VVV. V. V’yUkhin

V. V. V’yUkhin

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


V. V. V’yUkhin has a total of 32 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Physico-chemical analysis of 12Kh18N9TL steel melts for quality control of cast products

    by D. P. Shvetsov, O. A. Chikova, V. S. Tsepelev, N. I. Sinitsin, V. V. V’yUkhin

    The authors studied the behavior of slag inclusions in four samples taken during casting of austenitic corrosion-resistant steel grade 12Kh18N9TL. The samples for the study were taken under production conditions after melting the charge ( 1 ), introducing Ti and FeMn, slag induction and additional loading ( 2 ), re-introducing Ti, slag induction ( 3 ), slag induction ( 4 ). The elemental composition and temperature of the melt were determined under production conditions. The physicochemical properties of the melts obtained from the selected samples were measured under laboratory conditions: surface tension and kinematic viscosity. The measurements were carried out in the temperature range from 1370 to 1760 °C in the mode of heating and subsequent cooling of the sample. When observing the sample during the measurement of surface tension, the release of slag inclusions from the volume of the drop occurs in the heating mode. During subsequent cooling of the formed drop of liquid steel, slag particles flow from the slag bath under the action of the Marangoni force. Analysis of the dependence of the slag particle ascent rate on its size showed that only particles up to 10 μm in size can remain in the melt volume, while larger particles have time to float to the surface of the liquid bath. It was found that slag particles up to 4 mm in size can flow onto the surface of the sample under the action of the Marangoni force. The volume fraction of slag inclusions was determined, and a correlation was established between it and the element composition of the sample. The authors made a conclusion about the effect of Ti additives in the melt as the cause of increase in the volume fraction of slag inclusions in the casting.

  • Open Access

    Microheterogeneous structure of liquid cast irons IChKh28N2 and ICh310Kh24M2F4TR

    by V. S. Tsepelev, N. I. Sinitsin, O. A. Chikova, M. G. Potapov, V. V. V’yUkhin

    The paper presents original experimental data on the viscosity and electrical resistivity of liquid cast irons IChKh28N2 and ICh310Kh24M2F4TR. The authors discuss the measurement results within the framework of the concept of metal melts microheterogeneity. Liquid cast iron in a micro­heterogeneous state is considered as a dispersed system consisting of dispersed Fe – 30 % Cr particles distributed in a Fe – 3 % C dispersion medium. The concept of colloidal microheterogeneity (microheterogeneity) of Fe – C melts was first formulated by Wertman & Samarin more than 80 years ago and found another confirmation in this work. The introduction of theoretical approaches to the rheology of dispersed systems into the analysis of the temperature dependences of the viscosity of microheterogeneous melts made it possible to estimate the parameters of microheterogeneity: the volume fraction and size of dispersed particles. The volume fraction of dispersed particles was determined using the Taylor equation for the viscosity of dispersed systems and size of dispersed particles – within the framework of the theory of absolute reaction rates. Analysis of the temperature dependences of microheterogeneous melts electrical resistivity within the framework of the theory of transport phenomena (in this case, conductivity) in inhomogeneous media (microheterogeneous melts) made it possible to estimate the volume fraction of dispersed particles. The volume fraction of dispersed particles based on data on the electrical resistivity of liquid cast iron was determined using the Odelevsky equation for the inhomogeneous media conductivity. The cluster size was determined by the ratio of the melt electrical resistivity at the liquidus temperature and the analysis temperature, taking into account the known data for the mean free path and the electron scattering coefficient of liquid iron. The volume fraction of dispersed particles in liquid cast iron was 0.2 – 0.1 at the liquidus temperature. With increasing temperature, the volume fraction of dispersed particles decreases. The cluster size in liquid cast iron was about 3 nm at the liquidus temperature, and with increasing temperature the cluster size decreased to 1 – 2 nm. The results obtained are of practical importance: increasing the performance properties of cast iron castings is possible by high-temperature melt treatment (HTMT) in order to change the crystallization conditions and obtain a modified structure. Studies of the microheterogeneous structure of liquid cast irons and assessment of microheterogeneity parameters make it possible to substantiate and propose the optimal HTMT mode in order to improve the performance characteristics of products made of wear-resistant cast irons alloyed with chromium.


  • Open Access

    Structural changes in the melt of a heat-resistant nickel alloy as phase transition of the second order

    by O. B. Mil’dEr, D. A. Tarasov, A. G. Tyagunov, V. S. Tsepelev, V. V. V’yUkhin, A. L. Levonyan, O. V. Anoshina, В . С. Цепелев

    Information about the behavior of melts of the high-temperature nickel alloys is the basis for creating new smelting technologies that significantly increase the service properties of metal products, as well as solve a number of technological problems. The results of numerous studies indicate structural changes occurring in various metal melts under the influence of temperature and time. For many years, there has been a scientific discussion about the nature of these phenomena, and a common opinion was formulated on a number of issues. Structural changes in metallic liquids are presented as a second-order phase transition, where a liquid of higher density is replaced by a liquid of lower density. These transformations in the structures of liquid metals are called liquid-liquid transition (LLT). Studies of the structure-sensitive properties of melts of the heat-resistant nickel alloys also reveal structural changes that irreversibly transform the melt into a microhomogeneous state. The research results presented in this article confirmed that structural changes in melts of the high-temperature nickel alloys are also a second-order phase transition, as evidenced by the breakage of atomic microgroups, uniform redistribution of alloying elements, and the formation of new clusters characterized by smaller sizes and greater chemical homogeneity. Therefore, these changes can be characterized as LLT, while this does not contradict the previously substantiated quasi-crystalline model of the microinhomogeneous state of liquid heat-resistant nickel alloys.

  • Electrical Resistivity of Liquid Fe–Mn Alloys

    by O. A. Chikova, N. I. Sinitsin, V. V. V’yUkhin


  • Open Access

    Thermophysical Properties of the Fe48Cr15Mo14C15B6Y2 Alloy in Liquid State

    by Dmytro S. Kozak, Vladimir S. Tsepelev, Viktor V. Konaskov, Viktor V. Vyukhin, Vladislav Y. Zadorozhnyy, Andrey I. Bazlov, Askar R. Kvaratskheliya, Andrey A. Tsarkov, Jan F. M. Van Impe

    In this work, the physical properties of Fe48Cr15Mo14C15B6Y2 alloy in liquid state at high temperature are studied. It was observed that the basic physical characteristics of the alloy, such as viscosity, electrical resistivity, and density, decrease with an increase of the temperature to 1700 °C. An abnormal increasing rate of viscosity for Fe48Cr15Mo14C15B6Y2 alloy in the temperature range from 1360 to 1550 °C was noted. The measurement of the electrical resistivity and density did not reveal any anomalies in the same temperature range.


  • Open Access

    Influence of melt superheating treatment on cast structure of Al–Sn alloys

    by O. A. Chikova, V. V. Vyukhin, V. S. Tsepelev

    The study covers the effect of Melt Superheating Treatment (MST) for Al–Sn alloys. To determine the optimal superheating temperature, the authors measured the temperature dependences of the kinematic viscosity, electrical resistivity, density and surface tension of Al–Sn melts with tin contents of 10, 20, 30, 40, and 50 wt.%. According to the measurement results, the temperature t* was determined for each Al–Sn alloy sample. Heating to this temperature breaks down the micro-inhomogeneous state and leads to the heterogeneous liquid – homogeneous liquid structural transition. Melt superheating (MST) results in a decrease in melt viscosity. It was found that the temperature t* rises with increasing tin concentration in the Al–Sn melt. An increase in the tin content in the Al–Sn melt also leads to a decrease in the absolute values of kinematic viscosity and surface tension, while the electrical resistivity and density increase accordingly. Thus, the Melt Superheating Treatment (MST) mode for Al–Sn alloys was determined. The effect of MST of Al–50wt.%Sn melt on the microstructure and mechanical properties of the ingot was studied in order to determine the structural sensitivity to the degree of melt overheating, and to find a new strategy to improve the shaping ability of the Al–Sn alloy two-phase structure. The results demonstrated that the method of resistivity and viscosity determination are more sensitive and effective for melt superheating temperature (MST mode) evaluation. In addition, the desired modified Al–Sn ingot structure can be formed under normal casting conditions; MST can contribute to the modified ingot structure formation by increasing the solidification time and decreasing the average solidification rate by reducing melt viscosity after superheating.

  • Viscosity of the Samarium and Co–25% Sm–18% Fe–5% Cu–3% Zr Alloy Melts

    by I. V. Slinkin, O. A. Chikova, V. V. V’YUkhin

    The kinematic viscosities of the melts of samarium (99.9% Sm) and Co–25% Sm–18% Fe–5% Cu–3% Zr alloy are measured by the oscillating crucible method. The studies have been performed to optimize the parameters of the metallurgical manufacturing of sintered permanent KS25 magnets (Co–25% Sm–18% Fe–5% Cu–3% Zr).

  • Viscosity of Cu–Ni Melts

    by O. A. Chikova, G. A. Tkachuk, V. V. V’YUkhin

    The kinematic viscosity of Cu–Ni melts with nickel contents of 10, 20, 30, 40, 50, 60, 70, 80, and 90 at % is measured. Kinematic viscosity is measured using the damped torsional vibrations...


  • Open Access

    THE INVESTIGATION OF PHYSICAL PROPERTIES OF «IRON» METEORITE MELTS

    by V. S. Tsepelev, Array М. Поводатор, V. I. Grokhovskii, V. V. V’yUkhin, V. V. Konashkov, Array С. Цепелев, Array И. Гроховский

    ИССЛЕДОВАНИЕ ФИЗИЧЕСКИХ СВОЙСТВ РАСПЛАВОВ «ЖЕЛЕЗНЫХ» МЕТЕОРИТОВ