- Do Haeng Hur
Materials Safety Technology Development Division, Korea Atomic Energy Research Institute, Daejeon 34057, Republic of Korea
12 shared publications - Soon-Hyeok Jeon
Materials Safety Technology Development Division, Korea Atomic Energy Research Institute, Daejeon 34057, Republic of Korea
10 shared publications Soon-Hyeok Jeon
7 shared publicationsDo Haeng Hur
3 shared publications- Jeoh Han
Materials Safety Technology Development Division, Korea Atomic Energy Research Institute, Daejeon 34057, Korea
3 shared publications - Yeong-Ho Son
Nuclear Materials Research Division, Korea Atomic Energy Research Institute, 989-111, Daedeok-daero, Yuseong-gu, Daejeon 34057, Korea
3 shared publications
Latest Publications
- Open Access
Comparison of Durability and Gamma-Ray Shielding Performance of High-Velocity Oxygen Fuel Tungsten Carbide-Based Coatings on Cold-Rolled Steel Surface
This paper provides a comparative evaluation of the mechanical properties, corrosion resistance, and gamma-ray shielding performance of four different types of tungsten carbide (WC)-NiCr coatings deposited on cold-rolled steel surfaces, which are used as materials for low- and intermediate-level radioactive waste (LILW) storage containers. The four types of coatings were classified as WC-85, WC-73, WC-66, and WC-39 according to their WC content and were applied to the cold-rolled steel surfaces using the High-Velocity Oxygen Fuel (HVOF) spraying process. The performance of the layered coatings was analyzed in terms of their microstructure, hardness, wear resistance, adhesion strength, corrosion properties, and gamma-ray shielding characteristics. Coatings with elevated WC contents showed enhanced mechanical properties and gamma-ray shielding effectiveness, whereas coatings with relatively lower WC contents and higher NiCr contents exhibited greater corrosion resistance. This paper discusses the performance of WC-NiCr coatings from the viewpoint of enhancing the durability and safety of commercial LILW storage containers.
Open AccessComparison of Durability and Gamma-Ray Shielding Performance of High-Velocity Oxygen Fuel Tungsten Carbide-Based Coatings on Cold-Rolled Steel Surface
This paper provides a comparative evaluation of the mechanical properties, corrosion resistance, and gamma-ray shielding performance of four different types of tungsten carbide (WC)-NiCr coatings deposited on cold-rolled steel surfaces, which are used as materials for low- and intermediate-level radioactive waste (LILW) storage containers. The four types of coatings were classified as WC-85, WC-73, WC-66, and WC-39 according to their WC content and were applied to the cold-rolled steel surfaces using the High-Velocity Oxygen Fuel (HVOF) spraying process. The performance of the layered coatings was analyzed in terms of their microstructure, hardness, wear resistance, adhesion strength, corrosion properties, and gamma-ray shielding characteristics. Coatings with elevated WC contents showed enhanced mechanical properties and gamma-ray shielding effectiveness, whereas coatings with relatively lower WC contents and higher NiCr contents exhibited greater corrosion resistance. This paper discusses the performance of WC-NiCr coatings from the viewpoint of enhancing the durability and safety of commercial LILW storage containers.
- Open Access
- 23 July 2024
- Published by Elsevier in Nuclear Engineering and Technology
- Vol. 56 (12) , 5405-5413
Defect monitoring system of the internal structures of a sodium fast reactor using an artificial intelligence model
- 23 July 2024
- Published by Elsevier in Nuclear Engineering and Technology
- Vol. 56 (12) , 5405-5413
Open AccessDefect monitoring system of the internal structures of a sodium fast reactor using an artificial intelligence model
- Open Access
- 23 May 2023
- Published by Elsevier in Nuclear Engineering and Technology
- Vol. 55 (9) , 3183-3193
Radiochemical behavior of nitrogen species in high temperature water
- 23 May 2023
- Published by Elsevier in Nuclear Engineering and Technology
- Vol. 55 (9) , 3183-3193
Open AccessRadiochemical behavior of nitrogen species in high temperature water
- Open Access
On the Use of NaOH Solution to Simulate the Crevice Conditions of a Nuclear Steam Generator
The corrosion behavior and integrity of steam generator (SG) tube materials have frequently been tested in solutions containing sodium hydroxide (NaOH), assuming that NaOH is a typical contaminant concentrated in the crevices of SGs in a pressurized water reactor. The purpose of this study was to investigate the adequacy of using concentrated NaOH solutions to simulate the crevice environments of SGs. The dissolution behavior of magnetite deposit flakes formed in an operating SG was tested in a 0.4 wt.% NaOH solution at 300 °C, and the thermodynamic stability of magnetite was investigated using the potential-pH diagram for an iron–water system. The magnetite deposits were rapidly dissolved in the test solution, which was supported by the fact that magnetite is thermodynamically unstable under the test condition to dissolve to dihypoferrite ions (HFeO2−). These results indicate that research data obtained from concentrated NaOH solutions are not appropriate to apply to the crevice environments of SGs.
Open AccessOn the Use of NaOH Solution to Simulate the Crevice Conditions of a Nuclear Steam Generator
The corrosion behavior and integrity of steam generator (SG) tube materials have frequently been tested in solutions containing sodium hydroxide (NaOH), assuming that NaOH is a typical contaminant concentrated in the crevices of SGs in a pressurized water reactor. The purpose of this study was to investigate the adequacy of using concentrated NaOH solutions to simulate the crevice environments of SGs. The dissolution behavior of magnetite deposit flakes formed in an operating SG was tested in a 0.4 wt.% NaOH solution at 300 °C, and the thermodynamic stability of magnetite was investigated using the potential-pH diagram for an iron–water system. The magnetite deposits were rapidly dissolved in the test solution, which was supported by the fact that magnetite is thermodynamically unstable under the test condition to dissolve to dihypoferrite ions (HFeO2−). These results indicate that research data obtained from concentrated NaOH solutions are not appropriate to apply to the crevice environments of SGs.
- Open Access
- 13 April 2022
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 18, 3396-3409
Microstructure and high-temperature mechanical properties of TP310HCbN welded joint
- 13 April 2022
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 18, 3396-3409
Open AccessMicrostructure and high-temperature mechanical properties of TP310HCbN welded joint
- Open Access
Magnetite-Accelerated Corrosion of SA508 Tubesheet Material and Its Effect on Steam Generator Tube Denting
The objective of this work is to investigate the magnetite-accelerated corrosion phenomenon of SA508 used as tubesheet material in simulated secondary side environments of pressurized water reactors through immersion and electrochemical tests. The presence of sulfate ions induced the fast growth of a corrosion product layer on SA508, and this phenomenon was accelerated when the SA508 was coupled to magnetite. From the perspective of electrochemical behavior, it was found that SA508 behaves as an anodic member in the coupling system with magnetite, resulting in an increased corrosion rate.
Open AccessMagnetite-Accelerated Corrosion of SA508 Tubesheet Material and Its Effect on Steam Generator Tube Denting
The objective of this work is to investigate the magnetite-accelerated corrosion phenomenon of SA508 used as tubesheet material in simulated secondary side environments of pressurized water reactors through immersion and electrochemical tests. The presence of sulfate ions induced the fast growth of a corrosion product layer on SA508, and this phenomenon was accelerated when the SA508 was coupled to magnetite. From the perspective of electrochemical behavior, it was found that SA508 behaves as an anodic member in the coupling system with magnetite, resulting in an increased corrosion rate.
- Open Access
Stress Corrosion Cracking Behavior of Alloy 600 Coupled to Magnetite under High-Temperature Caustic Conditions
This study aims to investigate and explain the magnetite-accelerated stress corrosion cracking phenomenon of Alloy 600 under caustic conditions, based on the electrochemical behavior. After the SCC test that lasted for 300 h, no cracks were observed in any of the magnetite-free specimens, whereas cracks with a depth of 150 to 280 μm were generated in all the magnetite-deposited specimens. Furthermore, the electrochemical behavior of magnetite and Alloy 600 demonstrated that Alloy 600 behaved as an anode in the coupling system with magnetite. In this coupling system, the electrochemical potential of Alloy 600 can be shifted into the range potentially susceptible to stress corrosion cracking.
Open AccessStress Corrosion Cracking Behavior of Alloy 600 Coupled to Magnetite under High-Temperature Caustic Conditions
This study aims to investigate and explain the magnetite-accelerated stress corrosion cracking phenomenon of Alloy 600 under caustic conditions, based on the electrochemical behavior. After the SCC test that lasted for 300 h, no cracks were observed in any of the magnetite-free specimens, whereas cracks with a depth of 150 to 280 μm were generated in all the magnetite-deposited specimens. Furthermore, the electrochemical behavior of magnetite and Alloy 600 demonstrated that Alloy 600 behaved as an anode in the coupling system with magnetite. In this coupling system, the electrochemical potential of Alloy 600 can be shifted into the range potentially susceptible to stress corrosion cracking.
- Open Access
Galvanic Corrosion of SA106 Gr.B Coupled with Magnetite in Alkaline Solution at Various Temperatures
The effect of temperature on the galvanic corrosion behavior of SA106 Gr.B carbon-manganese steel was studied in an alkaline aqueous solution at various temperatures (30, 60, and 90 °C) via electrochemical corrosion tests. At all temperatures studied, carbon-manganese steel acted as the anode of the galvanic cell composed of carbon-manganese steel and magnetite because the corrosion potential of carbon-manganese steel was significantly lower than that of magnetite. The corrosion current density of carbon-manganese steel significantly increased due to the galvanic effect irrespective of temperature used in this study. With the increase in temperature, the extent of the galvanic effect on the corrosion current density of carbon-manganese steel and reductive dissolution of magnetite gradually increased. When the area ratio of magnetite to carbon-manganese steel increased, the corrosion rate of the carbon-manganese steel in contact with magnetite further increased.
Open AccessGalvanic Corrosion of SA106 Gr.B Coupled with Magnetite in Alkaline Solution at Various Temperatures
The effect of temperature on the galvanic corrosion behavior of SA106 Gr.B carbon-manganese steel was studied in an alkaline aqueous solution at various temperatures (30, 60, and 90 °C) via electrochemical corrosion tests. At all temperatures studied, carbon-manganese steel acted as the anode of the galvanic cell composed of carbon-manganese steel and magnetite because the corrosion potential of carbon-manganese steel was significantly lower than that of magnetite. The corrosion current density of carbon-manganese steel significantly increased due to the galvanic effect irrespective of temperature used in this study. With the increase in temperature, the extent of the galvanic effect on the corrosion current density of carbon-manganese steel and reductive dissolution of magnetite gradually increased. When the area ratio of magnetite to carbon-manganese steel increased, the corrosion rate of the carbon-manganese steel in contact with magnetite further increased.
- Open Access
Micro-Galvanic Corrosion of Steam Generator Materials within Pores of Magnetite Flakes in Alkaline Solutions
In secondary coolant system of the pressurized water reactors, the reduced corrosion products such as metallic Cu and Pb particles were accumulated in the pores of the magnetite flakes and electrically contacted to the steam generator materials. The micro-galvanic corrosion behavior of steam generator materials (steam generator tube materials: Alloy 600 and Alloy 690, steam generator tube sheet materials: SA508 Gr.3) contacted to the corrosion products (magnetite, Cu, and Pb) was investigated in an alkaline solution. The steam generator materials considered in this study were all the anodic elements of the galvanic pair because their corrosion potentials were lower than those of the corrosion products. The corrosion rate of the steam generator materials was increased by the galvanic coupling with the each corrosion products, and was more accelerated with increasing the area ratio of the corrosion products to the steam generator materials. Among the corrosion products, Cu has the largest galvanic effect on steam generator materials in the pores when area ratio of cathode to anode is 10.
Open AccessMicro-Galvanic Corrosion of Steam Generator Materials within Pores of Magnetite Flakes in Alkaline Solutions
In secondary coolant system of the pressurized water reactors, the reduced corrosion products such as metallic Cu and Pb particles were accumulated in the pores of the magnetite flakes and electrically contacted to the steam generator materials. The micro-galvanic corrosion behavior of steam generator materials (steam generator tube materials: Alloy 600 and Alloy 690, steam generator tube sheet materials: SA508 Gr.3) contacted to the corrosion products (magnetite, Cu, and Pb) was investigated in an alkaline solution. The steam generator materials considered in this study were all the anodic elements of the galvanic pair because their corrosion potentials were lower than those of the corrosion products. The corrosion rate of the steam generator materials was increased by the galvanic coupling with the each corrosion products, and was more accelerated with increasing the area ratio of the corrosion products to the steam generator materials. Among the corrosion products, Cu has the largest galvanic effect on steam generator materials in the pores when area ratio of cathode to anode is 10.
- Open Access
Corrosion Behavior of SA508 Coupled with and without Magnetite in EDTA-Based Solutions
The effects of magnetite on the corrosion behavior of SA508 were studied in 10% and 20% EDTA-based chemical cleaning solutions at 93 °C and 121 °C using electrochemical and immersion tests. SA508 was the anode of the galvanic pair between SA508 and magnetite. The galvanic coupling shifted the mixed corrosion potential of SA508 in the positive direction and thus increased its corrosion rate. The increase of the EDTA concentration and solution temperature led to an increase in the extent of the galvanic effect.
Open AccessCorrosion Behavior of SA508 Coupled with and without Magnetite in EDTA-Based Solutions
The effects of magnetite on the corrosion behavior of SA508 were studied in 10% and 20% EDTA-based chemical cleaning solutions at 93 °C and 121 °C using electrochemical and immersion tests. SA508 was the anode of the galvanic pair between SA508 and magnetite. The galvanic coupling shifted the mixed corrosion potential of SA508 in the positive direction and thus increased its corrosion rate. The increase of the EDTA concentration and solution temperature led to an increase in the extent of the galvanic effect.