YNYuko Nagasawa

Yuko Nagasawa

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Yuko Nagasawa has a total of 17 co-authors. Here are the top co-authors by number of shared publications:

  • Yasushi Hibino

    Division of Dental Biomaterials Science, Department of Restorative and Biomaterials Sciences, Meikai University School of Dentistry, Sakado, Japan

    6 shared publications
  • Hiroshi Nakajima

    Division of Dental Biomaterials Science, Department of Restorative and Biomaterials Sciences, Meikai University School of Dentistry, Sakado, Japan

    4 shared publications
  • Yoshikazu Eda

    Division of Dental Biomaterials Science, Department of Restorative and Biomaterials Sciences, Meikai University School of Dentistry, Sakado, Japan

    4 shared publications
  • Hiroshi Nakajima

    Department of Materials Science, Osaka Metropolitan University, Sakai, Japan

    3 shared publications
  • Hirotaka Shigeta

    Division of Dental Biomaterials Science, Department of Restorative and Biomaterials Sciences, Meikai University School of Dentistry, Sakado, Japan

    2 shared publications
  • Shigeki Matsumoto

    Division of Oral Rehabilitation, Department of Restorative and Biomaterials Sciences, Meikai University School of Dentistry, Sakado, Japan

    2 shared publications

Latest Publications

  • Effect of air-thinning a two-step adhesive layer on bond strength to tooth substrates

    by Yuko Nagasawa, Yoshikazu Eda, Shigeki Matsumoto, Hiroshi Nakajima, Yasushi Hibino

    This study investigated the effect of air-thinning to a two-step adhesive (G2-BOND Universal) on the microtensile bond strength (µTBS) between bovine teeth (enamel, dentin) and a resin composite (G-ænial A′CHORD). The adhesive was applied with or without air-blowing before light curing on the bovine enamel and dentin surfaces finished using 320-grit SiC paper. After resin composite buildup, µTBS specimens (1.0 mm × 1.0 mm cross-sectional area) were fabricated. The µTBS values were determined 24 h, 4 weeks, and 6 months after the specimen preparation. Furthermore, the adhesive layer thicknesses were measured on the SEM photographs of the specimens’ fractured site after the µTBS test. Except for the enamel specimens at 6 months, no significant differences were observed in µTBS determined at any time periods between specimens with and without air-blowing (p > 0.05). µTBS values in air-blown specimens increased from 24 h to 4 weeks, and the values in non-air-blown specimens were greater at 6 months than at 24 h. Specimens subjected to air-blowing showed significantly thinner adhesive layer than those without at any time periods (p < 0.05). Although air-blowing reduced adhesive layer thickness, it did not affect the bond strength except for the enamel specimens at 6 months.


  • Effect of sandblasting and/or priming treatment on the shear bond strength of self-adhesive resin cement to CAD/CAM blocks

    by Yuko Nagasawa, Yoshikazu Eda, Hirotaka Shigeta, Marco Ferrari, Hiroshi Nakajima, Yasushi Hibino

    The aim of this study was to investigate the effect of two different priming agents and/or sandblasting on the shear bond strength of self-adhesive resin cement to the resin composite for core build-up to CAD/CAM blocks. A CAD/CAM ceramic block (GN I CERAMIC BLOCK, GC) and a CAD/CAM resin composite block (CERASMART 270, GC), a self-adhesive resin cement (G-CEM ONE, GC) and two different primers, i.e., a multipurpose primer (MP; G-Multi Primer, GC) and a ceramic primer (CP; Ceramic Primer II, GC), were examined. Five different surface treatments with priming and/or sandblasting and no surface treatment (control) were performed on the block. Disk specimens (6 mm in diameter and 4 mm in thickness) made from core composites were cemented to the blocks after the surface treatments. Then, the 24-h shear bond strength of the resin cement between the block and the resin composite core was determined (n = 15). Sandblasted specimens had greater bond strength than controls for both blocks (p < 0.05). Priming to both blocks significantly increased the bond strength of resin cement compared to that of controls (p < 0.05). Although Weibull moduli were not significantly changed among all surface treatments for both blocks, the strengths with 5% and 95% failure probability of sandblasted and/or primed blocks were estimated to be greater than those of controls. The combination of priming and sandblasting to the CAD/CAM composite and ceramic surface was effective in increasing the bond strength of the resin cement.


  • Open Access

    Effect of surface treatment of CAD/CAM resin composites on the shear bond strength of self-adhesive resin cement

    by Yuko Nagasawa, Yasushi Hibino, Yoshikazu Eda, Hiroshi Nakajima

    This study examined the effects of sandblasting, hydrofluoric acid etching and priming on the shear bond strength of self-adhesive resin cement between seven different CAD/CAM resin composites and a resin composite core material at 24-h after cement mixing. Five surface treatments [control (C), sandblasting (S), priming (P), sandblasting with priming (SP), and 9% HF etching with priming (HFP)] were performed respectively for disc specimens of CAD/CAM blocks. There were no significant differences in bond strength among the C, S, and P, except for one block (p>0.05). SP showed a greater bond strength than S. Weibull moduli were not changed significantly among all treatments for all blocks, whereas the strengths with 5% and 95% failure probability of SP and HFP showed greater values than the others. The bond strengths of HFP were comparable to those of SP. Priming after sandblasting or HF etching could be effective to increase the bond strength of CAD/CAM blocks.


  • Open Access

    Characteristics of a new dental stone mixed by shaking

    by Yuko Nagasawa, Yasushi Hibino, Hirotaka Shigeta, Yoshikazu Eda, Shigeki Matsumoto, Hiroshi Nakajima

    This study evaluated the physical and mechanical properties of a dental stone mixed by shaking. A shake-mix dental stone (Shake! Mix STONE; SM) was characterized in comparison with three conventional dental stones. The fluidity at pouring time, setting time, density, powder particle distributions, linear setting expansion, compressive strength and surface reproduction of detail for dental stones were investigated. The marginal adaptations of cast crowns to dies made with each stone were also determined. SM had higher fluidity and faster setting time than the other stones (p<0.05). The setting expansion of SM at 2 h was lower than those of other two stones (p<0.05). The 15-min compressive strength of SM was higher than the others (p0.05). In spite of the different mixing method, the shake-mix type dental stone had comparable physical and mechanical properties to the conventional dental stones.


  • Open Access

    Effect of composition of experimental fluorinated soft lining materials on bond strength to denture base resin

    by Yoshihito Hoshino, Hiroshi Nakajima, Norihisa Akiba, Yasushi Hibino, Yuko Nagasawa, Yasunori Sumi, Shunsuke Minakuchi

    The purpose of the present study was to investigate the effect of the composition of experimental fluorinated soft lining materials on bond strength to denture base resin. Vinylidene fluoride/hexafluoro propylene copolymer (2-6F), tridecafluorooctyl methacrylate (13FMA), methoxy diethylene glycol methacrylate (MDGMA), and silica (as filler) were used for fabrication of the experimental soft lining materials. Nine experimental soft lining materials having various compositions of 2-6F, 13FMA, and MDGMA were prepared. Shear and tensile bond strength tests were performed before and after immersion in water. The water sorption for the materials was also measured. An increase in the content of acrylic monomer, MDGMA, in the experimental materials increased the bond strength before immersion in water but reduced the bond strength after immersion in water as compared to that before immersion in water. The inclusion of fluorinated monomer (13FMA) in the materials appeared to affect water sorption.


  • Open Access

    Retention of crowns cemented on implant abutments with temporary cements

    by Yuko Nagasawa, Yasushi Hibino, Hiroshi Nakajima

    This study was to examine the retentive force of crowns to implant abutments with commercial temporary cements. Six different temporary cements were investigated. Cast crowns were cemented to the abutments using each cement and their retentive forces to abutments were determined 7 or 28 days after cementing (n=10). The retentive force of the cements to abutments varied widelyamong the products [27–109 N (7-day), 18–80 N (28-days)]. The retentive force of all the cements was not reduced as the time elapsed, except for two products tested. The polycarboxylate cements and paste-mixing type eugenol-free cements revealed comparable retentive force after 28 days of storage. The powder-liquid type cements showed a positive correlation (p<0.05) between the retentive force and the shear strength, while a negative correlation (p<0.05) was obtained for paste-mixing type cement between the retentive force and compressive strength. Mechanical strength of temporary cements could not be a prominent predicting factor for retention of the crowns on the abutments.


  • Open Access

    Correlation between the Strength of Glass Ionomer Cements and Their Bond Strength to Bovine Teeth

    by Yasushi Hibino, Ken-Ichi Kuramochi, Atsushi Harashima, Muneaki Honda, Atsushi Yamazaki, Yuko Nagasawa, Taniichiro Yamaga, Hiroshi Nakajima

    This study examined the possible correlation between the strength of glass ionomers and their adhesive strength to bovine teeth. The shear bond strengths of three different brands of glass Ionomer mixed at four different P/L ratios to bovine teeth were measured 24 hours after the cement specimens were prepared. The correlation between shear bond strength and mechanical strength reported in our previous study was also examined. No significant (p>0.05) increases in the bond strength to bovine teeth were found in any of the cements when the mixing ratio increased. The present study showed no significant (p>0.05) correlation between mechanical strength of cement and its bond strength to bovine teeth. Rather than trying to increase the strength of the cement, it would be more effective to enhance the adhesive bond strength through procedures such as surface conditioning or cleaning of the tooth structure when glass ionomers are used as luting agents.