Optimizing diphenyl(2,4,6‐trimethylbenzoyl)phosphine oxide concentration and post‐curing time to balance mechanical properties and color stability in a three‐dimensional‐printed restorative resin
Authors:
- Eloah Nunes de AlmeidaEAEloah Nunes de Almeida
- Vinicius da Nóbrega MarquesVMVinicius da Nóbrega Marques
- Ido Luiz de Azevedo FeitenIFIdo Luiz de Azevedo Feiten
- André Luis Faria‐E‐SilvaAFAndré Luis Faria‐E‐Silva
- Larissa Maria CavalcanteLCLarissa Maria Cavalcante
- Luis Felipe SchneiderLSLuis Felipe Schneider
Open Access
- 10 August 2026
- journal article
- research article
- Published by Wiley in European Journal of Oral Sciences
- p. e70125
Abstract
Three‐dimensional (3D) printing is widely used in dental restorations; however, optimization of photoinitiator concentration and post‐curing protocols remains critical to achieve a balance between mechanical and esthetic performance. This study evaluated the combined effect of diphenyl(2,4,6‐trimethylbenzoyl)phosphine oxide (TPO) concentration and post‐curing time on mechanical properties and color stability of a 3D‐printed restorative resin. A commercial photoinitiator‐free resin (BioPrint Prov, Horus 3D) was supplemented with TPO at 0.5, 1.0, and 1.5 wt% and fabricated using a digital light processing printer. Specimens were post‐cured for 30, 45, or 60 min under UV light, while non‐post‐cured (NoPC) samples served as controls. Flexural strength and elastic modulus were evaluated using a three‐point bending test. Color stability and translucency were assessed using spectrophotometry (CIELab/Δ E 00 ) under storage conditions, including dry storage, water immersion, and coffee aging. Data were analyzed using two‐way anova and Tukey's test. The 1.0% TPO and 30 min post‐curing combination provided best performance, with highest flexural strength and lowest color change after staining. Higher TPO concentration and prolonged post‐curing increased color alteration and yellowness. NoPC specimens showed inferior mechanical properties and greater discoloration. Translucency remained more stable in post‐curing groups. These findings indicate optimized photoinitiator concentration and controlled post‐curing time improve mechanical and esthetic outcomes in 3D‐printed restorative resins.Keywords
This publication has 25 references indexed in Scilit:
- The influence of filler load in 3D printing resin-based compositesDental Materials, 2024
- The influence of printing angle on color and translucency of 3D printed resins for dental restorationsDental Materials, 2023
- The selection of photoinitiators for photopolymerization of biodegradable polymers and its application in digital light processing additive manufacturingJournal of Biomedical Materials Research Part A, 2021
- 3D printing restorative materials using a stereolithographic technique: a systematic reviewDental Materials, 2021
- Highly filled resins for DLP-based printing of low density, high modulus materialsAdditive Manufacturing, 2021
- Cytotoxic and genotoxic potential of the type I photoinitiators BAPO and TPO on human oral keratinocytes and V79 fibroblastsDental Materials, 2018
- Translucency thresholds for dental materialsDental Materials, 2018
- 3D Printing of Polymer Nanocomposites via StereolithographyMacromolecular Materials and Engineering, 2017
- Color stability, conversion, water sorption and solubility of dental composites formulated with different photoinitiator systemsJournal of Dentistry, 2013
- Competitive light absorbers in photoactive dental resin-based materialsDental Materials, 2012