Takafumi Egoshi
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Takafumi Egoshi has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
- Yohsuke Taira
Division of Cariology and Restorative Dentistry, Department of Prosthetic Dentistry, Graduate School of Biomedical Sciences, Nagasaki University
3 shared publications - Kei Kaida
Department of Prosthetic Dentistry, Division of Cariology and Restorative Dentistry, Nagasaki University Graduate School of Biomedical Sciences
2 shared publications - Shizuka Yamada
Department of Cariology, Nagasaki University Graduate School of Biomedical Sciences, Nagasaki 852-8588, Japan
2 shared publications Kei Kaida
Division of Cariology and Restorative Dentistry, Department of Prosthetic Dentistry, Graduate School of Biomedical Sciences, Nagasaki University, Nagasaki, Japan
1 shared publicationKohji Kamada
Department of General Dentistry, Nagasaki University Hospital, Nagasaki, Japan
1 shared publication- Kohji Kamada
Department of Applied Prosthodontics Graduate School of Biomedical Sciences Nagasaki University Nagasaki Japan
1 shared publication
Latest Publications
- Open Access
- 1 January 2026
- Published by Nihon University School of Dentistry in Journal of Oral Science
- Vol. 68 (4) , 268-270
Genipin-mediated dentin biomodification using nanobubble water
Genipin is a naturally derived cross-linking agent used to stabilize collagen-based biomaterials. This study evaluated dentin biomodification following intracanal application of genipin solutions prepared with Milli-Q water or nanobubble water. Bovine root canals were treated with different concentrations of genipin, and collagenase resistance, dentin discoloration, and dentin hardness were assessed. Genipin concentration significantly affected all outcomes, while the solvent significantly affected hydroxyproline levels and dentin hardness. No significant solvent-concentration interactions were detected. These findings suggest that nanobubble water may influence genipin-mediated dentin biomodification and warrant further investigation as a vehicle for intracanal genipin application.
- 1 January 2026
- Published by Nihon University School of Dentistry in Journal of Oral Science
- Vol. 68 (4) , 268-270
Open AccessGenipin-mediated dentin biomodification using nanobubble water
Genipin is a naturally derived cross-linking agent used to stabilize collagen-based biomaterials. This study evaluated dentin biomodification following intracanal application of genipin solutions prepared with Milli-Q water or nanobubble water. Bovine root canals were treated with different concentrations of genipin, and collagenase resistance, dentin discoloration, and dentin hardness were assessed. Genipin concentration significantly affected all outcomes, while the solvent significantly affected hydroxyproline levels and dentin hardness. No significant solvent-concentration interactions were detected. These findings suggest that nanobubble water may influence genipin-mediated dentin biomodification and warrant further investigation as a vehicle for intracanal genipin application.
- 24 September 2024
- Published by Wiley in European Journal of Oral Sciences
- Vol. 132 (5) , e13017
Effects of sodium copper‐ and sodium iron‐chlorophyllin primers on resin bonding to dentin
This study evaluated the effects of two chlorophyll derivatives, sodium copper chlorophyllin (Cu‐Chl) and sodium iron chlorophyllin (Fe‐Chl), on the bond strength between a self‐curing luting agent (4‐META/MMA‐TBB resin) and dentin. Five aqueous primers containing 35% 2‐hydroxyethylmethacrylate with 0.007% Cu‐Chl, 0.07% Cu‐Chl, 0.007% Fe‐Chl, 0.07% Fe‐Chl, or neither Cu‐Chl nor Fe‐Chl (no‐Chl) were prepared. The extracted human dentin surfaces were etched with 10% phosphoric acid (10PA), primed, and bonded to a resin block using the 4‐META/MMA‐TBB resin. A conventional etching agent (10‐3) and 10PA without primer (PA/no‐primer) were used as controls. The microtensile bond strength was determined after 48 h. The arithmetic medians for 20 stick specimens were calculated and statistically analyzed using a nonparametric Steel‐Dwass test (α = 0.05). The maximum bond strength was achieved in the 0.007% Cu‐Chl group, followed by those in the 0.07% Cu‐Chl, 0.07% Fe‐Chl, 10‐3, 0.007% Fe‐Chl, no‐Chl, and PA/no‐primer groups. No significant difference was observed between 0.007% Fe‐Chl, 0.07% Fe‐Chl, and 10‐3. The bond strength to dentin etched with 10PA was influenced by the type and concentration of the chlorophyll derivatives applied. Cu‐Chl rather than Fe‐Chl should be useful as a component of surface treatment agents for bonding 4‐META/MMA‐TBB resin to dentin.
- 24 September 2024
- Published by Wiley in European Journal of Oral Sciences
- Vol. 132 (5) , e13017
Effects of sodium copper‐ and sodium iron‐chlorophyllin primers on resin bonding to dentin
This study evaluated the effects of two chlorophyll derivatives, sodium copper chlorophyllin (Cu‐Chl) and sodium iron chlorophyllin (Fe‐Chl), on the bond strength between a self‐curing luting agent (4‐META/MMA‐TBB resin) and dentin. Five aqueous primers containing 35% 2‐hydroxyethylmethacrylate with 0.007% Cu‐Chl, 0.07% Cu‐Chl, 0.007% Fe‐Chl, 0.07% Fe‐Chl, or neither Cu‐Chl nor Fe‐Chl (no‐Chl) were prepared. The extracted human dentin surfaces were etched with 10% phosphoric acid (10PA), primed, and bonded to a resin block using the 4‐META/MMA‐TBB resin. A conventional etching agent (10‐3) and 10PA without primer (PA/no‐primer) were used as controls. The microtensile bond strength was determined after 48 h. The arithmetic medians for 20 stick specimens were calculated and statistically analyzed using a nonparametric Steel‐Dwass test (α = 0.05). The maximum bond strength was achieved in the 0.007% Cu‐Chl group, followed by those in the 0.07% Cu‐Chl, 0.07% Fe‐Chl, 10‐3, 0.007% Fe‐Chl, no‐Chl, and PA/no‐primer groups. No significant difference was observed between 0.007% Fe‐Chl, 0.07% Fe‐Chl, and 10‐3. The bond strength to dentin etched with 10PA was influenced by the type and concentration of the chlorophyll derivatives applied. Cu‐Chl rather than Fe‐Chl should be useful as a component of surface treatment agents for bonding 4‐META/MMA‐TBB resin to dentin.
- Open Access
- 26 September 2018
- Published by Elsevier in Journal of Dental Sciences
- Vol. 14 (1) , 109-112
Effect of tetrabutylammonium dihydrogen trifluoride treatment on durability of resin–titanium bond strengths
- 26 September 2018
- Published by Elsevier in Journal of Dental Sciences
- Vol. 14 (1) , 109-112
Open AccessEffect of tetrabutylammonium dihydrogen trifluoride treatment on durability of resin–titanium bond strengths
- 28 December 2013
- Published by Wiley in European Journal of Oral Sciences
- Vol. 122 (1) , 84-88
Surface modification with alumina blasting and H2SO4–HCl etching for bonding two resin‐composite veneers to titanium
The purpose of this study was to investigate the effect of an experimental surface treatment with alumina blasting and acid etching on the bond strengths between each of two resin composites and commercially pure titanium. The titanium surface was blasted with alumina and then etched with 45wt% H2SO4 and 15wt% HCl (H2SO4-HCl). A light- and heat-curing resin composite (Estenia) and a light-curing resin composite (Ceramage) were used with adjunctive metal primers. Veneered specimens were subjected to thermal cycling between 4 and 60°C for 50,000 cycles, and the shear bond strengths were determined. The highest bond strengths were obtained for Blasting/H2SO4-HCl/Estenia (30.2 ± 4.5 MPa) and Blasting/Etching/Ceramage (26.0 ± 4.5 MPa), the values of which were not statistically different, followed by Blasting/No etching/Estenia (20.4 ± 2.4 MPa) and Blasting/No etching/Ceramage (0.8 ± 0.3 MPa). Scanning electron microscopy observations revealed that alumina blasting and H2SO4-HCl etching creates a number of micro- and nanoscale cavities on the titanium surface, which contribute to adhesive bonding.
- 28 December 2013
- Published by Wiley in European Journal of Oral Sciences
- Vol. 122 (1) , 84-88
Surface modification with alumina blasting and H2SO4–HCl etching for bonding two resin‐composite veneers to titanium
The purpose of this study was to investigate the effect of an experimental surface treatment with alumina blasting and acid etching on the bond strengths between each of two resin composites and commercially pure titanium. The titanium surface was blasted with alumina and then etched with 45wt% H2SO4 and 15wt% HCl (H2SO4-HCl). A light- and heat-curing resin composite (Estenia) and a light-curing resin composite (Ceramage) were used with adjunctive metal primers. Veneered specimens were subjected to thermal cycling between 4 and 60°C for 50,000 cycles, and the shear bond strengths were determined. The highest bond strengths were obtained for Blasting/H2SO4-HCl/Estenia (30.2 ± 4.5 MPa) and Blasting/Etching/Ceramage (26.0 ± 4.5 MPa), the values of which were not statistically different, followed by Blasting/No etching/Estenia (20.4 ± 2.4 MPa) and Blasting/No etching/Ceramage (0.8 ± 0.3 MPa). Scanning electron microscopy observations revealed that alumina blasting and H2SO4-HCl etching creates a number of micro- and nanoscale cavities on the titanium surface, which contribute to adhesive bonding.