SASebnem Sevil Arpaci

Sebnem Sevil Arpaci

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Sebnem Sevil Arpaci has a total of 7 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Microstructural Evolution and Physico-Mechanical Response of Cement-Bonded Fiberboards: A Comparative Study on Cement Type and Fiber Ratio

    by Emrecan Arpaci, Sebnem S. Arpaci, Ergun Guntekin

    This study investigates the interplay between Portland cement strength class (32.5, 42.5, and 52.5) and fiber/cement ratio (ranging from 1/2 to 1/5 by weight) to optimize the physical-mechanical and thermal performance of cement-bonded fiberboards. The experimental data revealed a distinct trade-off: while reducing the fiber content towards a 1/5 ratio significantly improved flexural strength and dimensional stability through matrix densification, it inevitably compromised thermal insulation. Among the binders evaluated, the 42.5 strength class emerged as the most effective option, outperforming the 32.5 class and, notably, offering a more balanced profile than the 52.5 class. The highest stiffness was recorded with the 42.5 cement at a 1/5 ratio (modulus of elasticity (MOE): 5902 ± 532 N/mm2; modulus of rupture (MOR): 12.49 ± 0.6 N/mm2), yielding performance metrics comparable to the 1/4 ratio (MOR: 12.78 N/mm2). Furthermore, this formulation demonstrated superior moisture resistance, achieving water absorption (WA) values as low as 18.9%. Thermal conductivity (TC) measurements at 20 °C confirmed that while fiber-rich mixtures (1/2 ratio) favored insulation, the 42.5 cement at a 1/4 ratio maintained a competitive conductivity value (λ = 0.1625 W/mK), lower than that of the 52.5 grade, thereby striking a critical balance between structural integrity and thermal efficiency. Statistical analyses (Two-way ANOVA, p < 0.05) corroborated the significant influence of both cement type and mix ratio. Microstructural insights from Fourier transform infrared spectroscopy (FTIR), X-ray diffraction (XRD), and scanning electron microscopy (SEM) suggest that the superior performance of the 42.5 cement is associated with optimized hydration kinetics and a well-graded particle size distribution (D50 = 14.80 µm), which together facilitated effective fiber encapsulation.

  • Open Access

    Optimizing Mechanical and Thermal Properties of Slag-Based Geopolymer Fiber Boards via Fiber Pretreatment and Reinforcement Type

    by Sebnem Sevil Arpaci, Ergun Guntekin

    This study aims to optimize the physical, mechanical, and thermal properties of 100% Ground Granulated Blast Furnace Slag (GGBFS) based geopolymer wood-composite panels. Pine fibers were utilized as the primary reinforcement matrix, while glass and hemp fibers were introduced as secondary reinforcements at varying proportions (3%, 6%, 9% by weight). The research investigated the effects of fiber pretreatments (hot water vs. 1% NaOH) and reinforcement hybridization. Results indicate that GGBFS successfully geopolymerized, forming a hybrid N-A-S-H and C-A-S-H gel network. Quantitative analysis revealed that 9% glass fiber reinforcement yielded the highest mechanical performance, achieving a Modulus of Rupture (MOR) of 10.05 N/mm2 and Internal Bond (IB) strength of 1.32 N/mm2, alongside superior water resistance (1.0% Thickness Swelling). Conversely, while hemp fiber inclusion reduced mechanical strength (MOR: 5.77 N/mm2 at 9%), it significantly enhanced thermal insulation, reducing thermal conductivity to 0.10 W/m·K. It was observed that aggressive NaOH pretreatment caused alkali-induced degradation of pine fibers, negatively impacting the composite’s integrity compared to hot water treatment. This study demonstrates the feasibility of tailoring 100% slag-based geopolymer composites for either structural (glass-reinforced) or insulating (hemp-reinforced) applications using industrial by-products.


  • Open Access

    Microstructural Evolution and Physico-Mechanical Response of Cement-Bonded Fiberboards: A Comparative Study on Cement Type and Fiber Ratio

    by Emrecan Arpaci, Sebnem S. Arpaci, Ergun Guntekin

    This study investigates the critical interplay between cement grade (32.5, 42.5, 52.5) and fiber/cement ratio (1/2 to 1/5) in determining the performance of cement-bonded fiberboards. Experimental results highlighted a fundamental trade-off: while reducing the fiber content significantly enhanced mechanical strength and moisture resistance, it naturally diminished thermal insulation capabilities. The analysis identified the 42.5 cement at a 1/4 ratio as the optimal formulation, offering the most effective balance between structural integrity and physical stability. To understand the mechanism behind this performance, the study employed multi-scale characterization using FTIR, XRD, and SEM. These analyses revealed that the superior properties of the optimal formulation stem from a denser hydration product network and improved fiber encapsulation. Specifically, the 42.5 cement facilitated a more robust Calcium-Silicate-Hydrate (C-S-H) gel formation compared to the 32.5 types, creating a stronger fiber-matrix interface. These findings provide a scientific basis for tailoring fiberboard production, demonstrating that material properties can be precisely engineered for either load-bearing or insulating applications.


  • Open Access

    Optimizing Mechanical and Thermal Properties of Slag-Based Geopolymer Fiber Boards via Fiber Pretreatment and Reinforcement Type

    by Sebnem Sevil Arpaci, Ergun Guntekin

    This study aims to optimize the physical, mechanical, and thermal properties of 100% Ground Granulated Blast Furnace Slag (GGBFS) based geopolymer wood-composite panels. Pine fibers were used as the primary reinforcement, while glass and hemp fibers were added as secondary reinforcements. The research investigated the effects of fiber pretreatments (hot water and 1% sodium hydroxide (NaOH) solution and varying proportions (3%, 6%, 9% by weight) of these secondary reinforcements on the slag-based geopolymer matrix. Properties such as density, water absorption (WA), thickness swelling (TS), thermal conductivity (λ), modulus of rupture (MOR), modulus of elasticity (MOE), and internal bond (IB) strength were determined. Furthermore, microstructural and chemical interactions were examined through Fourier Transform Infrared Spectroscopy (FTIR), X-ray Diffraction (XRD), and Scanning Electron Microscopy (SEM) analyses. Results indicate that GGBFS successfully geopolymerized upon alkali activation, exhibiting strong mechanical properties due to the formation of N-A-S-H and C-A-S-H gels. While hot water pretreatment provided a slight improvement in the fiber-matrix interface, NaOH pretreatment led to alkali-induced degradation, causing significant reductions in performance. Glass fiber reinforcement generally resulted in higher density and systematically increased MOR, MOE, and IB values, significantly enhancing the mechanical performance and water resistance of the composites. In contrast, hemp fiber reinforcement typically yielded lower density values and reduced mechanical properties due to fiber agglomeration and high hydrophilicity. However, HF-containing groups, particularly with 9% addition, showed a notable reduction in thermal conductivity (down to 0.10 W/m·K), suggesting potential for lightweight insulation applications. FTIR, XRD, and SEM analyses corroborated the effects of fiber-matrix interactions and microstructural defects on the observed macro-properties. This study provides valuable insights into utilizing industrial and agricultural wastes in geopolymer composites, supporting sustainable and carbon-neutral construction goals.

  • Open Access

    Nano seryum-oksit ile muamele edilen odunun hızlandırılmış yaşlandırma testi sonrasında renk ve yüzey kimyasındaki değişimi

    by Uğur Özkan, Sebnem Sevil Arpaci, Eylem Di̇zMan Tomak

    Doğal biyolojik polimer olan ahşap malzemenin, diğer yapı malzemelerine kıyasla önemli avantajları bulunmaktadır. Ancak ahşap malzeme, dış ortam koşullarında dayanıklı bir yapıya sahip olmadığı için mutlaka emprenye edilerek veya çeşitli üst yüzey işlemleri yapılarak kullanılmalıdır. Bu çalışmada, sarıçam (Pinus sylvestris L.) örnekleri %0,1; %0,2; %0,5; %0,7; %1; %2; %3; %4 ve %5 konsantrasyonda nano seryum oksit (CeO2) ile muamele edilmiş ve örneklerin hızlandırılmış yaşlandırma testi sonrasında renk değişimi ile yüzey kimyasındaki değişim araştırılmıştır. Hızlandırılmış yaşlandırma testine maruz bırakılan örneklerde başlangıçtan sonra 2, 4, 6, 8, 12, 16, 20, 24, 48, 72, 96, 120, 144 ve 168 saatte renk ve yüzey kimyasındaki değişim belirlenmiştir. Seryum oksidin etkinliği aynı konsantrasyon değerlerinde hazırlanan Tanalith-E çözeltisi ile muamele edilen örnekler ile kıyaslanmıştır. Böylece, seryum oksidin dış ortama maruz kalan ahşap malzemenin yüzey özelliklerinin iyileştirilmesinde, referans maddeye kıyasla kullanılabilirliği değerlendirilmiştir. Çalışma sonucunda, seryum oksit ve Tanalith-E ile muamele edilen örneklerde kontrol örneklerine kıyasla yüzey özellikleri korunmuştur. Araştırılan yüzey özelliklerindeki değişim en fazla, yaşlandırma testinin ilk saatlerinde gözlenmiş, seryum oksidin bakır bazlı emprenye maddesine (Tanalith-E) benzer sonuçlar verdiği bulunmuştur.

  • Decay Resistance of Weathered Beech Wood

    by Sebnem Sevil Arpaci, Merve Cambazoğlu, Eylem Di̇zman Tomak

    Wood is susceptible to photo-degradation in outdoor applications, and deformations occur on its surface such as micro or macro cracks, color changes etc. Especially, cracks make wood material more vulnerable to biotic attacks. In this study, decay resistance of natural and accelerated weathered beech samples was investigated by a brown (Coniophora puteana) and white rot (Coriolus versicolor) fungi attacks. For this purpose, beech samples exposed to natural weathering (NW) for 393 days, and accelerated weathering (AW) for 1512h, and then subjected to decay test in malt extract agar medium for 2 and 4 weeks. After 2 weeks of decay testing, weight loss of samples by C. versicolor was found to be 24.30% for controls, 13.29% for AW samples and 24.38% for NW samples. In the case of C. puteana, it was found as 21.15%, 21.49% and 30.61% for controls, AW samples and NW samples, respectively. Weight loss of samples by C. versicolor was found to be 61.82% for controls, 30.72% for AW samples and 37.62% for NW samples, after 4 weeks of decay testing. The weight loss by 4 weeks exposure of C. puteana was found to be 21.43%, 28.44% and 37.67% for controls, AW samples and NW samples, respectively. Natural weathering caused more weight loss than accelerated weathering test for both fungi species.