Abstract
To better understand hydrogen (H) trapping kinetics at the nanoscale, we recently introduced an approach consisting of in situ H implantation inside an atom probe analysis chamber operated at cryogenic temperature. This method enables implantation of H2+ ions with energies up to 1 keV, allowing H to penetrate approximately 10 nm beneath the surface of an atom probe tomography (APT) specimen. Here, we investigate the expansion of APT samples following H implantation in two metallic systems: nickel (Ni) and titanium (Ti). In Ni, a significant expansion of ≈10–15% was observed by comparing transmission electron microscopy images acquired before and after implantation. In Ti, expansion could not be directly imaged due to specimen degradation caused by room-temperature transfer; however, APT analyses revealed a substantial shift in evaporation voltage (10–40%), consistent with pronounced Ti tip volume expansion.Keywords
This publication has 29 references indexed in Scilit:
- Hydrogen trapping and desorption of dual precipitates in tempered low-carbon martensitic steelActa Materialia, 2020
- Hydrogen embrittlement in different materials: A reviewInternational Journal of Hydrogen Energy, 2018
- Understanding and mitigating hydrogen embrittlement of steels: a review of experimental, modelling and design progress from atomistic to continuumJournal of Materials Science, 2018
- Hydrogen in Metals2014
- Atom Probe Microscopy2012
- The H−Ni (Hydrogen-Nickel) systemBulletin of Alloy Phase Diagrams, 1989
- Storing energy in metal hydrides: a review of the physical metallurgyJournal of Materials Science, 1983
- On the heats of formation of the binary hydrides of transition metalsJournal of the Less Common Metals, 1980
- A classification of hydrogen traps in steelMetallurgical Transactions A, 1979
- Lattice strains due to hydrogen in metals1978