I. D. Kovalev
Merzhanov Institute of Structural Macrokinetics and Material Science, Russian Academy of Sciences
10 shared publicationsB. S. Seplyarskii
Merzhanov Institute of Structural Macrokinetics and Materials Science, Russian Academy of Sciences, Chernogolovka, Russia
9 shared publications- Dmitrii Yu. Kovalev
Merzhanov Institute of Structural Macrokinetics and Materials Science of the Russian Academy of Sciences
8 shared publications - Alexander S. Shchukin
Merzhanov Institute of Structural Macrokinetics and Materials Science Russian Academy of Sciences
7 shared publications - Alexander S. Rogachev
Merzhanov Institute of Structural Macrokinetics and Materials Science, Russian Academy of Sciences, Chernogolovka, Russia
6 shared publications - Evgeny Alexandrovich Levashov
National University of Science and Technology “MISIS
6 shared publications
Latest Publications
- 1 June 2026
- Published by Pleiades Publishing Ltd in Combustion, Explosion, and Shock Waves
- Vol. 62 (3) , 463-473
Influence of Component Ratio, Mechanical Activation, and Preclamping of Samples on Combustion in the (5Ti + 3Si) + (Ti + 2B) System
This paper examines the influence of component ratio, mechanical activation, and preclamping of samples on the combustion speed and elongation of unclamped samples during synthesis and the phase composition and morphology of combustion products in the (5Ti + 3Si) + (Ti + 2B) system. The combustion front did not reach the lower end face of the sample prepared from a 5Ti + 3Si starting mixture. Preclamping, mechanical activation of the 5Ti + 3Si mixture, or the addition of a Ti + 2B mixture enabled complete combustion of the sample. Mechanical activation of (100 – x)(5Ti + 3Si) + x(Ti + 2B) mixtures increased the elongation and combustion speed of the samples. The combustion speed was shown to have a tendency to decrease with increasing 5Ti + 3Si content. Preclamping increased the combustion speed of the samples prepared from the mechanically activated mixtures and had little or no effect on the combustion speed of the samples prepared from the starting mixtures (except for the Ti + 2B mixture). For some starting mixtures, preclamping led to shrinkage of the samples. The samples containing 20% 5Ti + 3Si mixture had the highest combustion speed. The elongation of the samples prepared from the (100 – x)(5Ti + 3Si) + x(Ti + 2B) starting mixtures was a nonmonotonic function of their composition, with extrema. Neither preclamping of the samples nor mechanical activation of the starting mixtures caused changes in the phase composition of the combustion products.
- 1 June 2026
- Published by Pleiades Publishing Ltd in Combustion, Explosion, and Shock Waves
- Vol. 62 (3) , 463-473
Influence of Component Ratio, Mechanical Activation, and Preclamping of Samples on Combustion in the (5Ti + 3Si) + (Ti + 2B) System
This paper examines the influence of component ratio, mechanical activation, and preclamping of samples on the combustion speed and elongation of unclamped samples during synthesis and the phase composition and morphology of combustion products in the (5Ti + 3Si) + (Ti + 2B) system. The combustion front did not reach the lower end face of the sample prepared from a 5Ti + 3Si starting mixture. Preclamping, mechanical activation of the 5Ti + 3Si mixture, or the addition of a Ti + 2B mixture enabled complete combustion of the sample. Mechanical activation of (100 – x)(5Ti + 3Si) + x(Ti + 2B) mixtures increased the elongation and combustion speed of the samples. The combustion speed was shown to have a tendency to decrease with increasing 5Ti + 3Si content. Preclamping increased the combustion speed of the samples prepared from the mechanically activated mixtures and had little or no effect on the combustion speed of the samples prepared from the starting mixtures (except for the Ti + 2B mixture). For some starting mixtures, preclamping led to shrinkage of the samples. The samples containing 20% 5Ti + 3Si mixture had the highest combustion speed. The elongation of the samples prepared from the (100 – x)(5Ti + 3Si) + x(Ti + 2B) starting mixtures was a nonmonotonic function of their composition, with extrema. Neither preclamping of the samples nor mechanical activation of the starting mixtures caused changes in the phase composition of the combustion products.
- 1 December 2025
- Published by Pleiades Publishing Ltd in Combustion, Explosion, and Shock Waves
- Vol. 61 (6) , 886-894
Effect of Fixed Sample Length Conditions and Mechanical Activation of the Starting Mixture on Combustion in the Ti + C System
This paper examines the effect of fixed sample length conditions and mechanical activation of the starting mixture on the combustion rate and sample elongation during the synthesis process and the phase composition and morphology of the combustion products in the Ti + C system. Milling for 9 min in air in an AGO-2 mill at an acceleration of 90g with 9-mm-diameter steel balls as grinding media led to partial mechanochemical synthesis: the resultant mixture contained TiC along with unreacted titanium and carbon. After ball milling for 9 min, the mixture became pyrophoric and occasionally ignited when withdrawn from the grinding vial. Mechanical activation for less than 9 min led to an increase in the combustion rate of the mixture and a decrease in particle size in comparison with the combustion rate and particle size of the starting mixture. Increasing the MA time from 1 to below 9 min caused an increase in the amount of impurity gas in the mixture, resulting in a larger sample elongation. Mechanical activation for a relatively long time led to disintegration of the sample during the combustion process. Keeping the sample length fixed led to a considerable increase in combustion rate, but had no effect on the phase composition of the synthesis products, as did mechanical activation of the starting mixture.
- 1 December 2025
- Published by Pleiades Publishing Ltd in Combustion, Explosion, and Shock Waves
- Vol. 61 (6) , 886-894
Effect of Fixed Sample Length Conditions and Mechanical Activation of the Starting Mixture on Combustion in the Ti + C System
This paper examines the effect of fixed sample length conditions and mechanical activation of the starting mixture on the combustion rate and sample elongation during the synthesis process and the phase composition and morphology of the combustion products in the Ti + C system. Milling for 9 min in air in an AGO-2 mill at an acceleration of 90g with 9-mm-diameter steel balls as grinding media led to partial mechanochemical synthesis: the resultant mixture contained TiC along with unreacted titanium and carbon. After ball milling for 9 min, the mixture became pyrophoric and occasionally ignited when withdrawn from the grinding vial. Mechanical activation for less than 9 min led to an increase in the combustion rate of the mixture and a decrease in particle size in comparison with the combustion rate and particle size of the starting mixture. Increasing the MA time from 1 to below 9 min caused an increase in the amount of impurity gas in the mixture, resulting in a larger sample elongation. Mechanical activation for a relatively long time led to disintegration of the sample during the combustion process. Keeping the sample length fixed led to a considerable increase in combustion rate, but had no effect on the phase composition of the synthesis products, as did mechanical activation of the starting mixture.
- 24 September 2025
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 16 (5) , 1505-1515
Synthesis of a Composite Material in Combustion Mode from a Mixture of Ti + 2B and Composite Ni–Al Particles with Different Ratios of Components
—To obtain a composite with interpenetrating intermetallic/ceramic phases (of type IPC, interpenetrating phase composites) by the self-propagating high-temperature synthesis (SHS) method, the Ni–Al–Ti–2B powder system was used. It consisted of mechanically activated composite particles-granules (Ni + Al) and a mixture of finely dispersed boron and titanium powder. The quantitative ratio between the granules and the Ti + 2B mixture was varied. For all compositions, the synthesis was carried out in the combustion mode without heating. In the combustion wave front, the chemical reactions occurred in the composite granules and in the mixture around the granules, between titanium and boron. As a result of combustion a porous framework of titanium diboride was formed; a melt of nickel aluminides penetrated into the pores of the framework. The metal–ceramic combustion product is characterized by developed porosity and a composite structure with diboride and intermetallic phases located like interpenetrating frameworks. The TiB2–NiAl structure depends on the ratio of components in the mixture. The pores formed in place of the granules, repeating their shape.
- 24 September 2025
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 16 (5) , 1505-1515
Synthesis of a Composite Material in Combustion Mode from a Mixture of Ti + 2B and Composite Ni–Al Particles with Different Ratios of Components
—To obtain a composite with interpenetrating intermetallic/ceramic phases (of type IPC, interpenetrating phase composites) by the self-propagating high-temperature synthesis (SHS) method, the Ni–Al–Ti–2B powder system was used. It consisted of mechanically activated composite particles-granules (Ni + Al) and a mixture of finely dispersed boron and titanium powder. The quantitative ratio between the granules and the Ti + 2B mixture was varied. For all compositions, the synthesis was carried out in the combustion mode without heating. In the combustion wave front, the chemical reactions occurred in the composite granules and in the mixture around the granules, between titanium and boron. As a result of combustion a porous framework of titanium diboride was formed; a melt of nickel aluminides penetrated into the pores of the framework. The metal–ceramic combustion product is characterized by developed porosity and a composite structure with diboride and intermetallic phases located like interpenetrating frameworks. The TiB2–NiAl structure depends on the ratio of components in the mixture. The pores formed in place of the granules, repeating their shape.
- 8 September 2024
- Published by The Russian Academy of Sciences in Химическая физика
- Vol. 43 (3) , 76-86
The Effect of Nickel Content and Mechanical Activation on Combustion in the 5Ti + 3Si + хNi System
Intermetallic alloys were synthesized in the 5Ti + 3Si + xNi system by the method of self-propagating high-temperature synthesis (SHS) and mechanosynthesis. The influence of nickel content on the morphology, size and yield of composite particles after mechanical activation (MA) of mixtures was studied. The dependences of the maximum temperatures and combustion rates, phase composition, morphology and elongation of synthesis products on the nickel content for the initial and MA mixtures are studied. Under the conditions of the experiments conducted in this work, combustion process was able to realize and at the same time the samples burned completely at a nickel content of 10 to 60 wt.% in the 5Ti + 3Si + xNi system. After MA, the samples from the 5Ti + 3Si mixture burned to the end, and during the activation of the 5Ti + 3Si + 40% Ni mixture, mechanochemical synthesis occurred. With increasing nickel content combustion temperature decreases, and combustion velocity behaves nonmonotonically, increases the size of composite particles and decreases the yield of the mixture after MA. MA practically did not affect the maximum combustion temperatures of mixtures of 5Ti + 3Si + xNi. A multiple (from 0.7 to 2.9 cm/s) increase in the burning rate of samples from MA mixtures with an increase in the Ni content from 20 to 30 wt. % was recorded. An increase in the nickel content leads to an increase in the content of triple phases and the amount of melt in the synthesis products of mixtures of 5Ti + 3Si + xNi. Shrinkage of product samples increases with increasing nickel content in the initial mixtures. After MA, the shrinkage of the product samples is replaced by their growth. Explanations of the observed dependencies are proposed.
- 8 September 2024
- Published by The Russian Academy of Sciences in Химическая физика
- Vol. 43 (3) , 76-86
The Effect of Nickel Content and Mechanical Activation on Combustion in the 5Ti + 3Si + хNi System
Intermetallic alloys were synthesized in the 5Ti + 3Si + xNi system by the method of self-propagating high-temperature synthesis (SHS) and mechanosynthesis. The influence of nickel content on the morphology, size and yield of composite particles after mechanical activation (MA) of mixtures was studied. The dependences of the maximum temperatures and combustion rates, phase composition, morphology and elongation of synthesis products on the nickel content for the initial and MA mixtures are studied. Under the conditions of the experiments conducted in this work, combustion process was able to realize and at the same time the samples burned completely at a nickel content of 10 to 60 wt.% in the 5Ti + 3Si + xNi system. After MA, the samples from the 5Ti + 3Si mixture burned to the end, and during the activation of the 5Ti + 3Si + 40% Ni mixture, mechanochemical synthesis occurred. With increasing nickel content combustion temperature decreases, and combustion velocity behaves nonmonotonically, increases the size of composite particles and decreases the yield of the mixture after MA. MA practically did not affect the maximum combustion temperatures of mixtures of 5Ti + 3Si + xNi. A multiple (from 0.7 to 2.9 cm/s) increase in the burning rate of samples from MA mixtures with an increase in the Ni content from 20 to 30 wt. % was recorded. An increase in the nickel content leads to an increase in the content of triple phases and the amount of melt in the synthesis products of mixtures of 5Ti + 3Si + xNi. Shrinkage of product samples increases with increasing nickel content in the initial mixtures. After MA, the shrinkage of the product samples is replaced by their growth. Explanations of the observed dependencies are proposed.
- 1 August 2024
- Published by Pleiades Publishing Ltd in Combustion, Explosion, and Shock Waves
- Vol. 60 (4) , 543-550
Effect of Fe–Co–Cr Content and Mechanical Activation on Ni–Al–(Fe–Co–Cr) Combustion
This paper describes the study of the effect of mechanical activation and amount of a Fe + Co + Cr binder on burning rate, maximum temperature, sample elongation during combustion, composite particle size after activation, mixture yield after activation, and phase composition and morphology of synthesis products in a Ni–Al–(Fe–Co–Cr) mixture. Mechanical activation of a Ni + Al + \(x\)(Fe + Co + Cr) mixture allows for samples to burn at room temperature with a Fe + Co + Cr binder content of up to 40%. Activating the mixtures increases burning rate, combustion temperature, sample elongation, and sample porosity; however, the sample strength decreases. An increase in the Fe + Co + Cr binder content in the activated Ni + Al + \(x\)(Fe + Co + Cr) mixture makes the mixture yield after mechanical activation greater, reduces the composite particle size, and elongates the synthesis product samples. The burning rate of activated mixtures nonmonotonically depends on the Fe + Co + Cr binder content and has a maximum at a binder content of 10%. High-entropy alloys, which are solid solutions based on NiAl and Ni3Al intermetallic compounds, are synthesized using self-propagation high-temperature synthesis.- 1 August 2024
- Published by Pleiades Publishing Ltd in Combustion, Explosion, and Shock Waves
- Vol. 60 (4) , 543-550
Effect of Fe–Co–Cr Content and Mechanical Activation on Ni–Al–(Fe–Co–Cr) Combustion
This paper describes the study of the effect of mechanical activation and amount of a Fe + Co + Cr binder on burning rate, maximum temperature, sample elongation during combustion, composite particle size after activation, mixture yield after activation, and phase composition and morphology of synthesis products in a Ni–Al–(Fe–Co–Cr) mixture. Mechanical activation of a Ni + Al + \(x\)(Fe + Co + Cr) mixture allows for samples to burn at room temperature with a Fe + Co + Cr binder content of up to 40%. Activating the mixtures increases burning rate, combustion temperature, sample elongation, and sample porosity; however, the sample strength decreases. An increase in the Fe + Co + Cr binder content in the activated Ni + Al + \(x\)(Fe + Co + Cr) mixture makes the mixture yield after mechanical activation greater, reduces the composite particle size, and elongates the synthesis product samples. The burning rate of activated mixtures nonmonotonically depends on the Fe + Co + Cr binder content and has a maximum at a binder content of 10%. High-entropy alloys, which are solid solutions based on NiAl and Ni3Al intermetallic compounds, are synthesized using self-propagation high-temperature synthesis.- 15 April 2024
- Published by The Russian Academy of Sciences in Химическая физика
- Vol. 43 (4) , 66-73
The effect of cobalt content and mechanical activation on combustion in the Ni + Al + Co system
The effect of mechanical activation (MA) and cobalt content on the combustion velocity and maximum combustion temperature, elongation of samples during synthesis, the size of composite particles of the mixture after MA, phase composition and morphology of combustion products in the Ni + Al + Co system is investigated in this work. Activation of the Ni + Al + xCo mixture allowed the samples to burn at room temperature, with a cobalt content of up to 50 wt. %. An increase in the cobalt content in Ni + Al + xCo mixtures led to a decrease in the size of composite particles after MA, elongation of product samples and the maximum synthesis temperature. After MA, the elongation of the product samples and combustion velocity increased many times, the maximum synthesis temperature increased. With an increase in the cobalt content in the Ni + Al + Co mixture, combustion velocity first increases (at 10% Co), then decreases. Solid solutions based on NiAl and Ni3Al intermetallides were synthesized by the SHS method.
- 15 April 2024
- Published by The Russian Academy of Sciences in Химическая физика
- Vol. 43 (4) , 66-73
The effect of cobalt content and mechanical activation on combustion in the Ni + Al + Co system
The effect of mechanical activation (MA) and cobalt content on the combustion velocity and maximum combustion temperature, elongation of samples during synthesis, the size of composite particles of the mixture after MA, phase composition and morphology of combustion products in the Ni + Al + Co system is investigated in this work. Activation of the Ni + Al + xCo mixture allowed the samples to burn at room temperature, with a cobalt content of up to 50 wt. %. An increase in the cobalt content in Ni + Al + xCo mixtures led to a decrease in the size of composite particles after MA, elongation of product samples and the maximum synthesis temperature. After MA, the elongation of the product samples and combustion velocity increased many times, the maximum synthesis temperature increased. With an increase in the cobalt content in the Ni + Al + Co mixture, combustion velocity first increases (at 10% Co), then decreases. Solid solutions based on NiAl and Ni3Al intermetallides were synthesized by the SHS method.
- 1 April 2024
- Published by Pleiades Publishing Ltd in Russian Journal of Physical Chemistry B
- Vol. 18 (2) , 485-493
The Effect of the Nickel Content and Mechanical Activation on Combustion in the 5Ti + 3Si + xNi System
Intermetallic alloys are synthesized in the 5Ti + 3Si + xNi system by the method of self-propagating high-temperature synthesis (SHS) and mechanosynthesis. The influence of the nickel content on the morphology, size, and yield of composite particles after the mechanical activation (MA) of the mixtures is studied. The dependencies of the maximum temperatures and combustion rates, phase composition, morphology, and elongation of synthesis products on the nickel content for the initial and MA mixtures are studied. Under the conditions of the experiments conducted in this study, the combustion process is realized and at the same time the samples burn completely at a nickel content of 10 to 60 wt % in the 5Ti + 3Si + xNi system. After the MA, the samples from the 5Ti + 3Si mixture burn completely, and during the activation of the 5Ti + 3Si + 40% Ni mixture, mechanochemical synthesis takes place. With the increasing nickel content, the combustion temperature decreases, and the combustion rate behaves nonmonotonically, the size of composite particles increases and the yield of the mixture after MA decreases. MA practically does not affect the maximum combustion temperatures of mixtures of 5Ti + 3Si + xNi. A multiple (from 0.7 to 2.9 cm/s) increase in the burning rate of samples from MA mixtures with an increase in the Ni content from 20 to 30 wt % is recorded. An increase in the nickel content leads to an increase in the content of triple phases and the amount of melt in the synthesis products of mixtures of 5Ti + 3Si + xNi.
- 1 April 2024
- Published by Pleiades Publishing Ltd in Russian Journal of Physical Chemistry B
- Vol. 18 (2) , 485-493
The Effect of the Nickel Content and Mechanical Activation on Combustion in the 5Ti + 3Si + xNi System
Intermetallic alloys are synthesized in the 5Ti + 3Si + xNi system by the method of self-propagating high-temperature synthesis (SHS) and mechanosynthesis. The influence of the nickel content on the morphology, size, and yield of composite particles after the mechanical activation (MA) of the mixtures is studied. The dependencies of the maximum temperatures and combustion rates, phase composition, morphology, and elongation of synthesis products on the nickel content for the initial and MA mixtures are studied. Under the conditions of the experiments conducted in this study, the combustion process is realized and at the same time the samples burn completely at a nickel content of 10 to 60 wt % in the 5Ti + 3Si + xNi system. After the MA, the samples from the 5Ti + 3Si mixture burn completely, and during the activation of the 5Ti + 3Si + 40% Ni mixture, mechanochemical synthesis takes place. With the increasing nickel content, the combustion temperature decreases, and the combustion rate behaves nonmonotonically, the size of composite particles increases and the yield of the mixture after MA decreases. MA practically does not affect the maximum combustion temperatures of mixtures of 5Ti + 3Si + xNi. A multiple (from 0.7 to 2.9 cm/s) increase in the burning rate of samples from MA mixtures with an increase in the Ni content from 20 to 30 wt % is recorded. An increase in the nickel content leads to an increase in the content of triple phases and the amount of melt in the synthesis products of mixtures of 5Ti + 3Si + xNi.
- 1 April 2024
- Published by Pleiades Publishing Ltd in Russian Journal of Physical Chemistry B
- Vol. 18 (2) , 510-515
The Effect of the Cobalt Content and Mechanical Activation on Combustion in the Ni + Al + Co System
The effect of mechanical activation (MA) and the cobalt content on the combustion velocity, maximum combustion temperature, elongation of samples during synthesis, the size of composite particles of the mixture after MA, phase composition, and morphology of combustion products in the Ni + Al + Co system is studied. Activation of the Ni + Al + xCo mixture allowed the samples to burn at room temperature, with a cobalt content of up to 50 wt %. An increase in the cobalt content in the Ni + Al + xCo mixtures led to a decrease in the size of composite particles after MA, elongation of product samples, and the maximum synthesis temperature. After MA, the elongation of the product samples and combustion velocity increased many times, and the maximum synthesis temperature increased. With an increase in the cobalt content in the Ni + Al + Co mixture, the combustion velocity first increases (at Co content of 10%), then decreases. Solid solutions based on NiAl and Ni3Al intermetallic compounds are synthesized by the self-propagating high-temperature synthesis (SHS) method.
- 1 April 2024
- Published by Pleiades Publishing Ltd in Russian Journal of Physical Chemistry B
- Vol. 18 (2) , 510-515
The Effect of the Cobalt Content and Mechanical Activation on Combustion in the Ni + Al + Co System
The effect of mechanical activation (MA) and the cobalt content on the combustion velocity, maximum combustion temperature, elongation of samples during synthesis, the size of composite particles of the mixture after MA, phase composition, and morphology of combustion products in the Ni + Al + Co system is studied. Activation of the Ni + Al + xCo mixture allowed the samples to burn at room temperature, with a cobalt content of up to 50 wt %. An increase in the cobalt content in the Ni + Al + xCo mixtures led to a decrease in the size of composite particles after MA, elongation of product samples, and the maximum synthesis temperature. After MA, the elongation of the product samples and combustion velocity increased many times, and the maximum synthesis temperature increased. With an increase in the cobalt content in the Ni + Al + Co mixture, the combustion velocity first increases (at Co content of 10%), then decreases. Solid solutions based on NiAl and Ni3Al intermetallic compounds are synthesized by the self-propagating high-temperature synthesis (SHS) method.
- 1 October 2023
- Published by Pleiades Publishing Ltd in Combustion, Explosion, and Shock Waves
- Vol. 59 (5) , 567-575
Effect of Aluminum Content and Mechanical Activation on Ti–Si–Al Synthesis
This paper describes synthesis in 5Ti + 3Si + \(x\)Al(\(x = 0{-}40\)%) activated mixtures and in an 5Ti + 3Si + 10% Al initial mixture. The effect of mechanical activation and aluminum content on burning rate, maximum combustion temperature, morphology, elongation, integrity, and phase composition of combustion products is studied. Mechanical activation expands the limit of Al content to 40% at which samples can burn without preheating. The following intermetallic alloys are synthesized on the basis of Ti–Si–Al: solid solutions based on Ti(Si\(_{0.75}\)Al\(_{0.25})_{2 }\) titanium silicide and those based on Ti(Al\(_{0.9}\)Si\(_{0.1})_{3}\) aluminide titanium.- 1 October 2023
- Published by Pleiades Publishing Ltd in Combustion, Explosion, and Shock Waves
- Vol. 59 (5) , 567-575
Effect of Aluminum Content and Mechanical Activation on Ti–Si–Al Synthesis
This paper describes synthesis in 5Ti + 3Si + \(x\)Al(\(x = 0{-}40\)%) activated mixtures and in an 5Ti + 3Si + 10% Al initial mixture. The effect of mechanical activation and aluminum content on burning rate, maximum combustion temperature, morphology, elongation, integrity, and phase composition of combustion products is studied. Mechanical activation expands the limit of Al content to 40% at which samples can burn without preheating. The following intermetallic alloys are synthesized on the basis of Ti–Si–Al: solid solutions based on Ti(Si\(_{0.75}\)Al\(_{0.25})_{2 }\) titanium silicide and those based on Ti(Al\(_{0.9}\)Si\(_{0.1})_{3}\) aluminide titanium.- 1 April 2023
- Published by Pleiades Publishing Ltd in Russian Journal of Physical Chemistry B
- Vol. 17 (2) , 381-387
Verification of the Conclusions of the Microheterogeneous Model of Gas-Free Combustion at the Macroscopic Level
The combustion velocities of two fractions of mechanically activated Ni + Al mixtures are compared in this paper. The combustion of pressed samples and samples of bulk density is studied. The main aim of the study is to experimentally verify the main conclusions of the microheterogeneous model of gas-free combustion at the macrolevel using an activated Ni + Al mixture as an example. The relative elongation, the combustion velocity of the samples, the macrostructure, and phase composition of the synthesis products are studied. The combustion velocity is maintained with a change in the density of the samples and slightly increases with a decrease in the size of the composite particles. It is established that pressed samples during combustion elongate more strongly than samples from bulk density. Samples consisting of large particles elongate more strongly during combustion than samples consisting of smaller particles. The phase composition of combustion products depends on the fraction of composite particles and sample density. An explanation of the regularities observed in this study is proposed.
- 1 April 2023
- Published by Pleiades Publishing Ltd in Russian Journal of Physical Chemistry B
- Vol. 17 (2) , 381-387
Verification of the Conclusions of the Microheterogeneous Model of Gas-Free Combustion at the Macroscopic Level
The combustion velocities of two fractions of mechanically activated Ni + Al mixtures are compared in this paper. The combustion of pressed samples and samples of bulk density is studied. The main aim of the study is to experimentally verify the main conclusions of the microheterogeneous model of gas-free combustion at the macrolevel using an activated Ni + Al mixture as an example. The relative elongation, the combustion velocity of the samples, the macrostructure, and phase composition of the synthesis products are studied. The combustion velocity is maintained with a change in the density of the samples and slightly increases with a decrease in the size of the composite particles. It is established that pressed samples during combustion elongate more strongly than samples from bulk density. Samples consisting of large particles elongate more strongly during combustion than samples consisting of smaller particles. The phase composition of combustion products depends on the fraction of composite particles and sample density. An explanation of the regularities observed in this study is proposed.