Hareenanden Ramasawmy
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Hareenanden Ramasawmy has a total of 17 co-authors. Here are the top co-authors by number of shared publications:
Jaykumar Chummun
University of Mauritius
7 shared publications- François Benjamin Vincent Florens
Tropical Island Biodiversity, Ecology and Conservation Pole of Research, Department of Biosciences and Ocean Studies, Faculty of Science, University of Mauritius, Le Réduit, Mauritius
5 shared publications - Barisoa Harijaona Rafidison
Department of Mechanical and Production, University of Mauritius, Réduit, Mauritius
4 shared publications J. Chummun
University of Mauritius Reduit Republic of Mauritius, Mauritius, East Africa
3 shared publicationsP. D. Emrith
University of Mauritius Reduit Republic of Mauritius, Mauritius, East Africa
2 shared publicationsA. B. Bhurtun
University of Mauritius
1 shared publication
Latest Publications
- 9 February 2026
- Published by SAGE Publications in Journal of Reinforced Plastics and Composites
- Vol. 45 (21-22) , 4954-4968
Development of an effective non-woven fibre mat via wet-laid process for structural composite reinforcement applications
The use of structural composite materials demands high homogeneity to ensure efficient load transfer. A wet-laid web process, incorporating 2% by weight of hydroxyethylcellulose (HEC) as a bonding agent, was employed to fabricate non-woven mats, using randomly distributed fibres of a native Mauritius Screwpine ( Pandanus utilis ). Morphological analysis revealed that the resulting mats exhibited superior homogeneity compared to commercial E-glass mats. Three polyester composites were fabricated with fibre mat contents of 10.7%, 21.4%, and 32.1% (corresponding to one, two, and three layers, respectively). The composite with the highest tensile and flexural strengths was selected for manufacturing a 550 mm wind turbine blade (WTB). A flap-wise static test, conducted in accordance with BS EN 61400-2, confirmed that the blade could withstand worst-case loading with a 39% safety margin before failure. The results demonstrate the composite’s suitability for structural applications, with the non-woven mat’s flexibility enabling easy adaptation to complex mould geometries.
- 9 February 2026
- Published by SAGE Publications in Journal of Reinforced Plastics and Composites
- Vol. 45 (21-22) , 4954-4968
Development of an effective non-woven fibre mat via wet-laid process for structural composite reinforcement applications
The use of structural composite materials demands high homogeneity to ensure efficient load transfer. A wet-laid web process, incorporating 2% by weight of hydroxyethylcellulose (HEC) as a bonding agent, was employed to fabricate non-woven mats, using randomly distributed fibres of a native Mauritius Screwpine ( Pandanus utilis ). Morphological analysis revealed that the resulting mats exhibited superior homogeneity compared to commercial E-glass mats. Three polyester composites were fabricated with fibre mat contents of 10.7%, 21.4%, and 32.1% (corresponding to one, two, and three layers, respectively). The composite with the highest tensile and flexural strengths was selected for manufacturing a 550 mm wind turbine blade (WTB). A flap-wise static test, conducted in accordance with BS EN 61400-2, confirmed that the blade could withstand worst-case loading with a 39% safety margin before failure. The results demonstrate the composite’s suitability for structural applications, with the non-woven mat’s flexibility enabling easy adaptation to complex mould geometries.
- 12 July 2025
- Published by Springer Nature in Cellulose
- Vol. 32 (12) , 6965-6986
Packing arrangements of cellulose I allomorphs and cell wall thickness: key factors influencing the tensile strength of banana fibres
- 12 July 2025
- Published by Springer Nature in Cellulose
- Vol. 32 (12) , 6965-6986
Packing arrangements of cellulose I allomorphs and cell wall thickness: key factors influencing the tensile strength of banana fibres
- 11 October 2023
- Published by Wiley in ChemistrySelect
- Vol. 8 (38)
Enhanced Yield of Sodium Alginate Extracted from Padina gymnospora Using a Greener Microwave and Ultrasound Hybrid System
In this study, alginate was extracted from Padina gymnospora (PG) by applying the sequential combination of microwaves followed by ultrasounds (at low power and amplitude settings) using an organic acid pre‐treatment. The optimum alginate yield was investigated by varying the type of acid (oxalic and formic) and seaweed particle size range (0.295–0.495 and 0.146–0.246 mm). The extracted sodium alginate was then characterised in terms of FTIR, 1 H‐NMR, M/G ratio, viscosity and colour. The synergistic effect of the microwave‐ultrasound hybrid system for short timeframes (15 min each) successfully improved the alginate yield without compromising its structural composition, while allowing for a milder and greener organic acid to be used for the acid pre‐treatment. The highest alginate yield (~64 %) was obtained using formic acid and the smaller particle size range (0.146–0.246 mm). The latter thus highlights the importance of particle size reduction and optimisation. FTIR, NMR and viscosity analyses revealed a low guluronic acid content of alginate with a high M/G ratio (7.7±1.0–9.3±0.1) and low viscosity (2.92±0.09–3.05±0.06 cP), which was found to be inherent to the species used. The proposed novel method therefore opens prospects for the industry since it is both environmentally and economically sustainable.
- 11 October 2023
- Published by Wiley in ChemistrySelect
- Vol. 8 (38)
Enhanced Yield of Sodium Alginate Extracted from Padina gymnospora Using a Greener Microwave and Ultrasound Hybrid System
In this study, alginate was extracted from Padina gymnospora (PG) by applying the sequential combination of microwaves followed by ultrasounds (at low power and amplitude settings) using an organic acid pre‐treatment. The optimum alginate yield was investigated by varying the type of acid (oxalic and formic) and seaweed particle size range (0.295–0.495 and 0.146–0.246 mm). The extracted sodium alginate was then characterised in terms of FTIR, 1 H‐NMR, M/G ratio, viscosity and colour. The synergistic effect of the microwave‐ultrasound hybrid system for short timeframes (15 min each) successfully improved the alginate yield without compromising its structural composition, while allowing for a milder and greener organic acid to be used for the acid pre‐treatment. The highest alginate yield (~64 %) was obtained using formic acid and the smaller particle size range (0.146–0.246 mm). The latter thus highlights the importance of particle size reduction and optimisation. FTIR, NMR and viscosity analyses revealed a low guluronic acid content of alginate with a high M/G ratio (7.7±1.0–9.3±0.1) and low viscosity (2.92±0.09–3.05±0.06 cP), which was found to be inherent to the species used. The proposed novel method therefore opens prospects for the industry since it is both environmentally and economically sustainable.
- 1 November 2021
- Published by Taylor & Francis in Journal of Natural Fibers
- Vol. 19 (14) , 9600-9613
Slaked Lime Solution as a Viable Eco-friendly Treatment to Improve the Tensile Strength of Maize Stem Fibers
In this study, the effect of the environmentally friendly slaked lime solution on the tensile strength of maize stem fibers was investigated and compared with the tensile strength obtained with a 3% wt NaOH and 10% wt NaHCO3 solutions. Maize fibers from dried stems were manually extracted, cleaned, and treated with the respective three solutions at different soaking periods. The results showed that a maximum increase in tensile strength of 165.1% was obtained with the NaOH treatment (at 24 hours) followed by an increase of 107.1% (at 21 hours) for the Ca(OH)2, and a 46.6% (at 18 hours) increase for the NaHCO3 treatment. Analysis of the FTIR spectra revealed that the significant improvement in the tensile strength for the NaOH treatment is attributed to the partial transformation of cellulose I to cellulose II. However, the increase in the strength of the Ca(OH)2-treated fibers has been attributed first, to the significant reduction in the fiber cross-sectional area, second, to the removal of specific amorphous constituents such as hemicellulose, and to the formation of a stable calcium pectinate layer, which improves the fiber’s resistance to fracture.
- 1 November 2021
- Published by Taylor & Francis in Journal of Natural Fibers
- Vol. 19 (14) , 9600-9613
Slaked Lime Solution as a Viable Eco-friendly Treatment to Improve the Tensile Strength of Maize Stem Fibers
In this study, the effect of the environmentally friendly slaked lime solution on the tensile strength of maize stem fibers was investigated and compared with the tensile strength obtained with a 3% wt NaOH and 10% wt NaHCO3 solutions. Maize fibers from dried stems were manually extracted, cleaned, and treated with the respective three solutions at different soaking periods. The results showed that a maximum increase in tensile strength of 165.1% was obtained with the NaOH treatment (at 24 hours) followed by an increase of 107.1% (at 21 hours) for the Ca(OH)2, and a 46.6% (at 18 hours) increase for the NaHCO3 treatment. Analysis of the FTIR spectra revealed that the significant improvement in the tensile strength for the NaOH treatment is attributed to the partial transformation of cellulose I to cellulose II. However, the increase in the strength of the Ca(OH)2-treated fibers has been attributed first, to the significant reduction in the fiber cross-sectional area, second, to the removal of specific amorphous constituents such as hemicellulose, and to the formation of a stable calcium pectinate layer, which improves the fiber’s resistance to fracture.
- 20 August 2021
- Published by Springer Nature in Waste and Biomass Valorization
- Vol. 13 (2) , 1349-1361
Investigation of the Effect of the Fibre Inter-Node Length on the Tensile Strength of Maize Stem Fibres at Different Growth Stages
- 20 August 2021
- Published by Springer Nature in Waste and Biomass Valorization
- Vol. 13 (2) , 1349-1361
Investigation of the Effect of the Fibre Inter-Node Length on the Tensile Strength of Maize Stem Fibres at Different Growth Stages
- 15 July 2021
- Published by Springer Nature in Waste and Biomass Valorization
- Vol. 13 (1) , 255-269
Effective Treatment of Musa acuminata Fibre Using Wood Ash Solution to Produce Bio-Composite with Enhanced Mechanical Properties
- 15 July 2021
- Published by Springer Nature in Waste and Biomass Valorization
- Vol. 13 (1) , 255-269
Effective Treatment of Musa acuminata Fibre Using Wood Ash Solution to Produce Bio-Composite with Enhanced Mechanical Properties
- Open Access
- 31 March 2021
- Published by Springer Nature in Research Square
Variation in the Inter-Node Length During Plant Growth Influences the Tensile Strength of Maize Stem Fibres.
This study describes an investigation of the evolution of the mechanical and chemical properties of maize stem fibres with the growth stages of the plant, and how the tensile strength is influenced by the presence of nodes along the fibre length. Furthermore the variation of the tensile strength and chemical functional groups among four common maize varieties were determined. In this context, the fibres were characterised by performing tensile test, density & linear density tests, Fourier Transform infra-red spectroscopy (FTIR), X-ray diffraction (XRD), Thermo-gravimetric analysis (TGA) and surface morphology (SEM image analysis). The fibres were all extracted manually, and in some cases preceded by a water retting process for ten days. The thermal analysis, FTIR and x-ray results showed that in general the fibres from the different maize varieties and from the different growth stages are semi-crystalline in nature. The SEM micrographs revealed the presence of equi-spaced nodes along the fibre length, which are believed to be due to the growth stresses induced in the plant stem. The inter-node distance varied in relation to the growth stage of the plant, and yielded a good correlation (coefficient of 0.91) with the tensile strength of the fibres. Finally a better fibre yield was obtained from the stem at the senescence stage of the maize plant.
- 31 March 2021
- Published by Springer Nature in Research Square
Open AccessVariation in the Inter-Node Length During Plant Growth Influences the Tensile Strength of Maize Stem Fibres.
This study describes an investigation of the evolution of the mechanical and chemical properties of maize stem fibres with the growth stages of the plant, and how the tensile strength is influenced by the presence of nodes along the fibre length. Furthermore the variation of the tensile strength and chemical functional groups among four common maize varieties were determined. In this context, the fibres were characterised by performing tensile test, density & linear density tests, Fourier Transform infra-red spectroscopy (FTIR), X-ray diffraction (XRD), Thermo-gravimetric analysis (TGA) and surface morphology (SEM image analysis). The fibres were all extracted manually, and in some cases preceded by a water retting process for ten days. The thermal analysis, FTIR and x-ray results showed that in general the fibres from the different maize varieties and from the different growth stages are semi-crystalline in nature. The SEM micrographs revealed the presence of equi-spaced nodes along the fibre length, which are believed to be due to the growth stresses induced in the plant stem. The inter-node distance varied in relation to the growth stage of the plant, and yielded a good correlation (coefficient of 0.91) with the tensile strength of the fibres. Finally a better fibre yield was obtained from the stem at the senescence stage of the maize plant.
- 29 October 2020
- Published by Springer Nature in SN Applied Sciences
- Vol. 2 (11) , 1-13
Using infrared spectrum analyses to predict tensile strength of fibres in a group of closely related plant species: case of Mascarenes Pandanus spp.
- 29 October 2020
- Published by Springer Nature in SN Applied Sciences
- Vol. 2 (11) , 1-13
Using infrared spectrum analyses to predict tensile strength of fibres in a group of closely related plant species: case of Mascarenes Pandanus spp.
- 27 June 2020
- Published by Taylor & Francis in Composite Interfaces
- Vol. 28 (4) , 429-443
Hydroxyethylcellulose use simplifies mat manufacture and improves interfacial cohesion of alkaline-treated Pandanus utilis fibres in polyester composite
A simple method of bonding mutually perpendicular layers of alkaline-treated fibres, through the use of Hydroxyethylcellulose, has been studied as an alternative to woven fibre-mat. Following alkaline process optimisation by using the Taguchi DoE methodology, fibres treatment with 0.5% wt NaOH for 14 hours improved the tensile strength by 36% compared to the untreated fibres. Interfacial-Shear-Stress (measured by pull-out tests) was improved by 32% after the optimal alkaline-treatment. Furthermore, an improvement of 5% in Interfacial-Shear-Stress was achieved after a coating with 2 wt. % Hydroxyethylcellulose. Thus, Hydroxyethylcellulose increases the shear stress, and decreases friction without adverse impact on fibre strength.
- 27 June 2020
- Published by Taylor & Francis in Composite Interfaces
- Vol. 28 (4) , 429-443
Hydroxyethylcellulose use simplifies mat manufacture and improves interfacial cohesion of alkaline-treated Pandanus utilis fibres in polyester composite
A simple method of bonding mutually perpendicular layers of alkaline-treated fibres, through the use of Hydroxyethylcellulose, has been studied as an alternative to woven fibre-mat. Following alkaline process optimisation by using the Taguchi DoE methodology, fibres treatment with 0.5% wt NaOH for 14 hours improved the tensile strength by 36% compared to the untreated fibres. Interfacial-Shear-Stress (measured by pull-out tests) was improved by 32% after the optimal alkaline-treatment. Furthermore, an improvement of 5% in Interfacial-Shear-Stress was achieved after a coating with 2 wt. % Hydroxyethylcellulose. Thus, Hydroxyethylcellulose increases the shear stress, and decreases friction without adverse impact on fibre strength.
- 21 July 2019
- Published by Taylor & Francis in Journal of Natural Fibers
- Vol. 18 (4) , 607-619
Palm Leaves as Potential Natural-fibre Source for a Tropical Island Developing State
The mechanical and chemical properties of fibers, extracted from four Mascarene endemic palm species, were determined in the untreated and mercerized states. Tensile strength of the fibers increased by 26% for the Hurricane fibers and to 92% for Bottle palm. Fibers from the Blue Latan gave the highest strength of 208 MPa. TCI index suggests that increase in strength is due to the transformation of cellulose I to II. FTIR and DSC tests confirm that hemicellulose was not completely removed during mercerization; its complete removal will yield stronger fiber, making the Blue Latan fiber a potential candidate for composites manufacture.
- 21 July 2019
- Published by Taylor & Francis in Journal of Natural Fibers
- Vol. 18 (4) , 607-619
Palm Leaves as Potential Natural-fibre Source for a Tropical Island Developing State
The mechanical and chemical properties of fibers, extracted from four Mascarene endemic palm species, were determined in the untreated and mercerized states. Tensile strength of the fibers increased by 26% for the Hurricane fibers and to 92% for Bottle palm. Fibers from the Blue Latan gave the highest strength of 208 MPa. TCI index suggests that increase in strength is due to the transformation of cellulose I to II. FTIR and DSC tests confirm that hemicellulose was not completely removed during mercerization; its complete removal will yield stronger fiber, making the Blue Latan fiber a potential candidate for composites manufacture.