Soon-Hyeok Jeon
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Soon-Hyeok Jeon has a total of 39 co-authors. Here are the top co-authors by number of shared publications:
- Do Haeng Hur
Materials Safety Technology Development Division, Korea Atomic Energy Research Institute, Daejeon 34057, Republic of Korea
16 shared publications - Geun Dong Song
Korea Atomic Energy Research Institute, 989-111 Deadeok-daero, Yuseong-gu, Daejeon 34057, Korea
10 shared publications - Jeoh Han
Materials Safety Technology Development Division, Korea Atomic Energy Research Institute, Daejeon 34057, Korea
4 shared publications - Ji-Min Lee
Materials Safety Technology Development Division, Korea Atomic Energy Research Institute, 989-111, Daedeok-daero, Yuseong-gu, Daejeon 34057, Korea
3 shared publications - Jong-Hyeon Lee
Graduate School of Materials Science & Engineering, Chungnam National University, 99 Daehak-ro, Yuseong-gu, Daejeon 34134, Republic of Korea
3 shared publications - Yeong-Ho Son
Nuclear Materials Research Division, Korea Atomic Energy Research Institute, 989-111, Daedeok-daero, Yuseong-gu, Daejeon 34057, Korea
3 shared publications
Latest Publications
- Open Access
- 28 November 2024
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 33, 9232-9248
Effect of plastic deformation on microstructure and general corrosion behavior of alloy 690 in SG crevice condition of PWR secondary system containing hydrogen
- 28 November 2024
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 33, 9232-9248
Open AccessEffect of plastic deformation on microstructure and general corrosion behavior of alloy 690 in SG crevice condition of PWR secondary system containing hydrogen
- Open Access
- 26 November 2024
- Published by Elsevier in Nuclear Engineering and Technology
- Vol. 57 (5) , 103336
Characteristics of corrosion products in low-pressure and high-pressure feedwater heaters in an operating pressurized water reactor
- 26 November 2024
- Published by Elsevier in Nuclear Engineering and Technology
- Vol. 57 (5) , 103336
Open AccessCharacteristics of corrosion products in low-pressure and high-pressure feedwater heaters in an operating pressurized water reactor
- Open Access
A New Mechanism for the Inhibition of SA106 Gr.B Carbon Steel Corrosion by Nitrite in Alkaline Water
The purpose of this study was to investigate the composition of oxide films formed on SA106 Gr.B carbon steel in nitrite solutions at 35 °C for 1000 h. The product of the reduction of nitrite during the corrosion inhibition process was also examined. The X-ray photoelectron spectroscopy results revealed that a thin Fe3O4 film was formed and ammonium ions were adsorbed on the outermost surface of the oxide film. The presence of ammonium ions was also demonstrated by ion chromatography. These results indicate that nitrites are reduced to ammonium ions, which in turn promotes the formation of the protective Fe3O4 film.
Open AccessA New Mechanism for the Inhibition of SA106 Gr.B Carbon Steel Corrosion by Nitrite in Alkaline Water
The purpose of this study was to investigate the composition of oxide films formed on SA106 Gr.B carbon steel in nitrite solutions at 35 °C for 1000 h. The product of the reduction of nitrite during the corrosion inhibition process was also examined. The X-ray photoelectron spectroscopy results revealed that a thin Fe3O4 film was formed and ammonium ions were adsorbed on the outermost surface of the oxide film. The presence of ammonium ions was also demonstrated by ion chromatography. These results indicate that nitrites are reduced to ammonium ions, which in turn promotes the formation of the protective Fe3O4 film.
- Open Access
On the Use of NaOH Solution to Simulate the Crevice Conditions of a Nuclear Steam Generator
The corrosion behavior and integrity of steam generator (SG) tube materials have frequently been tested in solutions containing sodium hydroxide (NaOH), assuming that NaOH is a typical contaminant concentrated in the crevices of SGs in a pressurized water reactor. The purpose of this study was to investigate the adequacy of using concentrated NaOH solutions to simulate the crevice environments of SGs. The dissolution behavior of magnetite deposit flakes formed in an operating SG was tested in a 0.4 wt.% NaOH solution at 300 °C, and the thermodynamic stability of magnetite was investigated using the potential-pH diagram for an iron–water system. The magnetite deposits were rapidly dissolved in the test solution, which was supported by the fact that magnetite is thermodynamically unstable under the test condition to dissolve to dihypoferrite ions (HFeO2−). These results indicate that research data obtained from concentrated NaOH solutions are not appropriate to apply to the crevice environments of SGs.
Open AccessOn the Use of NaOH Solution to Simulate the Crevice Conditions of a Nuclear Steam Generator
The corrosion behavior and integrity of steam generator (SG) tube materials have frequently been tested in solutions containing sodium hydroxide (NaOH), assuming that NaOH is a typical contaminant concentrated in the crevices of SGs in a pressurized water reactor. The purpose of this study was to investigate the adequacy of using concentrated NaOH solutions to simulate the crevice environments of SGs. The dissolution behavior of magnetite deposit flakes formed in an operating SG was tested in a 0.4 wt.% NaOH solution at 300 °C, and the thermodynamic stability of magnetite was investigated using the potential-pH diagram for an iron–water system. The magnetite deposits were rapidly dissolved in the test solution, which was supported by the fact that magnetite is thermodynamically unstable under the test condition to dissolve to dihypoferrite ions (HFeO2−). These results indicate that research data obtained from concentrated NaOH solutions are not appropriate to apply to the crevice environments of SGs.
- Open Access
Magnetite Deposition Behavior on Alloy 600 and Alloy 690 Tubes in Simulated PWR Secondary Water
Fouling due to magnetite deposition has been a major concern for steam generator (SG) tubing of pressurized water reactors (PWRs). Alloy 690 SG tubes are now used for new plants or are scheduled to replace old Alloy 600 tubes of operating plants. The purpose of this study is to investigate the magnetite deposition behavior on the two different SG tube materials: Alloy 600 and Alloy 690. Deposition tests were conducted under a sub-cooled nucleate flow boiling condition in simulated secondary water of a PWR at 270 °C. After these tests, we observed that the tube surfaces were covered with deposits composed of porous magnetite particles. We found approximately 30% more magnetite deposits on Alloy 600 than on Alloy 690. The electrostatic repulsive force between the magnetite particles and the Alloy 600 surface was only half of that between the magnetite particles and the Alloy 690 surface, resulting in an increase in the deposit mass.
Open AccessMagnetite Deposition Behavior on Alloy 600 and Alloy 690 Tubes in Simulated PWR Secondary Water
Fouling due to magnetite deposition has been a major concern for steam generator (SG) tubing of pressurized water reactors (PWRs). Alloy 690 SG tubes are now used for new plants or are scheduled to replace old Alloy 600 tubes of operating plants. The purpose of this study is to investigate the magnetite deposition behavior on the two different SG tube materials: Alloy 600 and Alloy 690. Deposition tests were conducted under a sub-cooled nucleate flow boiling condition in simulated secondary water of a PWR at 270 °C. After these tests, we observed that the tube surfaces were covered with deposits composed of porous magnetite particles. We found approximately 30% more magnetite deposits on Alloy 600 than on Alloy 690. The electrostatic repulsive force between the magnetite particles and the Alloy 600 surface was only half of that between the magnetite particles and the Alloy 690 surface, resulting in an increase in the deposit mass.
- Open Access
Effects of Zinc Addition on the Corrosion Behavior of Pre-Filmed Alloy 690 in Borated and Lithiated Water at 330 °C
The purpose of this work is to quantify the effects of dissolved zinc cations on corrosion and release rates from a pre-filmed Alloy 690 steam generator tubing material that was subsequently exposed to water containing zinc. The corrosion tests were performed in circulating 2 ppm Li and 1000 ppm B water without and with 60 ppb zinc at 330 °C. Gravimetric analyses and oxide characterization revealed that the corrosion rates, release rates, and oxide thicknesses decreased by subsequent exposure of the pre-filmed Alloy 690 to zinc. These benefits are attributed to the formation of a chromium-rich inner oxide layer incorporating zinc.
Open AccessEffects of Zinc Addition on the Corrosion Behavior of Pre-Filmed Alloy 690 in Borated and Lithiated Water at 330 °C
The purpose of this work is to quantify the effects of dissolved zinc cations on corrosion and release rates from a pre-filmed Alloy 690 steam generator tubing material that was subsequently exposed to water containing zinc. The corrosion tests were performed in circulating 2 ppm Li and 1000 ppm B water without and with 60 ppb zinc at 330 °C. Gravimetric analyses and oxide characterization revealed that the corrosion rates, release rates, and oxide thicknesses decreased by subsequent exposure of the pre-filmed Alloy 690 to zinc. These benefits are attributed to the formation of a chromium-rich inner oxide layer incorporating zinc.
- Open Access
Effects of Advanced Amines on Magnetite Deposition of Steam Generator Tubes in Secondary System
Ethanolamine (ETA) is widely used to control the pH value in the secondary water of pressurized water reactors. However, it is necessary to consider other advanced amines which can replace ETA due to its serious human hazards and environmental treatment problems. The purpose of this study is to contemplate the effects of three advanced amines (ETA, 3-methoxypropylamine (MPA), and dimethylamine (DMA)) on the magnetite deposition behavior of a thermally treated (TT) Alloy 690 tubes by using a steam generator (SG) tube fouling loop in simulated secondary water. All particles were identified as a magnetite and were polyhedral or spherical in shape. When using ETA, MPA, and DMA, the average porosity of the deposits was about 34.7%, 33.0%, and 24.6%, respectively. The amount of deposits was largest when ETA was added, and it decreased by 41% when adding MPA and 55% when adding DMA. The mechanism of magnetite deposition was discussed in terms of zeta potentials of both the magnetite particles and the Alloy 690TT surface and magnetite solubility depending on the amines. To compare the potential for replacing ETA with other advanced amines, the various factors such as SG integrity, human hazards, and environmental treatment problems were discussed.
Open AccessEffects of Advanced Amines on Magnetite Deposition of Steam Generator Tubes in Secondary System
Ethanolamine (ETA) is widely used to control the pH value in the secondary water of pressurized water reactors. However, it is necessary to consider other advanced amines which can replace ETA due to its serious human hazards and environmental treatment problems. The purpose of this study is to contemplate the effects of three advanced amines (ETA, 3-methoxypropylamine (MPA), and dimethylamine (DMA)) on the magnetite deposition behavior of a thermally treated (TT) Alloy 690 tubes by using a steam generator (SG) tube fouling loop in simulated secondary water. All particles were identified as a magnetite and were polyhedral or spherical in shape. When using ETA, MPA, and DMA, the average porosity of the deposits was about 34.7%, 33.0%, and 24.6%, respectively. The amount of deposits was largest when ETA was added, and it decreased by 41% when adding MPA and 55% when adding DMA. The mechanism of magnetite deposition was discussed in terms of zeta potentials of both the magnetite particles and the Alloy 690TT surface and magnetite solubility depending on the amines. To compare the potential for replacing ETA with other advanced amines, the various factors such as SG integrity, human hazards, and environmental treatment problems were discussed.
- Open Access
Zeta Potentials of Magnetite Particles and Alloy 690 Surfaces in Alkaline Solutions
Magnetite particles deposited on the secondary side of a steam generator (SG) can degrade the integrity and performance of pressurized water reactors. Therefore, it is necessary to produce the data of fundamental interfacial electrokinetic properties of magnetite particles and SG tube materials. This study investigated the zeta potentials of magnetite nanoparticles and Alloy 690 surfaces, which were dependent on the pH value, pH agent, and the presence of NaCl. The zeta potentials of the magnetite nanoparticles increased in the negative direction as the pH increased, regardless of the pH agent. At the same pH value, the absolute values of the zeta potentials with different pH agents were: ethanolamine < ammonia < morpholine. In the presence of NaCl, the zeta potentials of the particles further increased negatively. The meaning of the measured zeta potentials was discussed in terms of the dispersion stability and the agglomeration of the particles. Based on the relationship between the zeta potentials of the particles and Alloy 690 surfaces, the magnetite deposition on Alloy 690 was also discussed. Furthermore, the empirical formulas for the pH-dependent zeta potentials of magnetite particles in each alkaline solution were suggested.
Open AccessZeta Potentials of Magnetite Particles and Alloy 690 Surfaces in Alkaline Solutions
Magnetite particles deposited on the secondary side of a steam generator (SG) can degrade the integrity and performance of pressurized water reactors. Therefore, it is necessary to produce the data of fundamental interfacial electrokinetic properties of magnetite particles and SG tube materials. This study investigated the zeta potentials of magnetite nanoparticles and Alloy 690 surfaces, which were dependent on the pH value, pH agent, and the presence of NaCl. The zeta potentials of the magnetite nanoparticles increased in the negative direction as the pH increased, regardless of the pH agent. At the same pH value, the absolute values of the zeta potentials with different pH agents were: ethanolamine < ammonia < morpholine. In the presence of NaCl, the zeta potentials of the particles further increased negatively. The meaning of the measured zeta potentials was discussed in terms of the dispersion stability and the agglomeration of the particles. Based on the relationship between the zeta potentials of the particles and Alloy 690 surfaces, the magnetite deposition on Alloy 690 was also discussed. Furthermore, the empirical formulas for the pH-dependent zeta potentials of magnetite particles in each alkaline solution were suggested.
- Open Access
Simulation of Porous Magnetite Deposits on Steam Generator Tubes in Circulating Water at 270 °C
In the secondary side of pressurized water reactors (PWRs), the main corrosion product accumulated on the steam generator (SG) tubes is magnetite, which has a porous structure. The purpose of this work is to simulate the porous magnetite deposited to the SG tubes using a loop system. We newly developed a circulating loop system for a porous magnetite deposition test. A test section was designed as a single hydraulic flow channel, and a cartridge heater was fabricated and mounted into a commercial SG tube to provide an equal heating source for the primary water. After the deposition test, the simulated magnetite deposits were characterized for comparison to real SG tube deposits collected from an operating PWR plant. The magnetite deposits produced using the loop system were appropriate for simulating the real SG tube deposits because the particle characteristics, phase, and porous morphology are closely similar to those of real deposit samples. Using the loop system, the chemical impurities such as Na and Cl can be easily concentrated within the pores of the simulated magnetite deposits. These simulated magnetite samples are expected to be widely utilized in various research fields such as the heat transfer degradation and magnetite accelerated corrosion of SG tubes.
Open AccessSimulation of Porous Magnetite Deposits on Steam Generator Tubes in Circulating Water at 270 °C
In the secondary side of pressurized water reactors (PWRs), the main corrosion product accumulated on the steam generator (SG) tubes is magnetite, which has a porous structure. The purpose of this work is to simulate the porous magnetite deposited to the SG tubes using a loop system. We newly developed a circulating loop system for a porous magnetite deposition test. A test section was designed as a single hydraulic flow channel, and a cartridge heater was fabricated and mounted into a commercial SG tube to provide an equal heating source for the primary water. After the deposition test, the simulated magnetite deposits were characterized for comparison to real SG tube deposits collected from an operating PWR plant. The magnetite deposits produced using the loop system were appropriate for simulating the real SG tube deposits because the particle characteristics, phase, and porous morphology are closely similar to those of real deposit samples. Using the loop system, the chemical impurities such as Na and Cl can be easily concentrated within the pores of the simulated magnetite deposits. These simulated magnetite samples are expected to be widely utilized in various research fields such as the heat transfer degradation and magnetite accelerated corrosion of SG tubes.
- Open Access
Magnetite-Accelerated Corrosion of SA508 Tubesheet Material and Its Effect on Steam Generator Tube Denting
The objective of this work is to investigate the magnetite-accelerated corrosion phenomenon of SA508 used as tubesheet material in simulated secondary side environments of pressurized water reactors through immersion and electrochemical tests. The presence of sulfate ions induced the fast growth of a corrosion product layer on SA508, and this phenomenon was accelerated when the SA508 was coupled to magnetite. From the perspective of electrochemical behavior, it was found that SA508 behaves as an anodic member in the coupling system with magnetite, resulting in an increased corrosion rate.
Open AccessMagnetite-Accelerated Corrosion of SA508 Tubesheet Material and Its Effect on Steam Generator Tube Denting
The objective of this work is to investigate the magnetite-accelerated corrosion phenomenon of SA508 used as tubesheet material in simulated secondary side environments of pressurized water reactors through immersion and electrochemical tests. The presence of sulfate ions induced the fast growth of a corrosion product layer on SA508, and this phenomenon was accelerated when the SA508 was coupled to magnetite. From the perspective of electrochemical behavior, it was found that SA508 behaves as an anodic member in the coupling system with magnetite, resulting in an increased corrosion rate.