Benjamín Vargas-Arista
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Benjamín Vargas-Arista has a total of 36 co-authors. Here are the top co-authors by number of shared publications:
- Celso Eduardo Cruz-González
Centro de Ingenieria y Desarrollo Industrial
9 shared publications - Isidro Guzmán-Flores
Facultad de Sistemas, Universidad Autónoma de Coahuila, Saltillo, México
8 shared publications - Arturo Barba-Pingarrón
Centro de Ingeniería de Superficies y Acabados, Facultad de Ingeniería, Universidad Nacional Autónoma de México Ciudad Universitaria, Ciudad de México 04510, Mexico
2 shared publications - Everardo Efrén Granda Gutiérrez
Universidad Autónoma del Estado de México
2 shared publications - Saul Daniel Santillan Gutierrez
UNAM Campus Juriquilla, UNAM, Querétaro, Mexico
2 shared publications - Alberto Cuevas-Salgado
Tecnologico Nacional de Mexico, Instituto Tecnologico de Tlalnepantla
1 shared publication
Latest Publications
- 13 February 2023
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 32 (24) , 11275-11284
Mechanical and Fracture Behavior of Dissimilar Adhesive Joints, Dual Phase Steel/AA6061-T6, at Extreme Temperature
- 13 February 2023
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 32 (24) , 11275-11284
Mechanical and Fracture Behavior of Dissimilar Adhesive Joints, Dual Phase Steel/AA6061-T6, at Extreme Temperature
- Open Access
Corrosion Performance and Mechanical Strength in Aluminum 6061 Joints by Pulsed Gas Metal Arc Welding
In this paper, the analysis of electrochemical corrosion performance and mechanical strength of weld joints of aluminum 6061 in two-heat treatment conditions was performed. The joints were produced by gas metal arc welding in pulsed mode. The original material exhibited precipitates of and ” phases in a volume fraction (Vf) of 2.35%. When it was subjected to a solubilization process, these phases were present in a Vf = 2.97%. This increase is due to their change in shape and distribution in clusters within the aluminum matrix. After the welding process, the best sample in the solubilization condition reached 117 MPa, while the original material achieved 104 MPa, but all samples showed a fracture in the fusion zone. This is attributed to the heat input that produces high and low hardness zones along the heat-affected zone and the welding zone, respectively. Moreover, the change in microstructure and phase composition creates a galvanic couple, susceptible to electrochemical corrosion, which is more evident in the heat-affected zone than in the other weld regions, exhibiting uniform and localized corrosion, as was evident by electrochemical impedance spectroscopy. The heat from the welding process negatively affects the corrosion resistance, mainly in the heat-affected zone.Open AccessCorrosion Performance and Mechanical Strength in Aluminum 6061 Joints by Pulsed Gas Metal Arc Welding
In this paper, the analysis of electrochemical corrosion performance and mechanical strength of weld joints of aluminum 6061 in two-heat treatment conditions was performed. The joints were produced by gas metal arc welding in pulsed mode. The original material exhibited precipitates of and ” phases in a volume fraction (Vf) of 2.35%. When it was subjected to a solubilization process, these phases were present in a Vf = 2.97%. This increase is due to their change in shape and distribution in clusters within the aluminum matrix. After the welding process, the best sample in the solubilization condition reached 117 MPa, while the original material achieved 104 MPa, but all samples showed a fracture in the fusion zone. This is attributed to the heat input that produces high and low hardness zones along the heat-affected zone and the welding zone, respectively. Moreover, the change in microstructure and phase composition creates a galvanic couple, susceptible to electrochemical corrosion, which is more evident in the heat-affected zone than in the other weld regions, exhibiting uniform and localized corrosion, as was evident by electrochemical impedance spectroscopy. The heat from the welding process negatively affects the corrosion resistance, mainly in the heat-affected zone. - 13 July 2022
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 121 (7-8) , 4929-4940
Effect of curing post-treatment time on mechanical properties and stress distribution of adhesively bonded dissimilar steel-aluminum joints
- 13 July 2022
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 121 (7-8) , 4929-4940
Effect of curing post-treatment time on mechanical properties and stress distribution of adhesively bonded dissimilar steel-aluminum joints
- Open Access
- 30 June 2022
- Published by Editorial CSIC in Revista de Metalurgia
- Vol. 58 (2) , e218
On the application of the forming limit diagrams for quality control of blanks for wheelbarrow of ASTM A1008 carbon steel
The effectivity of the forming limit diagrams in manufacturing wheelbarrow by deep-drawing is shown because of the high material scrap rate which reduces productivity. Several chemical, mechanical testing and microstructural analysis were performed to examine sheet quality and their impact on these diagrams. Chemical analysis revealed that Steel 1 and Steel 3 sheets fulfilled the specification without assuring adequate forming process. However, the higher titanium content of Steel 2 improved its formability since it promoted the formation of fine precipitates, thus refining the grain size. This steel had the highest ASTM grain size number G (9.11), which is the lowest average grain size (13 µm) compared to the other steels, which had G values in the range 8.7 to 9.11. Moreover, Steel 2 sheets had the greatest plastic strain ratio (rm = 1.80), the highest strain-hardening exponent (n = 0.250), the lowest anisotropy ∆r = 0.31), yielding better results in deep-drawing strain distribution, the highest forming limit strain (28%) and the highest uniform elongation zone, favoring that failure sites did not occur.
- 30 June 2022
- Published by Editorial CSIC in Revista de Metalurgia
- Vol. 58 (2) , e218
Open AccessOn the application of the forming limit diagrams for quality control of blanks for wheelbarrow of ASTM A1008 carbon steel
The effectivity of the forming limit diagrams in manufacturing wheelbarrow by deep-drawing is shown because of the high material scrap rate which reduces productivity. Several chemical, mechanical testing and microstructural analysis were performed to examine sheet quality and their impact on these diagrams. Chemical analysis revealed that Steel 1 and Steel 3 sheets fulfilled the specification without assuring adequate forming process. However, the higher titanium content of Steel 2 improved its formability since it promoted the formation of fine precipitates, thus refining the grain size. This steel had the highest ASTM grain size number G (9.11), which is the lowest average grain size (13 µm) compared to the other steels, which had G values in the range 8.7 to 9.11. Moreover, Steel 2 sheets had the greatest plastic strain ratio (rm = 1.80), the highest strain-hardening exponent (n = 0.250), the lowest anisotropy ∆r = 0.31), yielding better results in deep-drawing strain distribution, the highest forming limit strain (28%) and the highest uniform elongation zone, favoring that failure sites did not occur.
- 3 July 2021
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 116 (5-6) , 1751-1761
On the manufacture of naval propellers by using self-hardening sand molds made by robotic arms
- 3 July 2021
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 116 (5-6) , 1751-1761
On the manufacture of naval propellers by using self-hardening sand molds made by robotic arms
- 8 February 2021
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 113 (5-6) , 1535-1546
On the effect of Qnet on compressive residual stresses and ductile toughness of dissimilar HAZ in robotic GMAW joints between A572-50 and A36 steels
- 8 February 2021
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 113 (5-6) , 1535-1546
On the effect of Qnet on compressive residual stresses and ductile toughness of dissimilar HAZ in robotic GMAW joints between A572-50 and A36 steels
- 22 October 2020
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 35 (11) , 1170-1184
Experimental and finite element analysis of a damaged API5L X52 pipeline with longitudinal crack repaired by adhesively bonded metallic patch
An alternative of repairment by means of Lord DC-80 adhesive and metallic patch on two API5L-X52 pipes steel with 10 mm in thickness, 122 mm outside diameter and 750 mm length, which were damaged by mechanically longitudinal crack with 5 mm depth is presented. Repaired pipes were submitted to pressure testing (0.68–9.8 MPa) and 3D-FEM was used to calculate the Von Mises stress and strain. Results indicated that measured strain was smaller than the allowed strain, then no yielding occurred. Pressure tests revealed that leakage occurred at 9.8 MPa, where seals failed but not the pipe or repaired assembly. FEM results showed that the adhesive served to join the steel patch and pipeline, which operated as a component that lead to lower stresses regarding to the internal pressure in pipeline. The Von Mises stress values increased with the increment of pressure resulting that for 9.8 MPa, the greatest stress was reached at both edges of the API-X52 piping, followed by metallic patch and finally, the adhesive with the lowest values. Cracked pipelines within the analyzed dimension sizes did not present integrity problems and it did not fail. This kind of repairment could be safely used for pipes that present external defects.
- 22 October 2020
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 35 (11) , 1170-1184
Experimental and finite element analysis of a damaged API5L X52 pipeline with longitudinal crack repaired by adhesively bonded metallic patch
An alternative of repairment by means of Lord DC-80 adhesive and metallic patch on two API5L-X52 pipes steel with 10 mm in thickness, 122 mm outside diameter and 750 mm length, which were damaged by mechanically longitudinal crack with 5 mm depth is presented. Repaired pipes were submitted to pressure testing (0.68–9.8 MPa) and 3D-FEM was used to calculate the Von Mises stress and strain. Results indicated that measured strain was smaller than the allowed strain, then no yielding occurred. Pressure tests revealed that leakage occurred at 9.8 MPa, where seals failed but not the pipe or repaired assembly. FEM results showed that the adhesive served to join the steel patch and pipeline, which operated as a component that lead to lower stresses regarding to the internal pressure in pipeline. The Von Mises stress values increased with the increment of pressure resulting that for 9.8 MPa, the greatest stress was reached at both edges of the API-X52 piping, followed by metallic patch and finally, the adhesive with the lowest values. Cracked pipelines within the analyzed dimension sizes did not present integrity problems and it did not fail. This kind of repairment could be safely used for pipes that present external defects.
- Open Access
- 30 June 2019
- Published by Editorial CSIC in Revista de Metalurgia
- Vol. 55 (2) , e143
Influencia del calor de entrada sobre el comportamiento a la fractura dúctil Charpy de la ZAC recalentada en uniones soldadas multipasos GMAW en acero HSLA utilizando análisis fractográfico digital
El efecto del calor de entrada sobre el comportamiento a la fractura de la zona afectada por el calor recalentada en uniones soldadas multipasos de acero ASTM A633 fue evaluado mediante la prueba de impacto, fractografía, microscopia electrónica de barrido y procesamiento digital de imágenes. Los resultados de impacto indicaron una reducción en la energía Charpy como función de la velocidad de alimentación de alambre, lo cual se confirmó mediante fractografias después del procesamiento digital de imágenes que mostraron una reducción en la fracción volumétrica de microhoyuelos en la fractura dúctil acompañada del incremento en la rapidez de alimentación, favoreciendo la fractura frágil con facetas de clivaje transgranular conteniendo marcas de rio. La fracción mínima de microhuecos y el tamaño más largo de facetas mostrando un mayor número de patrones de rio fueron encontrados a la máxima rapidez de alimentación de 200 mm·s-1. La microestructura heterogénea de la zona afectada por el calor formada por una red de ferrita acicular fina rodeada por ferrita aliotromorfica mostro que el incremento en la rapidez de alimentación indujo un refinamiento de grano por la formación de ferrita acicular, lo cual se relacionó con el deterioro de la energía absorbida y fractura frágil.
- 30 June 2019
- Published by Editorial CSIC in Revista de Metalurgia
- Vol. 55 (2) , e143
Open AccessInfluencia del calor de entrada sobre el comportamiento a la fractura dúctil Charpy de la ZAC recalentada en uniones soldadas multipasos GMAW en acero HSLA utilizando análisis fractográfico digital
El efecto del calor de entrada sobre el comportamiento a la fractura de la zona afectada por el calor recalentada en uniones soldadas multipasos de acero ASTM A633 fue evaluado mediante la prueba de impacto, fractografía, microscopia electrónica de barrido y procesamiento digital de imágenes. Los resultados de impacto indicaron una reducción en la energía Charpy como función de la velocidad de alimentación de alambre, lo cual se confirmó mediante fractografias después del procesamiento digital de imágenes que mostraron una reducción en la fracción volumétrica de microhoyuelos en la fractura dúctil acompañada del incremento en la rapidez de alimentación, favoreciendo la fractura frágil con facetas de clivaje transgranular conteniendo marcas de rio. La fracción mínima de microhuecos y el tamaño más largo de facetas mostrando un mayor número de patrones de rio fueron encontrados a la máxima rapidez de alimentación de 200 mm·s-1. La microestructura heterogénea de la zona afectada por el calor formada por una red de ferrita acicular fina rodeada por ferrita aliotromorfica mostro que el incremento en la rapidez de alimentación indujo un refinamiento de grano por la formación de ferrita acicular, lo cual se relacionó con el deterioro de la energía absorbida y fractura frágil.
- Open Access
- 6 March 2019
- Published by Gruppo Italiano Frattura in Fracture and Structural Integrity
- Vol. 13 (48) , 530-544
Fatigue strength evaluation and fracture behavior of joined dual phase steel/AA6061-T6 aluminum alloy
The fatigue strength evaluation and fracture behavior for a dual phase steel-AA6061-T6 bonded joints with three different adhesives (DC-80, Betamate 120 and MP55420) are presented in this paper. Single lap shear tests were used to determine maximum shear loads, for the single lap shear testing for 5.0 mm overlap length were 2 to 3.5 times higher in comparison to the 12.7 mm overlap length specimens. The results for the strain measurement revealed that higher strain-stress were developed in the 6061-T6 aluminum alloy adherend and in all cases they were lower than the adherends yield strength. Fatigue testing was carried out at 30, 50 and 70 % of the maximum shear load, 0.1 of reversibility load ratio (R) and 30 Hz of frequency. After testing, Basquin and Wholer graphs were built for each adhesive at 12.7 and 50.0 mm of overlap length. The results suggested that at higher overlapping, the cyclic maximum load increased. Additionally, the maximum fatigue loading at 10^6 cycles for MP55420 adhesive was 1.3 kN for an overlapping of 12.7 mm and 2.9 kN for 50 mm. For DC80 adhesive was 1.75 kN for overlapping 12.7 mm and 4.8 kN for 50 mm. Finally, for the Betamate 120 adhesive was 1.8 kN for 12.7 mm of overlapping and 6 kN for 50 mm. The post-fracture visual inspection revealed that MP55420 and Betamate 120 adhesives had a cohesive failure, while the DC-80 showed cohesive-adhesive failure. Additionally, the scanning electron microscopy evaluation on the spew fillet revealed resolved striations and a network of small micro-dimples for the Betamate 120 and MP55420 adhesives. On the other hand, DC-80 adhesive exhibited notable facet fragile failure that was confirmed by the shape of stress-strain plot with straight line from the origin to the point of fracture.
- 6 March 2019
- Published by Gruppo Italiano Frattura in Fracture and Structural Integrity
- Vol. 13 (48) , 530-544
Open AccessFatigue strength evaluation and fracture behavior of joined dual phase steel/AA6061-T6 aluminum alloy
The fatigue strength evaluation and fracture behavior for a dual phase steel-AA6061-T6 bonded joints with three different adhesives (DC-80, Betamate 120 and MP55420) are presented in this paper. Single lap shear tests were used to determine maximum shear loads, for the single lap shear testing for 5.0 mm overlap length were 2 to 3.5 times higher in comparison to the 12.7 mm overlap length specimens. The results for the strain measurement revealed that higher strain-stress were developed in the 6061-T6 aluminum alloy adherend and in all cases they were lower than the adherends yield strength. Fatigue testing was carried out at 30, 50 and 70 % of the maximum shear load, 0.1 of reversibility load ratio (R) and 30 Hz of frequency. After testing, Basquin and Wholer graphs were built for each adhesive at 12.7 and 50.0 mm of overlap length. The results suggested that at higher overlapping, the cyclic maximum load increased. Additionally, the maximum fatigue loading at 10^6 cycles for MP55420 adhesive was 1.3 kN for an overlapping of 12.7 mm and 2.9 kN for 50 mm. For DC80 adhesive was 1.75 kN for overlapping 12.7 mm and 4.8 kN for 50 mm. Finally, for the Betamate 120 adhesive was 1.8 kN for 12.7 mm of overlapping and 6 kN for 50 mm. The post-fracture visual inspection revealed that MP55420 and Betamate 120 adhesives had a cohesive failure, while the DC-80 showed cohesive-adhesive failure. Additionally, the scanning electron microscopy evaluation on the spew fillet revealed resolved striations and a network of small micro-dimples for the Betamate 120 and MP55420 adhesives. On the other hand, DC-80 adhesive exhibited notable facet fragile failure that was confirmed by the shape of stress-strain plot with straight line from the origin to the point of fracture.
- Open Access
- 1 March 2017
- Published by FapUNIFESP (SciELO) in Soldagem & Inspeção
- Vol. 22 (1) , 72-86
Effect of Torch Weaving on the Microstructure, Tensile and Impact Resistances, and Fracture of the HAZ and Weld Bead by Robotic GMAW Process on ASTM A36 Steel
The effect of torch weaving on the microstructure, tensile strength, impact resistance and fracturing in robotic welded joints using varing welding speeds, voltages and currents was evaluated through fractography using scanning electron microscopy, tension, impact and micro-hardness tests and optic microscopy. Results indicated that linear, sinusoidal and circular weavings favored an increase of the width of the HAZ as well as a slight increase in yield resistance accompanied by hardening in comparison with a triangular weave. The latter favored larger impact energy in the HAZ with less width, containing coarse-grained ferrite due to lower tensile strength and Vickers hardness. A circular weave generated the highest level of hardening and the lowest energy absorbed in the HAZ as a consequence of an increase in yield strength related to the fine needles of acicular ferrite. A linear weave favored the greatest width of the HAZ compared with other weld weavings due to heat accumulation along the fusion line of the welded joint. Hardening and loss of toughness were evaluated through fractographic analysis showing mixed fractures mainly composed of brittle fracturing made by transgranular cleavages with facets containing well defined river patterns.
- 1 March 2017
- Published by FapUNIFESP (SciELO) in Soldagem & Inspeção
- Vol. 22 (1) , 72-86
Open AccessEffect of Torch Weaving on the Microstructure, Tensile and Impact Resistances, and Fracture of the HAZ and Weld Bead by Robotic GMAW Process on ASTM A36 Steel
The effect of torch weaving on the microstructure, tensile strength, impact resistance and fracturing in robotic welded joints using varing welding speeds, voltages and currents was evaluated through fractography using scanning electron microscopy, tension, impact and micro-hardness tests and optic microscopy. Results indicated that linear, sinusoidal and circular weavings favored an increase of the width of the HAZ as well as a slight increase in yield resistance accompanied by hardening in comparison with a triangular weave. The latter favored larger impact energy in the HAZ with less width, containing coarse-grained ferrite due to lower tensile strength and Vickers hardness. A circular weave generated the highest level of hardening and the lowest energy absorbed in the HAZ as a consequence of an increase in yield strength related to the fine needles of acicular ferrite. A linear weave favored the greatest width of the HAZ compared with other weld weavings due to heat accumulation along the fusion line of the welded joint. Hardening and loss of toughness were evaluated through fractographic analysis showing mixed fractures mainly composed of brittle fracturing made by transgranular cleavages with facets containing well defined river patterns.