Latest Publications

  • Open Access

    Effect of Annealing Atmosphere on the Microstructure and High-Frequency Magnetic Properties of FeSiCr Soft Magnetic Composites

    by Chijiawen Fang, Jie Zhang, Jianwei Zheng, Dongsheng Shi, Wenjin Wu, Jingwu Zheng, Liang Qiao, Wei Cai, Yao Ying, Juan Li, et al.

    Annealing is a critical step in the fabrication of soft magnetic composites (SMCs), and precise coordination of annealing atmosphere and temperature is essential for optimizing their performance. In this study, FeSiCr SMCs were annealed under three different atmospheres (air, nitrogen, and argon) across a range of temperatures, and the effects of the annealing atmosphere on their microstructure and soft magnetic properties were systematically investigated. The results demonstrate that annealing in an inert atmosphere, particularly argon, within the temperature range of 450–750 °C, yields superior magnetic properties compared with air annealing. After annealing under argon at 550 °C, the effective magnetic permeability (μe) reached 47.5, and the power loss (Pcv) was 1457.3 kW/m3 at 1000 kHz and 30 mT. These improvements are primarily attributed to effective stress relaxation and the substantial retention of the polyvinyl butyral (PVB) insulating layer. With further increases in annealing temperature, the magnetic properties deteriorate rapidly due to the complete decomposition of PVB and the formation of conductive chromium carbides. Under such conditions, air annealing exhibits distinct advantages. Selective oxidation of FeSiCr occurs, leading to the formation of a dense chromium oxide insulating layer that enhances magnetic performance (after annealing at 850 °C, μe = 47.9, Pcv = 1632.0 kW/m3). Moreover, the mechanical properties were significantly improved, with the radial crush strength increasing from 22.36 N in the unannealed state to 330 N after annealing. These results indicate that the comprehensive performance of SMCs can be effectively tailored through the appropriate selection of annealing atmosphere and temperature, providing valuable guidance for the design and optimization of high-performance SMCs.


  • Open Access

    A Novel Strategy for High Quantum Efficiency Composite Oxide Far-Red Phosphors: Ca14Mg5.94Li0.03In0.03Ga9.95O35:0.05Mn4+

    by Juan Li, Huiying Ye, Fachangsheng Zhong, Peng Wu, Menghao Chang, Linkun Han, Jingwu Zheng, Liang Qiao, Jing Yu, Yao Ying, et al.

    Far-red phosphors featuring high quantum efficiency and emission bands that strongly overlap with the absorption spectra of plant pigments are crucial for advancing plant cultivation lighting technology. Restricted by the large Stokes shift, far-red phosphors typically exhibit low energy efficiency. Moreover, many far-red phosphors suffer from low quantum efficiency, which has emerged as a critical issue in the research of these materials. To address the issue, conventional strategies—including crystal field engineering, defect engineering, and sensitizer doping—have been widely adopted to enhance their emission intensity. In this work, we propose a novel and effective strategy to improve the emission performance of far-red phosphors: low-melting-point magnesium chloride has been introduced as a flux to regulate the reaction pathway of the composite oxide phosphor Ca14Mg5.94Li0.03In0.03Ga9.95O35:0.05Mn4+ (CMLIGO:0.05Mn4+). The cubic intermediate product with a structure analogous to the target product has been designed to form a compact lattice structure and reduce crystal defects, thereby enhancing the luminescence intensity and quantum efficiency of the phosphor. The Ca14Mg5.94Li0.03In0.03Ga9.95O35:0.05Mn4+@3 wt% MgCl2 (CMLIGO:0.05Mn4+@3 wt% MgCl2) shows a broad excitation band (250–600 nm) and far-red emission centered at 720 nm (650–800 nm). Under 365 nm excitation, the CMLIGO:0.05Mn4+@3 wt% MgCl2 exhibits an internal quantum efficiency of 91.4%. Benefiting from its high internal quantum efficiency and the emission band that matches well with the absorption spectrum of phytochrome in the far-red absorbing form (phytochrome Pfr), CMLIGO:0.05Mn4+@3 wt% MgCl2 demonstrates promising potential for applications in plant cultivation lighting. This work offers a new direction for synthesizing and modification of composite oxide phosphors.

  • A sustainable phosphorization treatment on the high-temperature oxidation resistance of Nd-Fe-B magnetic powders

    by Wei Cai, Xinqi Zhang, Jianwei Zheng, Jingwu Zheng, Rongyao Li, Haibo Chen, Liang Qiao, Yao Ying, Wangchang Li, Jing Yu, et al.


  • Open Access

    Investigation of the Impact of SmFeN Doping on the Anisotropic NdFeB/SmFeN Composite Magnets

    by Wei Cai, Xinqi Zhang, Zhiping Shi, Haibo Chen, Qiaomin Zhu, Kun Jiang, Liang Qiao, Yao Ying, Wangchang Li, Jing Yu, et al.

    By incorporating various types of permanent magnetic powders, composite magnets with cost-effectiveness and a wide range of magnetic properties can be achieved. In this study, the anisotropic composite magnets were fabricated using the hot press forming method, which involved blending neodymium iron boron (NdFeB) powder and samarium iron nitrogen (SmFeN) powder. The experiment demonstrated that the magnet density reaches its maximum point when the doping level of SmFeN reaches 20 wt.%, aligning remarkably well with the corresponding theoretical value of 19.22 wt.% achieved through a cubic stacking arrangement. In the absence of an applied magnetic field or under a sufficiently high oriented magnetic field (3 T), the remanence variation pattern in composite magnets doped with different amounts of SmFeN aligns consistently with the density pattern, yielding a maximum value of 20%. However, in the actual solidification process, the orientation field is insufficient (e.g., 1.5 T), necessitating a doping amount that exceeds the value corresponding to peak density by 28% to achieve optimal remanence. This observation suggests that the incorporation of a higher proportion of small-sized and relatively low coercivity SmFeN magnetic powder can effectively facilitate the rotational alignment of neighboring large-sized NdFeB magnetic powder under weak magnetic fields, thereby inducing a synergistic effect.


  • Open Access

    Preparation of Densified Fine-Grain High-Frequency MnZn Ferrite Using the Cold Sintering Process

    by Yao Ying, Linghuo Hu, Zhaocheng Li, Jingwu Zheng, Jing Yu, Wangchang Li, Liang Qiao, Wei Cai, Juan Li, Daxin Bao, et al.

    The densified MnZn ferrite ceramics were prepared using the cold sintering process under pressure, with an acetate ethanol solution used as the transient solvent. The effects of the transient solvent, the pressure and annealing temperature on the density, and the micromorphology and magnetic properties of the sintered MnZn ferrites were studied. The densified MnZn ferrite was obtained using the cold sintering process and its relative density reached up to 85.4%. The transient solvent and high pressure are essential to the cold sintering process for MnZn ferrite. The annealing treatment is indispensable in obtaining the sample with the higher density. The relative density was further increased to 97.2% for the sample annealed at 950 °C for 6 h. The increase in the annealing temperature reduces the power loss at high frequencies.


  • Open Access

    Low Core Losses of Fe-Based Soft Magnetic Composites with an Zn-O-Si Insulating Layer Obtained by Coupling Synergistic Photodecomposition

    by Siyuan Wang, Jingwu Zheng, Danni Zheng, Liang Qiao, Yao Ying, Yiping Tang, Wei Cai, Wangchang Li, Jing Yu, Juan Li, et al.

    The major method used to reduce the magnetic loss of soft magnetic composites (SMCs) is to coat the magnetic powder with an insulating layer, but the permeability is usually sacrificed in the process. In order to achieve a better balance between low losses and high permeability, a novel photodecomposition method was used in this study to create a ZnO insulating layer. The effect of the concentration of diethyl zinc on the formation of a ZnO insulating film by photodecomposition was studied. The ZnO film was best formed with a diethyl zinc n-hexane solution at a concentration of around 0.40 mol/L. Combined with conventional coupling treatment processes, a thin and dense insulating layer was coated on the surface of iron powder in situ. Treating the iron powder before coating by photodecomposition led to a synergistic effect, significantly reduced core loss, and the effective permeability only decreased slightly. An iron-based soft magnetic composite with a loss value of 124 kW/m3 and an effective permeability of 107 was obtained at the frequency of 100 kHz and a magnetic field intensity of 20 mT.


  • Open Access

    Magnetic Properties and Microstructure of Ce-Cu-Al Low Melting Alloy Bonding Sm2Fe17N3 Magnet Fabricated by the Hot-Pressing Method

    by Jingwu Zheng, Shitong Yu, Heng Huang, Rongyao Li, Wei Cai, Haibo Chen, Juan Li, Liang Qiao, Yao Ying, Wangchang Li, et al.

    Sm2Fe17N3 compounds, having excellent intrinsic magnetic properties, are prone to decomposition at high temperatures; thus, a low melting point metal binder is the key to prepare high performance bulk magnets at low temperatures. In this paper, a new low melting point alloy Ce72Cu28-xAlx was used as the binders, and high-performance Ce-based alloy bonding Sm2Fe17N3 magnets were realized by the hot-pressing method. The experimental results demonstrated that the content of Al in the Ce-based alloys had an important influence on the performance of the magnets. High performance Sm-Fe-N bonded magnets with remanence of 10.19 KGs and maximum magnetic energy product of 21.06 MGOe were achieved by using 5 wt.% Ce72Cu22Al6 alloy as a binder. At the same time, it was found that the Ce72Cu28-xAlx alloy has a lower density and better bonding effect than the common Zn binder. Its bonding magnets still have higher performance even with extremely high oxygen content. Therefore, Ce72Cu28-xAlx alloy with low melting point is a promising new rare earth-based alloy binder. If the oxygen content of the alloy powders could be reduced, higher performance Sm2Fe17N3 bonded magnets can be prepared.


  • Open Access

    Injection Molding and Sintering of ZrO2 Ceramic Powder Modified by a Zirconate Coupling Agent

    by Qiangyi Mao, Liang Qiao, Jingwu Zheng, Yao Ying, Jing Yu, Wangchang Li, Shenglei Che, Wei Cai

    Ceramic injection molding is a near-net shape-processing technique, producing ceramic components with low tooling costs and complex shapes. In this paper, ZrO2 ceramics with high loading content in the green part were prepared by powder modification using zirconate coupling agent, injection molding and sintering, which benefited decreasing the usage of binders and deformation of ceramics. The rheological characteristics of feedstocks, densities, microstructures and mechanical properties of green and sintered parts with the different coupling media and sintering temperatures were studied. The results showed that the addition of a zirconate coupling agent with ethanol medium obviously increased the flowability of feedstocks and benefited achieving the green parts with high powder loading (86.5 wt.%) and bending strength (12.9 MPa) and the final unbroken ceramics. In addition, the sintering temperatures from 1500–1575 °C had no significant effects on the density, hardness, and surface morphology of the ceramic samples. However, the bending strength increased and some large grains with transgranular fracture occurred on the fractural surface at the sintering temperature of 1575 °C.


  • Preparation, Microstructure, and Magnetic Properties of Electrodeposited Nanocrystalline L10 FePt Films

    by Yao Ying, Huibin Wang, Jingwu Zheng, Jing Yu, Wangchang Li, Liang Qiao, Wei Cai, Shenglei Che


  • Open Access

    Preparation of submicron-sized Sm2Fe17N3 fine powder by ultrasonic spray pyrolysis-hydrogen reduction (USP-HR) and subsequent reduction–diffusion process

    by Jingwu Zheng, Shijun Tian, Kaihua Liu, Wei Cai, Yiping Tang, Liang Qiao, Yao Ying, Wangchang Li, Jing Yu, Youhao Liu, et al.

    A new reduction–diffusion method for preparing submicron-sized Sm2Fe17N3 was developed. First, submicron-sized α-Fe/Sm2O3 composite precursors with good dispersibility were prepared directly by ultrasonic spray pyrolysis and hydrogen reduction (USP-HR). Then, the precursor was successfully converted into Sm2Fe17N3 powder by Ca reduction–diffusion and nitridation. The results displayed that the precursor prepared by USP-HR was a monodisperse homogeneous composite of spherical particles of α-Fe and Sm2O3. α-Fe and Sm2O3 exist in an intercalated structure in the composite spherical particles. This creates conditions for the preparation of ultrafine Sm2Fe17N3 particles with uniform sizes and dispersity. The results show that Sm2Fe17N3 is a single-phase, composed of submicron-sized particles with no other impurity phases. The physical property measurement system shows that the coercivity of 0.616 ± 0.347 µm particles reaches 14.7 kOe.