Adriana Oliveira Carvalho
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
Adriana Oliveira Carvalho has a total of 49 co-authors. Here are the top co-authors by number of shared publications:
Marcelo Giannini
Department of Clinical Restorative Dentistry, University of Uberaba, Uberaba, Brazil
6 shared publications- Marcelo Giannini
Department of Restorative Dentistry, Piracicaba Dental School University of Campinas Piracicaba São Paulo Brazil
6 shared publications Pascal Magne
Don and Sybil Harrington Professor of Esthetic Dentistry, Restorative Sciences, Herman Ostrow School of Dentistry, University of Southern California, Los Angeles, CA, USA
4 shared publications- Ana Paula Almeida Ayres
Restorative Dentistry, Universidade de Uberaba, Uberaba, Brazil
3 shared publications - Frederick Allen Rueggeberg
Augusta University, USA
3 shared publications Greciana Bruzi
Department of Operative Dentistry,Federal University of Alfenas (UNIFAL-MG),Alfenas,Brazil
3 shared publications
Latest Publications
- Open Access
- 1 January 2026
- Published by Wiley in International Journal of Dentistry
- Vol. 2026 (1)
Impact of Preparation Thickness and Restorative Material on the Marginal Fit of CAD‐CAM Complete Crowns
Statement of Problem: A lack of consensus exists on whether the preparation thickness and choice of restorative material can affect the marginal adaptation of complete CAD‐CAM crowns. Purpose: To evaluate the impact of preparation thickness and restorative material on the marginal adaptation of CAD‐CAM complete crowns. Materials and Methods: Two human mandibular right second molars were prepared with the following characteristics: conventional preparation (CP)—1.0 mm chamfer, 2 mm reduction of the occlusal surface, ~6° convergence angle, and 1.5 mm axial reduction; ultrathin preparation (UFP)—0.5 mm finish line, 0.7 mm reduction of the occlusal and axial surface. The teeth were scanned using an intraoral scanner (IOs), and the crowns were designed and milled. Ten crowns were produced in each group ( n = 10): feldspathic ceramic (FC), resin composite (RC), lithium silicate ceramic reinforced with zirconia (LSZ), and lithium disilicate ceramic (LDS). The marginal gap was analyzed at 4 points using a stereomicroscope. Data analysis used two‐way analysis of variance (ANOVA) and the Tukey test ( α = 0.05). Results: CP (65.00 ± 16.62 to 84.22 ± 20.87 µm) showed the lowest marginal discrepancy values, with a statistical difference from UFP (110.40 ± 28.64 to 183.83 ± 40.23 µm). In the CP group, there was no statistically significant difference between the materials. In the UFP, there was a difference between FC and RC compared to LSZ and LDS. Conclusions: The preparation’s thickness impacted the marginal adaptation of CAD‐CAM full crowns, and the CP showed a lower discrepancy compared to the ultrathin preparation. The performance of the materials in the CP was similar. However, there was better marginal adaptation of FC crowns and RCs in ultrathin preparations.
- 1 January 2026
- Published by Wiley in International Journal of Dentistry
- Vol. 2026 (1)
Open AccessImpact of Preparation Thickness and Restorative Material on the Marginal Fit of CAD‐CAM Complete Crowns
Statement of Problem: A lack of consensus exists on whether the preparation thickness and choice of restorative material can affect the marginal adaptation of complete CAD‐CAM crowns. Purpose: To evaluate the impact of preparation thickness and restorative material on the marginal adaptation of CAD‐CAM complete crowns. Materials and Methods: Two human mandibular right second molars were prepared with the following characteristics: conventional preparation (CP)—1.0 mm chamfer, 2 mm reduction of the occlusal surface, ~6° convergence angle, and 1.5 mm axial reduction; ultrathin preparation (UFP)—0.5 mm finish line, 0.7 mm reduction of the occlusal and axial surface. The teeth were scanned using an intraoral scanner (IOs), and the crowns were designed and milled. Ten crowns were produced in each group ( n = 10): feldspathic ceramic (FC), resin composite (RC), lithium silicate ceramic reinforced with zirconia (LSZ), and lithium disilicate ceramic (LDS). The marginal gap was analyzed at 4 points using a stereomicroscope. Data analysis used two‐way analysis of variance (ANOVA) and the Tukey test ( α = 0.05). Results: CP (65.00 ± 16.62 to 84.22 ± 20.87 µm) showed the lowest marginal discrepancy values, with a statistical difference from UFP (110.40 ± 28.64 to 183.83 ± 40.23 µm). In the CP group, there was no statistically significant difference between the materials. In the UFP, there was a difference between FC and RC compared to LSZ and LDS. Conclusions: The preparation’s thickness impacted the marginal adaptation of CAD‐CAM full crowns, and the CP showed a lower discrepancy compared to the ultrathin preparation. The performance of the materials in the CP was similar. However, there was better marginal adaptation of FC crowns and RCs in ultrathin preparations.
- Open Access
- 14 September 2020
- Published by Escola Bahiana de Medicina e Saude Publica in Journal of Dentistry & Public Health
- Vol. 11 (2) , 159-166
O uso do sistema CAD/CAM para confecção de próteses fixas: aplicações e limitações
O sistema CAD/CAM, sigla derivada do inglês Computer Aided Design / Computer Aided Manufacturing, é uma tecnologia baseada no desenho de uma estrutura protética em um computador seguida de sua confecção em uma máquina de fresagem. Tem como objetivo a simplificação na produção de estruturas protéticas, otimização do tempo de trabalho e a produção de estruturas com alto padrão de qualidade e estética. O emprego desta tecnologia consiste em três etapas: digitalização do preparo protético, planejamento virtual e produção da restauração. O preparo dentário pode ser digitalizado fora da cavidade oral, sobre o modelo de gesso, ou dentro da cavidade oral, através de um sistema de digitalização intra-oral. Após efetuada a digitalização do preparo, a imagem será transferida para um programa de desenho assistido por computador (CAD), pelo qual o operador poderá desenhar de forma virtual a restauração. Através de uma fresadora ou da impressão digital em 3D, o sistema CAM irá reproduzir a reabilitação desejada. Dependendo da estrutura e do seu objetivo, pode-se optar por diversos materiais, como em resina acrílica, cerâmica, híbrido, metal, e resinas compostas. O objetivo do presente trabalho é explanar o uso do sistema CAD/CAM na Odontologia para confecção de próteses fixas através de um levantamento nas bases de dados Lilacs, Pubmed, Scielo e Google Acadêmico. Pôde-se concluir que a tecnologia CAD/CAM aumenta a versatilidade, a precisão e o custo-benefício da confecção de restaurações indiretas. Acredita-se que em breve, fará parte da rotina clínica da maioria dos cirurgiões-dentistas.
- 14 September 2020
- Published by Escola Bahiana de Medicina e Saude Publica in Journal of Dentistry & Public Health
- Vol. 11 (2) , 159-166
Open AccessO uso do sistema CAD/CAM para confecção de próteses fixas: aplicações e limitações
O sistema CAD/CAM, sigla derivada do inglês Computer Aided Design / Computer Aided Manufacturing, é uma tecnologia baseada no desenho de uma estrutura protética em um computador seguida de sua confecção em uma máquina de fresagem. Tem como objetivo a simplificação na produção de estruturas protéticas, otimização do tempo de trabalho e a produção de estruturas com alto padrão de qualidade e estética. O emprego desta tecnologia consiste em três etapas: digitalização do preparo protético, planejamento virtual e produção da restauração. O preparo dentário pode ser digitalizado fora da cavidade oral, sobre o modelo de gesso, ou dentro da cavidade oral, através de um sistema de digitalização intra-oral. Após efetuada a digitalização do preparo, a imagem será transferida para um programa de desenho assistido por computador (CAD), pelo qual o operador poderá desenhar de forma virtual a restauração. Através de uma fresadora ou da impressão digital em 3D, o sistema CAM irá reproduzir a reabilitação desejada. Dependendo da estrutura e do seu objetivo, pode-se optar por diversos materiais, como em resina acrílica, cerâmica, híbrido, metal, e resinas compostas. O objetivo do presente trabalho é explanar o uso do sistema CAD/CAM na Odontologia para confecção de próteses fixas através de um levantamento nas bases de dados Lilacs, Pubmed, Scielo e Google Acadêmico. Pôde-se concluir que a tecnologia CAD/CAM aumenta a versatilidade, a precisão e o custo-benefício da confecção de restaurações indiretas. Acredita-se que em breve, fará parte da rotina clínica da maioria dos cirurgiões-dentistas.
- 1 April 2019
- Published by Japan Prosthodontic Society in Journal of Prosthodontic Research
- Vol. 63 (2) , 232-238
Effect of indirect restorative material and thickness on light transmission at different wavelengths
The aim of this study was to evaluate the influence of indirect restorative material type and thickness on the transmission of different wavelengths from a broad-banded dental curing light. Four dental indirect restorative materials for computer-aided design and computer-aided manufacturing (CAD/CAM) were evaluated: [RC] resin/ceramic hybrid material (Lava Ultimate), [FC] feldspathic ceramic (VitaBlocs), and two zirconia-based ceramics ([ZK] Katana; and [ZL] Lava). Total loss of irradiance (TL) was measured for blue (WB, 425-490nm) and violet (WV, 350-425nm) wavelengths. Specimens of 15×15mm with varying thicknesses (0.5, 1.0, 1.5, and 2.0mm) were fabricated (n=5). A plasma-arc dental light-curing unit was used (Arc Light-II). To assess TL as a function of wavelength, a software (Spectra Suite v5.1) connected to a spectroradiometer (USB2000) and an integrating sphere (CTSM-LSM-60-SF) was used. Data was subjected to statistical analysis (two-way ANOVA and post-hoc Tukey test, α=0.05). A 0.5mm interposition resulted in TL from 50.5 to 67.2%, depending on material. Increased thickness resulted in higher TL for all materials. FC showed less TL compared to ZK. In general, WV showed higher TL than did WB, and WV/WB proportion decreased with increasing thickness. Indirect materials significantly reduced TL, and this effect is greater with increasing thickness. WV showed lower penetration compared to WB.
- 1 April 2019
- Published by Japan Prosthodontic Society in Journal of Prosthodontic Research
- Vol. 63 (2) , 232-238
Effect of indirect restorative material and thickness on light transmission at different wavelengths
The aim of this study was to evaluate the influence of indirect restorative material type and thickness on the transmission of different wavelengths from a broad-banded dental curing light. Four dental indirect restorative materials for computer-aided design and computer-aided manufacturing (CAD/CAM) were evaluated: [RC] resin/ceramic hybrid material (Lava Ultimate), [FC] feldspathic ceramic (VitaBlocs), and two zirconia-based ceramics ([ZK] Katana; and [ZL] Lava). Total loss of irradiance (TL) was measured for blue (WB, 425-490nm) and violet (WV, 350-425nm) wavelengths. Specimens of 15×15mm with varying thicknesses (0.5, 1.0, 1.5, and 2.0mm) were fabricated (n=5). A plasma-arc dental light-curing unit was used (Arc Light-II). To assess TL as a function of wavelength, a software (Spectra Suite v5.1) connected to a spectroradiometer (USB2000) and an integrating sphere (CTSM-LSM-60-SF) was used. Data was subjected to statistical analysis (two-way ANOVA and post-hoc Tukey test, α=0.05). A 0.5mm interposition resulted in TL from 50.5 to 67.2%, depending on material. Increased thickness resulted in higher TL for all materials. FC showed less TL compared to ZK. In general, WV showed higher TL than did WB, and WV/WB proportion decreased with increasing thickness. Indirect materials significantly reduced TL, and this effect is greater with increasing thickness. WV showed lower penetration compared to WB.
- Open Access
- 4 December 2018
- Published by Springer Nature in Applied Adhesion Science
- Vol. 6 (1) , 10
Bonding of CAD/CAM lithium disilicate restorations with regular and flowable composite resin with and without wetting resin
- 4 December 2018
- Published by Springer Nature in Applied Adhesion Science
- Vol. 6 (1) , 10
Open AccessBonding of CAD/CAM lithium disilicate restorations with regular and flowable composite resin with and without wetting resin
- Open Access
- 23 October 2017
- Published by Springer Nature in Applied Adhesion Science
- Vol. 5 (1) , 17
Post-etching cleaning influences the resin shear bond strength to CAD/CAM lithium-disilicate ceramics
- 23 October 2017
- Published by Springer Nature in Applied Adhesion Science
- Vol. 5 (1) , 17
Open AccessPost-etching cleaning influences the resin shear bond strength to CAD/CAM lithium-disilicate ceramics
- Open Access
- 15 August 2016
- Published by Springer Nature in Applied Adhesion Science
- Vol. 4 (1) , 16
Bond strength and micromorphology of resin-dentin interface of etch-and-rinse dentin bonding agents after 1-year of water storage
- 15 August 2016
- Published by Springer Nature in Applied Adhesion Science
- Vol. 4 (1) , 16
Open AccessBond strength and micromorphology of resin-dentin interface of etch-and-rinse dentin bonding agents after 1-year of water storage
- Open Access
- 30 June 2016
- Published by Associacao Brasileira de Odontologia Rio de Janeiro (ABORJ) in Revista Brasileira de Odontologia
- Vol. 73 (2) , 096
Efeito do peróxido de hidrogênio na permeabilidade dental
Objetivo: Este trabalho avaliou o efeito de quatro agentes clareadores na permeabilidade dental. Dentes bovinos foram divididos em quatro grupos (n = 10). A permeabilidade inicial dos dentes foi determinada previamente ao clareamento, utilizando equipamento de permeabilidade. Em seguida, foram aplicados os géis clareadores e a permeabilidade novamente mensurada. Os resultados foram expressos em porcentagem de aumento da permeabilidade e os dados submetidos à análise estatística (ANOVA e teste Tukey). O Whiteness HP Maxx resultou em maior aumento de permeabilidade (145,7±76,3), quando comparado com Whiteness HP Blue (57,5±36,1) e Pola Office Plus (72,7±19,5). Esses produtos não apresentaram diferença estatística com relação ao Opalescence Boost PF (101,4±46,3). Todos os agentes clareadores testados aumentaram a permeabilidade. A intensidade desse aumento foi dependente do produto utilizado.
- 30 June 2016
- Published by Associacao Brasileira de Odontologia Rio de Janeiro (ABORJ) in Revista Brasileira de Odontologia
- Vol. 73 (2) , 096
Open AccessEfeito do peróxido de hidrogênio na permeabilidade dental
Objetivo: Este trabalho avaliou o efeito de quatro agentes clareadores na permeabilidade dental. Dentes bovinos foram divididos em quatro grupos (n = 10). A permeabilidade inicial dos dentes foi determinada previamente ao clareamento, utilizando equipamento de permeabilidade. Em seguida, foram aplicados os géis clareadores e a permeabilidade novamente mensurada. Os resultados foram expressos em porcentagem de aumento da permeabilidade e os dados submetidos à análise estatística (ANOVA e teste Tukey). O Whiteness HP Maxx resultou em maior aumento de permeabilidade (145,7±76,3), quando comparado com Whiteness HP Blue (57,5±36,1) e Pola Office Plus (72,7±19,5). Esses produtos não apresentaram diferença estatística com relação ao Opalescence Boost PF (101,4±46,3). Todos os agentes clareadores testados aumentaram a permeabilidade. A intensidade desse aumento foi dependente do produto utilizado.
- 26 November 2015
- Vol. 14 (6) , 543-549
Effects of Water Storage on Bond Strength and Dentin Sealing Ability Promoted by Adhesive Systems
Purpose: To evaluate the dentin bond strength (BS) and sealing ability (SA) promoted by adhesive systems after 24 h or 6 months of water storage. Materials and Methods: The tested adhesive systems were: one three-step etch-and-rinse adhesive (Adper Scotchbond Multi-Purpose, SBMP) and three single-step self-etching systems (Adper Easy Bond, Bond Force, and G-Bond Plus). Bovine incisors were used for both evaluations, BS (n = 11) and SA (n = 5). To examine BS, the buccal surface was ground with SiC paper to expose a flat dentin surface. After adhesive application, a block of resin composite was incrementally built up over the bonded surface and sectioned into sticks. These bonded specimens were subjected to microtensile bond strength testing after 24 h and 6 months of water storage using a universal testing machine. For SA analysis, enamel was removed from the buccal surfaces. The teeth were connected to a device to measure the initial SA (10 psi), and the second measurement was taken after treating dentin with EDTA. Afterwards, the adhesive systems were applied to dentin and the SA was re-measured for each adhesive after 24 h and 6 months of water storage. The SA was expressed in terms of percentage of dentinal sealing. BS and SA data were submitted to two-way ANOVA and Tukey's test (alpha = 0.05). Results: All adhesives showed a reduction of SA after 6 months of water storage. The SA promoted by self-etching adhesives was higher than that of SBMP. No adhesive system showed a reduction of the BS after 6 months. Conclusion: Sealing ability was affected by water storage, while no changes in microtensile bond strength were observed after 6 months of water storage. The single-step self-etching systems showed greater sealing ability than did SBMP, even after 6 months of storage in water
- 26 November 2015
- Vol. 14 (6) , 543-549
Effects of Water Storage on Bond Strength and Dentin Sealing Ability Promoted by Adhesive Systems
Purpose: To evaluate the dentin bond strength (BS) and sealing ability (SA) promoted by adhesive systems after 24 h or 6 months of water storage. Materials and Methods: The tested adhesive systems were: one three-step etch-and-rinse adhesive (Adper Scotchbond Multi-Purpose, SBMP) and three single-step self-etching systems (Adper Easy Bond, Bond Force, and G-Bond Plus). Bovine incisors were used for both evaluations, BS (n = 11) and SA (n = 5). To examine BS, the buccal surface was ground with SiC paper to expose a flat dentin surface. After adhesive application, a block of resin composite was incrementally built up over the bonded surface and sectioned into sticks. These bonded specimens were subjected to microtensile bond strength testing after 24 h and 6 months of water storage using a universal testing machine. For SA analysis, enamel was removed from the buccal surfaces. The teeth were connected to a device to measure the initial SA (10 psi), and the second measurement was taken after treating dentin with EDTA. Afterwards, the adhesive systems were applied to dentin and the SA was re-measured for each adhesive after 24 h and 6 months of water storage. The SA was expressed in terms of percentage of dentinal sealing. BS and SA data were submitted to two-way ANOVA and Tukey's test (alpha = 0.05). Results: All adhesives showed a reduction of SA after 6 months of water storage. The SA promoted by self-etching adhesives was higher than that of SBMP. No adhesive system showed a reduction of the BS after 6 months. Conclusion: Sealing ability was affected by water storage, while no changes in microtensile bond strength were observed after 6 months of water storage. The single-step self-etching systems showed greater sealing ability than did SBMP, even after 6 months of storage in water
- 1 October 2015
- Published by Elsevier in The Journal of Prosthetic Dentistry
- Vol. 114 (4) , 574-579
Fatigue resistance of ultrathin CAD/CAM complete crowns with a simplified cementation process
- 1 October 2015
- Published by Elsevier in The Journal of Prosthetic Dentistry
- Vol. 114 (4) , 574-579
Fatigue resistance of ultrathin CAD/CAM complete crowns with a simplified cementation process
- Open Access
- 1 August 2015
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 26 (4) , 363-367
Indirect Restoration Thickness and Time after Light-Activation Effects on Degree of Conversion of Resin Cement
This study evaluated the effects of indirect restorative materials, curing conditions and time on the degree of conversion (DC) of a dual-cured resin cement using infrared spectroscopy. The resin cement (RelyX Unicem 2, 3M ESPE) was applied to the diamond surface of a horizontal attenuated-total-reflectance unit and activated using one of following conditions: self-cure, direct light exposure, light exposure through indirect restorative materials (resin nano-ceramic: Lava Ultimate, 3M ESPE or feldspathic ceramic: Vita Blocks Mark II, Vita Zahnfabrik). Four thicknesses (0.5, 1.0, 1.5 or 2.0 mm) of each indirect material were analyzed, and the light-activation was performed using a blue LED light. Data (n=5) were analyzed by three-way ANOVA, Tukey's post hoc and Dunnett's tests (α=5%). No significant differences in DC were observed between indirect materials of similar thickness. All groups exhibited higher DC after 10 min than after 5 min. At both times points, the self-cure group exhibited significantly lower DC than all the light exposure groups. Only when the overlying indirect restoration had a thickness of 2 mm did DC decrease significantly. The presence of a thick, indirect restoration can decrease the DC of resin cement. DC after 10 min was higher than after 5 min. The self-cure mode yielded lower DC than the light-activating one.
- 1 August 2015
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 26 (4) , 363-367
Open AccessIndirect Restoration Thickness and Time after Light-Activation Effects on Degree of Conversion of Resin Cement
This study evaluated the effects of indirect restorative materials, curing conditions and time on the degree of conversion (DC) of a dual-cured resin cement using infrared spectroscopy. The resin cement (RelyX Unicem 2, 3M ESPE) was applied to the diamond surface of a horizontal attenuated-total-reflectance unit and activated using one of following conditions: self-cure, direct light exposure, light exposure through indirect restorative materials (resin nano-ceramic: Lava Ultimate, 3M ESPE or feldspathic ceramic: Vita Blocks Mark II, Vita Zahnfabrik). Four thicknesses (0.5, 1.0, 1.5 or 2.0 mm) of each indirect material were analyzed, and the light-activation was performed using a blue LED light. Data (n=5) were analyzed by three-way ANOVA, Tukey's post hoc and Dunnett's tests (α=5%). No significant differences in DC were observed between indirect materials of similar thickness. All groups exhibited higher DC after 10 min than after 5 min. At both times points, the self-cure group exhibited significantly lower DC than all the light exposure groups. Only when the overlying indirect restoration had a thickness of 2 mm did DC decrease significantly. The presence of a thick, indirect restoration can decrease the DC of resin cement. DC after 10 min was higher than after 5 min. The self-cure mode yielded lower DC than the light-activating one.