S. N. Maiti
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
S. N. Maiti has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
Kamini Sewda
Center for Polymer Science and Engineering, Indian Institute of Technology, New Delhi 110016, India
6 shared publicationsA. K. Gupta
Centre for Polymer Science and Engineering , Indian Institute of Technology , New Delhi, India
5 shared publicationsMohd. Nordin Ibrahim
Department of Process and Food Engineering, University Putra Malaysia, Serdang, Selangor, Malaysia
2 shared publicationsVinita Dubey
Defence Research & Development Establishment, Jhansi Road, Gwalior (MP)‐474 002, India
2 shared publications- A. K. Gupta
Centre for Polymer Science and Engineering, Indian Institute of Technology Delhi, New Delhi 110016, India
1 shared publication A. K. Jain
Centre for Materials Science and Technology, Indian Institute of Technology, New Delhi‐110 016, India
1 shared publication
Latest Publications
- 23 August 2011
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 123 (4) , 2122-2130
Effect of bark flour on melt rheological behavior of high density polyethylene
The melt rheological behavior of neem bark flour (BF) filled high density polyethylene (HDPE) has been studied at varying volume fraction (ϕf) from 0 to 0.26 at 180, 190, and 200°C in the shear rate range from 100 to 5000 s−1 using extruded pellets of the composites. The melt viscosity of HDPE increases with ϕf because the BF particles obstruct the flow of HDPE. With the incorporation of the coupling agent HDPE‐g‐MAH, the viscosity decreased compared to the corresponding compositions in the HDPE/BF systems due to a plasticizing/lubricating effect by HDPE‐g‐MAH. The composites obeyed power law behavior in the melt flow. The power law index decreases with increase in the filler content and increases with temperature for the corresponding systems while the consistency index showed the opposite trend. The activation energy for viscous flow exhibited inappreciable change with either ϕf or inclusion of the coupling agent, however, the pre‐exponential factor increased with filler concentration. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2012
- 23 August 2011
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 123 (4) , 2122-2130
Effect of bark flour on melt rheological behavior of high density polyethylene
The melt rheological behavior of neem bark flour (BF) filled high density polyethylene (HDPE) has been studied at varying volume fraction (ϕf) from 0 to 0.26 at 180, 190, and 200°C in the shear rate range from 100 to 5000 s−1 using extruded pellets of the composites. The melt viscosity of HDPE increases with ϕf because the BF particles obstruct the flow of HDPE. With the incorporation of the coupling agent HDPE‐g‐MAH, the viscosity decreased compared to the corresponding compositions in the HDPE/BF systems due to a plasticizing/lubricating effect by HDPE‐g‐MAH. The composites obeyed power law behavior in the melt flow. The power law index decreases with increase in the filler content and increases with temperature for the corresponding systems while the consistency index showed the opposite trend. The activation energy for viscous flow exhibited inappreciable change with either ϕf or inclusion of the coupling agent, however, the pre‐exponential factor increased with filler concentration. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2012
- 27 October 2010
- Published by SAGE Publications in Journal of Composite Materials
- Vol. 45 (9) , 1007-1016
Effect of bark flour on viscoelastic behavior of high density polyethylene
The dynamic mechanical behavior of high density polyethylene (HDPE) in HDPE/bark flour (BF) composites on varying the volume fraction (Φf) of BF (filler) from 0 to 0.26 has been studied. The storage modulus decreases with increase in BF content up to Φf = 0.07, which is attributed to a pseudolubricating effect by the filler. The storage modulus for the composites at Φ f = 0.20 is higher than HDPE in all other temperature zones due to enhanced mechanical restraint by the dispersed phase. At Φf = 0.07, the loss moduli were either marginally lower or similar to that of HDPE, which is due to the ball-bearing effect of the filler as well as decrease in the crystallinity of HDPE. Above Φf = 0.07, the loss moduli were higher than HDPE. The α-relaxation region of the damping peak shifted toward the higher temperature side with increase in BF content. In the presence of the coupling agent, maleic anhydride-grafted HDPE (HDPE-g-MAH), the storage modulus values were marginally lower than those of the HDPE/BF systems. In the HDPE/BF/HDPE—g—MAH composites, the variations of the loss moduli were similar but values lower than those of the HDPE/BF systems. Damping peak shift in the α-region toward higher temperature was more than those of the HDPE/BF systems, which may be due to the hindrance to the relaxation due to an enhanced phase interaction. The values of tan δ were higher than the rule of mixture for both the composites.
- 27 October 2010
- Published by SAGE Publications in Journal of Composite Materials
- Vol. 45 (9) , 1007-1016
Effect of bark flour on viscoelastic behavior of high density polyethylene
The dynamic mechanical behavior of high density polyethylene (HDPE) in HDPE/bark flour (BF) composites on varying the volume fraction (Φf) of BF (filler) from 0 to 0.26 has been studied. The storage modulus decreases with increase in BF content up to Φf = 0.07, which is attributed to a pseudolubricating effect by the filler. The storage modulus for the composites at Φ f = 0.20 is higher than HDPE in all other temperature zones due to enhanced mechanical restraint by the dispersed phase. At Φf = 0.07, the loss moduli were either marginally lower or similar to that of HDPE, which is due to the ball-bearing effect of the filler as well as decrease in the crystallinity of HDPE. Above Φf = 0.07, the loss moduli were higher than HDPE. The α-relaxation region of the damping peak shifted toward the higher temperature side with increase in BF content. In the presence of the coupling agent, maleic anhydride-grafted HDPE (HDPE-g-MAH), the storage modulus values were marginally lower than those of the HDPE/BF systems. In the HDPE/BF/HDPE—g—MAH composites, the variations of the loss moduli were similar but values lower than those of the HDPE/BF systems. Damping peak shift in the α-region toward higher temperature was more than those of the HDPE/BF systems, which may be due to the hindrance to the relaxation due to an enhanced phase interaction. The values of tan δ were higher than the rule of mixture for both the composites.
- 4 August 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 118 (4) , 2264-2275
Crystallization and melting behavior of HDPE in HDPE/teak wood flour composites and their correlation with mechanical properties
The nonisothermal crystallization behavior and melting characteristics of high‐density polyethylene (HDPE) in HDPE/teak wood flour (TWF) composites have been studied by differential scanning calorimetry (DSC) and wide angle X‐ray diffraction (WAXD) methods. Composite formulations of HDPE/TWF were prepared by varying the volume fraction (ϕf) of TWF (filler) from 0 to 0.32. Various crystallization parameters evaluated from the DSC exotherms were used to study the nonisothermal crystallization behavior. The melting temperature (Tm) and crystallization temperature (Tp) of the composites were slightly higher than those of the neat HDPE. The enthalpy of melting and crystallization (%) decrease with increase in the filler content. Because the nonpolar polymer HDPE and polar TWF are incompatible, to enhance the phase interaction maleic anhydride grafted HDPE (HDPE‐g‐MAH) was used as a coupling agent. A shift in the crystallization and melting peak temperatures toward the higher temperature side and broadening of the crystallization peak (increased crystallite size distribution) were observed whereas crystallinity of HDPE declines with increase in ϕf in both DSC and WAXD. Linear correlations were obtained between crystallization parameters and tensile and impact strength. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010
- 4 August 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 118 (4) , 2264-2275
Crystallization and melting behavior of HDPE in HDPE/teak wood flour composites and their correlation with mechanical properties
The nonisothermal crystallization behavior and melting characteristics of high‐density polyethylene (HDPE) in HDPE/teak wood flour (TWF) composites have been studied by differential scanning calorimetry (DSC) and wide angle X‐ray diffraction (WAXD) methods. Composite formulations of HDPE/TWF were prepared by varying the volume fraction (ϕf) of TWF (filler) from 0 to 0.32. Various crystallization parameters evaluated from the DSC exotherms were used to study the nonisothermal crystallization behavior. The melting temperature (Tm) and crystallization temperature (Tp) of the composites were slightly higher than those of the neat HDPE. The enthalpy of melting and crystallization (%) decrease with increase in the filler content. Because the nonpolar polymer HDPE and polar TWF are incompatible, to enhance the phase interaction maleic anhydride grafted HDPE (HDPE‐g‐MAH) was used as a coupling agent. A shift in the crystallization and melting peak temperatures toward the higher temperature side and broadening of the crystallization peak (increased crystallite size distribution) were observed whereas crystallinity of HDPE declines with increase in ϕf in both DSC and WAXD. Linear correlations were obtained between crystallization parameters and tensile and impact strength. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010
- 22 March 2010
- Published by Taylor & Francis in Polymer-Plastics Technology and Engineering
- Vol. 49 (4) , 418-425
Effect of Teak Wood Flour on Melt Rheological Behaviour of High Density Polyethylene
The melt rheological studies on HDPE/TWF (teak wood flour) composites were studied at (volume fraction) Φf = 0.00−0.32 and at 180°C, 190°C and 200°C. Viscosity of HDPE/TWF composites increases with Φf while decreases with increase in temperature. Addition of coupling agent, maleic anhydride grafted HDPE (HDPE-g-MAH) enhances viscosity as compared to the corresponding HDPE/TWF. This was attributed to increase in interaction between TWF and HDPE by HDPE-g-MAH which in turn stiffens the system. The power law coefficient, n, decreases with increase in Φf and increase in temperature and lower for HDPE/TWF/HDPE-g-MAH composites as compared to HDPE/TWF composites. The consistency index increases with increase in Φf and were higher for HDPE/TWF/HDPE-g-MAH.
- 22 March 2010
- Published by Taylor & Francis in Polymer-Plastics Technology and Engineering
- Vol. 49 (4) , 418-425
Effect of Teak Wood Flour on Melt Rheological Behaviour of High Density Polyethylene
The melt rheological studies on HDPE/TWF (teak wood flour) composites were studied at (volume fraction) Φf = 0.00−0.32 and at 180°C, 190°C and 200°C. Viscosity of HDPE/TWF composites increases with Φf while decreases with increase in temperature. Addition of coupling agent, maleic anhydride grafted HDPE (HDPE-g-MAH) enhances viscosity as compared to the corresponding HDPE/TWF. This was attributed to increase in interaction between TWF and HDPE by HDPE-g-MAH which in turn stiffens the system. The power law coefficient, n, decreases with increase in Φf and increase in temperature and lower for HDPE/TWF/HDPE-g-MAH composites as compared to HDPE/TWF composites. The consistency index increases with increase in Φf and were higher for HDPE/TWF/HDPE-g-MAH.
- 4 June 2009
- Published by Taylor & Francis in Polymer-Plastics Technology and Engineering
- Vol. 48 (7) , 775-780
Crystallization of Polypropylene in PP/PDMS/Nano-SiO2Ternary Composite
Effect of dispersion morphology, resulting from different mixing sequences used in making ternary composite polypropylene (PP)/poly(dimethylsiloxane) (PDMS)/nano SiO2, on the crystallization of PP phase is studied. Mixing sequence is found to have significant effect on the dispersion morphology of the ternary composite, which in turn affected the crystallization of the PP matrix of the ternary composite. Crystallization behaviour of PP, studied by the differential scanning calorimetry, is discussed for the effect of different dispersion morphologies on overall crystallization process rate, nucleation rate, crystal size distribution and crystallinity.
- 4 June 2009
- Published by Taylor & Francis in Polymer-Plastics Technology and Engineering
- Vol. 48 (7) , 775-780
Crystallization of Polypropylene in PP/PDMS/Nano-SiO2Ternary Composite
Effect of dispersion morphology, resulting from different mixing sequences used in making ternary composite polypropylene (PP)/poly(dimethylsiloxane) (PDMS)/nano SiO2, on the crystallization of PP phase is studied. Mixing sequence is found to have significant effect on the dispersion morphology of the ternary composite, which in turn affected the crystallization of the PP matrix of the ternary composite. Crystallization behaviour of PP, studied by the differential scanning calorimetry, is discussed for the effect of different dispersion morphologies on overall crystallization process rate, nucleation rate, crystal size distribution and crystallinity.
- 11 February 2009
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 112 (3) , 1826-1834
Mechanical properties of teak wood flour‐reinforced HDPE composites
Mechanical properties such as tensile and impact strength behavior of teak wood flour (TWF)‐filled high‐density polyethylene (HDPE) composites were evaluated at 0–0.32 volume fraction (Φf) of TWF. Tensile modulus and strength initially increased up to Φf = 0.09, whereas a decrease is observed with further increase in the Φf. Elongation‐at‐break and Izod impact strength decreased significantly with increase in the Φf. The crystallinity of HDPE also decreased with increase in the TWF concentration. The initial increase in the tensile modulus and strength was attributed to the mechanical restraint, whereas decrease in the tensile properties at Φf > 0.09 was due to the predominant effect of decrease in the crystallinity of HDPE. The mechanical restraint decreased the elongation and Izod impact strength. In the presence of coupling agent, maleic anhydride‐grafted HDPE (HDPE‐g‐MAH), the tensile modulus and strength enhanced significantly because of enhanced interphase adhesion. However, the elongation and Izod impact strength decreased because of enhanced mechanical restraint on account of increased phase interactions. Scanning electron microscopy showed a degree of better dispersion of TWF particles because of enhanced phase adhesion in the presence of HDPE‐g‐MAH. © 2009 Wiley Periodicals, Inc. J Appl Polym Sci, 2009
- 11 February 2009
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 112 (3) , 1826-1834
Mechanical properties of teak wood flour‐reinforced HDPE composites
Mechanical properties such as tensile and impact strength behavior of teak wood flour (TWF)‐filled high‐density polyethylene (HDPE) composites were evaluated at 0–0.32 volume fraction (Φf) of TWF. Tensile modulus and strength initially increased up to Φf = 0.09, whereas a decrease is observed with further increase in the Φf. Elongation‐at‐break and Izod impact strength decreased significantly with increase in the Φf. The crystallinity of HDPE also decreased with increase in the TWF concentration. The initial increase in the tensile modulus and strength was attributed to the mechanical restraint, whereas decrease in the tensile properties at Φf > 0.09 was due to the predominant effect of decrease in the crystallinity of HDPE. The mechanical restraint decreased the elongation and Izod impact strength. In the presence of coupling agent, maleic anhydride‐grafted HDPE (HDPE‐g‐MAH), the tensile modulus and strength enhanced significantly because of enhanced interphase adhesion. However, the elongation and Izod impact strength decreased because of enhanced mechanical restraint on account of increased phase interactions. Scanning electron microscopy showed a degree of better dispersion of TWF particles because of enhanced phase adhesion in the presence of HDPE‐g‐MAH. © 2009 Wiley Periodicals, Inc. J Appl Polym Sci, 2009
- 11 May 2007
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 105 (5) , 2598-2604
Mechanical properties of HDPE/bark flour composites
Tensile and impact properties of Neem bark flour (BF) containing high density polyethylene (HDPE) composites were studied at 0–0.26 volume fraction of filler. Tensile modulus and strength and breaking elongation decreased with increase in BF concentration. The decrease in tensile modulus and strength was attributed to the decrease in crystallinity of the polymer compared to the imposed mechanical restraint by the BF. Analysis of tensile strength data indicated formation of stress concentration in the interphase. Because of this stress concentration and the mechanical restraint, the elongation‐at‐break and Izod impact strength decreased. Use of a coupling agent, HDPE‐g‐MAH, brings about enhanced phase adhesion, increasing the tensile modulus and strength. Enhanced adhesion marginally lowers composite ductility at higher filler contents and aids stress transfer increasing the Izod impact strength inappreciably. Scanning electron microscopic studies indicated better dispersion of BF particles and enhanced interphase adhesion in presence of the coupling agent. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci, 2007
- 11 May 2007
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 105 (5) , 2598-2604
Mechanical properties of HDPE/bark flour composites
Tensile and impact properties of Neem bark flour (BF) containing high density polyethylene (HDPE) composites were studied at 0–0.26 volume fraction of filler. Tensile modulus and strength and breaking elongation decreased with increase in BF concentration. The decrease in tensile modulus and strength was attributed to the decrease in crystallinity of the polymer compared to the imposed mechanical restraint by the BF. Analysis of tensile strength data indicated formation of stress concentration in the interphase. Because of this stress concentration and the mechanical restraint, the elongation‐at‐break and Izod impact strength decreased. Use of a coupling agent, HDPE‐g‐MAH, brings about enhanced phase adhesion, increasing the tensile modulus and strength. Enhanced adhesion marginally lowers composite ductility at higher filler contents and aids stress transfer increasing the Izod impact strength inappreciably. Scanning electron microscopic studies indicated better dispersion of BF particles and enhanced interphase adhesion in presence of the coupling agent. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci, 2007
- 13 April 2005
- Published by Taylor & Francis in International Journal of Polymeric Materials and Polymeric Biomaterials
- Vol. 54 (6) , 527-539
Mechanical Properties of ABS/CSM Rubber Blends
Impact behavior and tensile properties of acrylonitrile butadiene styrene (ABS) terpolyer/Chlorsulfonated Polyethylene (CSM) blends are studied at CSM concentrations of 0 to 30.6 vol%. The data are presented as functions of CSM content. Predictive models have been employed to analyze the tensile properties. Impact behavior has been analyzed on the basis of interphase adhesion. Scanning electron microscopy (SEM) has been used to study the adhesion between the matrix and the elastomeric phase.
- 13 April 2005
- Published by Taylor & Francis in International Journal of Polymeric Materials and Polymeric Biomaterials
- Vol. 54 (6) , 527-539
Mechanical Properties of ABS/CSM Rubber Blends
Impact behavior and tensile properties of acrylonitrile butadiene styrene (ABS) terpolyer/Chlorsulfonated Polyethylene (CSM) blends are studied at CSM concentrations of 0 to 30.6 vol%. The data are presented as functions of CSM content. Predictive models have been employed to analyze the tensile properties. Impact behavior has been analyzed on the basis of interphase adhesion. Scanning electron microscopy (SEM) has been used to study the adhesion between the matrix and the elastomeric phase.
- 13 April 2005
- Published by Taylor & Francis in International Journal of Polymeric Materials and Polymeric Biomaterials
- Vol. 54 (6) , 467-482
Mechanical Properties of Impact i-PP/CSM Rubber Blends
The impact strength and the tensile behavior of an impact grade of isotactic polypropylene (impact i-pp)/chlorosulfonated polyethylene (CSM) rubber blends are studied at the CSM rubber concentrations 0 to 23.4 vol%. The impact strength, which increased with CSM rubber concentration, has been analyzed on the basis of the interphase adhesion and crazing mechanisms. Tensile modulus and strength decreased whereas breaking elongation increased with increase in CSM rubber content. Predictive models have been used to explain the tensile modulus and strength properties. Scanning electron microscopy has been employed to study the phase structure.
- 13 April 2005
- Published by Taylor & Francis in International Journal of Polymeric Materials and Polymeric Biomaterials
- Vol. 54 (6) , 467-482
Mechanical Properties of Impact i-PP/CSM Rubber Blends
The impact strength and the tensile behavior of an impact grade of isotactic polypropylene (impact i-pp)/chlorosulfonated polyethylene (CSM) rubber blends are studied at the CSM rubber concentrations 0 to 23.4 vol%. The impact strength, which increased with CSM rubber concentration, has been analyzed on the basis of the interphase adhesion and crazing mechanisms. Tensile modulus and strength decreased whereas breaking elongation increased with increase in CSM rubber content. Predictive models have been used to explain the tensile modulus and strength properties. Scanning electron microscopy has been employed to study the phase structure.
- 13 November 2003
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 91 (1) , 644-650
Effect of wood fibers on the rheological properties of i‐PP/wood fiber composites
The effects of wood fibers on the melt rheological behavior of isotactic poly(propylene) (i‐PP)/wood fiber (WF) composites have been studied at WF concentrations of 0–32.2 vol % at 493 K. Shear stress–shear rate variations obeyed a power law equation, and the composites exhibited shear thinning, which increased with filler content. At a low shear rate, the apparent melt viscosity increased, while melt elasticity, after an initial decrease, also increased with WF concentration. At a higher shear rate, after an initial decrease, the melt viscosity showed an increase, as did melt elasticity, with increase in filler content. A titanate coupling agent, LICA 38, used to modify the wood fiber surface, modified these rheological parameters by functioning as a plasticizer/lubricant. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 91: 644–650, 2004
- 13 November 2003
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 91 (1) , 644-650
Effect of wood fibers on the rheological properties of i‐PP/wood fiber composites
The effects of wood fibers on the melt rheological behavior of isotactic poly(propylene) (i‐PP)/wood fiber (WF) composites have been studied at WF concentrations of 0–32.2 vol % at 493 K. Shear stress–shear rate variations obeyed a power law equation, and the composites exhibited shear thinning, which increased with filler content. At a low shear rate, the apparent melt viscosity increased, while melt elasticity, after an initial decrease, also increased with WF concentration. At a higher shear rate, after an initial decrease, the melt viscosity showed an increase, as did melt elasticity, with increase in filler content. A titanate coupling agent, LICA 38, used to modify the wood fiber surface, modified these rheological parameters by functioning as a plasticizer/lubricant. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 91: 644–650, 2004