Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Juan Manuel Gonzalez has a total of 140 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Thermal oxidation, mechanical response and tribological performance of WS2 coatings deposited by magnetron sputtering

    by Mauricio Nango-Blanco, Daniel Toribio-Gurrola, Luis Miguel Ballesteros-Ospina, Jean Carlos Zambrano-Luna, Alexander Ruden-Muñoz, Juan Pablo Trujillo-Lemus, Cesar Andrés-Amaya, Carlos Eduardo Rodríguez, Juan Manuel González-Carmona

  • Open Access

    AEGD-Assisted Plasma Nitriding of AISI M2 Steel: Influence of Treatment Time on Structure and Scratch Resistance

    by Sebastián Martínez García, Leonardo Bohórquez Santiago, Alexander Ruden, Julián Felipe Villada Castillo, Abel Hurtado-Macías, Guillermo César Mondragón-Rodríguez, Jhon Alexander Villada-Villalobos, Juan Manuel González-Carmona

    The effect of treatment time on arc-enhanced glow discharge plasma-assisted nitriding (AEGD-PAN) of AISI M2 high-speed steel was investigated for non-heat-treated and heat-treated substrates. Nitriding treatments were carried out at 350 °C for 1.5 and 3.5 h, producing diffusion layers with thicknesses ranging from approximately 38 to 75 µm without formation of a continuous brittle compound layer. X-ray diffraction combined with Rietveld refinement revealed the progressive formation of γ′-Fe4N and ε-Fe23N nitrides together with lattice expansion of the α-Fe matrix, indicating nitrogen supersaturation and precipitation strengthening within the diffusion zone. Heat-treated specimens exhibited higher surface hardness, reaching ~1350 HV0.1, while non-heat-treated substrates developed pronounced hardness gradients associated with diffusion-controlled layer growth. Scratch testing showed improved resistance to contact-induced damage with increasing nitriding time, particularly for the 3.5 h treatment, where lateral cracking was significantly reduced and load-bearing capacity increased. Multi-pass scratch wear tests revealed a reduction in the Archard wear coefficient by up to four orders of magnitude compared with untreated M2 steel. These results demonstrate that AEGD-PAN at moderate temperature enables efficient diffusion layer formation and significant improvement in the tribological performance of high-alloy tool steels.

  • Open Access

    Effect of the substrate bias and substrate type on microstructure, adhesion and nanomechanical response of arc-PVD c-TiCxNy coatings

    by Williams Hincapie Campos, Jorge Armando Villalba, Angelica Maria Benitez-Castro, V.D. Saldarriaga-Montoya, Juan Munoz Saldana, Juan Gonzalez, D.G. Espinosa-Arbeláez, Guillermo Cesar Mondragon Rodriguez

    Hard and superhard coatings are key surface engineering solutions for cutting and forming tools, where performance relies on high wear resistance, mechanical reliability, and adhesion under severe contact stresses. In this work, cubic TiCₓNy coatings were deposited by cathodic arc physical vapor deposition (arc PVD) using two substrate bias voltages (-50 and -100 V) on three substrates with different thermomechanical responses: Si (111), heat-treated AISI H13 tool steel, and Ti6Al4V alloy (Ti64). The combined influence of substrate bias and substrate type was systematically evaluated in terms of surface morphology and roughness, chemical composition and C/N ratio, crystalline structure and texture, crystallite size, adhesion behavior, and nanomechanical response. All coatings crystallized in a single-phase face-centered cubic TiCₓNy structure, exhibiting substrate dependent (111) or (200) preferred orientations. Increasing the bias voltage produced substrate-dependent compositional trends. The C/N ratio slightly decreased on Si (0.50 to 0.47) and increased on H13 (0.50 to 0.68) and on Ti64 (0.54 to 0.61), consistent with the interplay between bias-driven resputtering processes and substrate-influenced kinetics and energy dissipation. In parallel, the microstructural response to bias voltage was strongly dependent on the substrate. Increasing bias voltage promoted grain refinement in coatings deposited on H13 steel, whereas an opposite trend consisting of crystallite coalescence and growth was observed for coatings grown on the more compliant Ti64 substrate. In contrast, coatings deposited on Si exhibited slightly increasing crystallite sizes, indicating that the additional ion energy was partially dissipated through re-sputtering and stress accumulation rather than through effective grain restructuring. Nanoindentation measurements revealed that hardness and elastic modulus (E) show only a weak dependence on bias voltage within the investigated range, while the substrate material exerts a dominant influence on the measured mechanical response. The highest hardness was ~39 GPa and narrowest Weibull distributions (62.2%) were obtained for coatings on H13, indicating superior mechanical homogeneity and load-bearing capacity. In comparison, coatings deposited on Ti64 displayed lower hardness, increased data dispersion, and reduced adhesion, consistent with enhanced substrate compliance and reduced elastic–plastic constraint. No monotonic correlation between hardness and C/N ratio was observed, indicating that composition, microstructure, residual stress, and substrate constraint act jointly. Overall, the results demonstrate that substrate properties dominate and can modulate bias-related effects in arc-PVD TiCxNy coatings, underscoring the need to explicitly consider substrate effects in coating design and application.

  • Open Access

    Erosive Wear Behavior of Fiberglass-Reinforced Epoxy Laminate Composites Modified with SiO2 Nanoparticles Fabricated by Resin Infusion

    by Angel Sebastian Alvarez Lozano, Armando Irvin Martínez Pérez, Edgar Ernesto Vera Cárdenas, Juan Manuel González Carmona, Arturo Mendoza Galván

    This work presents a study on the evaluation of the erosive wear behavior of laminated composites, manufactured using the vacuum-assisted resin infusion (VARI) method with a glass fiber-reinforced epoxy matrix modified with SiO2 nanoparticles (0.0, 1.5, and 3.0 wt.%). Results indicate that nanoparticle concentration and dispersion state critically influence the mechanical and tribological performance. The composite FG-1.5-SiO2 with 1.5 wt.% SiO2 exhibited optimal nanoparticle distribution, as confirmed by FTIR, GIXRD, and SEM analyses, with the lowest surface roughness (Ra = 0.215 μm), highest hardness (35.58 HV), and highest elastic modulus (19.66 GPa). These enhancements contributed to a 38% improvement in erosion rate compared to the unmodified laminated composite, with the lowest total mass loss (0.0261 mg) and erosion rate (2.3360 × 10−5 mg/g). Profilometry and SEM results revealed shallower wear depths and reduced matrix removal, indicating stronger fiber–matrix interface integrity. In contrast, the 3.0 wt.% SiO2 composite (FG-3-SiO2) suffered from nanoparticle agglomeration, which increased surface roughness, diminished mechanical properties, and reduced erosion resistance to levels comparable to the unreinforced material. The results indicate that homogeneous dispersion at an optimal concentration (1.5 wt.%) is crucial for improving erosion resistance, while agglomeration at higher concentrations negates the potential benefits of nanoparticle incorporation. These findings highlight the need to optimize nanoparticle dispersion for the development of fiberglass/epoxy composites with greater durability and erosion resistance in demanding applications.


  • Open Access

    Erosive Wear Behavior of Fiberglass Reinforced Epoxy Laminate Composites Modified with SiO2 Nanoparticles Fabricated by Resin Infusion

    by Angel Sebastían Alvarez Lozano, Armando Irvin Martínez Pérez, Edgar Ernesto Vera-Cardenás, Juan Manuel González-Carmona, Arturo Mendoza-Galván

    This work presents a study on the erosive wear behavior of laminated composites, manufactured using the vacuum assisted resin infusion (VARI) method with an epoxy matrix reinforced with glass fibers and modified with SiO2 nanoparticles. Three materials were fabricated with SiO2 nanoparticle concentrations of 0, 1.5, and 3 wt% to evaluate the effect of nanoparticle addition and dispersion on mechanical and microstructural properties, as well as erosion resistance. The results showed that the FG-1.5-SiO2 composite, containing 1.5 wt% SiO2 nanoparticles, exhibited the best nanoparticle dispersion, as evidenced by FTIR, GIXRD, and SEM analyses. This material displayed the lowest surface roughness (Ra = 0.215 μm), the highest Vickers hardness (35.58), and the highest modulus of elasticity (19.66 GPa), indicating an effective load transfer and adequate interfacial interaction. In erosion tests, the FG-1.5-SiO2 material demonstrated the lowest total mass loss (0.0261 mg) and the lowest erosion rate (2.3360E-5 mg/g), representing an approximately 38 % improvement in erosion resistance compared to the reference material without nanoparticles (FG-0-SiO2). Profilometry and SEM analyses confirmed that this composite FG-1.5-SiO2 exhibited less severe erosional damage, with shallower wear depth, characterized by less matrix removal and a stronger fiber-matrix interface. On the other hand, the composite with 3 wt% SiO2 (FG-3-SiO2) showed poor dispersion and agglomeration, resulting in increased roughness, lower mechanical properties, and erosion resistance similar to that of the material without nanoparticle reinforcement. This was attributed to the agglomerates acting as stress concentrators and structural defects that facilitate material detachment.


  • Study of friction and wear by reciprocating ball plane contact in TiAlON oxynitride coatings

    by J.C. Mendoza-Mendoza, E.E. Vera-Cardenas, C. Ortega-Portilla, L.M. Ballesteros, A.I. Martínez-Pérez, A. Hurtado-Macias, J.M. González-Carmona


  • Open Access

    Review of: "Investigating the Mechanical and Tribological Effects of MoS2 Reinforcement in AZ91 Magnesium Alloy: A Comprehensive Experimental Study"

    by Juan Manuel González Carmona

    The information related to MoS2 found in the materials and methods section seems disconnected from the document. I consider that it should be taken into account for the introduction section, where it should be limited to the influence that the materi...

  • Open Access

    Effect of Temperature on the Structure and Tribological Properties of Ti, TiN and Ti/TiN Coatings Deposited by Cathodic Arc PVD

    by Carolina Ortega-Portilla, Andrea Giraldo, Jorge Andrés Cardona, Alexander Ruden, Guillermo César Mondragón, Juan Pablo Trujillo, Arturo Gómez Ortega, Juan Manuel González-Carmona, Edgar Adrián Franco Urquiza

    Monolayers of Ti and TiN coatings, as well as a Ti/TiN bilayer coating, were deposited on AISI M2 steel substrates using the PVD cathodic arc technique. The coatings had a thickness close to 5 μm and an average roughness between 98.6 and 110.1 μm due to the presence of microdroplets on the surface. The crystalline structure of the materials was analyzed using Grazing Incidence X-ray Diffraction (GIXRD) with an increase in temperature to study the dynamics of oxide formation. A phase composition study was conducted using the Rietveld refinement method. At the temperatures where critical growth of titanium oxides, both anatase and rutile, was observed, pin-on-disk tests were performed to study the tribological properties of the materials at high temperatures. It was determined that the oxidation temperature of Ti is around 450 °C, promoting the formation of a combination of anatase and rutile. However, the formation of rutile inhibits the formation of anatase, which is stable above 600 °C. In contrast, TiN showed an oxidation temperature of 550 °C, with an exclusive growth of the rutile phase. The Ti/TiN bilayer exhibited mixed behavior, with the initial growth of anatase promoted by Ti, followed by the formation of rutile. Oxidation and tribo-oxidation dominated the wear behavior of the surfaces, showing a transition from mechanisms related to abrasion at low and medium temperatures to a combination of abrasion and adhesion mechanisms at high temperatures (800 °C).


  • Open Access

    The Scratch Resistance of a Plasma-Assisted DUPLEX-Treated 17-4 Precipitation-Hardened Stainless Steel Additively Manufactured by Laser Powder Bed Fusion

    by Arturo Gómez-Ortega, Julián Andrés Pinilla-Bedoya, Carolina Ortega-Portilla, Christian Félix-Martínez, Guillermo César Mondragón-Rodríguez, Diego Germán Espinosa-Arbeláez, James Pérez-Barrera, Juan Manuel González-Carmona, Edgar Adrián Franco Urquiza

    Additive manufacturing (AM) or 3D printing of metals is gaining popularity due to its flexibility when fabricating parts with highly complex designs, as well as when simplifying manufacturing steps and optimizing process times. In this investigation, 17-4 PH stainless steel was additively manufactured using Laser Powder Bed Fusion (L-PBF), followed by functionalization through a DUPLEX treatment. This treatment involved a plasma-assisted nitriding process, followed by the deposition of an arc-PVD c-Al0.7Cr0.3N hard coating. The microstructural modifications resulting from plasma nitriding (such as the formation of Fe2,3N and Fe4N and the αN or expanded martensite phases) and the surface improvements with the c-Al0.7Cr0.3N coating on the 3D-printed 17-4 PH steel are evaluated in comparison to conventionally manufactured 17-4 PH steel. These microstructural characteristics are correlated with the mechanical response of the treated surfaces. As a result of the plasma nitriding process, the hardness of the 3D-printed 17-4 PH SS increased by approximately 260%. The wear, measured through dynamic and static scratch testing, was reduced by approximately 31%. This improvement was attributed to the modification of adhesive failure mechanisms, leading to a reduction in wear volume, improved coating adhesion, and enhanced scratch resistance.