N. I. Sinitsin
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
N. I. Sinitsin has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
O. A. Chikova
Ural Federal University named after the first President of Russia B.N. Yeltsin; Ural State Pedagogical University
8 shared publicationsV. V. V’YUkhin
Ural Federal University, Yekaterinburg, Russia
5 shared publications- Olga Anatolievna Chikova
Ural Federal University named after the first President of Russia B.N. Yeltsin
4 shared publications - V. V. V’yUkhin
Ural Federal University named after the first President of Russia B.N. Yeltsin
4 shared publications - Vladimir S. Tsepelev
Ural Federal University named after the first President of Russia B.N. Yeltsin
3 shared publications - D. P. Shvetsov
Ural Federal University named after the first President of Russia B.N. Yeltsin; LLC “Precision Casting Center
1 shared publication
Latest Publications
- Open Access
- 8 November 2025
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 68 (5) , 534-542
Physico-chemical analysis of 12Kh18N9TL steel melts for quality control of cast products
The authors studied the behavior of slag inclusions in four samples taken during casting of austenitic corrosion-resistant steel grade 12Kh18N9TL. The samples for the study were taken under production conditions after melting the charge ( 1 ), introducing Ti and FeMn, slag induction and additional loading ( 2 ), re-introducing Ti, slag induction ( 3 ), slag induction ( 4 ). The elemental composition and temperature of the melt were determined under production conditions. The physicochemical properties of the melts obtained from the selected samples were measured under laboratory conditions: surface tension and kinematic viscosity. The measurements were carried out in the temperature range from 1370 to 1760 °C in the mode of heating and subsequent cooling of the sample. When observing the sample during the measurement of surface tension, the release of slag inclusions from the volume of the drop occurs in the heating mode. During subsequent cooling of the formed drop of liquid steel, slag particles flow from the slag bath under the action of the Marangoni force. Analysis of the dependence of the slag particle ascent rate on its size showed that only particles up to 10 μm in size can remain in the melt volume, while larger particles have time to float to the surface of the liquid bath. It was found that slag particles up to 4 mm in size can flow onto the surface of the sample under the action of the Marangoni force. The volume fraction of slag inclusions was determined, and a correlation was established between it and the element composition of the sample. The authors made a conclusion about the effect of Ti additives in the melt as the cause of increase in the volume fraction of slag inclusions in the casting.
- 8 November 2025
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 68 (5) , 534-542
Open AccessPhysico-chemical analysis of 12Kh18N9TL steel melts for quality control of cast products
The authors studied the behavior of slag inclusions in four samples taken during casting of austenitic corrosion-resistant steel grade 12Kh18N9TL. The samples for the study were taken under production conditions after melting the charge ( 1 ), introducing Ti and FeMn, slag induction and additional loading ( 2 ), re-introducing Ti, slag induction ( 3 ), slag induction ( 4 ). The elemental composition and temperature of the melt were determined under production conditions. The physicochemical properties of the melts obtained from the selected samples were measured under laboratory conditions: surface tension and kinematic viscosity. The measurements were carried out in the temperature range from 1370 to 1760 °C in the mode of heating and subsequent cooling of the sample. When observing the sample during the measurement of surface tension, the release of slag inclusions from the volume of the drop occurs in the heating mode. During subsequent cooling of the formed drop of liquid steel, slag particles flow from the slag bath under the action of the Marangoni force. Analysis of the dependence of the slag particle ascent rate on its size showed that only particles up to 10 μm in size can remain in the melt volume, while larger particles have time to float to the surface of the liquid bath. It was found that slag particles up to 4 mm in size can flow onto the surface of the sample under the action of the Marangoni force. The volume fraction of slag inclusions was determined, and a correlation was established between it and the element composition of the sample. The authors made a conclusion about the effect of Ti additives in the melt as the cause of increase in the volume fraction of slag inclusions in the casting.
- Open Access
- 29 October 2024
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 67 (5) , 579-592
Microheterogeneous structure of liquid cast irons IChKh28N2 and ICh310Kh24M2F4TR
The paper presents original experimental data on the viscosity and electrical resistivity of liquid cast irons IChKh28N2 and ICh310Kh24M2F4TR. The authors discuss the measurement results within the framework of the concept of metal melts microheterogeneity. Liquid cast iron in a microheterogeneous state is considered as a dispersed system consisting of dispersed Fe – 30 % Cr particles distributed in a Fe – 3 % C dispersion medium. The concept of colloidal microheterogeneity (microheterogeneity) of Fe – C melts was first formulated by Wertman & Samarin more than 80 years ago and found another confirmation in this work. The introduction of theoretical approaches to the rheology of dispersed systems into the analysis of the temperature dependences of the viscosity of microheterogeneous melts made it possible to estimate the parameters of microheterogeneity: the volume fraction and size of dispersed particles. The volume fraction of dispersed particles was determined using the Taylor equation for the viscosity of dispersed systems and size of dispersed particles – within the framework of the theory of absolute reaction rates. Analysis of the temperature dependences of microheterogeneous melts electrical resistivity within the framework of the theory of transport phenomena (in this case, conductivity) in inhomogeneous media (microheterogeneous melts) made it possible to estimate the volume fraction of dispersed particles. The volume fraction of dispersed particles based on data on the electrical resistivity of liquid cast iron was determined using the Odelevsky equation for the inhomogeneous media conductivity. The cluster size was determined by the ratio of the melt electrical resistivity at the liquidus temperature and the analysis temperature, taking into account the known data for the mean free path and the electron scattering coefficient of liquid iron. The volume fraction of dispersed particles in liquid cast iron was 0.2 – 0.1 at the liquidus temperature. With increasing temperature, the volume fraction of dispersed particles decreases. The cluster size in liquid cast iron was about 3 nm at the liquidus temperature, and with increasing temperature the cluster size decreased to 1 – 2 nm. The results obtained are of practical importance: increasing the performance properties of cast iron castings is possible by high-temperature melt treatment (HTMT) in order to change the crystallization conditions and obtain a modified structure. Studies of the microheterogeneous structure of liquid cast irons and assessment of microheterogeneity parameters make it possible to substantiate and propose the optimal HTMT mode in order to improve the performance characteristics of products made of wear-resistant cast irons alloyed with chromium.
- 29 October 2024
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 67 (5) , 579-592
Open AccessMicroheterogeneous structure of liquid cast irons IChKh28N2 and ICh310Kh24M2F4TR
The paper presents original experimental data on the viscosity and electrical resistivity of liquid cast irons IChKh28N2 and ICh310Kh24M2F4TR. The authors discuss the measurement results within the framework of the concept of metal melts microheterogeneity. Liquid cast iron in a microheterogeneous state is considered as a dispersed system consisting of dispersed Fe – 30 % Cr particles distributed in a Fe – 3 % C dispersion medium. The concept of colloidal microheterogeneity (microheterogeneity) of Fe – C melts was first formulated by Wertman & Samarin more than 80 years ago and found another confirmation in this work. The introduction of theoretical approaches to the rheology of dispersed systems into the analysis of the temperature dependences of the viscosity of microheterogeneous melts made it possible to estimate the parameters of microheterogeneity: the volume fraction and size of dispersed particles. The volume fraction of dispersed particles was determined using the Taylor equation for the viscosity of dispersed systems and size of dispersed particles – within the framework of the theory of absolute reaction rates. Analysis of the temperature dependences of microheterogeneous melts electrical resistivity within the framework of the theory of transport phenomena (in this case, conductivity) in inhomogeneous media (microheterogeneous melts) made it possible to estimate the volume fraction of dispersed particles. The volume fraction of dispersed particles based on data on the electrical resistivity of liquid cast iron was determined using the Odelevsky equation for the inhomogeneous media conductivity. The cluster size was determined by the ratio of the melt electrical resistivity at the liquidus temperature and the analysis temperature, taking into account the known data for the mean free path and the electron scattering coefficient of liquid iron. The volume fraction of dispersed particles in liquid cast iron was 0.2 – 0.1 at the liquidus temperature. With increasing temperature, the volume fraction of dispersed particles decreases. The cluster size in liquid cast iron was about 3 nm at the liquidus temperature, and with increasing temperature the cluster size decreased to 1 – 2 nm. The results obtained are of practical importance: increasing the performance properties of cast iron castings is possible by high-temperature melt treatment (HTMT) in order to change the crystallization conditions and obtain a modified structure. Studies of the microheterogeneous structure of liquid cast irons and assessment of microheterogeneity parameters make it possible to substantiate and propose the optimal HTMT mode in order to improve the performance characteristics of products made of wear-resistant cast irons alloyed with chromium.
- 2 October 2024
- Published by Elsevier in Physica B: Condensed Matter
- Vol. 695
Abnormal resistivity behavior of Co–Cu alloys and responsible metastable liquid phase separation
- 2 October 2024
- Published by Elsevier in Physica B: Condensed Matter
- Vol. 695
Abnormal resistivity behavior of Co–Cu alloys and responsible metastable liquid phase separation
- Open Access
- 8 April 2022
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 65 (3) , 179-187
Thermodynamic stability of microheterogenic states in Fe – Mn – C melts
Possibility of existence of microheterogeneous states in Fe – Mn – C melts was analyzed carried out according to the concepts of chemical thermodynamics. Microheterogeneous state of a chemically inhomogeneous Fe – Mn – C melt was understood as presence of dispersed Fe – C particles in it, which are suspended in Mn – C environment and separated from it by interface. Hypothesis of microheterogeneous state of Fe – Mn – C melts is supported by numerous experimental data on their thermodynamic and physical properties. Identification of anomalies in temperature dependences of physical properties of Fe – Mn – C melts made it possible to determine temperature values above which the melt superheating treatment (MST) leads to destruction of microheterogeneity, i.e., the liquid – liquid structure transition (LLT) in the melt. LLT is understood by authors as a structural transition “microheterogeneous melt – homogeneous solution” and this is expressed in destruction of microheterogeneous state when the melt is heated to a temperature determined for each composition (MST). This paper describes a method for theoretical determination of temperature range where microheterogeneous state of the Fe – Mn – C melt is thermodynamically stable. Thermodynamic stability of dispersed Fe – C particles in the Mn – C medium was estimated according to the equations proposed by Kaptay for a regular solution. It was assumed that interface between the melt of dispersed Fe – C particles with sizes from 2 to 34 nm, distributed in the Mn – C dispersion medium and separated from it by an interface with increased carbon content. This result of the assessment is consistent with the data on size of the structural units of a viscous flow obtained earlier within framework of the theory of absolute reaction rates.
- 8 April 2022
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 65 (3) , 179-187
Open AccessThermodynamic stability of microheterogenic states in Fe – Mn – C melts
Possibility of existence of microheterogeneous states in Fe – Mn – C melts was analyzed carried out according to the concepts of chemical thermodynamics. Microheterogeneous state of a chemically inhomogeneous Fe – Mn – C melt was understood as presence of dispersed Fe – C particles in it, which are suspended in Mn – C environment and separated from it by interface. Hypothesis of microheterogeneous state of Fe – Mn – C melts is supported by numerous experimental data on their thermodynamic and physical properties. Identification of anomalies in temperature dependences of physical properties of Fe – Mn – C melts made it possible to determine temperature values above which the melt superheating treatment (MST) leads to destruction of microheterogeneity, i.e., the liquid – liquid structure transition (LLT) in the melt. LLT is understood by authors as a structural transition “microheterogeneous melt – homogeneous solution” and this is expressed in destruction of microheterogeneous state when the melt is heated to a temperature determined for each composition (MST). This paper describes a method for theoretical determination of temperature range where microheterogeneous state of the Fe – Mn – C melt is thermodynamically stable. Thermodynamic stability of dispersed Fe – C particles in the Mn – C medium was estimated according to the equations proposed by Kaptay for a regular solution. It was assumed that interface between the melt of dispersed Fe – C particles with sizes from 2 to 34 nm, distributed in the Mn – C dispersion medium and separated from it by an interface with increased carbon content. This result of the assessment is consistent with the data on size of the structural units of a viscous flow obtained earlier within framework of the theory of absolute reaction rates.
- 1 January 2022
- Published by Pleiades Publishing Ltd in Physics of Metals and Metallography
- Vol. 123 (1) , 85-91
Effect of Crystallization Conditions on the Microstructure, Crystal Structure, and Mechanical Properties of a Fe–Mn–C Alloy in Microvolumes
The results of the comparative study of the microstructure, crystal structure, and mechanical properties in microvolumes of the Fe–25 wt % Mn–2 wt % С alloy crystallized from melt in different structural states—homogeneous and heterogeneous—were presented. The study was performed by means of scanning electron microscopy Energy Dispersive X-Ray Spectroscopy (EDX), electron backscatter diffraction (EBSD), and nanoindentation. The destruction of microheterogeneity in the Fe–Mn–C melts was established to lead to an increase in the dendrite parameter, the size of crystallites, and the fraction of low-angle boundaries under cooling and further crystallization. The surface of austenite dendrites was revealed to contain manganese-rich liquation layers, which had a thickness 〈L〉 = 60 µm and a manganese content of 35–40% and led to deformation nonuniformity of an ingot. The adhesion strength of the liquation layer to the body of an austenite dendrite was estimated as Kint = 9.6–13.1 MPa m0.5 and could not be a reason for the destruction of an ingot.
- 1 January 2022
- Published by Pleiades Publishing Ltd in Physics of Metals and Metallography
- Vol. 123 (1) , 85-91
Effect of Crystallization Conditions on the Microstructure, Crystal Structure, and Mechanical Properties of a Fe–Mn–C Alloy in Microvolumes
The results of the comparative study of the microstructure, crystal structure, and mechanical properties in microvolumes of the Fe–25 wt % Mn–2 wt % С alloy crystallized from melt in different structural states—homogeneous and heterogeneous—were presented. The study was performed by means of scanning electron microscopy Energy Dispersive X-Ray Spectroscopy (EDX), electron backscatter diffraction (EBSD), and nanoindentation. The destruction of microheterogeneity in the Fe–Mn–C melts was established to lead to an increase in the dendrite parameter, the size of crystallites, and the fraction of low-angle boundaries under cooling and further crystallization. The surface of austenite dendrites was revealed to contain manganese-rich liquation layers, which had a thickness 〈L〉 = 60 µm and a manganese content of 35–40% and led to deformation nonuniformity of an ingot. The adhesion strength of the liquation layer to the body of an austenite dendrite was estimated as Kint = 9.6–13.1 MPa m0.5 and could not be a reason for the destruction of an ingot.
- 4 December 2021
- Published by Pleiades Publishing Ltd in Russian Journal of Physical Chemistry A
- Vol. 95 (12) , 2492-2498
Surface Tension of Fe–Mn–C Melts
The results of surface tension measurements for melts of the Fe–Mn–C system with 5.0–25.0 wt % Mn and 0.4–2.2 wt % C were given. Anomalies in the temperature dependences of the surface tension coefficient of Fe–Mn–C melts were found, which are interpreted as evidence for the irreversible destruction of microheterogeneity. The microheterogeneity destruction temperature was determined.
- 4 December 2021
- Published by Pleiades Publishing Ltd in Russian Journal of Physical Chemistry A
- Vol. 95 (12) , 2492-2498
Surface Tension of Fe–Mn–C Melts
The results of surface tension measurements for melts of the Fe–Mn–C system with 5.0–25.0 wt % Mn and 0.4–2.2 wt % C were given. Anomalies in the temperature dependences of the surface tension coefficient of Fe–Mn–C melts were found, which are interpreted as evidence for the irreversible destruction of microheterogeneity. The microheterogeneity destruction temperature was determined.
- 1 October 2021
- Published by Springer Nature in Russian Physics Journal
- Vol. 64 (6) , 1039-1046
Electrical Resistivity of Liquid Fe–Mn Alloys
- 1 October 2021
- Published by Springer Nature in Russian Physics Journal
- Vol. 64 (6) , 1039-1046
Electrical Resistivity of Liquid Fe–Mn Alloys
- 30 September 2021
- Published by Ore and Metals Publishing House in Chernye Metally
- p. 62-68
Influence of microheterogeneity destruction on microstructure and crystal structure of Fe-12% Mn-1%C alloy ingots
The results of comparative analysis of microstructure, crystal structure and mechanical properties in submicrovolumes of Fe-12%(wt.)Mn-1%(wt.)C alloys crystallized from the melt in different structural state: with destruction and without destruction of microheterogeneity are presented. Earlier, the authors found that overheating of the Fe-12%(wt.)Mn-1%(wt.)C melt to a temperature of 1700 °C leads to destruction of microheterogeneity, which changes the crystallization conditions of the ingot. Microheterogeneity means the presence in the melt of dispersed particles enriched in iron, which are suspended in an environment of a different composition and separated from it by a clear interfacial surface. The study of alloys was performed by scanning electron microscopy, energy dispersion analysis (EDS), the method of backscattered electron diffraction (EBSD) and nanoindentation. It was found that the destruction of the microheterogeneity of Fe-12%(wt.)Mn-1%(wt.)C melts during cooling and subsequent crystallization led to an increase in the dendritic parameter from 85 to 120 μm with increasing length of secondary branches of dendrites, crystallite size and small angle borders. Regardless of the crystallization conditions, manganese-enriched liquation layers with a thickness of L ~ 70–120 μm with a manganese content of 20 % (wt.) are formed on the surface of austenite dendrites, which leads to deformation inhomogeneity of the ingot. Based on the nanoindentation data, it is calculated that the adhesion of the manganese-enriched segregation layer to the body of austenite dendrites (Kint) for the sample crystallized after destruction of the microheterogeneous state increased by 1.2 times. The fracture energy along the boundary layer and the austenite dendrite body (Gc) also increased by 1.4 times. Average hardness values of the Young’s modulus of austenite dendrites did not change after the destruction of microheterogeneity. The mechanical characteristics of the ingot crystallized after the destruction of the microheterogeneity of the Fe-12%(wt.)Mn-1%(wt.)C melt under impact load generally improved.The work was performed using the equipment of UrSU UCSU “Modern Nanotechnology”.The study was performed with the financial support of the Russian Foundation for Basic Research within the research project No. 19-33-90198.
- 30 September 2021
- Published by Ore and Metals Publishing House in Chernye Metally
- p. 62-68
Influence of microheterogeneity destruction on microstructure and crystal structure of Fe-12% Mn-1%C alloy ingots
The results of comparative analysis of microstructure, crystal structure and mechanical properties in submicrovolumes of Fe-12%(wt.)Mn-1%(wt.)C alloys crystallized from the melt in different structural state: with destruction and without destruction of microheterogeneity are presented. Earlier, the authors found that overheating of the Fe-12%(wt.)Mn-1%(wt.)C melt to a temperature of 1700 °C leads to destruction of microheterogeneity, which changes the crystallization conditions of the ingot. Microheterogeneity means the presence in the melt of dispersed particles enriched in iron, which are suspended in an environment of a different composition and separated from it by a clear interfacial surface. The study of alloys was performed by scanning electron microscopy, energy dispersion analysis (EDS), the method of backscattered electron diffraction (EBSD) and nanoindentation. It was found that the destruction of the microheterogeneity of Fe-12%(wt.)Mn-1%(wt.)C melts during cooling and subsequent crystallization led to an increase in the dendritic parameter from 85 to 120 μm with increasing length of secondary branches of dendrites, crystallite size and small angle borders. Regardless of the crystallization conditions, manganese-enriched liquation layers with a thickness of L ~ 70–120 μm with a manganese content of 20 % (wt.) are formed on the surface of austenite dendrites, which leads to deformation inhomogeneity of the ingot. Based on the nanoindentation data, it is calculated that the adhesion of the manganese-enriched segregation layer to the body of austenite dendrites (Kint) for the sample crystallized after destruction of the microheterogeneous state increased by 1.2 times. The fracture energy along the boundary layer and the austenite dendrite body (Gc) also increased by 1.4 times. Average hardness values of the Young’s modulus of austenite dendrites did not change after the destruction of microheterogeneity. The mechanical characteristics of the ingot crystallized after the destruction of the microheterogeneity of the Fe-12%(wt.)Mn-1%(wt.)C melt under impact load generally improved.The work was performed using the equipment of UrSU UCSU “Modern Nanotechnology”.The study was performed with the financial support of the Russian Foundation for Basic Research within the research project No. 19-33-90198.
- 31 May 2021
- Published by Pleiades Publishing Ltd in Russian Journal of Physical Chemistry A
- Vol. 95 (5) , 902-909
Viscosity of Al–In Melts
Original experimental data on the viscosity of liquid Al–In alloys are presented. Measuring results are discussed within the concept of microheterogeneity of metal melts in the context of studying the conditions for the existence of microheterogeneity. Based on the experimental data, a conclusion is reached about the patterns of the evolution of microheterogeneity upon a change in the melt temperature, and a numerical estimate is made of the parameters of the microheterogeneous structure of liquid Al–In alloys, particularly the size of dispersed particles.
- 31 May 2021
- Published by Pleiades Publishing Ltd in Russian Journal of Physical Chemistry A
- Vol. 95 (5) , 902-909
Viscosity of Al–In Melts
Original experimental data on the viscosity of liquid Al–In alloys are presented. Measuring results are discussed within the concept of microheterogeneity of metal melts in the context of studying the conditions for the existence of microheterogeneity. Based on the experimental data, a conclusion is reached about the patterns of the evolution of microheterogeneity upon a change in the melt temperature, and a numerical estimate is made of the parameters of the microheterogeneous structure of liquid Al–In alloys, particularly the size of dispersed particles.
- 1 February 2021
- Published by Pleiades Publishing Ltd in Russian Journal of Physical Chemistry A
- Vol. 95 (2) , 244-249
Viscosity of Fe–Mn–С Melts
The kinematic viscosity of Fe–Mn–C melts is measured with Mn contents of 5.0, 7.5, 10.0, 12.0, 15.0, 17.5, 20.0, and 25.0 wt % and C contents of 0.4 to 2.2 wt %. The kinematic viscosity is measured using damped torsional vibrations of a crucible with a melt upon the heating and subsequent cooling of the samples. The temperatures at which the characteristics of the viscous flow change and the liquid–liquid structural transition occurs in Fe–Mn–C melts are determined using the results from measuring the kinematic viscosity.
- 1 February 2021
- Published by Pleiades Publishing Ltd in Russian Journal of Physical Chemistry A
- Vol. 95 (2) , 244-249
Viscosity of Fe–Mn–С Melts
The kinematic viscosity of Fe–Mn–C melts is measured with Mn contents of 5.0, 7.5, 10.0, 12.0, 15.0, 17.5, 20.0, and 25.0 wt % and C contents of 0.4 to 2.2 wt %. The kinematic viscosity is measured using damped torsional vibrations of a crucible with a melt upon the heating and subsequent cooling of the samples. The temperatures at which the characteristics of the viscous flow change and the liquid–liquid structural transition occurs in Fe–Mn–C melts are determined using the results from measuring the kinematic viscosity.