure Evolution in TiNi-Based Alloys under Warm Deformation and its Effect on Martensite TransformationsMaterials Science Foundations, 2015
- Effect of the grain/subgrain size on the strain-rate sensitivity and deformability of Ti–50 at%Ni alloyMaterials Science and Engineering: A, 2015
- Extreme grain refinement by severe plastic deformation: A wealth of challenging scienceActa Materialia, 2013
- Mechanical properties of nanocrystalline materialsProgress in Materials Science, 2006