Xuejian Wang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Xuejian Wang has a total of 8 co-authors. Here are the top co-authors by number of shared publications:
- Enyu Guo
Key Laboratory of Solidification Control and Digital Preparation Technology (Liaoning Province), School of Materials Science and Engineering Dalian University of Technology Dalian China
2 shared publications - Tongmin Wang
Key Laboratory of Solidification Control and Digital Preparation Technology (Liaoning Province) School of Materials Science and Engineering Dalian University of Technology Dalian China
2 shared publications - Bingyang Gao
Key Laboratory of Solidification Control and Digital Preparation Technology (Liaoning Province), School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China
1 shared publication - Huijun Kang
Key Laboratory of Solidification Control and Digital Preparation Technology (Liaoning Province) School of Materials Science and Engineering Dalian University of Technology Dalian China
1 shared publication - Jing Ren
Key Laboratory of Solidification Control and Digital Preparation Technology (Liaoning Province), School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China
1 shared publication - Shuang Jun Nie
Key Laboratory of Solidification Control and Digital Preparation Technology (Liaoning Province), School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China
1 shared publication
Latest Publications
- Open Access
Influence of Alloyed Ga on the Microstructure and Corrosion Properties of As-Cast Mg–5Sn Alloys
In this paper, the microstructures and corrosion behaviors of as-cast Mg–5Sn–xGa alloys with varying Ga content (x = 0, 0.5, 1, 2, 3 wt %) were investigated. The results indicated that Ga could not only adequately refine the grain structure of the alloys, but could also improve the corrosion resistance. The microstructures of all alloys exhibited typical dendritic morphology. No Ga-rich secondary phases were detected when 0.5 wt % Ga was added, while only the morphology of Mg2Sn phase was changed. However, when the addition rate of Ga exceeded 0.5 wt %, an Mg5Ga2 intermetallic compound started to form from the interdendritic region. The volume fraction of Mg5Ga2 monotonically increased with the increasing Ga addition level. Although Mg5Ga2 phase was cathode phase, its pitting sensitivity was weaker than Mg2Sn. In addition, the standard potential of Ga (−0.55 V) was lower than that of Sn (−0.14 V), which relieved the driving force of the secondary phases for the micro-galvanic corrosion. An optimized composition of 3 wt % Ga was concluded based on the immersion tests and polarization measurements, which recorded the best corrosion resistance.
Open AccessInfluence of Alloyed Ga on the Microstructure and Corrosion Properties of As-Cast Mg–5Sn Alloys
In this paper, the microstructures and corrosion behaviors of as-cast Mg–5Sn–xGa alloys with varying Ga content (x = 0, 0.5, 1, 2, 3 wt %) were investigated. The results indicated that Ga could not only adequately refine the grain structure of the alloys, but could also improve the corrosion resistance. The microstructures of all alloys exhibited typical dendritic morphology. No Ga-rich secondary phases were detected when 0.5 wt % Ga was added, while only the morphology of Mg2Sn phase was changed. However, when the addition rate of Ga exceeded 0.5 wt %, an Mg5Ga2 intermetallic compound started to form from the interdendritic region. The volume fraction of Mg5Ga2 monotonically increased with the increasing Ga addition level. Although Mg5Ga2 phase was cathode phase, its pitting sensitivity was weaker than Mg2Sn. In addition, the standard potential of Ga (−0.55 V) was lower than that of Sn (−0.14 V), which relieved the driving force of the secondary phases for the micro-galvanic corrosion. An optimized composition of 3 wt % Ga was concluded based on the immersion tests and polarization measurements, which recorded the best corrosion resistance.
- Open Access
The Influence of Holding Time on the Microstructure Evolution of Mg–10Zn–6.8Gd–4Y Alloy during Semi-Solid Isothermal Heat Treatment
A semi-solid microstructure of Mg–10Zn–6.8Gd–4Y alloys is acquired via an isothermal heat treatment process, and the effects of the holding time on the microstructure evolution of Mg–10Zn–6.8Gd–4Y alloys are investigated. The results show that the microstructure of the cast alloy is composed of primary α-Mg dendritic grains with a eutectic structure (W-phase and eutectic Mg) distributed at the grain boundaries. The primary α-Mg dendritic grains grow in size with increasing holding time, and they tend to grow into more globular structures in the initial stage; they then become a bit more dendritic, as small branches grow from the grain boundaries after holding the sample at 580 °C for 10 min. Meanwhile, the interdiffusion of magnesium atoms within the eutectic region, and between the primary α-Mg and eutectic structure, leads to the formation of fine and relatively globular eutectic Mg grains in the eutectic structure after holding for 10 min. The eutectic Mg grains begin to grow, coarsen, coalesce, or be swallowed by the surrounding primary grains, causing fluctuations of the general grain size. Over the whole isothermal heat treatment process, two mechanisms—coalescence and Ostwald ripening—dominate the grain coarsening.
Open AccessThe Influence of Holding Time on the Microstructure Evolution of Mg–10Zn–6.8Gd–4Y Alloy during Semi-Solid Isothermal Heat Treatment
A semi-solid microstructure of Mg–10Zn–6.8Gd–4Y alloys is acquired via an isothermal heat treatment process, and the effects of the holding time on the microstructure evolution of Mg–10Zn–6.8Gd–4Y alloys are investigated. The results show that the microstructure of the cast alloy is composed of primary α-Mg dendritic grains with a eutectic structure (W-phase and eutectic Mg) distributed at the grain boundaries. The primary α-Mg dendritic grains grow in size with increasing holding time, and they tend to grow into more globular structures in the initial stage; they then become a bit more dendritic, as small branches grow from the grain boundaries after holding the sample at 580 °C for 10 min. Meanwhile, the interdiffusion of magnesium atoms within the eutectic region, and between the primary α-Mg and eutectic structure, leads to the formation of fine and relatively globular eutectic Mg grains in the eutectic structure after holding for 10 min. The eutectic Mg grains begin to grow, coarsen, coalesce, or be swallowed by the surrounding primary grains, causing fluctuations of the general grain size. Over the whole isothermal heat treatment process, two mechanisms—coalescence and Ostwald ripening—dominate the grain coarsening.