M. M. Verdian
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
M. M. Verdian has a total of 6 co-authors. Here are the top co-authors by number of shared publications:
- Keyvan Raeissi
Department of Materials Engineering, Isfahan University of Technology, Isfahan, Iran
15 shared publications M. Salehi
15 shared publicationsM. Abbasi
Advanced Materials Research Center, Department of Materials Engineering, Najafabad Branch, Islamic Azad University, Najafabad, Iran
1 shared publicationM. Ashja
Advanced Materials Research Center, Department of Materials Engineering, Najafabad Branch, Islamic Azad University, Najafabad, Iran
1 shared publicationS. Heshmati-Manesh
School of Metallurgy and Materials Engineering, University of Tehran, Tehran, P.O. Box: 14395-553, Iran
1 shared publicationS. Sabooni
1 shared publication
Latest Publications
- 4 July 2018
- Published by Taylor & Francis in Transactions of the IMF
- Vol. 96 (4) , 206-211
Corrosion behaviour of HVOF-sprayed Co–Cr–W–C coating in NaCl solution
Stellite 6 (Co–Cr–W–C) coating was deposited on carbon steel substrate by high-velocity oxyfuel spraying. The electrochemical corrosion behaviour of the coatings was investigated in 3.5% NaCl solutions at 25°C by means of polarisation studies and electrochemical impedance spectroscopy (EIS) measurements. The immersion time before corrosion tests was 0.5 and 24 h. The results showed that the corrosion rate of the coatings was lower than that of the steel substrate by one order of magnitude. An active–passive behaviour was observed during anodic polarisation of the coatings at both immersion times. The degree of substrate attack after polarisation tests of coated samples was not considerable. EIS measurement showed that two-time constants were observed in Nyquist plots of the coatings.
- 4 July 2018
- Published by Taylor & Francis in Transactions of the IMF
- Vol. 96 (4) , 206-211
Corrosion behaviour of HVOF-sprayed Co–Cr–W–C coating in NaCl solution
Stellite 6 (Co–Cr–W–C) coating was deposited on carbon steel substrate by high-velocity oxyfuel spraying. The electrochemical corrosion behaviour of the coatings was investigated in 3.5% NaCl solutions at 25°C by means of polarisation studies and electrochemical impedance spectroscopy (EIS) measurements. The immersion time before corrosion tests was 0.5 and 24 h. The results showed that the corrosion rate of the coatings was lower than that of the steel substrate by one order of magnitude. An active–passive behaviour was observed during anodic polarisation of the coatings at both immersion times. The degree of substrate attack after polarisation tests of coated samples was not considerable. EIS measurement showed that two-time constants were observed in Nyquist plots of the coatings.
- 1 March 2017
- Published by SAGE Publications in Surface Engineering
- Vol. 33 (3) , 186-191
Processing and properties of CuAl2 intermetallic coatings
CuAl2 intermetallic powders were consolidated using an atmospheric plasma spraying process. Based on X-ray diffractometry results, no phase change occurred during thermal spraying. The investigation of optical micrographs showed that about 7% porosity was present in the microstructure of the coatings. The coatings showed hardness value up to 575 HV(50 g). The polarisation tests and electrochemical spectroscopy measurements were utilised for electrochemical investigation of the coatings in 1 M H2SO4 and 3.5% NaCl media. In H2SO4 environment, the coated and uncoated samples showed similar corrosion rates. However, the coating showed a lower corrosion rate than the substrate in NaCl solution by an order of magnitude. Corrosion of the steel substrate occurred in the NaCl solution, no corrosion was observed in the H2SO4. GRAPHICAL ABSTRACT
- 1 March 2017
- Published by SAGE Publications in Surface Engineering
- Vol. 33 (3) , 186-191
Processing and properties of CuAl2 intermetallic coatings
CuAl2 intermetallic powders were consolidated using an atmospheric plasma spraying process. Based on X-ray diffractometry results, no phase change occurred during thermal spraying. The investigation of optical micrographs showed that about 7% porosity was present in the microstructure of the coatings. The coatings showed hardness value up to 575 HV(50 g). The polarisation tests and electrochemical spectroscopy measurements were utilised for electrochemical investigation of the coatings in 1 M H2SO4 and 3.5% NaCl media. In H2SO4 environment, the coated and uncoated samples showed similar corrosion rates. However, the coating showed a lower corrosion rate than the substrate in NaCl solution by an order of magnitude. Corrosion of the steel substrate occurred in the NaCl solution, no corrosion was observed in the H2SO4. GRAPHICAL ABSTRACT
- 1 January 2017
- Published by Elsevier
- p. 191-206
3.13 Finishing and Post-Treatment of Thermal Spray Coatings
- 1 January 2017
- Published by Elsevier
- p. 191-206
3.13 Finishing and Post-Treatment of Thermal Spray Coatings
- 17 August 2016
- Published by Taylor & Francis in Materials and Manufacturing Processes
- Vol. 32 (4) , 383-388
Al-Cu-Fe Coatings Manufactured by Flame Spraying Process
Two-hour milled (activated) Al–20Cu–15Fe (at%) powders were subjected to annealing at 600°C for 1 h. The phase and microstructural evolutions were characterized by X-ray diffractometry and scanning electron microscopy. Al7Cu2Fe and Al60Cu30Fe10 phases were formed after annealing. Both annealed and milled powders were consolidated using the flame spraying process. In both cases, FeAl(Cu) was the major phase while some oxides and α-Fe(Al,Cu) were also found. The coating produced from the milled powder was severely cracked and showed higher oxide content. The coating prepared from the annealed powder showed better quality. It was annealed at 600°C for 1 h to investigate the thermal stability of the various phases. All phases persevered after annealing while the Fe2Al5 phase was formed as a new phase.
- 17 August 2016
- Published by Taylor & Francis in Materials and Manufacturing Processes
- Vol. 32 (4) , 383-388
Al-Cu-Fe Coatings Manufactured by Flame Spraying Process
Two-hour milled (activated) Al–20Cu–15Fe (at%) powders were subjected to annealing at 600°C for 1 h. The phase and microstructural evolutions were characterized by X-ray diffractometry and scanning electron microscopy. Al7Cu2Fe and Al60Cu30Fe10 phases were formed after annealing. Both annealed and milled powders were consolidated using the flame spraying process. In both cases, FeAl(Cu) was the major phase while some oxides and α-Fe(Al,Cu) were also found. The coating produced from the milled powder was severely cracked and showed higher oxide content. The coating prepared from the annealed powder showed better quality. It was annealed at 600°C for 1 h to investigate the thermal stability of the various phases. All phases persevered after annealing while the Fe2Al5 phase was formed as a new phase.
- 16 April 2015
- Published by Taylor & Francis in Transactions of the IMF
- Vol. 93 (3) , 164-168
Role of thickness on electrochemical behaviour of Ni2Si coatings in NaCl solution
- 16 April 2015
- Published by Taylor & Francis in Transactions of the IMF
- Vol. 93 (3) , 164-168
Role of thickness on electrochemical behaviour of Ni2Si coatings in NaCl solution
- 25 January 2015
- Published by Taylor & Francis in Transactions of the IMF
- Vol. 93 (1) , 38-43
Corrosion behaviour of Ni2Si intermetallic coatings in nitric acid solutions
- 25 January 2015
- Published by Taylor & Francis in Transactions of the IMF
- Vol. 93 (1) , 38-43
Corrosion behaviour of Ni2Si intermetallic coatings in nitric acid solutions
- 1 September 2014
- Published by SAGE Publications in Surface Engineering
- Vol. 30 (9) , 670-674
Characterisation and corrosion performance of HVOF sprayed Ni–10 wt-%Ti coatings
Mechanically alloyed Ni–10 wt-%Ti powders were deposited on 1045 steel substrate using high velocity oxy-fuel (HVOF) thermal spraying process. The microstructure and phase composition of coatings were evaluated by scanning electron microscopy (SEM) and X-ray diffraction (XRD) analysis. The results showed that the phase composition of feedstock powders was preserved during spraying and only supersaturated Ni(Ti) solid solution was present in the coatings. The hardness measurements showed that the hardness of coatings was about 510 HV (50 g). Tafel polarisation tests performed after 1 h immersion revealed that the corrosion behaviour of HVOF Ni–Ti coatings was not affected by substrate. However, delamination of air plasma sprayed (APS) Ni–10 wt-%Ti coatings and significant corrosion of substrate was observed in similar conditions. For HVOF Ni–Ti coating and after 24 h of immersion time, the corrosion of underlying substrate was observed after polarisation measurements but no delamination of coating occurred.
- 1 September 2014
- Published by SAGE Publications in Surface Engineering
- Vol. 30 (9) , 670-674
Characterisation and corrosion performance of HVOF sprayed Ni–10 wt-%Ti coatings
Mechanically alloyed Ni–10 wt-%Ti powders were deposited on 1045 steel substrate using high velocity oxy-fuel (HVOF) thermal spraying process. The microstructure and phase composition of coatings were evaluated by scanning electron microscopy (SEM) and X-ray diffraction (XRD) analysis. The results showed that the phase composition of feedstock powders was preserved during spraying and only supersaturated Ni(Ti) solid solution was present in the coatings. The hardness measurements showed that the hardness of coatings was about 510 HV (50 g). Tafel polarisation tests performed after 1 h immersion revealed that the corrosion behaviour of HVOF Ni–Ti coatings was not affected by substrate. However, delamination of air plasma sprayed (APS) Ni–10 wt-%Ti coatings and significant corrosion of substrate was observed in similar conditions. For HVOF Ni–Ti coating and after 24 h of immersion time, the corrosion of underlying substrate was observed after polarisation measurements but no delamination of coating occurred.
- 1 April 2014
- Published by SAGE Publications in Materials Science and Technology
- Vol. 30 (4) , 481-485
On corrosion behaviour of HVOF sprayed Ni3Si intermetallic powders
Ni3Si intermetallic powders were deposited onto 420 stainless steel substrate using high velocity oxy-fuel (HVOF) process. In this regard, microstructure properties relationships were evaluated in fabricated coatings. X-ray diffractometery, scanning electron microscopy, microhardness testing, potentiodynamic polarisation and electrochemical impedance spectroscopy (EIS) measurements were performed to study the phase composition, microstructure and properties of the coatings. The microstructure of coatings was composed of supersaturated Ni(Si) solid solution islands embedded in an Ni5Si2 matrix. The results showed that this microstructure strongly affected properties of coatings. In this regard, the hardness of coatings was found to be 620 HV(50 g) due to presence of Ni5Si2. It was also found that the corrosion rate of HVOF Ni–Si coatings in 70H2SO4 medium was lower than that of stainless steel substrate. Further investigations showed that the microgalvanic corrosion between Ni(Si) and Ni5Si2 phases was a determinant factor in corrosion performance of HVOF Ni–Si coatings.
- 1 April 2014
- Published by SAGE Publications in Materials Science and Technology
- Vol. 30 (4) , 481-485
On corrosion behaviour of HVOF sprayed Ni3Si intermetallic powders
Ni3Si intermetallic powders were deposited onto 420 stainless steel substrate using high velocity oxy-fuel (HVOF) process. In this regard, microstructure properties relationships were evaluated in fabricated coatings. X-ray diffractometery, scanning electron microscopy, microhardness testing, potentiodynamic polarisation and electrochemical impedance spectroscopy (EIS) measurements were performed to study the phase composition, microstructure and properties of the coatings. The microstructure of coatings was composed of supersaturated Ni(Si) solid solution islands embedded in an Ni5Si2 matrix. The results showed that this microstructure strongly affected properties of coatings. In this regard, the hardness of coatings was found to be 620 HV(50 g) due to presence of Ni5Si2. It was also found that the corrosion rate of HVOF Ni–Si coatings in 70H2SO4 medium was lower than that of stainless steel substrate. Further investigations showed that the microgalvanic corrosion between Ni(Si) and Ni5Si2 phases was a determinant factor in corrosion performance of HVOF Ni–Si coatings.
- 1 February 2014
- Published by Elsevier in Surface and Coatings Technology
- Vol. 240, 70-75
Corrosion resistance of HVOF-sprayed Ni2Si intermetallic coatings in hot H2SO4 medium
- 1 February 2014
- Published by Elsevier in Surface and Coatings Technology
- Vol. 240, 70-75
Corrosion resistance of HVOF-sprayed Ni2Si intermetallic coatings in hot H2SO4 medium