Nikolay V. Kobernik
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Nikolay V. Kobernik has a total of 78 co-authors. Here are the top co-authors by number of shared publications:
A. S. Pankratov
Scientific and Educational Welding and Control Center, Bauman Moscow State Technical University (National Research University), Moscow, Russia
8 shared publicationsA. L. Galinovskii
Bauman Moscow State Technical University (National Research University), Moscow, Russia
5 shared publicationsYu. V. Andriyanov
Scientific and Educational Welding and Control Center, Bauman Moscow State Technical University (National Research University), Moscow, Russia
5 shared publicationsA. G. Orlik
Bauman Moscow State Technical University (National Research University, Kaluga, Russia
4 shared publicationsN. P. Aleshin
Welding and Monitoring Research Center, Bauman Moscow State Technical University, Moscow, Russia
4 shared publicationsA.S. Pankratov
3 shared publications
Latest Publications
- 1 January 2026
- Published by Science & Technology in Electrical Metallurgy
- No. 1
FRACTOGRAPHIC STUDIES OF SINGLE-CRYSTAL HEAT-RESISTANT NICKEL ALLOY SUBJECTED TO THERMOMECHANICAL LOADING BY COMPRESSIVE
Tensile tests were conducted at room and elevated temperatures on specimens of single-crystal heat-resistant nickel alloy grade SLZhS5-VI. These tests revealed a significant increase in the plastic characteristics of samples subjected to thermomechanical loading by compressive. Subsequent fractographic analysis of the destuction surfaces of the samples allowed to hypothesize that the observed effect is due to a reduction in discontinuities, microporosity and microcracks, as well as an increase in the strength of the alloy-inclusion boundary due to the use of thermomechanical loading by compressive.
- 1 January 2026
- Published by Science & Technology in Electrical Metallurgy
- No. 1
FRACTOGRAPHIC STUDIES OF SINGLE-CRYSTAL HEAT-RESISTANT NICKEL ALLOY SUBJECTED TO THERMOMECHANICAL LOADING BY COMPRESSIVE
Tensile tests were conducted at room and elevated temperatures on specimens of single-crystal heat-resistant nickel alloy grade SLZhS5-VI. These tests revealed a significant increase in the plastic characteristics of samples subjected to thermomechanical loading by compressive. Subsequent fractographic analysis of the destuction surfaces of the samples allowed to hypothesize that the observed effect is due to a reduction in discontinuities, microporosity and microcracks, as well as an increase in the strength of the alloy-inclusion boundary due to the use of thermomechanical loading by compressive.
- 1 January 2026
- Published by Science & Technology in Electrical Metallurgy
- No. 1
FRICTION STIR SPOT WELDING OF THIN SHEETS OF 6013 T4 ALLOY
The results of a study of the friction stir spot welding (FSS) process of lap joints of 1 mm thick 6013T4 aluminum alloy sheets are presented. It is shown that the mechanical properties of spot joints of the alloy under study depend on the main parameters of the welding mode: the duration of the welding process, the rotation frequency of the working tool, axial pressing force on the working tool. For a welding duration of 3 with a rational range of change of the remaining parameters of the welding mode are: the rotation frequency of the working tool is 1000-1800 rpm and the axial pressing force of the tool is 4300-4500 N. The specified friction stir welding mode ensures the formation of points with a destructive force of tear-off of 780 N and a shear force of 2280 N. In this case, welding is carried out without cleaning the contacting surfaces of the sheets in the overlap zone. It was noted that the use of two-stage friction stir spot welding allows for an increase in the value of the destructive shear force by 13% and on 24% of the destructive force on rupture compared to their values for spots obtained by friction stir spot welding. It has been established that contact spot welding of overlap joints of 6013T4 alloy sheets provides the highest mechanical characteristics of the spots: shear force of 3806 N with a tear force of 2381 N. It is noted that this welding process requires careful preparation of the sheet surfaces for welding, and after welding, imprints from the welding machine electrodes remain on the surface.
- 1 January 2026
- Published by Science & Technology in Electrical Metallurgy
- No. 1
FRICTION STIR SPOT WELDING OF THIN SHEETS OF 6013 T4 ALLOY
The results of a study of the friction stir spot welding (FSS) process of lap joints of 1 mm thick 6013T4 aluminum alloy sheets are presented. It is shown that the mechanical properties of spot joints of the alloy under study depend on the main parameters of the welding mode: the duration of the welding process, the rotation frequency of the working tool, axial pressing force on the working tool. For a welding duration of 3 with a rational range of change of the remaining parameters of the welding mode are: the rotation frequency of the working tool is 1000-1800 rpm and the axial pressing force of the tool is 4300-4500 N. The specified friction stir welding mode ensures the formation of points with a destructive force of tear-off of 780 N and a shear force of 2280 N. In this case, welding is carried out without cleaning the contacting surfaces of the sheets in the overlap zone. It was noted that the use of two-stage friction stir spot welding allows for an increase in the value of the destructive shear force by 13% and on 24% of the destructive force on rupture compared to their values for spots obtained by friction stir spot welding. It has been established that contact spot welding of overlap joints of 6013T4 alloy sheets provides the highest mechanical characteristics of the spots: shear force of 3806 N with a tear force of 2381 N. It is noted that this welding process requires careful preparation of the sheet surfaces for welding, and after welding, imprints from the welding machine electrodes remain on the surface.
- 1 January 2026
- Published by Science & Technology in Electrical Metallurgy
- No. 1
CLADDING BY COPPER POWDER OF TITANIUM CARBIDE PARTICLES IN A PLANETARY MILL
The results of a study of titanium carbide powder cladding with copper powder during processing in a planetary mill are presented, along with the results of an analysis of changes in bulk density, fractional composition, and reduced particle size. The cladding coating on the titanium carbide surface is examined in detail, and the nature of its formation is revealed.
- 1 January 2026
- Published by Science & Technology in Electrical Metallurgy
- No. 1
CLADDING BY COPPER POWDER OF TITANIUM CARBIDE PARTICLES IN A PLANETARY MILL
The results of a study of titanium carbide powder cladding with copper powder during processing in a planetary mill are presented, along with the results of an analysis of changes in bulk density, fractional composition, and reduced particle size. The cladding coating on the titanium carbide surface is examined in detail, and the nature of its formation is revealed.
- 1 June 2025
- Published by Pleiades Publishing Ltd in Russian Metallurgy (Metally)
- Vol. 2025 (6) , 1471-1477
Effect of Titanium Carbide in a Flux Cored Wire Charge on the Structure of a Deposited Metal
Changes in the microstructure and hardness of the metal deposited with flux-cored wires 2.0 and 1.6 mm in diameter, which are characterized by different contents (from 9.8 to 29 wt %) and types of titanium carbide, are studied during their deposition with a nonconsumable electrode. The structure of the deposited metal is shown to contain both retained coarse titanium carbide and fine titanium carbide particles no more than 10 μm in size. The effect of nickel added to the composition of flux cored wire charge, both in the form of pure nickel and as part of TiC + Ni composite granules prepared by combined processing of nickel and titanium carbide powders in a planetary mill, on changes in the structure formation and the hardness of the deposited metal is studied. The use of nickel in the flux cored filler wire is shown to decrease the amount of introduced titanium carbide and to increase the hardness.
- 1 June 2025
- Published by Pleiades Publishing Ltd in Russian Metallurgy (Metally)
- Vol. 2025 (6) , 1471-1477
Effect of Titanium Carbide in a Flux Cored Wire Charge on the Structure of a Deposited Metal
Changes in the microstructure and hardness of the metal deposited with flux-cored wires 2.0 and 1.6 mm in diameter, which are characterized by different contents (from 9.8 to 29 wt %) and types of titanium carbide, are studied during their deposition with a nonconsumable electrode. The structure of the deposited metal is shown to contain both retained coarse titanium carbide and fine titanium carbide particles no more than 10 μm in size. The effect of nickel added to the composition of flux cored wire charge, both in the form of pure nickel and as part of TiC + Ni composite granules prepared by combined processing of nickel and titanium carbide powders in a planetary mill, on changes in the structure formation and the hardness of the deposited metal is studied. The use of nickel in the flux cored filler wire is shown to decrease the amount of introduced titanium carbide and to increase the hardness.
- 1 June 2025
- Published by Pleiades Publishing Ltd in Russian Metallurgy (Metally)
- Vol. 2025 (6) , 1478-1484
Effect of the Flux-Cored Powder Wire Charge Composition on the Stability of Surfacing
Effect of K2CO3, TiO2, and CaF2 on the stability of surfacing, when these components are introduced into the composition of flux-cored wire charge of the C–Cr–B alloying system intended for the deposition of abrasion-resistant coatings, is studied. Oscillograms of the deposition of the fabricated flux-cored wires are obtained under various conditions ensuring electrode metal transfer with and without short circuits. The oscillograms are used to reveal the effect of the components of flux-cored wires charge on the stability of the process. The effect of the introduced components on the coefficient of burnout and splashing losses and the fraction of participating the base metal are detected under various surfacing conditions.
- 1 June 2025
- Published by Pleiades Publishing Ltd in Russian Metallurgy (Metally)
- Vol. 2025 (6) , 1478-1484
Effect of the Flux-Cored Powder Wire Charge Composition on the Stability of Surfacing
Effect of K2CO3, TiO2, and CaF2 on the stability of surfacing, when these components are introduced into the composition of flux-cored wire charge of the C–Cr–B alloying system intended for the deposition of abrasion-resistant coatings, is studied. Oscillograms of the deposition of the fabricated flux-cored wires are obtained under various conditions ensuring electrode metal transfer with and without short circuits. The oscillograms are used to reveal the effect of the components of flux-cored wires charge on the stability of the process. The effect of the introduced components on the coefficient of burnout and splashing losses and the fraction of participating the base metal are detected under various surfacing conditions.
- 1 January 2025
- Published by Pleiades Publishing Ltd in Russian Metallurgy (Metally)
- Vol. 2025 (1) , 165-170
Cladding of Titanium Carbide Powders with Nickel for Use in Flux-Cored Wires
—The results of studying the cladding of titanium carbide powders with nickel using a planetary mill are presented. When titanium carbide with a smooth surface and nickel are processed simultaneously, only fragmentary coating of the carbide surface with nickel is found to occur. The maximum coverage area of titanium carbide with nickel (3.4%) is achieved at a planetary mill rotation speed of 250 rpm. Here, the titanium content in nickel increases up to 10.50 wt %. The use of titanium carbide with a pumice-like structure is found to promote the cladding of the carbide with nickel. The obtained results can serve as a basis for developing a new approach to preparing nickel-based materials for manufacturing flux-cored wires used for the deposition of wear-resistant coatings.
- 1 January 2025
- Published by Pleiades Publishing Ltd in Russian Metallurgy (Metally)
- Vol. 2025 (1) , 165-170
Cladding of Titanium Carbide Powders with Nickel for Use in Flux-Cored Wires
—The results of studying the cladding of titanium carbide powders with nickel using a planetary mill are presented. When titanium carbide with a smooth surface and nickel are processed simultaneously, only fragmentary coating of the carbide surface with nickel is found to occur. The maximum coverage area of titanium carbide with nickel (3.4%) is achieved at a planetary mill rotation speed of 250 rpm. Here, the titanium content in nickel increases up to 10.50 wt %. The use of titanium carbide with a pumice-like structure is found to promote the cladding of the carbide with nickel. The obtained results can serve as a basis for developing a new approach to preparing nickel-based materials for manufacturing flux-cored wires used for the deposition of wear-resistant coatings.
- 1 January 2025
- Published by Pleiades Publishing Ltd in Russian Metallurgy (Metally)
- Vol. 2025 (1) , 160-164
Resistance of a Weld Metal to Various Types of Wear
—Effect of ferrotitanium introduced in the charge composition of a flux-cored wire on the microstructure of the weld metal is considered. The deposited coatings are tested for hydroabrasive wear and wear due to friction against a partially fixed abrasive. A relationship between changes in the microstructure and the wear resistance indicators is found.
- 1 January 2025
- Published by Pleiades Publishing Ltd in Russian Metallurgy (Metally)
- Vol. 2025 (1) , 160-164
Resistance of a Weld Metal to Various Types of Wear
—Effect of ferrotitanium introduced in the charge composition of a flux-cored wire on the microstructure of the weld metal is considered. The deposited coatings are tested for hydroabrasive wear and wear due to friction against a partially fixed abrasive. A relationship between changes in the microstructure and the wear resistance indicators is found.
- 1 June 2023
- Published by Pleiades Publishing Ltd in Russian Metallurgy (Metally)
- Vol. 2023 (6) , 657-664
Formation of a Composite Structure in a Deposited Fe–Cr–C + TiC (NbC) Metal
The formation of a composite structure in a deposited Fe–Cr–C + TiC (NbC) metal using complex (ex-situ) alloying with the use of refractory titanium and niobium carbides as part of a charge of a filler flux-cored wire is considered. The influence of the content of these carbides on the structure and properties of the deposited metal has been studied. The formation of a composite structure in the course of surfacing using polyreinforcement is also considered and studied using titanium and niobium carbides as an example.
- 1 June 2023
- Published by Pleiades Publishing Ltd in Russian Metallurgy (Metally)
- Vol. 2023 (6) , 657-664
Formation of a Composite Structure in a Deposited Fe–Cr–C + TiC (NbC) Metal
The formation of a composite structure in a deposited Fe–Cr–C + TiC (NbC) metal using complex (ex-situ) alloying with the use of refractory titanium and niobium carbides as part of a charge of a filler flux-cored wire is considered. The influence of the content of these carbides on the structure and properties of the deposited metal has been studied. The formation of a composite structure in the course of surfacing using polyreinforcement is also considered and studied using titanium and niobium carbides as an example.
- 26 May 2023
- Published by Springer Nature in Metallurgist
- Vol. 67 (1-2) , 201-208
Influence of Silicon Carbide Introduced into a Flux-Cored Wire Charge on Deposited Metal Structure
- 26 May 2023
- Published by Springer Nature in Metallurgist
- Vol. 67 (1-2) , 201-208
Influence of Silicon Carbide Introduced into a Flux-Cored Wire Charge on Deposited Metal Structure
- 1 December 2022
- Published by Pleiades Publishing Ltd in Russian Metallurgy (Metally)
- Vol. 2022 (13) , 1836-1841
Effect of Chromium Carbide on the Structure of a Sprayed Metal upon Its Introduction into the Composition of a Filler Flux-Cored Wire Charge
—A scheme of arc spraying with a flux-cored wire in a protecting gas atmosphere using a filler flux-cored wire is considered. In this scheme, a filler wire is fed from the side of the tail part of the welding bath. The filler flux-cored wire charges contain chromium carbide. Chromium carbide is shown to decompose during spraying, which leads to alloying of the sprayed metal with chromium and carbon. The use of chromium carbide is found to increase the coefficient of transition of carbon and chromium into the sprayed metal. When ferrochrome is completely replaced with chromium carbide, needlelike chromium carbide forms in the sprayed metal.
- 1 December 2022
- Published by Pleiades Publishing Ltd in Russian Metallurgy (Metally)
- Vol. 2022 (13) , 1836-1841
Effect of Chromium Carbide on the Structure of a Sprayed Metal upon Its Introduction into the Composition of a Filler Flux-Cored Wire Charge
—A scheme of arc spraying with a flux-cored wire in a protecting gas atmosphere using a filler flux-cored wire is considered. In this scheme, a filler wire is fed from the side of the tail part of the welding bath. The filler flux-cored wire charges contain chromium carbide. Chromium carbide is shown to decompose during spraying, which leads to alloying of the sprayed metal with chromium and carbon. The use of chromium carbide is found to increase the coefficient of transition of carbon and chromium into the sprayed metal. When ferrochrome is completely replaced with chromium carbide, needlelike chromium carbide forms in the sprayed metal.