Jie Liu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Jie Liu has a total of 70 co-authors. Here are the top co-authors by number of shared publications:
Yuzhu Li
Yantai University
5 shared publicationsHui Guo
Yantai Univ, Sch Chem & Chem Engn, Yantai 264005, Peoples R China
4 shared publicationsXinyue Zhang
Yantai Univ, Sch Chem & Chem Engn, Yantai 264005, Peoples R China
4 shared publicationsZhenliang Feng
Yantai University
4 shared publicationsBo Fang
Yantai Univ, Sch Chem & Chem Engn, Yantai 264005, Peoples R China
3 shared publications- Bin Wang
School of Chemistry and Materials Science Ludong University Yantai China
2 shared publications
Latest Publications
- Open Access
Anti-Permeability Formation Process of Epoxy Coatings Under Simulated Shallow Seawater
The formation of anti-permeability is a critical step in the in-situ repair of organic anti-corrosion coatings under seawater, yet it is significantly influenced by the surrounding marine environment, particularly seawater temperature and applied cathodic polarization potential. In this study, we systematically investigated the effects of temperature and cathodic polarization potential on the permeability of curing epoxy coatings in simulated shallow seawater. Our results demonstrate that the anti-permeability formation process is governed by the competition between seawater penetration and coating curing. At lower temperatures, the EIS-derived evolution of coating resistance suggested heterogeneous electrolyte uptake across the coating surface, whereas at elevated temperatures, the electrochemical response indicated a more uniform progression of ionic ingress. Moreover, enhanced cathodic polarization accelerated both seawater penetration and the curing reaction of the epoxy coating. The underlying mechanisms of temperature- and polarization-dependent permeability formation were discussed in detail, providing theoretical insights into the top-down permeation process during underwater curing, which may inform the development of more effective in situ repair strategies for organic coatings.
Open AccessAnti-Permeability Formation Process of Epoxy Coatings Under Simulated Shallow Seawater
The formation of anti-permeability is a critical step in the in-situ repair of organic anti-corrosion coatings under seawater, yet it is significantly influenced by the surrounding marine environment, particularly seawater temperature and applied cathodic polarization potential. In this study, we systematically investigated the effects of temperature and cathodic polarization potential on the permeability of curing epoxy coatings in simulated shallow seawater. Our results demonstrate that the anti-permeability formation process is governed by the competition between seawater penetration and coating curing. At lower temperatures, the EIS-derived evolution of coating resistance suggested heterogeneous electrolyte uptake across the coating surface, whereas at elevated temperatures, the electrochemical response indicated a more uniform progression of ionic ingress. Moreover, enhanced cathodic polarization accelerated both seawater penetration and the curing reaction of the epoxy coating. The underlying mechanisms of temperature- and polarization-dependent permeability formation were discussed in detail, providing theoretical insights into the top-down permeation process during underwater curing, which may inform the development of more effective in situ repair strategies for organic coatings.
- 7 April 2026
- Published by SAGE Publications in Corrosion Engineering, Science and Technology: The International Journal of Corrosion Processes and Corrosion Control
- Vol. 61 (8) , 1295-1308
Corrosion failure behaviours of PCBs in different marine atmospheric environments
The corrosion failure behaviours of PCB-ImAg and PCB-ImSn were investigated after exposure in the atmospheric environments of Wanning and Yantai for 12 months under a shed. The results showed that after exposure in Wanning for 12 months, the change of PCB-ImAg impedance value was that the damaged Ag layer formed a galvanic system with the Cu substrate. Meanwhile, after exposure in Yantai, the change of PCB-ImSn impedance value was mainly due to the dissolution of the Sn layer accelerated by SO 2 . The corrosion products of printed circuit boards (PCBs) were basically the same in the atmospheric environments of Wanning and Yantai. However, the SO 2 content in the Yantai environment was higher than that in Wanning, and CuSO 4 ·3Cu(OH) 2 was detected in the corrosion products from Yantai. PCBs showed different degrees of electrochemical migration (ECM) in both atmospheric environments. The atmospheric environment of Wanning was more prone to the electrochemical migration of copper because the PCB surface was more likely to form a thin liquid film. In summary, it was confirmed that the corrosion failure behaviours of PCB-ImAg and PCB-ImSn had obvious environmental dependence on ECM behaviour, which was mainly related to the content of SO 2 in different atmospheric environments and the formation of a thin liquid film.
- 7 April 2026
- Published by SAGE Publications in Corrosion Engineering, Science and Technology: The International Journal of Corrosion Processes and Corrosion Control
- Vol. 61 (8) , 1295-1308
Corrosion failure behaviours of PCBs in different marine atmospheric environments
The corrosion failure behaviours of PCB-ImAg and PCB-ImSn were investigated after exposure in the atmospheric environments of Wanning and Yantai for 12 months under a shed. The results showed that after exposure in Wanning for 12 months, the change of PCB-ImAg impedance value was that the damaged Ag layer formed a galvanic system with the Cu substrate. Meanwhile, after exposure in Yantai, the change of PCB-ImSn impedance value was mainly due to the dissolution of the Sn layer accelerated by SO 2 . The corrosion products of printed circuit boards (PCBs) were basically the same in the atmospheric environments of Wanning and Yantai. However, the SO 2 content in the Yantai environment was higher than that in Wanning, and CuSO 4 ·3Cu(OH) 2 was detected in the corrosion products from Yantai. PCBs showed different degrees of electrochemical migration (ECM) in both atmospheric environments. The atmospheric environment of Wanning was more prone to the electrochemical migration of copper because the PCB surface was more likely to form a thin liquid film. In summary, it was confirmed that the corrosion failure behaviours of PCB-ImAg and PCB-ImSn had obvious environmental dependence on ECM behaviour, which was mainly related to the content of SO 2 in different atmospheric environments and the formation of a thin liquid film.
- 30 August 2025
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 36 (24) , 1-14
Corrosion behavior and mechanism of PCB–ENIG in marine atmospheric environment
- 30 August 2025
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 36 (24) , 1-14
Corrosion behavior and mechanism of PCB–ENIG in marine atmospheric environment
- 14 June 2024
- Published by Springer Nature in Journal of Materials Science
- Vol. 59 (26) , 12092-12110
Effect of environmental pressure on the corrosion behavior of sacrificial anode magnesium alloy in simulated cementing cement hole solution
- 14 June 2024
- Published by Springer Nature in Journal of Materials Science
- Vol. 59 (26) , 12092-12110
Effect of environmental pressure on the corrosion behavior of sacrificial anode magnesium alloy in simulated cementing cement hole solution
- 11 April 2024
- Published by Elsevier in Progress in Organic Coatings
- Vol. 191
Modified epoxy coatings based on BI@ZIF-8@TA for the application of long-effective corrosion protection
- 11 April 2024
- Published by Elsevier in Progress in Organic Coatings
- Vol. 191
Modified epoxy coatings based on BI@ZIF-8@TA for the application of long-effective corrosion protection
- Open Access
Corrosion Behavior of Alkyd-Resin-Coated Carbon Steel under Cathodic Polarization in Both Static and Flowing Seawater
The effect of cathodic polarization on the corrosion behavior of alkyd-resin-coated carbon steel with an artificial coating defect was researched using a wire beam electrode (WBE) and electrochemical impedance spectroscopy (EIS) in both static and flowing simulated solutions. The microscopic morphology and chemical structure of the organic coating were characterized by scanning electron microscopy (SEM) and infrared spectroscopy (FT-IR) to reveal the degradation mechanisms of organic coatings under different polarization potentials. The study found that the failure process of the alkyd coating could be accelerated by cathodic polarization. After 312 h of immersion, the impedance under −1100 mV was one order of magnitude lower than that under the open-circuit potential (OCP). The coating delamination became serious with the negative shifting of polarization potential, and the delamination area ratio under −1100 mV in both static and flowing seawater rose to 23% and 14%, respectively. Interestingly, the flowing condition of the immersion solution that combined with cathodic polarization exhibited a synergistic effect, which could accelerate (in the earlier stage) and then alleviate the delamination of the coating. Furthermore, the results showed that both the diffusion of the corrosion particles and the anodic dissolution reaction of the metal could be significantly affected by cathodic polarization and the flowing condition of the solution, which provides a possible approach to gain insight into the delamination of organic coating.
Open AccessCorrosion Behavior of Alkyd-Resin-Coated Carbon Steel under Cathodic Polarization in Both Static and Flowing Seawater
The effect of cathodic polarization on the corrosion behavior of alkyd-resin-coated carbon steel with an artificial coating defect was researched using a wire beam electrode (WBE) and electrochemical impedance spectroscopy (EIS) in both static and flowing simulated solutions. The microscopic morphology and chemical structure of the organic coating were characterized by scanning electron microscopy (SEM) and infrared spectroscopy (FT-IR) to reveal the degradation mechanisms of organic coatings under different polarization potentials. The study found that the failure process of the alkyd coating could be accelerated by cathodic polarization. After 312 h of immersion, the impedance under −1100 mV was one order of magnitude lower than that under the open-circuit potential (OCP). The coating delamination became serious with the negative shifting of polarization potential, and the delamination area ratio under −1100 mV in both static and flowing seawater rose to 23% and 14%, respectively. Interestingly, the flowing condition of the immersion solution that combined with cathodic polarization exhibited a synergistic effect, which could accelerate (in the earlier stage) and then alleviate the delamination of the coating. Furthermore, the results showed that both the diffusion of the corrosion particles and the anodic dissolution reaction of the metal could be significantly affected by cathodic polarization and the flowing condition of the solution, which provides a possible approach to gain insight into the delamination of organic coating.
- 21 October 2020
- Published by Wiley in Materials and Corrosion
- Vol. 72 (4) , 732-742
Studies on waterline corrosion processes and corrosion product characteristics of carbon steel in 3.5 wt% NaCl solution
The waterline corrosion behaviors of carbon steel partially immersed in a 3.5 wt% NaCl solution were investigated using the wire beam electrode technique, and the effects of corrosion products on the processes of waterline corrosion were analyzed. The results demonstrated that the initial stage and development stage of waterline corrosion were mainly controlled by the concentration and diffusion of dissolved oxygen, respectively, and the deceleration stage of waterline corrosion was mainly affected by corrosion products. The main component of the yellow corrosion products was γ‐FeOOH, and γ‐FeOOH that exhibited a high reduction reactivity could be involved in the cathodic reaction. The black corrosion products were mainly composed of Fe3O4 with strong thermodynamic stability and the processes of dissolved oxygen diffusion and ion transports were obviously affected due to the continuous accumulation of Fe3O4 on the surface of the electrodes. Polarity reversals were observed on the single electrodes below the waterline, but the reasons for the phenomena were different from each other.
- 21 October 2020
- Published by Wiley in Materials and Corrosion
- Vol. 72 (4) , 732-742
Studies on waterline corrosion processes and corrosion product characteristics of carbon steel in 3.5 wt% NaCl solution
The waterline corrosion behaviors of carbon steel partially immersed in a 3.5 wt% NaCl solution were investigated using the wire beam electrode technique, and the effects of corrosion products on the processes of waterline corrosion were analyzed. The results demonstrated that the initial stage and development stage of waterline corrosion were mainly controlled by the concentration and diffusion of dissolved oxygen, respectively, and the deceleration stage of waterline corrosion was mainly affected by corrosion products. The main component of the yellow corrosion products was γ‐FeOOH, and γ‐FeOOH that exhibited a high reduction reactivity could be involved in the cathodic reaction. The black corrosion products were mainly composed of Fe3O4 with strong thermodynamic stability and the processes of dissolved oxygen diffusion and ion transports were obviously affected due to the continuous accumulation of Fe3O4 on the surface of the electrodes. Polarity reversals were observed on the single electrodes below the waterline, but the reasons for the phenomena were different from each other.