Effects of Solder Powder Particle Size and Substrate Surface Finish on Degradation Properties of Solder Joints
Open Access
- 30 June 2022
- journal article
- research article
- Published by The Korean Welding and Joining Society in Journal of Welding and Joining
- Vol. 40 (3) , 207-214
Abstract
In this study, the degradation characteristics of solder joints composed of powder-size Sn-3.0Ag-0.5Cu and the substrate surface finish are compared. Reflow is performed at a N2 ambient to apply an organic solderability preservative (OSP), electroless nickel/immersion gold (ENIG) substrates, and solder pastes of Type 6 (5-15 ㎛) and Type 7 (2-11 ㎛). Subsequently, a thermal shock test (TST) is performed for 1,500 cycles at a temperature of -40 ℃ to 125 ℃ (dwell time of 10 min) to analyze the deterioration characteristics. After N2 reflow is performed, the void content of the OSP substrate/solder joints is higher than that of the ENIG substrate/solder joints, and the shear strength of the ENIG substrate/solder joints is higher than that of the OSP substrate/solder joints. After 500 TST cycles, the shear strength at the OSP substrate/Type 7 solder joints does not decrease, whereas the shear strength at the ENIG substrate/Type 7 solder joints decreases by approximately 25%. Cross-sectional analysis shows that Cu6Sn5 and (Ni,Cu)3Sn4 intermetallic compounds (IMCs) emerged in the OSP and ENIG interfaces, respectively. The increasing rate of IMC thickness at the Type 7 solder joints is higher than that at the Type 6 solder joints. Fracture analysis shows that the OSP and ENIG joints fractured in the solder and solder/IMC interfaces, respectively. The IMC of the OSP and ENIG joints exhibit scallop and needle shapes, respectively. The ENIG joints fractured at the solder/IMC interface because of a stress concentration in the needle-type IMC. After 1500 TST cycles, the shear strength of all samples decreases by more than 50%. Cross-sectional analysis shows a crack at the solder joints of all samples after 1,000 cycles. The decrease in shear strength is caused by these cracks.Keywords
Funding Information
- Ministry of Trade, Industry and Energy (20017409, 20017419)
This publication has 9 references indexed in Scilit:
- Optimization of FC-CSP and MLCC Soldering Process Using Type 7 Solder PasteJournal of Welding and Joining, 2022
- MLCC Solder Joint Property with Vacuum and Hot Air Reflow Soldering ProcessesJournal of Welding and Joining, 2021
- Flip Chip - Chip Scale Package Bonding Technology with Type 7 Solder Paste PrintingJournal of Welding and Joining, 2021
- Fine Pitch Solder Paste (T7) for System in Package (SiP) Applications2018
- Performance of Fine and Ultra-Fine Lead-Free Powders for Solder Paste Applications2018
- Influence of nanoparticle addition on the formation and growth of intermetallic compounds (IMCs) in Cu/Sn–Ag–Cu/Cu solder joint during different thermal conditionsScience and Technology of Advanced Materials, 2015
- Degradation Behavior of Solder Joint and Implementation Technology for Lead-free Automotive ElectronicsJournal of Welding and Joining, 2013
- Effects of fine size lead-free solder ball on the interfacial reactions and joint reliability2010
- A comparative study of ENIG and Cu OSP surface finishes on the mechanical reliability of Sn-3.0Ag-0.5Cu and Sn-36.8Pb-0.4Ag Solders2006