WMWahyu Mayangsari

Wahyu Mayangsari

*This is an algorithmically generated author record based on publicly available information.

Wahyu Mayangsari has a total of 45 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • A Novel Method in Valorization of Ferronickel Slag as Nano Silica and Heavy Metals Amphoteric Adsorbent by Hydrothermal Process

    by Wahyu Mayangsari, Aga Ridhova, Shifa Salsa Bila, Arival Jefry, Kahlil Lukmanul Akmal, Eni Febriana, Agus Budi Prasetyo, Reza Miftahul Ulum, Azizah Intan Pangesty, Johny Wahyuadi Soedarsono

  • Impregnated-Alkaline Roasting for Tailoring Nanoporous Silica from Ferronickel Slag Waste

    by Wahyu Mayangsari, Agus Budi Prasetyo, Eni Febriana, Rudi Subagja, Johny W. Soedarsono


  • Open Access

    Exploration of rice husk ash as a green corrosion inhibitor immersed in NH4Cl 7.5 % solution

    by Agus Paul Setiawan Kaban, Johny Wahyuadi Soedarsono, Mochammad Syaiful Anwar, Wahyu Mayangsari, Ahmad Maksum, Aga Ridhova, Rini Riastuti, Dedy Iskandar, Ayende


  • Open Access

    Novel method for minimizing reactant in the synthesis of sodium silicate solution from mixed-phase quartz-amorphous SIO2

    by Eni Febriana, Wahyu Mayangsari, Sigit Dwi Yudanto, Eko Sulistiyono, Murni Handayani, Florentinus Firdiyono, Ahmad Maksum, Agus Budi Prasetyo, J.W. Soedarsono


  • Open Access

    THE EFFECT OF MIXING METHODS BEFORE THE DECOMPOSITION PROCESS OF FERRONICKEL SLAG

    by Wahyu Mayangsari, Agus Budi Prasetyo, Eni Febriana, Ahmad Maksum, Rudi Subagja, F Firdiyono, Johny Wahyuadi Soedarsono

    Ferronickel slag is a by-product that was obtained from ferronickel production and contains Si and Mg as the main elements. Decomposition process using alkali could decrease energy consumption to process ferronickel slag by decreasing its melting point. The mixing methods prior to the decomposition process could significantly affect interaction between reactants over the process, therefore it is essential to study. The aim of this study is to determine the effect of mixing methods of ferronickel slag and NaOH prior decomposition process on the chemical composition, phase, and microstructure of decomposed ferronickel slag. Two different mixing methods, physical mixing, and impregnation, followed by roasting process at 350 ℃ for 60 minutes were performed, characterized, and analyzed. Thermodynamic analysis was calculated and shows having a good agreement with the characterization results which formation of sodium silicate, magnesium hydroxide and iron oxide were identified. Distribution of product layer of RI can be determined, while spotty decomposition was clearly identified. The effectiveness of impregnation over physical mixing was investigated.


  • High energy density asymmetric supercapacitors enabled by La-induced defective MnO2 and biomass-derived activated carbon

    by Angga Hermawan, Fredina Destyorini, Andri Hardiansyah, Vani Novita Alviani, Wahyu Mayangsari, Wibisono, Ni Luh Wulan Septiani, Rike Yudianti, Brian Yuliarto


  • Open Access

    Pyro-Hydrometallurgy Routes to Recover Silica from Indonesian Ferronickel Slag

    by Reza M. Ulum, Natalin, Rini Riastuti, Wahyu Mayangsari, Agus B. Prasetyo, Johny W. Soedarsono, Ahmad Maksum

    Ferronickel slag is a by-product of nickel smelting that provides an abundant silica source. Based on data, every ton of nickel production is equal to eight tons of ferronickel slag production, increasing without any recycling process. It is essential to create an end-to-end process for nickel production and its by-products because this would be a problem in the future and is relevant for many industrialized countries. This study describes a strategy to process ferronickel slag to produce silica. A pyrometallurgy–hydrometallurgy process and ferronickel slag were used to increase the silica content. The process was conducted through alkali fusion; the ferronickel slag was mixed with sodium carbonate at a temperature of 1000 °C for an hour and continued via leaching, precipitation, and cleaning processes. The leaching process was conducted with four concentrations (4 M, 6 M, 8 M, and 10 M) of sodium hydroxide and three different leaching durations (2 h, 4 h, and 6 h). Using hydrochloric acid (HCl) at pH 2 and deionized (DI) water cleaning, the precipitation process was adopted to synthesize a silica powder with the lowest agglomeration and enhance its purity. Characterization was carried out using X-ray Diffraction (XRD), Scanning Electron Microscopy–Energy-Dispersive Emission (SEM-EDS), X-ray Fluorescence (XRF), and Inductively Coupled Plasma–Optical Emission Spectroscopy (ICP-OES). This study highlighted silica characteristics that indicate high recovery by 85% through alkali fusion, HCl leaching, precipitation, and deionized water cleaning.


  • Open Access

    Insight on Corrosion Prevention of C1018 in 1.0 M Hydrochloric Acid Using Liquid Smoke of Rice Husk Ash: Electrochemical, Surface Analysis, and Deep Learning Studies

    by Agus Paul Setiawan Kaban, Johny Wahyuadi Soedarsono, Wahyu Mayangsari, Mochammad Syaiful Anwar, Ahmad Maksum, Aga Ridhova, Rini Riastuti

    This work reports the anti-corrosion behavior of liquid smoke from rice husk ash to unveil the contribution of its active compounds in 1 M HCl solution. In this study, the developed methodology to test, analyze, and model the novel type of green corrosion inhibitor for C1018 was characterized using Electrochemical impedance spectroscopy (EIS), Potentiodynamic polarization, and deep learning methods. The inhibitor structure was characterized by Fourier transform infrared analysis (FTIR) and Ultraviolet–visible spectroscopy (UV-Vis). The surface characterization of mild steel immersed in blank and 80 ppm solution inhibitor was performed using Atomic force microscopy (AFM) analysis. The corrosion test results show that the inhibitor is considered a mixed-type inhibitor to achieve the optimum inhibition of 80 ppm at 323 K, reaching up to 99% inhibition efficiency. The AFM results show a smoother surface given a lower skewness parameter at −0.5190 nm on the treated mild steel. The artificial neural network demonstrates the lower overfitting on the inhibited steel, a higher accuracy prediction of 81.08%, and a lower loss rate of 0.6001 to model the relationship between the EIS and Potentiodynamic polarization and the evolution of the passive layer on the treated mild steel. The experiment agrees well with the prediction result to model the adsorbed inhibitor. The work can be used as a guideline to pave the way for subsequent applicability in developing green corrosion inhibitors based on experimental and artificial intelligence approaches.


  • Open Access

    Unraveling the study of liquid smoke from rice husks as a green corrosion inhibitor in mild steel under 1 M HCl

    by Agus Kaban, Wahyu Mayangsari, Mochammad Anwar, Ahmad Maksum, Taufik Aditiyawarman, Johny Soedarsono, Aga Ridhova, Rini Riastuti

    The work provides the more comprehensive development of Liquid Smoke from Rice Husks Ash (RHA). Notably, the study focuses on the interaction between the primary molecules of inhibitor and mild steel, including thermodynamic calculation and surface treatment upon addition of inhibitor. The electrochemical impedance spectroscopy (EIS) and potentiodynamic polarization (PP) characterization were utilized to evaluate the anticorrosion of RHA. The Raman Spectroscopy pre and post-addition of RHA’s inhibitor were used to compare the adsorbed functional group of inhibitors. Moreover, the thermodynamic calculation of the inhibitor’s adsorption determines the types of adsorption of the inhibitor. As a result of the adsorption process, the Scanning Electronic Microscope-Energy Dispersive X-Ray (SEM-EDX) aided by The Atomic Force Microscopy (AFM) and Contact Angle Test was implemented to unveil the surface treatment and the change of elemental composition after the addition of an 80 ppm inhibitor. The PP and EIS results show a significant depression of the current density at ‒2.75 μA·cm2 in 80 ppm solution with the highest inhibition efficiency of 99.82 %. The superior inhibition correlates to the adsorption of Si–OH, C–C, C–O–C, >C=O, complex structure, and –OH at wavenumber 458, 662, 1095, 1780, and 3530 cm-1. The LS shows a significant surface area of protection of 0.9982 and high adsorption constant (Kads) at 11.648. The calculated ΔGads of ‒6.59 kJ/mol unveils the chemisorption in nature. At the same time, a combination of 20 and 80 ppm solution is predicted adsorbed horizontally to reduce the contact between the solution and substrate, as shown in SEM and AFM results. It also increases the contact angle and their corresponding hydrophobicity


  • Open Access

    The Effect of Roasting Prior to The Leaching Process of Alkalinized Ferronickel Slag Followed by Precipitation Process

    by Wahyu Mayangsari, Agus Budi Prasetyo, Eni Febriana, Januar Irawan, Rudi Subagja, Florentinus Firdiyono, Johny Wahyuadi Soedarsono

    Terak feronikel dihasilkan sebagai produk samping dari produksi feronikel. terak feronikel mempunyai potensi sebagai bahan baku beberapa komponen berharga karena komposisinya melalui proses bertahap. Tujuan dari penelitian ini adalah untuk mengetahui pengaruh dari proses pemanggangan campuran terak feronikel dan Na2CO3 sebelum leaching air panas dan presipitasi untuk menghasilkan endapan silika. Proses pemanggangan terak feronikel dengan penambahan Na2CO3 telah dilakukan untuk pembentukan natrium silikat. Kemudian dilarutkan melalui proses pelindian menggunakan air panas 90 ° C selama 120 menit. Endapan silika didapatkan dengan proses presipitasi sodium silikat terlarut diikuti dengan pemeraman selama tiga hari. Berdasarkan hasilnya, pemanggangan menyebabkan perubahan komposisi yang mempengaruhi persen pelindian dan perolehan silika. Reaksi terjadi dari permukaan ke inti yang dibuktikan dengan pengecilan ukuran residu pelindian dari RAF nya. Natrium silikat dalam bentuk Na4SiO4 diketahui terlarut Ketika pelindian air dilakukan. Pengendapan dan pemeraman larutan natrium silikat telah menghasilkan endapan silika dengan ukuran partikel lebih dari 100 mm. pemanggangan pada 1000 ° C selama 240 menit menghasilkan perolehan silika tertinggi.