Clever Aparecido Valentin
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Clever Aparecido Valentin has a total of 27 co-authors. Here are the top co-authors by number of shared publications:
- Jefferson Lins da Silva
Universidade de São Paulo
16 shared publications - Marcelo Kobelnik
Department of Geotechnical Engineering , São Carlos School of Engineering of São Carlos , University of São Paulo , São Paulo , Brazil , usp.br
10 shared publications - Maria Alejandra Aparicio-Ardila
Universidade de São Paulo
8 shared publications - Marta Pereira da Luz
Pontifícia Universidade Católica de Goiás, Brazil
7 shared publications - Fernando Luiz Lavoie
Department of Civil Engineering, Mauá Institute of Technology, São Caetano do Sul 09580-900, Brazil
5 shared publications - Maria de Lurdes Lopes
University of Porto
4 shared publications
Latest Publications
- Open Access
- 1 January 2026
- Published by Wiley in International Journal of Polymer Science
- Vol. 2026 (1) , 8006062
Durability of Nonwoven Geotextile (PP and PET) Under Natural Weathering: A Comprehensive Evaluation Using Thermal, Mechanical, and Microstructural Analysis
This study evaluates the long‐term durability of two commercial nonwoven geotextiles—polypropylene (PP) and polyester (PET)—subjected to natural weathering for up to 36 months. The materials were analyzed using mechanical tests (tensile strength, puncture resistance), thermal methods (TGA, DSC, and DMA), and scanning electron microscopy (SEM) to assess degradation in their physical, mechanical, and microstructural properties. Results showed significantly higher degradation in the PP geotextile compared with PET, with up to 84% loss in tensile strength after 36 months. The PET geotextile retained more than 50% of its strength, not reaching the 50% degradation threshold within the study period. Thermal analyses confirmed changes in molecular structure, with PP showing a more pronounced loss of thermal stability. SEM images further supported these findings, revealing greater fiber damage in PP. The findings highlight the superior performance of PET geotextiles under long‐term environmental exposure, supporting their selection in applications requiring enhanced durability.
- 1 January 2026
- Published by Wiley in International Journal of Polymer Science
- Vol. 2026 (1) , 8006062
Open AccessDurability of Nonwoven Geotextile (PP and PET) Under Natural Weathering: A Comprehensive Evaluation Using Thermal, Mechanical, and Microstructural Analysis
This study evaluates the long‐term durability of two commercial nonwoven geotextiles—polypropylene (PP) and polyester (PET)—subjected to natural weathering for up to 36 months. The materials were analyzed using mechanical tests (tensile strength, puncture resistance), thermal methods (TGA, DSC, and DMA), and scanning electron microscopy (SEM) to assess degradation in their physical, mechanical, and microstructural properties. Results showed significantly higher degradation in the PP geotextile compared with PET, with up to 84% loss in tensile strength after 36 months. The PET geotextile retained more than 50% of its strength, not reaching the 50% degradation threshold within the study period. Thermal analyses confirmed changes in molecular structure, with PP showing a more pronounced loss of thermal stability. SEM images further supported these findings, revealing greater fiber damage in PP. The findings highlight the superior performance of PET geotextiles under long‐term environmental exposure, supporting their selection in applications requiring enhanced durability.
- 22 April 2025
- Published by Springer Nature in International Journal of Geosynthetics and Ground Engineering
- Vol. 11 (3) , 1-12
Colored HDPE Textured Geomembranes Exposed to UV: Laboratory Insights into Material Degradation
- 22 April 2025
- Published by Springer Nature in International Journal of Geosynthetics and Ground Engineering
- Vol. 11 (3) , 1-12
Colored HDPE Textured Geomembranes Exposed to UV: Laboratory Insights into Material Degradation
- 31 January 2025
- Published by Emerald Publishing in Geosynthetics International
- Vol. 32 (1) , 169-179
Natural weathering effects of nonwoven geotextile exposed to different climate conditions
Humidity, air temperature, rainfall and solar radiation all contribute to the weathering of geosynthetics. Over time, their useful life can be affected and changes in properties can be observed, which affects the performance of these materials. As geosynthetics durability analyses must encompass each work condition, assessing the climate effects is essential for design purposes. This study exposed a nonwoven needle-punched poly(ethylene) terephthalate geotextile to natural weathering in three Brazilian cities (different exogenous environments) for 18 months. Mechanical tests were conducted to evaluate the geotextile changes due to weathering. This was demonstrated by the results: exposure to weather leads to the deterioration of the geotextile mechanical properties and increased stiffness. After four months, the tensile strength fell by half, while the deformation needed more than 12 months to have this same reduction; ultraviolet radiation intensity was the most effective weathering condition in the field; humidity and rainfall can affect the stiffness of geotextiles; the impact of accumulated climate factors gradually showed a convergence in the response of geotextile to weathering. Thus, this work highlights the need to evaluate the climate conditions in each location to understand the material's behavior on the exposure time.
- 31 January 2025
- Published by Emerald Publishing in Geosynthetics International
- Vol. 32 (1) , 169-179
Natural weathering effects of nonwoven geotextile exposed to different climate conditions
Humidity, air temperature, rainfall and solar radiation all contribute to the weathering of geosynthetics. Over time, their useful life can be affected and changes in properties can be observed, which affects the performance of these materials. As geosynthetics durability analyses must encompass each work condition, assessing the climate effects is essential for design purposes. This study exposed a nonwoven needle-punched poly(ethylene) terephthalate geotextile to natural weathering in three Brazilian cities (different exogenous environments) for 18 months. Mechanical tests were conducted to evaluate the geotextile changes due to weathering. This was demonstrated by the results: exposure to weather leads to the deterioration of the geotextile mechanical properties and increased stiffness. After four months, the tensile strength fell by half, while the deformation needed more than 12 months to have this same reduction; ultraviolet radiation intensity was the most effective weathering condition in the field; humidity and rainfall can affect the stiffness of geotextiles; the impact of accumulated climate factors gradually showed a convergence in the response of geotextile to weathering. Thus, this work highlights the need to evaluate the climate conditions in each location to understand the material's behavior on the exposure time.
- 29 January 2025
- Published by Emerald Publishing in Geosynthetics International
- Vol. 32 (6) , 808-817
Natural weathering effects on white, green, and black HDPE textured GMs
This study investigates the degradation of textured High-Density Polyethene (HDPE) geomembranes (GMs) subjected to natural weathering for 8.5 to 10.5 years. The GMs, denoted as GM-W/B (white and black), GM-G (green) and GM-B (black), had a nominal thickness of 1.00 mm and were manufactured using a flat die process with texture on both surfaces. Standard Oxidation Induction Time (Std-OIT) tests and Thermogravimetric Analysis (TG/DTG) were performed to assess the antioxidant depletion and thermal decomposition. Additionally, degradation due to Ultraviolet (UV) radiation and environmental agents was assessed through retained physical and mechanical properties, including the Melt Flow Index (MFI) measured under various loading conditions. Antioxidant depletion and TG/DTG analyses indicated that environmental exposure compromised the thermal stability of these GMs. Among the tested GMs, GM-W/B exhibited the greatest reduction in both Std-OIT and MFI, followed by GM-G and GM-B, suggesting a direct correlation between these properties. While GM-B appeared to be still in the antioxidant depletion stage (Stage I), GM-W/B and GM-G showed signs of degradation beyond Stage I. This study provides insights into the degradation of textured HDPE GMs in the face of weathering exposure effects and the durability of colored HDPE GMs.
- 29 January 2025
- Published by Emerald Publishing in Geosynthetics International
- Vol. 32 (6) , 808-817
Natural weathering effects on white, green, and black HDPE textured GMs
This study investigates the degradation of textured High-Density Polyethene (HDPE) geomembranes (GMs) subjected to natural weathering for 8.5 to 10.5 years. The GMs, denoted as GM-W/B (white and black), GM-G (green) and GM-B (black), had a nominal thickness of 1.00 mm and were manufactured using a flat die process with texture on both surfaces. Standard Oxidation Induction Time (Std-OIT) tests and Thermogravimetric Analysis (TG/DTG) were performed to assess the antioxidant depletion and thermal decomposition. Additionally, degradation due to Ultraviolet (UV) radiation and environmental agents was assessed through retained physical and mechanical properties, including the Melt Flow Index (MFI) measured under various loading conditions. Antioxidant depletion and TG/DTG analyses indicated that environmental exposure compromised the thermal stability of these GMs. Among the tested GMs, GM-W/B exhibited the greatest reduction in both Std-OIT and MFI, followed by GM-G and GM-B, suggesting a direct correlation between these properties. While GM-B appeared to be still in the antioxidant depletion stage (Stage I), GM-W/B and GM-G showed signs of degradation beyond Stage I. This study provides insights into the degradation of textured HDPE GMs in the face of weathering exposure effects and the durability of colored HDPE GMs.
- Open Access
Mechanical and Thermoanalytical Study of Polypropylene Geomats Exposed in the Field and the Laboratory
A Hydroelectric Power Plant (HPP) presents erosion problems on reservoir slopes and margins. Geomats are a biotechnical composite technology increasingly used to protect soils against erosion. Survivability or durability of geomats is essential for successful application. This work analyses the degradation of geomats exposed in the field for more than six years. These geomats were used as erosion-control treatment in a slope at HPP Simplício in Brazil. The degradation of the geomats in the laboratory was also analysed through exposure in a UV ageing chamber for 500 h and 1000 h. Degradation was quantitatively evaluated by testing the tensile strength of the geomat wires and thermal tests such as thermogravimetry (TG) and differential scanning calorimetry (DSC). The results showed that the geomat wires exposed in the field had a greater decrease in resistance compared to the samples exposed in the laboratory. In the samples collected in the field, it could be observed that the degradation of the virgin sample occurred earlier than in the exposed samples, contrary to what was observed in the TG tests carried out with the samples exposed in the laboratory. The DSC analysis showed that the samples had similar behaviours for the melting peaks. This evaluation of the wires of the geomats was presented as an alternative to analysing the tensile strengths of discontinuous geosynthetic materials such as the geomats.
Open AccessMechanical and Thermoanalytical Study of Polypropylene Geomats Exposed in the Field and the Laboratory
A Hydroelectric Power Plant (HPP) presents erosion problems on reservoir slopes and margins. Geomats are a biotechnical composite technology increasingly used to protect soils against erosion. Survivability or durability of geomats is essential for successful application. This work analyses the degradation of geomats exposed in the field for more than six years. These geomats were used as erosion-control treatment in a slope at HPP Simplício in Brazil. The degradation of the geomats in the laboratory was also analysed through exposure in a UV ageing chamber for 500 h and 1000 h. Degradation was quantitatively evaluated by testing the tensile strength of the geomat wires and thermal tests such as thermogravimetry (TG) and differential scanning calorimetry (DSC). The results showed that the geomat wires exposed in the field had a greater decrease in resistance compared to the samples exposed in the laboratory. In the samples collected in the field, it could be observed that the degradation of the virgin sample occurred earlier than in the exposed samples, contrary to what was observed in the TG tests carried out with the samples exposed in the laboratory. The DSC analysis showed that the samples had similar behaviours for the melting peaks. This evaluation of the wires of the geomats was presented as an alternative to analysing the tensile strengths of discontinuous geosynthetic materials such as the geomats.
- Open Access
Accelerated Aging Ultraviolet of a PET Nonwoven Geotextile and Thermoanalytical Evaluation
Nonwoven geotextiles are geosynthetic products that are highly susceptible to ultraviolet degradation because light can reach a large area of the material due to its fiber arrangement. Even with additives, which delay the degradation process, material decomposition still occurs, and therefore the product’s long-term durability can be affected. In this paper, the mechanical and thermal behavior of a commercial nonwoven polyester geotextile subjected to accelerated ultraviolet aging tests were evaluated. The deterioration was evaluated by comparing the physical properties (mass per unit area, thickness, and tensile strength) and thermal behavior (thermogravimetry—TG, thermomechanical analysis—TMA, and differential scanning calorimetry—DSC) before and after exposure times of 500 h and 1000 h. The results showed that the ultraviolet aging tests induced some damage in the polyester fibers, leading to the deterioration of their tensile strength. For 1000 h of exposure, in which the reduction was larger, scanning electron microscopy (SEM) found some superficial disruption of the fibers, indicative of damage. TG and DSC could not capture the effects of UV radiation on polymer degradation, unlike TMA. This latter technique was effective in showing the differences between specimens before and after UV exposure.
Open AccessAccelerated Aging Ultraviolet of a PET Nonwoven Geotextile and Thermoanalytical Evaluation
Nonwoven geotextiles are geosynthetic products that are highly susceptible to ultraviolet degradation because light can reach a large area of the material due to its fiber arrangement. Even with additives, which delay the degradation process, material decomposition still occurs, and therefore the product’s long-term durability can be affected. In this paper, the mechanical and thermal behavior of a commercial nonwoven polyester geotextile subjected to accelerated ultraviolet aging tests were evaluated. The deterioration was evaluated by comparing the physical properties (mass per unit area, thickness, and tensile strength) and thermal behavior (thermogravimetry—TG, thermomechanical analysis—TMA, and differential scanning calorimetry—DSC) before and after exposure times of 500 h and 1000 h. The results showed that the ultraviolet aging tests induced some damage in the polyester fibers, leading to the deterioration of their tensile strength. For 1000 h of exposure, in which the reduction was larger, scanning electron microscopy (SEM) found some superficial disruption of the fibers, indicative of damage. TG and DSC could not capture the effects of UV radiation on polymer degradation, unlike TMA. This latter technique was effective in showing the differences between specimens before and after UV exposure.
- Open Access
- 22 September 2021
- Published by Elsevier in Case Studies in Chemical and Environmental Engineering
- Vol. 4, 100133
Environmental protection liner in a biodegradable waste pond: A case study
- 22 September 2021
- Published by Elsevier in Case Studies in Chemical and Environmental Engineering
- Vol. 4, 100133
Open AccessEnvironmental protection liner in a biodegradable waste pond: A case study
- Open Access
- 13 August 2021
- Published by MDPI AG in Construction Materials
- Vol. 1 (2) , 122-133
Environmental Protection with HDPE Geomembranes in Mining Facility Constructions
The present work evaluated two high-density polyethylene (HDPE) geomembranes exhumed from mining facility constructions in Brazil. The MIN sample was exhumed from a pond for water use for the iron ore process after 7.92 years of exposure. The MIN2 sample was exhumed from a spillway channel of a ferronickel tailing dam after 10.08 years of service. The physical evaluations showed high depletion for antioxidants that work in the temperature range of 200 °C. The samples presented brittle tensile behavior and had similar behaviors between stress cracking and tensile. Low tensile elongation values and low-stress crack resistance were noted. The MIN2 sample presented a higher melt flow index (MFI) value and lower stress crack resistance. Thermogravimetric curves (TG) under synthetic air purge gas evaluation showed that both samples presented a similar behavior during the evaluation but had several mass losses. The results showed that exothermic and endothermic events occurred with loss of mass and showed no combustion events in the differential thermal analysis (DTA) curve evaluation. Differential scanning calorimetry (DSC) analysis showed no changes in the samples’ behavior. Thus, the results of tensile, stress cracking, and viscosity properties can demonstrate that changes in polymer structure occurred after field exposures.
- 13 August 2021
- Published by MDPI AG in Construction Materials
- Vol. 1 (2) , 122-133
Open AccessEnvironmental Protection with HDPE Geomembranes in Mining Facility Constructions
The present work evaluated two high-density polyethylene (HDPE) geomembranes exhumed from mining facility constructions in Brazil. The MIN sample was exhumed from a pond for water use for the iron ore process after 7.92 years of exposure. The MIN2 sample was exhumed from a spillway channel of a ferronickel tailing dam after 10.08 years of service. The physical evaluations showed high depletion for antioxidants that work in the temperature range of 200 °C. The samples presented brittle tensile behavior and had similar behaviors between stress cracking and tensile. Low tensile elongation values and low-stress crack resistance were noted. The MIN2 sample presented a higher melt flow index (MFI) value and lower stress crack resistance. Thermogravimetric curves (TG) under synthetic air purge gas evaluation showed that both samples presented a similar behavior during the evaluation but had several mass losses. The results showed that exothermic and endothermic events occurred with loss of mass and showed no combustion events in the differential thermal analysis (DTA) curve evaluation. Differential scanning calorimetry (DSC) analysis showed no changes in the samples’ behavior. Thus, the results of tensile, stress cracking, and viscosity properties can demonstrate that changes in polymer structure occurred after field exposures.
- Open Access
Laboratory Study of the Ultraviolet Radiation Effect on an HDPE Geomembrane
High-density polyethylene (HDPE) geomembranes are polymeric geosynthetic materials usually applied as a liner in environmental facilities due to their good mechanical properties, good welding conditions, and excellent chemical resistance. A geomembrane’s field performance is affected by different conditions and exposures, including ultraviolet radiation, thermal and oxidative exposure, and chemical contact. This article presents an experimental study with a 1.0 mm-thick HDPE virgin geomembrane exposed by the Xenon arc weatherometer for 2160 h and the ultraviolet fluorescent weatherometer for 8760 h to understand the geomembrane’s behavior under ultraviolet exposure. The evaluation was performed using the melt flow index (MFI) test, oxidative-induction time (OIT) tests, tensile test, differential scanning calorimetry (DSC) analysis, and Fourier transform infrared spectroscopy (FTIR) analysis. The sample exposed in the Xenon arc equipment showed a tendency to increase the MFI values during the exposure time. This upward trend may indicate morphological changes in the polymer. The tensile behavior analysis showed a tendency of the sample to lose ductility, without showing brittle behavior. The samples’ OIT test results under both device exposures showed faster antioxidant depletion for the standard OIT test than the high-pressure OIT test. The DSC and FTIR analyses did not demonstrate the polymer’s changes.
Open AccessLaboratory Study of the Ultraviolet Radiation Effect on an HDPE Geomembrane
High-density polyethylene (HDPE) geomembranes are polymeric geosynthetic materials usually applied as a liner in environmental facilities due to their good mechanical properties, good welding conditions, and excellent chemical resistance. A geomembrane’s field performance is affected by different conditions and exposures, including ultraviolet radiation, thermal and oxidative exposure, and chemical contact. This article presents an experimental study with a 1.0 mm-thick HDPE virgin geomembrane exposed by the Xenon arc weatherometer for 2160 h and the ultraviolet fluorescent weatherometer for 8760 h to understand the geomembrane’s behavior under ultraviolet exposure. The evaluation was performed using the melt flow index (MFI) test, oxidative-induction time (OIT) tests, tensile test, differential scanning calorimetry (DSC) analysis, and Fourier transform infrared spectroscopy (FTIR) analysis. The sample exposed in the Xenon arc equipment showed a tendency to increase the MFI values during the exposure time. This upward trend may indicate morphological changes in the polymer. The tensile behavior analysis showed a tendency of the sample to lose ductility, without showing brittle behavior. The samples’ OIT test results under both device exposures showed faster antioxidant depletion for the standard OIT test than the high-pressure OIT test. The DSC and FTIR analyses did not demonstrate the polymer’s changes.
- Open Access
Geomats Used to Control Erosion on Reservoir Margins in Brazilian Hydroelectric Power Plants
Erosion on reservoir margins causes losses in the production of energy in Hydroelectric Power Plants (HPPs), making it necessary to implement control techniques that ensure the reduction in sediment deposits inside reservoirs. Among these techniques, geomats (geosynthetic erosion mats) are widely used to control erosion processes in slopes and watercourses. This material protects the margins both in the short and long term, contributing to strengthening the vegetation’s roots developed in the erosion areas. This paper studies the performance of geomats (with and without sack gabion) installed in six margin sections distributed in three experimental units of the Brazilian HPPs called Porto Colômbia and Volta Grande. The geomat performance was evaluated over four years of monitoring through a qualitative evaluation matrix and differential bathymetry. The influence of ultraviolet (UV) radiation on the degradation of geomats installed in each section (natural conditions), as well as on geomat ultraviolet-aging samples in the laboratory (accelerated conditions), was also evaluated using differential scanning calorimetry (DSC). The results showed no significant difference in performance between using the erosion control technique consisting only of geomats and the technique consisting of geomats and sack gabion. The highest bathymetric difference value obtained in the present study was 1.62 m in the experimental unit VG1, controlled with geomat without the application of sack gabion on the margin.
Open AccessGeomats Used to Control Erosion on Reservoir Margins in Brazilian Hydroelectric Power Plants
Erosion on reservoir margins causes losses in the production of energy in Hydroelectric Power Plants (HPPs), making it necessary to implement control techniques that ensure the reduction in sediment deposits inside reservoirs. Among these techniques, geomats (geosynthetic erosion mats) are widely used to control erosion processes in slopes and watercourses. This material protects the margins both in the short and long term, contributing to strengthening the vegetation’s roots developed in the erosion areas. This paper studies the performance of geomats (with and without sack gabion) installed in six margin sections distributed in three experimental units of the Brazilian HPPs called Porto Colômbia and Volta Grande. The geomat performance was evaluated over four years of monitoring through a qualitative evaluation matrix and differential bathymetry. The influence of ultraviolet (UV) radiation on the degradation of geomats installed in each section (natural conditions), as well as on geomat ultraviolet-aging samples in the laboratory (accelerated conditions), was also evaluated using differential scanning calorimetry (DSC). The results showed no significant difference in performance between using the erosion control technique consisting only of geomats and the technique consisting of geomats and sack gabion. The highest bathymetric difference value obtained in the present study was 1.62 m in the experimental unit VG1, controlled with geomat without the application of sack gabion on the margin.