Luis Felipe Jochinms Schneider
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Luis Felipe Jochinms Schneider has a total of 85 co-authors. Here are the top co-authors by number of shared publications:
- Larissa Maria Cavalcante
Universidade Federal Fluminense
15 shared publications - André Luis Faria-E-Silva
Department of Dentistry, Dental School, Laval University, Québec QC, Canada
5 shared publications - Carmem Silvia Pfeifer
Oregon Health and Science University, USA
5 shared publications - Eloah Nunes de Almeida
Laboratory for Applied Biotechnology (LABA UFF), School of Dentistry Federal Fluminense University Niterói Brazil
4 shared publications - Ido Luiz de Azevedo Feiten
Laboratory for Applied Biotechnology (LABA UFF), School of Dentistry Federal Fluminense University Niterói Brazil
4 shared publications - Jack Liborio Ferracane
Department of Oral Rehabilitation and Biosciences, Oregon Health & Science University, Portland, OR, USA
4 shared publications
Latest Publications
- Open Access
- 8 October 2026
- Published by Elsevier in JADA Foundational Science
- Vol. 5
Comparative accuracy and repeatability of digital devices for dental shade matching
- 8 October 2026
- Published by Elsevier in JADA Foundational Science
- Vol. 5
Open AccessComparative accuracy and repeatability of digital devices for dental shade matching
- Open Access
- 7 October 2026
- Published by Elsevier in JADA Foundational Science
- Vol. 5
Optical properties of resin composites with different opacity levels
- 7 October 2026
- Published by Elsevier in JADA Foundational Science
- Vol. 5
Open AccessOptical properties of resin composites with different opacity levels
- Open Access
- 10 August 2026
- Published by Wiley in European Journal of Oral Sciences
- p. e70125
Optimizing diphenyl(2,4,6‐trimethylbenzoyl)phosphine oxide concentration and post‐curing time to balance mechanical properties and color stability in a three‐dimensional‐printed restorative resin
Three‐dimensional (3D) printing is widely used in dental restorations; however, optimization of photoinitiator concentration and post‐curing protocols remains critical to achieve a balance between mechanical and esthetic performance. This study evaluated the combined effect of diphenyl(2,4,6‐trimethylbenzoyl)phosphine oxide (TPO) concentration and post‐curing time on mechanical properties and color stability of a 3D‐printed restorative resin. A commercial photoinitiator‐free resin (BioPrint Prov, Horus 3D) was supplemented with TPO at 0.5, 1.0, and 1.5 wt% and fabricated using a digital light processing printer. Specimens were post‐cured for 30, 45, or 60 min under UV light, while non‐post‐cured (NoPC) samples served as controls. Flexural strength and elastic modulus were evaluated using a three‐point bending test. Color stability and translucency were assessed using spectrophotometry (CIELab/Δ E 00 ) under storage conditions, including dry storage, water immersion, and coffee aging. Data were analyzed using two‐way anova and Tukey's test. The 1.0% TPO and 30 min post‐curing combination provided best performance, with highest flexural strength and lowest color change after staining. Higher TPO concentration and prolonged post‐curing increased color alteration and yellowness. NoPC specimens showed inferior mechanical properties and greater discoloration. Translucency remained more stable in post‐curing groups. These findings indicate optimized photoinitiator concentration and controlled post‐curing time improve mechanical and esthetic outcomes in 3D‐printed restorative resins.
- 10 August 2026
- Published by Wiley in European Journal of Oral Sciences
- p. e70125
Open AccessOptimizing diphenyl(2,4,6‐trimethylbenzoyl)phosphine oxide concentration and post‐curing time to balance mechanical properties and color stability in a three‐dimensional‐printed restorative resin
Three‐dimensional (3D) printing is widely used in dental restorations; however, optimization of photoinitiator concentration and post‐curing protocols remains critical to achieve a balance between mechanical and esthetic performance. This study evaluated the combined effect of diphenyl(2,4,6‐trimethylbenzoyl)phosphine oxide (TPO) concentration and post‐curing time on mechanical properties and color stability of a 3D‐printed restorative resin. A commercial photoinitiator‐free resin (BioPrint Prov, Horus 3D) was supplemented with TPO at 0.5, 1.0, and 1.5 wt% and fabricated using a digital light processing printer. Specimens were post‐cured for 30, 45, or 60 min under UV light, while non‐post‐cured (NoPC) samples served as controls. Flexural strength and elastic modulus were evaluated using a three‐point bending test. Color stability and translucency were assessed using spectrophotometry (CIELab/Δ E 00 ) under storage conditions, including dry storage, water immersion, and coffee aging. Data were analyzed using two‐way anova and Tukey's test. The 1.0% TPO and 30 min post‐curing combination provided best performance, with highest flexural strength and lowest color change after staining. Higher TPO concentration and prolonged post‐curing increased color alteration and yellowness. NoPC specimens showed inferior mechanical properties and greater discoloration. Translucency remained more stable in post‐curing groups. These findings indicate optimized photoinitiator concentration and controlled post‐curing time improve mechanical and esthetic outcomes in 3D‐printed restorative resins.
- Open Access
- 14 May 2026
- Published by Wiley in European Journal of Oral Sciences
- p. e70106
The influence of post‐curing protocols on the optical properties of provisional and long‐term 3D‐printable resin composites
This study determined the influence of post‐curing protocols on the color stability of provisional and long‐term 3D‐printable resin composites. Disc‐shaped specimens were fabricated from a provisional (Prov) and long‐term (Crown) 3D‐printable resin composites using a digital light processing printer. Post‐curing protocols included exposure to 405 nm‐based light sources (Anycubic for 30 or 60 min in the standard mode or Procure 1) and one 385 nm‐based light source (Procure 2 with distinct protocols). Color parameters ( L *, a *, b *) were measured at baseline, after 14 and 21 d of dry storage, and after 7 d of water immersion. Post‐curing protocol, material, and storage condition significantly influenced color stability. High‐irradiance protocols resulted in the highest color change values, exceeding the clinical acceptability threshold (Δ E 00 > 1.8). Water immersion induced a significant whitening effect and increased total color change in all groups. The long‐term resin demonstrated superior color stability compared to the provisional one across all post‐curing protocols. The choice of post‐curing protocol is critical for aesthetic performance, as high‐irradiance parameters, while potentially beneficial for mechanical properties, can compromise chromatic stability, particularly in materials with low filler content.
- 14 May 2026
- Published by Wiley in European Journal of Oral Sciences
- p. e70106
Open AccessThe influence of post‐curing protocols on the optical properties of provisional and long‐term 3D‐printable resin composites
This study determined the influence of post‐curing protocols on the color stability of provisional and long‐term 3D‐printable resin composites. Disc‐shaped specimens were fabricated from a provisional (Prov) and long‐term (Crown) 3D‐printable resin composites using a digital light processing printer. Post‐curing protocols included exposure to 405 nm‐based light sources (Anycubic for 30 or 60 min in the standard mode or Procure 1) and one 385 nm‐based light source (Procure 2 with distinct protocols). Color parameters ( L *, a *, b *) were measured at baseline, after 14 and 21 d of dry storage, and after 7 d of water immersion. Post‐curing protocol, material, and storage condition significantly influenced color stability. High‐irradiance protocols resulted in the highest color change values, exceeding the clinical acceptability threshold (Δ E 00 > 1.8). Water immersion induced a significant whitening effect and increased total color change in all groups. The long‐term resin demonstrated superior color stability compared to the provisional one across all post‐curing protocols. The choice of post‐curing protocol is critical for aesthetic performance, as high‐irradiance parameters, while potentially beneficial for mechanical properties, can compromise chromatic stability, particularly in materials with low filler content.
- Open Access
- 7 May 2026
- Published by Wiley in Journal of Esthetic and Restorative Dentistry
- Vol. 38 (8) , 1598-1609
Reliability of Three Image‐Based Instrumental Color‐Measurement Methods
Objectives: To compare the precision of three clinically applicable, image‐based color assessment methods—smartphone imaging, a clinical colorimeter (Optishade), and a digital scanning device (Borea Cobra)—against a benchtop spectrophotometer for measuring CIELAB coordinates and CIEDE2000 (Δ E 00 ) color differences of composite resin shades. Materials and Methods: Three specimens from eight composite shades were measured using a benchtop spectrophotometer (reference) and the three test devices. Agreement for L*, a*, and b* was evaluated using linear regression and Bland–Altman analyses. Δ E 00 values relative to the reference and intershade Δ E 00 across shade pairs were analyzed using two‐way ANOVA and regression. Results: Optishade showed the closest agreement with the reference—with slopes near unity, high R 2 values—and the smallest biases and limits of agreement. Borea Cobra demonstrated good overall performance and strong agreement for a* and b*, though with greater data dispersion and device‐specific distortions in intershade differences. Smartphone measurements displayed systematic positive bias, lower slopes for chromatic axes, and wider limits of agreement, indicating reduced precision and compression of color differences. Conclusions: Optishade provided the most reliable quantitative measurements; Borea Cobra offered acceptable performance with specific limitations. Smartphone‐based imaging preserved shade ordering but was unsuitable for precise color quantification.
- 7 May 2026
- Published by Wiley in Journal of Esthetic and Restorative Dentistry
- Vol. 38 (8) , 1598-1609
Open AccessReliability of Three Image‐Based Instrumental Color‐Measurement Methods
Objectives: To compare the precision of three clinically applicable, image‐based color assessment methods—smartphone imaging, a clinical colorimeter (Optishade), and a digital scanning device (Borea Cobra)—against a benchtop spectrophotometer for measuring CIELAB coordinates and CIEDE2000 (Δ E 00 ) color differences of composite resin shades. Materials and Methods: Three specimens from eight composite shades were measured using a benchtop spectrophotometer (reference) and the three test devices. Agreement for L*, a*, and b* was evaluated using linear regression and Bland–Altman analyses. Δ E 00 values relative to the reference and intershade Δ E 00 across shade pairs were analyzed using two‐way ANOVA and regression. Results: Optishade showed the closest agreement with the reference—with slopes near unity, high R 2 values—and the smallest biases and limits of agreement. Borea Cobra demonstrated good overall performance and strong agreement for a* and b*, though with greater data dispersion and device‐specific distortions in intershade differences. Smartphone measurements displayed systematic positive bias, lower slopes for chromatic axes, and wider limits of agreement, indicating reduced precision and compression of color differences. Conclusions: Optishade provided the most reliable quantitative measurements; Borea Cobra offered acceptable performance with specific limitations. Smartphone‐based imaging preserved shade ordering but was unsuitable for precise color quantification.
- Open Access
- 5 May 2026
- Published by Elsevier in Dental Materials
- Vol. 42 (10) , 1730-1736
Instrumental and visual assessment of color changes in 3D‑printed denture tooth resins
- 5 May 2026
- Published by Elsevier in Dental Materials
- Vol. 42 (10) , 1730-1736
Open AccessInstrumental and visual assessment of color changes in 3D‑printed denture tooth resins
- Open Access
- 1 January 2026
- Published by FapUNIFESP (SciELO) in Brazilian Oral Research
- Vol. 40
In vitro analysis of dimensional stability of fast-setting irreversible hydrocolloids by digital scanning
This study aimed to evaluate the in vitro dimensional stability of Moldeer Fast compared with two commercially available extended-pour, fast-setting irreversible hydrocolloids using direct digital scanning of dental impressions. This experimental in vitro study was conducted using standardized impression techniques on a typodont. Impressions were obtained in random order by a single calibrated operator. Three irreversible hydrocolloids were evaluated: ColorChange (Cavex Holland BV), Hydrogum 5 (Zhermack Spa), and Moldeer Fast (DFL). Ten impressions were obtained per group according to the manufacturers’ instructions and scanned using an intraoral scanner at predetermined intervals (0 h, 24 h, 48 h, 72 h, 96 h, and 120 h). Impressions were stored under controlled temperature and humidity conditions. Four linear measurements were performed on color-masked images in a blind manner to assess dimensional changes over time: a) intercanine distance, b) intermolar distance, c) right canine-to-molar distance, and d) left canine-to-molar distance. Data were analyzed using repeated-measures ANOVA (α = 0.05). All materials exhibited minor dimensional changes, consisting predominantly of slight contraction. However, no statistically significant differences were observed over time (p > 0.05). Moldeer Fast therefore exhibited dimensional stability comparable to that of ColorChange and Hydrogum 5. All materials maintained clinically acceptable dimensional stability for up to five days, supporting their suitability for delayed digital scanning of irreversible hydrocolloid impressions.
- 1 January 2026
- Published by FapUNIFESP (SciELO) in Brazilian Oral Research
- Vol. 40
Open AccessIn vitro analysis of dimensional stability of fast-setting irreversible hydrocolloids by digital scanning
This study aimed to evaluate the in vitro dimensional stability of Moldeer Fast compared with two commercially available extended-pour, fast-setting irreversible hydrocolloids using direct digital scanning of dental impressions. This experimental in vitro study was conducted using standardized impression techniques on a typodont. Impressions were obtained in random order by a single calibrated operator. Three irreversible hydrocolloids were evaluated: ColorChange (Cavex Holland BV), Hydrogum 5 (Zhermack Spa), and Moldeer Fast (DFL). Ten impressions were obtained per group according to the manufacturers’ instructions and scanned using an intraoral scanner at predetermined intervals (0 h, 24 h, 48 h, 72 h, 96 h, and 120 h). Impressions were stored under controlled temperature and humidity conditions. Four linear measurements were performed on color-masked images in a blind manner to assess dimensional changes over time: a) intercanine distance, b) intermolar distance, c) right canine-to-molar distance, and d) left canine-to-molar distance. Data were analyzed using repeated-measures ANOVA (α = 0.05). All materials exhibited minor dimensional changes, consisting predominantly of slight contraction. However, no statistically significant differences were observed over time (p > 0.05). Moldeer Fast therefore exhibited dimensional stability comparable to that of ColorChange and Hydrogum 5. All materials maintained clinically acceptable dimensional stability for up to five days, supporting their suitability for delayed digital scanning of irreversible hydrocolloid impressions.
- 1 June 2025
- Published by VM Comunicações in ImplantNews Reabilitação Oral
- Vol. 10 (3)
Análise por elementos finitos 3D das tensões geradas sobre uma barra implantossuportada em prótese do tipo cantilever
Objetivos: avaliar, pela análise de elementos finitos tridimensionais, o comportamento do conjunto prótese/implante/componentes/osso. Material e métodos: Foram analisadas duas configurações distintas: uma com dois implantes e outra com três implantes na dissipação das tensões geradas por uma carga vertical de 500 N, aplicada sobre um cantiléver com extensão para mesial, na região de primeiro pré-molar inferior de uma barra implantossuportada. Resultados: Os implantes mesial e mediano absorveram predominantemente as tensões de compressão, enquanto o implante distal foi o mais submetido à tração; houve diminuição da intrusão do implante mesial, redução da compressão apical e menor risco de afrouxamento do seu parafuso; as tensões de tração no pilar e na face mesial do implante adjacente ao cantiléver foram atenuadas, diminuindo o risco de reabsorção óssea nessa região. Conclusão: O uso de três implantes em próteses do tipo cantiléver demonstrou benefícios significativos para a integridade do conjunto biomecânico, reduzindo a tendência de fratura e afrouxamento do parafuso distal. Palavras-chave: Prótese implantossuportada; Cantiléver; Implante dental; Biomecânica; Oclusão dentária.
- 1 June 2025
- Published by VM Comunicações in ImplantNews Reabilitação Oral
- Vol. 10 (3)
Análise por elementos finitos 3D das tensões geradas sobre uma barra implantossuportada em prótese do tipo cantilever
Objetivos: avaliar, pela análise de elementos finitos tridimensionais, o comportamento do conjunto prótese/implante/componentes/osso. Material e métodos: Foram analisadas duas configurações distintas: uma com dois implantes e outra com três implantes na dissipação das tensões geradas por uma carga vertical de 500 N, aplicada sobre um cantiléver com extensão para mesial, na região de primeiro pré-molar inferior de uma barra implantossuportada. Resultados: Os implantes mesial e mediano absorveram predominantemente as tensões de compressão, enquanto o implante distal foi o mais submetido à tração; houve diminuição da intrusão do implante mesial, redução da compressão apical e menor risco de afrouxamento do seu parafuso; as tensões de tração no pilar e na face mesial do implante adjacente ao cantiléver foram atenuadas, diminuindo o risco de reabsorção óssea nessa região. Conclusão: O uso de três implantes em próteses do tipo cantiléver demonstrou benefícios significativos para a integridade do conjunto biomecânico, reduzindo a tendência de fratura e afrouxamento do parafuso distal. Palavras-chave: Prótese implantossuportada; Cantiléver; Implante dental; Biomecânica; Oclusão dentária.
- 29 July 2024
- Published by Scifiniti Publishing in Biomaterials Connect
- Vol. 1 (1) , 1-10
Translucency and Polymerization Ability of Contemporary Resin Composites
Objective: The present study aimed to characterize the translucency and polymerization ability of commercially available contemporary resin composites. Methods: The resin composites considered in this study were Forma (Enamel, Body, and Dentin; Ultradent), Empress Direct (Enamel and Dentin; Ivoclar/Vivadent), Sirius-Z (Enamel and Dentin; DFL), and Orion (Enamel and Dentin; DFL). All photoactivation procedures were performed using the same light source (Valo Cordless, Ultradent, 20 s). The translucency parameter (TP) was determined with a benchtop spectrophotometer (X-Rite, SP60), and the degree of conversion (DC) as a function of thickness was assessed by Fourier transform infrared spectroscopy (FTIR) immediately after photoactivation and again after 1 h. The results were analyzed using analysis of variance (ANOVA) and Tukey’s tests. Pearson’s correlation tests were employed to investigate the relationship between opacity and polymerization ability. Results: Regarding TP, the values obtained among the enamel shades were similar, but a significant variation was observed in dentin shades (p = 0.0023). The degree of conversion (DC) was dependent on the material tested (p = 0.0021 for immediate evaluation and p = 0.0043 for readings taken after 1 h) and the analysis depth (p = 0.0002 for immediate evaluation and p = 0.0038 for readings taken after 1 h). However, the relationship between these two factors was dependent on the time of evaluation. Forma and Empress Direct resin composites exhibited lower polymerization potential for dentin shades. The relationship between opacity and polymerization potential was significant for the baseline evaluation but not significant when considering DC values taken after 1hour. In conclusion, regardless of the brand, enamel shades demonstrated similar TP and curing potential. Conversely, there was a large variation in these parameters for dentin shades. A delayed polymerization can offset slow initial polymerization depending on the resin composite.
- 29 July 2024
- Published by Scifiniti Publishing in Biomaterials Connect
- Vol. 1 (1) , 1-10
Translucency and Polymerization Ability of Contemporary Resin Composites
Objective: The present study aimed to characterize the translucency and polymerization ability of commercially available contemporary resin composites. Methods: The resin composites considered in this study were Forma (Enamel, Body, and Dentin; Ultradent), Empress Direct (Enamel and Dentin; Ivoclar/Vivadent), Sirius-Z (Enamel and Dentin; DFL), and Orion (Enamel and Dentin; DFL). All photoactivation procedures were performed using the same light source (Valo Cordless, Ultradent, 20 s). The translucency parameter (TP) was determined with a benchtop spectrophotometer (X-Rite, SP60), and the degree of conversion (DC) as a function of thickness was assessed by Fourier transform infrared spectroscopy (FTIR) immediately after photoactivation and again after 1 h. The results were analyzed using analysis of variance (ANOVA) and Tukey’s tests. Pearson’s correlation tests were employed to investigate the relationship between opacity and polymerization ability. Results: Regarding TP, the values obtained among the enamel shades were similar, but a significant variation was observed in dentin shades (p = 0.0023). The degree of conversion (DC) was dependent on the material tested (p = 0.0021 for immediate evaluation and p = 0.0043 for readings taken after 1 h) and the analysis depth (p = 0.0002 for immediate evaluation and p = 0.0038 for readings taken after 1 h). However, the relationship between these two factors was dependent on the time of evaluation. Forma and Empress Direct resin composites exhibited lower polymerization potential for dentin shades. The relationship between opacity and polymerization potential was significant for the baseline evaluation but not significant when considering DC values taken after 1hour. In conclusion, regardless of the brand, enamel shades demonstrated similar TP and curing potential. Conversely, there was a large variation in these parameters for dentin shades. A delayed polymerization can offset slow initial polymerization depending on the resin composite.
- Open Access
- 1 January 2024
- Published by FapUNIFESP (SciELO) in Brazilian Oral Research
- Vol. 38, e001
Cytotoxicity evaluation, antibacterial effect, and degree of conversion of QAM-containing adhesives
The aim of this study was to evaluate the influence of adding quaternary ammonium methacrylates (QAMs) to experimental adhesives by assessing the degree of conversion (DC), cytotoxicity against keratinocytes and fibroblasts, and antibacterial activity against biofilm formation. Two QAMs were added to an experimental adhesive: dimethylaminododecyl methacrylate bromododecane (DMADDM) or dimethylaminododecyl methacrylate bromohexadecane (DMAHDM) at three concentrations each: 1, 2.5, and 5 wt.%. Experimental adhesive without QAMs (control group) and commercially available Transbond XT Primer (3M Unitek, Monrovia, California, USA) were used for comparisons. The adhesives were tested for DC, cytotoxicity against keratinocytes and fibroblasts, and antibacterial activity against biofilm formation. DC, cytotoxicity against fibroblasts, and antibacterial activity were analyzed using one-way ANOVA and Tukey’s multiple comparisons. Cytotoxicity against keratinocytes was evaluated using the Kruskal Wallis and Dunn’s post-hoc (α = 5%) tests. Transbond showed lower DC as compared to 5% DMAHDM, 1% DMADDM, and 5% DMADDM (p < 0.05). However, all groups presented proper DC when compared to commercial adhesives in the literature. In the evaluation of cytotoxicity against keratinocytes, Transbond induced higher viability than 2.5 wt.% groups (p < 0.05). Against fibroblasts, Transbond induced higher viability as compared to 5 wt.% groups (p < 0.05). DMAHDM at 5 wt.% reduced biofilm formation when compared to all the other groups (p < 0.05). Despite their cytotoxic effect against keratinocytes, gingival fibroblasts showed higher viability. DMAHDM at 5 wt.% decreased Streptococcus mutans viability. The incorporation of DMAHDM at 5 wt.% may be a strategy for reducing the development of white spot lesions.
- 1 January 2024
- Published by FapUNIFESP (SciELO) in Brazilian Oral Research
- Vol. 38, e001
Open AccessCytotoxicity evaluation, antibacterial effect, and degree of conversion of QAM-containing adhesives
The aim of this study was to evaluate the influence of adding quaternary ammonium methacrylates (QAMs) to experimental adhesives by assessing the degree of conversion (DC), cytotoxicity against keratinocytes and fibroblasts, and antibacterial activity against biofilm formation. Two QAMs were added to an experimental adhesive: dimethylaminododecyl methacrylate bromododecane (DMADDM) or dimethylaminododecyl methacrylate bromohexadecane (DMAHDM) at three concentrations each: 1, 2.5, and 5 wt.%. Experimental adhesive without QAMs (control group) and commercially available Transbond XT Primer (3M Unitek, Monrovia, California, USA) were used for comparisons. The adhesives were tested for DC, cytotoxicity against keratinocytes and fibroblasts, and antibacterial activity against biofilm formation. DC, cytotoxicity against fibroblasts, and antibacterial activity were analyzed using one-way ANOVA and Tukey’s multiple comparisons. Cytotoxicity against keratinocytes was evaluated using the Kruskal Wallis and Dunn’s post-hoc (α = 5%) tests. Transbond showed lower DC as compared to 5% DMAHDM, 1% DMADDM, and 5% DMADDM (p < 0.05). However, all groups presented proper DC when compared to commercial adhesives in the literature. In the evaluation of cytotoxicity against keratinocytes, Transbond induced higher viability than 2.5 wt.% groups (p < 0.05). Against fibroblasts, Transbond induced higher viability as compared to 5 wt.% groups (p < 0.05). DMAHDM at 5 wt.% reduced biofilm formation when compared to all the other groups (p < 0.05). Despite their cytotoxic effect against keratinocytes, gingival fibroblasts showed higher viability. DMAHDM at 5 wt.% decreased Streptococcus mutans viability. The incorporation of DMAHDM at 5 wt.% may be a strategy for reducing the development of white spot lesions.