NPNatalia B. Pugacheva

Natalia B. Pugacheva

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


Natalia B. Pugacheva has a total of 110 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    The effect of laser processing on the structure and microhardness of a ZrO2-based thermal barrier coating

    by N. B. Pugacheva, A. E. Trokhacheva, T. M. Kryuchkova, I. S. Bakhteev

    The paper studies the effect of laser processing conditions at powers ranging between 90 and 150 W on a thermal barrier coating consisting of an Y2O3-stabilized ZrO2 outer layer and a NiCrAl metal substrate. The coating is sprayed on the 20Kh4FA steel. Scanning electron microscopy, energy dispersive analysis of the chemical composition of the coating, profilometry, and surface microhardness study were used in the research. The study of the structure, chemical element distribution, microhardness, and surface roughness of the thermal barrier coating has revealed that the laser processing of the surface causes partial melting of the ceramic layer to different depths, depending on laser power. A radiation power of 100 W proves to have the best effect on the state of the ceramic outer layer of the coating; namely, the hardness reaches 953 HV 0.030, there are no Cr, Ni or Fe on the surface, this being indicative of the soundness of the ZrO2+Y2O3 layer. The surface roughness of this coating is the lowest, 7.5 µm. When the processing power exceeds 100 W, there are Cr, Ni, and Fe on the surface; this indicates the presence of defects in the coating and has a detrimental effect on its thermal barrier properties. Besides, a relation has been found between the microhardness and thickness of the preserved metal substrate; namely, the microhardness increases as the substrate thickness decreases.

  • Open Access

    MICROSTRUCTURE, RESIDUAL STRESSES, TEXTURE, AND MECHANICAL PROPERTIES OF A WELDED JOINT IN VT1-0 ALLOY SHEETS

    by N. B. Pugacheva, S. M. Zadvorkin

    The grain structure, microstrain distribution, crystallographic texture and residual stresses in a CO2 laser welded joint of VT1-0 alloy sheets (technical titanium) are studied by EBSD and X-ray diffraction analysis. The mechanical properties of the welded joint are determined. It is shown that the weld structure is represented by differently directed large laths of the α-phase. The metal in the heat-affected zones is characterized by a mixed structure resulting from the polymorphic β→α transformation in the form of packets of secondary α-phase plates near the weld and polyhedral α-grains near the base metal. Multicomponent textures have been detected in all the zones of the welded joint. This creates prerequisites for decreased anisotropy of strength properties, which is typical of hexagonal crystals. The strength of the welded joint proves to be significantly higher than that of the base metal; namely, the ultimate strength of the joint is 660 MPa, and that of the base material is 500 MPa. The heat-affected zone is the most deformed zone in the welded joint, the share of deformed grains reaches 44%, and residual stresses do not exceed 10% of the yield strength.

  • Structural features and tribological properties of multilayer high-temperature plasma coatings

    by Natalia Pugacheva, Tatyana Bykova, Vitaly Sirosh, Alexey Makarov

    Introduction. Multilayer high-temperature coatings obtained using plasma spraying, are studied. The combination of layers of different chemical and phase compositions made it possible to increase wear resistance by 1.5–2.0 times. The purpose of this work is to study the influence of the chemical composition of sprayed coatings on the phase composition, structure, micromechanical and tribological characteristics under conditions of dry sliding friction of surface layers. Materials and methods of research. Coatings A and B consist of sequentially sprayed layers. The first and second layers were sprayed in a reducing atmosphere: the first layer was a heat-resistant self-fluxing powder of two systems: 1 – Fe-Cr-Si-Mn-B-C for coating A and 2 – Fe-Ni-Si-Mn-B-C for coating B; the second layer was a mixture of self-fluxing powder with iron powder in a 1:1 ratio. The third layer was obtained by spraying iron powder in an oxidizing atmosphere to form a metal oxide coating. To create a layer of scale on the surface, coated specimens were subjected to high-temperature annealing at a temperature of 1,000 ℃. The chemical composition and nature of the distribution of elements over the thickness of the coatings were determined by micro-X-ray spectral analysis using a TWSCAN scanning electron microscope with an Oxford energy-dispersive attachment. Microhardness and micromechanical properties were studied using an instrumental microhardness tester of the Fischerscope HM2000 XYm system at a load of 0.980 N. Determination of tribological properties was carried out on a laboratory installation using the “finger-disc” scheme at loads of 30, 75, 100 and 130 N. To measure roughness parameters and obtain 3-D profilometry of surfaces after testing, a non-contact profilometer-profiler Optical profiling system Veeco WYKO NT 1100 was used. Results and discussion. Metallographic studies have shown that the formed multilayer coatings consist of an internal metal layer and an external oxide layer with a total thickness of the entire coating up to 800–850 μm. It is established that the first sprayed layer has the highest level of microhardness, which is due to the high-volume fraction of the strengthening phases contained in it (~ 95 %). It is shown that the coating A has increased wear resistance, which is expressed by minimal weight loss (~ 1.5 times less than that of the coating of the coatimg B), the friction coefficient was f = 0.3 for coating A and f = 0.4 for coating B. The study of wear surfaces has shown that for all selected test loads under sliding friction conditions, the coating of both compositions was preserved, even at a maximum load of 130 N.

  • Changes in the Structure of the Fe–Ni–Ti–C–B Composite during Hot Plastic Deformation

    by N. B. Pugacheva, T. M. Bykova, D. I. Kryuchkov

    The change in the structure and hardness of the Fe–Ni–Ti–C–B system composite, obtained by the method of self-propagating high-temperature synthesis (SHS), after hot plastic deformation under uniaxial compression conditions is studied. The matrix of the composite is a solid solution of Ni and Ti in a γ‑Fe crystal lattice, and the strengthening phases are TiC, TiB2, Fe2B, Ni3Ti, and NiTi. It is shown that during uniaxial compression upon heating, recrystallization processes occur in the metal matrix of the composite, which facilitates further deformation. It is found that, after compression at a temperature of 910°C and a pressure of 300 MPa, the true deformation of the composite is 0.37. In this case, in the central part of the sample in the region of compressive stresses, the ratio of deformed and recrystallized grains is approximately the same. On the lateral surface of the samples, in the zone of action of tensile stresses, microcracks with a depth of less than 0.2 mm appear in zones of the eutectic γ + Fe2B structure.


  • Open Access

    The effect of the stress state on the deformability of an aluminum matrix composite with 10 vol% SiC particle filler

    by D. I. Vichuzhanin, S. V. Smirnov, N. B. Pugacheva, A. V. Nesterenko, P. A. Polyakov

    The effect of the stress state on the deformability of an aluminum matrix composite with 10 vol% of SiC particles is studied by using the damage criterion. Backward extrusion of a standard cup-shaped part is used as an example. The process is simulated by the finite element method to evaluate the stress-strain state and damage. It has been found that, in order to make a high-quality product, it is necessary to carry out extrusion under all-round compression at near-solidus temperatures. A laboratory die was designed and manufactured for the experimental verification of the simulation results. The die is peculiar in that the value of compressive stresses can be controlled during deformation. The extrusion process yields a defect-free product. It has been revealed that heating to near-solidus temperature breaks the initial cellular structure of the composite under external loading.


  • Open Access

    Mechanical properties of an Fe–Ti–Ni–B–C SHS composite

    by N. B. Pugacheva, A. V. Nokhrina, E. I. Senaeva, R. A. Savrai

    The paper studies the structure, mechanical properties and wear resistance of a composite produced by self-propagating high-temperature synthesis (SHS) with an average chemical composition, wt%: 35.47 ± 1.5 Fe; 24.08 ± 1.4 Ti; 13.99 ± 0.5 Ni; 17.91 ± 0.4 B; 8.54 ± 0.5 C. Testing has revealed that the composite has wear resistance on a level with one of the Hardox 500 wear-resistant steels. The composite is characterized by a wide range of values of transverse bending strength Rbm30 from 200 to 800 MPa. Steel 40X shows a bending strength Rbm30 of 1590 MPa, and the values of this characteristic for the Hardox 500 steel range between 2970 and 3020 MPa. The composite has low impact strength values KCU = 0.02 MJ/m2, compared with KCU = 0.35 MJ/m2 for steel 40X and KCU = 1.59 MJ/m2 for Hardox 500. The Fe–Ni–Ti–C–B SHS composite should not be used for bending parts and those experiencing shock loads; however, it suits perfectly for protecting the surfaces of parts subject to intense abrasive wear.


  • Open Access

    Deformation of Al–Zn–Mg–Cu composite samples under nonstationary thermomechanical conditions

    by D. I. Kryuchkov, N. B. Pugacheva, T. M. Bykova

    Kryuchkov D. I., Pugacheva N. B., Bykova T. M. Deformation of Al–zn–mg–cu Composite Samples under Nonstationary Thermomechanical Conditions // Diagnostics, Resource and Mechanics of materials and structures.- 2023 - Iss. 6.


  • Open Access

    Application of microindentation to the evaluation of strain distribution over the section of extruded aluminum alloy bars

    by V. P. Shveikin, I. S. Kamantsev, N. B. Pugacheva, S. M. Zadvorkin, E. I. Senaeva, A. V. Razinkin, Kamensk-Uralsky Metallurgical Works Jsc, T. V. Maltseva, Ural Federal University, N. A. Kalinina, et al.

    The paper proposes to supplement the monitoring of strain uniformity over the cross-section of extruded aluminum alloy bars, based on the macro- and microstructure in the central part, at ½ radius, and in the surface zone in several cross-sections along the length of press products, with microindentation of these sections. For this purpose, the microstructure, the loading diagram, and the pattern of the distribution of micromechanical properties across the cross-section of extruded bars made of the AD33 and D16 aluminum alloys are comparatively analyzed. These alloys differ in that in one alloy, AD33, the alloying elements strengthen the aluminum-based solid solution without forming independent phases, and in the other, D16, they form strengthening intermetallic compounds Al2CuMg. The microhardness of the AD33 alloy is ~55 HV 0.1, that of the D16 alloy being 120 HV 0.1. The alloys differ in the distribution of micromechanical properties over both the transverse and longitudinal sections of the extruded bars. It has been found that maximum homogeneity is characteristic of the central part of the rods made of both alloys. The microindentation data correlate with the changes in the microstructure and the results of assessing the distribution of microstrains in the crystal lattice of an aluminum-based solid solution over the cross-section of extruded products by EBSD using recrystallization maps. This makes it possible to recommend the microindentation method for assessing the distribution of strains over the cross-section of extruded aluminum alloy bars.


  • Open Access

    Studying the plastic deformability of a Ni–Fe–Cr–Ti–B–C composite

    by N. B. Pugacheva, D. I. Vichuzhanin, Т. М. Bykova, I. S. Kamantsev

    Studying the Plastic Deformability of a Ni–fe–cr–ti–b–c Composite / N. B. Pugacheva, D. I. Vichuzhanin, Т. М. Bykova, I. S. Kamantsev // Diagnostics, Resource and Mechanics of materials and structures.- 2023 - Iss. 5.


  • Role of surface phenomena in deformation and fracture of gas turbine blades and stamping tools under intense mechanical and thermal loading

    by B. N. Guzanov, N. B. Pugacheva, E. Yu. Slukin, S. M. Nikiforova

    A study of the damageability of most parts and products of modern technology, operated under non-stationary thermal and mechanical loading, shows that their premature failure is mainly due to changes occurring in the near-surface thin layers of steels and alloys, where, first of all, plastic deformation processes proceed intensively, origin and accumulation of centers of destruction. The analysis performed shows that the magnitude of surface damage can be very large and largely depends on contact with the external environment, the degree of impact of which is determined by its aggressiveness, state of aggregation and force contact pressure. In such operating conditions, the task of creating reliable surface hardening systems is quite difficult and in most cases should be reduced to the development of a good protective coating for a particular alloy and a particular application. In order to maintain the calculated durability and reliability of the parts of the blade apparatus of gas turbine plants, the article proposes to use protective multilayer combined coatings applied to the contact surface using the thermal diffusion and plasma spraying methods. Under conditions of moderate temperatures and non-stationary mechanical loading, which is typical for hot-forming dies, in order to achieve high protective properties, thermal diffusion boride coatings are proposed, applied in coatings based on specially developed active pastes.