Mengyuan Bi
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Mengyuan Bi has a total of 6 co-authors. Here are the top co-authors by number of shared publications:
- Hailong Yi
State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819, China
2 shared publications - Bing Zhang
State Key Laboratory of Metastable Materials Science and Technology Yanshan University 066004 Qinhuangdao China
1 shared publication - Daixiu Wei
Tohoku University - Institute for Materials Research
1 shared publication - Kang Yang
State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819, China
1 shared publication - Renyi Xie
State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819, China
1 shared publication - Yifan Zhang
State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819, China
1 shared publication
Latest Publications
- Open Access
High-Temperature Deformation Behaviors of the C-Doped and N-Doped High Entropy Alloys
High entropy alloys (HEAs) containing multi-principal metallic constituents have attracted much attention. A good understanding of their hot-deformation behavior and recrystallization mechanism is the prerequisite for microstructures tuning and for optimizing mechanical performance. Here, the flow behavior and recrystallization mechanism of the N-doped and C-doped face-centered cubic phase HEAs are produced at high temperatures by hot-compression at 1123–1273 K, with strain rates of 0.1–0.001 s−1. Constitutive equations were successfully constructed to reveal flow behavior, and stress-strain curves were predicted using strain compensated polynomial functions. Discontinuous and continuous dynamic recrystallization proceeded concurrently when compressed at a low temperature and high strain rate, whereas discontinuous recrystallization, which occurs at primary grain boundaries, became predominant at a high temperature and low strain rate, significantly contributing to the refinement and homogenization of the grains. For this reason, a relatively high temperature and a low strain rate, in which the recrystallized grains exhibit equiaxed morphology and very weak texture, are more suitable for refining grains. The average size of the grains was approximately 10 μm. This study sheds light on grain optimization and mechanical properties through thermomechanical processing.
Open AccessHigh-Temperature Deformation Behaviors of the C-Doped and N-Doped High Entropy Alloys
High entropy alloys (HEAs) containing multi-principal metallic constituents have attracted much attention. A good understanding of their hot-deformation behavior and recrystallization mechanism is the prerequisite for microstructures tuning and for optimizing mechanical performance. Here, the flow behavior and recrystallization mechanism of the N-doped and C-doped face-centered cubic phase HEAs are produced at high temperatures by hot-compression at 1123–1273 K, with strain rates of 0.1–0.001 s−1. Constitutive equations were successfully constructed to reveal flow behavior, and stress-strain curves were predicted using strain compensated polynomial functions. Discontinuous and continuous dynamic recrystallization proceeded concurrently when compressed at a low temperature and high strain rate, whereas discontinuous recrystallization, which occurs at primary grain boundaries, became predominant at a high temperature and low strain rate, significantly contributing to the refinement and homogenization of the grains. For this reason, a relatively high temperature and a low strain rate, in which the recrystallized grains exhibit equiaxed morphology and very weak texture, are more suitable for refining grains. The average size of the grains was approximately 10 μm. This study sheds light on grain optimization and mechanical properties through thermomechanical processing.
- Open Access
Significant Improvement the Mechanical Properties of CoCrNi Alloy by Tailoring a Dual FCC-Phase Structure
In this work, SixCoCrNi (x = 0, 0.1, 0.2, 0.3, 0.4, molar ratio) alloys were designed by introducing elemental Si into CoCrNi, a medium-entropy alloy (MEA). The effects of Si addition on the microstructure and mechanical properties of the as-cast SiCoCrNi alloys were investigated. The results suggested that a novel Si-rich face-centred cubic (FCC) phase formed in the Si0.3CoCrNi and Si0.4CoCrNi alloys. The Si-rich FCC phase, which featured high hardness and was located between the dendrites of the matrix FCC phase (with higher phase fraction), significantly increased the yield strength of the Si0.4CoCrNi alloys five times compared with the CoCrNi alloy.
Open AccessSignificant Improvement the Mechanical Properties of CoCrNi Alloy by Tailoring a Dual FCC-Phase Structure
In this work, SixCoCrNi (x = 0, 0.1, 0.2, 0.3, 0.4, molar ratio) alloys were designed by introducing elemental Si into CoCrNi, a medium-entropy alloy (MEA). The effects of Si addition on the microstructure and mechanical properties of the as-cast SiCoCrNi alloys were investigated. The results suggested that a novel Si-rich face-centred cubic (FCC) phase formed in the Si0.3CoCrNi and Si0.4CoCrNi alloys. The Si-rich FCC phase, which featured high hardness and was located between the dendrites of the matrix FCC phase (with higher phase fraction), significantly increased the yield strength of the Si0.4CoCrNi alloys five times compared with the CoCrNi alloy.