Fariza Eka Yunita
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Fariza Eka Yunita has a total of 34 co-authors. Here are the top co-authors by number of shared publications:
- Latifa Hanum Lalasari
National Research and Innovation Agency
3 shared publications - Nadia Chrisayu Natasha
Indonesian Institute of Sciences (LIPI)
3 shared publications - Tri Arini
National Research and Innovation Agency
3 shared publications A R Rhamdani
2 shared publications- Erlina Yustanti
Department of Metallurgy, Faculty of Engineering, University of Sultan Ageng Tirtayasa, Cilegon Banten 42435, Indonesia
2 shared publications F. Firdiyono
2 shared publications
Latest Publications
- Open Access
- 31 December 2023
- Published by National Research and Innovation Agency in Metalurgi
- Vol. 38 (3) , 109-116
Kinetic of Dissolution of Nickel Limonite Calcine by Sulfuric Acid Solution
Currently, more than 60% of nickel processing is carried out using nickel sulfide as a raw material. Nonetheless, due to the depletion reserves of nickel sulphide, nickel laterite has drawn a lot of interest to be processed as raw material. Nickel laterite in Indonesia is generally found in low grades, with nickel concentration of <1.15%. One method of treating nickel limonite is leaching in a sulfuric acid solution. This study aims to determine the reaction rate in the leaching process of calcine nickel limonite and the effect of sulfuric acid concentration and leaching temperature on the percent nickel extraction. In this research, the limonite ore from Pomalaa, Southeast Sulawesi, Indonesia, which has undergone a reduction process, was used as raw material. This research was conducted by leaching method on nickel limonite calcine using sulfuric acid reagent with 0.2, 0.5, and 1 M concentration variation, temperature variations of 60, 70, and 90°C, stirring speed 500 rpm, and %S/L (w/w) 10%. In this leaching research, the activation energy obtained at a sulfuric acid concentration of 0.2, 0.5, and 1 M are 13,7379 kJ/mol, 19,7582 kJ/mol, 20,3161 kJ/mol, respectively. The leaching process of nickel limonite calcine was controlled by diffusion. The optimum nickel extraction percentage in this study was 97.45%, obtained at a concentration of 1 M sulfuric acid, temperature of 70 °C, and leaching time of 240 minutes.
- 31 December 2023
- Published by National Research and Innovation Agency in Metalurgi
- Vol. 38 (3) , 109-116
Open AccessKinetic of Dissolution of Nickel Limonite Calcine by Sulfuric Acid Solution
Currently, more than 60% of nickel processing is carried out using nickel sulfide as a raw material. Nonetheless, due to the depletion reserves of nickel sulphide, nickel laterite has drawn a lot of interest to be processed as raw material. Nickel laterite in Indonesia is generally found in low grades, with nickel concentration of <1.15%. One method of treating nickel limonite is leaching in a sulfuric acid solution. This study aims to determine the reaction rate in the leaching process of calcine nickel limonite and the effect of sulfuric acid concentration and leaching temperature on the percent nickel extraction. In this research, the limonite ore from Pomalaa, Southeast Sulawesi, Indonesia, which has undergone a reduction process, was used as raw material. This research was conducted by leaching method on nickel limonite calcine using sulfuric acid reagent with 0.2, 0.5, and 1 M concentration variation, temperature variations of 60, 70, and 90°C, stirring speed 500 rpm, and %S/L (w/w) 10%. In this leaching research, the activation energy obtained at a sulfuric acid concentration of 0.2, 0.5, and 1 M are 13,7379 kJ/mol, 19,7582 kJ/mol, 20,3161 kJ/mol, respectively. The leaching process of nickel limonite calcine was controlled by diffusion. The optimum nickel extraction percentage in this study was 97.45%, obtained at a concentration of 1 M sulfuric acid, temperature of 70 °C, and leaching time of 240 minutes.
- Open Access
- 30 December 2022
- Published by National Research and Innovation Agency in Metalurgi
- Vol. 37 (3)
MORPHOLOGY AND RESISTIVITY VALUE OF FLOURINE-DOPED TIN OXIDE (FTO) USING INDONESIAN LOCAL DIMETHYLTIN DICHLORIIDE (DTMC) PRECURSORS
Transparent Conductive Oxide (TCO) is the main component for solar cell fabrication. One of the promising types of TCO is fluorine-doped tin oxide (FTO). The method used in depositing the conductive layer of FTO is spray pyrolysis with an ultrasonic nebulizer. The precursor is a local Indonesian product, dimethyl tin dichloride (DMTC), with doping ammonium fluoride (NH4F). The variable that used in this study were variations in deposition time (5. 10. 15. 20, and 25 minutes) with a fixed substrate temperature at 300°C and doping variations (un-doped, 2 wt.% doped and 8 wt.% doped) to see the effect of adding F doping to the precursor solution. The resistivity value with deposition time of 5. 10. 15. 20 and 25 minute (2 wt.% doped) is 0.218x100; 0.449x10-1; 1,567x10-2; 0.676x10-2 0.377x10-2 Ω.cm. For doping variations (un-doped, 2 wt% doped and 8 wt% doped) the value is 0.883x10-2; 0.377x10-2; 0.506x10-3 Ω.cm. There is a decreasing trend in the resistivity values obtained along with the increase in deposition time and the addition of doping to obtain better conductive properties. The grain size will increase with increasing deposition time and the addition of doping. The optimum resistivity value obtained in this study was 0.377x10-2 Ω.cm, obtained at the deposition time of 25 minutes with 2 wt.% doping.
- 30 December 2022
- Published by National Research and Innovation Agency in Metalurgi
- Vol. 37 (3)
Open AccessMORPHOLOGY AND RESISTIVITY VALUE OF FLOURINE-DOPED TIN OXIDE (FTO) USING INDONESIAN LOCAL DIMETHYLTIN DICHLORIIDE (DTMC) PRECURSORS
Transparent Conductive Oxide (TCO) is the main component for solar cell fabrication. One of the promising types of TCO is fluorine-doped tin oxide (FTO). The method used in depositing the conductive layer of FTO is spray pyrolysis with an ultrasonic nebulizer. The precursor is a local Indonesian product, dimethyl tin dichloride (DMTC), with doping ammonium fluoride (NH4F). The variable that used in this study were variations in deposition time (5. 10. 15. 20, and 25 minutes) with a fixed substrate temperature at 300°C and doping variations (un-doped, 2 wt.% doped and 8 wt.% doped) to see the effect of adding F doping to the precursor solution. The resistivity value with deposition time of 5. 10. 15. 20 and 25 minute (2 wt.% doped) is 0.218x100; 0.449x10-1; 1,567x10-2; 0.676x10-2 0.377x10-2 Ω.cm. For doping variations (un-doped, 2 wt% doped and 8 wt% doped) the value is 0.883x10-2; 0.377x10-2; 0.506x10-3 Ω.cm. There is a decreasing trend in the resistivity values obtained along with the increase in deposition time and the addition of doping to obtain better conductive properties. The grain size will increase with increasing deposition time and the addition of doping. The optimum resistivity value obtained in this study was 0.377x10-2 Ω.cm, obtained at the deposition time of 25 minutes with 2 wt.% doping.
- Open Access
- 25 June 2021
- Published by Private Company Technology Center in Eastern-European Journal of Enterprise Technologies
- Vol. 3 (5 (111)) , 6-12
Investigation of surfactant effect during synthesis of magnesium oxide nanoparticles from bittern using ultrasonic destruction process
Magnesium oxide (MgO) nanoparticles have been widely used in a variety of applications because of their good surface reactivity. Magnesium oxide from bittern has a larger surface area compared to magnesium oxide from calcined magnesite and magnesium ions precipitation from bittern using sodium hydroxide has higher purity than using calcium hydroxide or ammonium hydroxide. In this research, sodium hydroxide was added to a bittern solution obtaining magnesium hydroxide precipitate, followed by the calcination process to produce magnesium oxide. Nano magnesium oxide was synthesized by the ultrasonic destruction process using ethanol and 2-propanol as media. In this study, sonication time and particle concentration effect on the ultrasonic destruction process were investigated. During the process, the sonication time was varied between 8, 16, 32, 64, and 128 minutes while the magnesium oxide concentration was varied between 1 %, 2 %, and 3 %. Increasing sonication time and particle concentration will decrease the particle size. The previous study shows that particles with very small sizes tend to have an agglomeration effect. The aim of this work is to optimize nano magnesium oxide production from bittern. Surfactant addition was also studied to prevent agglomeration between particles. Four types of surfactant namely anionic (sodium lauryl sulfate), cationic (cetyl tri-methyl-ammonium bromide), amphoteric (fatty acid amido alkyl betaine), and non-ionic (nonylphenol 10 ethoxylated) with a concentration of 1 % and a volume of 0.125 ml were added during the second ultrasonic destruction process. All types of surfactants have a positive effect to prevent agglomeration during the ultrasonic destruction process, with the amphoteric surfactant having the highest performance
- 25 June 2021
- Published by Private Company Technology Center in Eastern-European Journal of Enterprise Technologies
- Vol. 3 (5 (111)) , 6-12
Open AccessInvestigation of surfactant effect during synthesis of magnesium oxide nanoparticles from bittern using ultrasonic destruction process
Magnesium oxide (MgO) nanoparticles have been widely used in a variety of applications because of their good surface reactivity. Magnesium oxide from bittern has a larger surface area compared to magnesium oxide from calcined magnesite and magnesium ions precipitation from bittern using sodium hydroxide has higher purity than using calcium hydroxide or ammonium hydroxide. In this research, sodium hydroxide was added to a bittern solution obtaining magnesium hydroxide precipitate, followed by the calcination process to produce magnesium oxide. Nano magnesium oxide was synthesized by the ultrasonic destruction process using ethanol and 2-propanol as media. In this study, sonication time and particle concentration effect on the ultrasonic destruction process were investigated. During the process, the sonication time was varied between 8, 16, 32, 64, and 128 minutes while the magnesium oxide concentration was varied between 1 %, 2 %, and 3 %. Increasing sonication time and particle concentration will decrease the particle size. The previous study shows that particles with very small sizes tend to have an agglomeration effect. The aim of this work is to optimize nano magnesium oxide production from bittern. Surfactant addition was also studied to prevent agglomeration between particles. Four types of surfactant namely anionic (sodium lauryl sulfate), cationic (cetyl tri-methyl-ammonium bromide), amphoteric (fatty acid amido alkyl betaine), and non-ionic (nonylphenol 10 ethoxylated) with a concentration of 1 % and a volume of 0.125 ml were added during the second ultrasonic destruction process. All types of surfactants have a positive effect to prevent agglomeration during the ultrasonic destruction process, with the amphoteric surfactant having the highest performance
- Open Access
- 18 June 2021
- Published by Private Company Technology Center in Eastern-European Journal of Enterprise Technologies
- Vol. 3 (6 (111)) , 80-88
The use of mica schist from Indonesia as raw material for lithium extraction process using sulfate roasting and acid leaching
Lithium minerals become a sub-economic raw material for lithium production to fulfill the lithium demand. This study is about lithium extraction from mica schist using the roasting and leaching processes. The mica schist located in Kebumen, Indonesia was used to study the phenomena during the lithium extraction process. Sodium sulfate was used as a roasting agent while 0.36 M sulfuric acid was used as a leaching agent. Solid/liquid ratio (1:5, 1:10, 1:15 and 1:20 (g/mL)) and leaching time (30, 60, 90 and 120 minutes) were used as variables in this study. The roasting process was done at 700 °С for 40 minutes while the leaching process was done at 70 °С and 350 rpm. The ratio of additive and mica schist was 1.5:1 (g/g). XRD, ICP-OES, and SEM were used to observe the formed compounds, chemical composition and morphology of the materials. HighScore Plus (HSP) was used to interpret the content of each compound in mica schist, roasted mica schist, and residue. ICP analysis confirmed that the mica schist contains 45.28 ppm of lithium. It is supported by XRD that lithium exists in mica schist as lepidolite (KLi2AlSi4O10(F,OH)2). Sulfate roasting did not affect the type of lepidolite but the lepidolite reactivity against the chemical agent. SEM analysis shows that the roasting process reduced the average particle size from 32.17 to 27.16 µm. ICP analysis of roasted mica schist shows that lithium concentration was reduced from 45.28 to 1.27 ppm. The optimum result from this study was 97.66 % extraction of lithium while solid/liquid ratio was 1:5 (g/ml) and leaching time was 30 minutes. HSP shows that lepidolite contents in initial mica schist, roasted mica schist and residue were 60.6; 24.3 and 18.7 %, respectively. Lithium concentration in the residue according to ICP analysis is 1.06 ppm.
- 18 June 2021
- Published by Private Company Technology Center in Eastern-European Journal of Enterprise Technologies
- Vol. 3 (6 (111)) , 80-88
Open AccessThe use of mica schist from Indonesia as raw material for lithium extraction process using sulfate roasting and acid leaching
Lithium minerals become a sub-economic raw material for lithium production to fulfill the lithium demand. This study is about lithium extraction from mica schist using the roasting and leaching processes. The mica schist located in Kebumen, Indonesia was used to study the phenomena during the lithium extraction process. Sodium sulfate was used as a roasting agent while 0.36 M sulfuric acid was used as a leaching agent. Solid/liquid ratio (1:5, 1:10, 1:15 and 1:20 (g/mL)) and leaching time (30, 60, 90 and 120 minutes) were used as variables in this study. The roasting process was done at 700 °С for 40 minutes while the leaching process was done at 70 °С and 350 rpm. The ratio of additive and mica schist was 1.5:1 (g/g). XRD, ICP-OES, and SEM were used to observe the formed compounds, chemical composition and morphology of the materials. HighScore Plus (HSP) was used to interpret the content of each compound in mica schist, roasted mica schist, and residue. ICP analysis confirmed that the mica schist contains 45.28 ppm of lithium. It is supported by XRD that lithium exists in mica schist as lepidolite (KLi2AlSi4O10(F,OH)2). Sulfate roasting did not affect the type of lepidolite but the lepidolite reactivity against the chemical agent. SEM analysis shows that the roasting process reduced the average particle size from 32.17 to 27.16 µm. ICP analysis of roasted mica schist shows that lithium concentration was reduced from 45.28 to 1.27 ppm. The optimum result from this study was 97.66 % extraction of lithium while solid/liquid ratio was 1:5 (g/ml) and leaching time was 30 minutes. HSP shows that lepidolite contents in initial mica schist, roasted mica schist and residue were 60.6; 24.3 and 18.7 %, respectively. Lithium concentration in the residue according to ICP analysis is 1.06 ppm.
- Open Access
- 1 July 2020
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 1569 (4)
Precipitation Rate Investigation on Precipitated Magnesium Carbonate by Ultrasonic of Magnesium Bicarbonate
Indonesia has a lot of dolomite reserves. Magnesium carbonate can be synthesized from dolomite. One of the main steps that requires a lot of energy are magnesium bicarbonate thermal decomposition. Magnesium bicarbonate solution are heated to make magnesium carbonate as precipitate. One of the ways to improve this process are by using ultrasonic waves as energy carrier. The purpose of this study is to find the effect of ultrasonic waves heating (sonochemistry) to thermal decomposition of magnesium bicarbonate. In this work, the author conducted ultrasonic heating with the amplitude of the waves varied around 20 µm and 30 µm for 35 minutes. Conventional heating using heat plate was also conducted and compared with ultrasonic heating. Higher decomposition ratio was reached on samples heated using ultrasonic waves with the value of 85.70% compared to conventional heating with decomposition ratio of only 50.08%. Amplitude effect on decomposition ratio were also observed. Higher amplitude made decomposition rate faster.
- 1 July 2020
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 1569 (4)
Open AccessPrecipitation Rate Investigation on Precipitated Magnesium Carbonate by Ultrasonic of Magnesium Bicarbonate
Indonesia has a lot of dolomite reserves. Magnesium carbonate can be synthesized from dolomite. One of the main steps that requires a lot of energy are magnesium bicarbonate thermal decomposition. Magnesium bicarbonate solution are heated to make magnesium carbonate as precipitate. One of the ways to improve this process are by using ultrasonic waves as energy carrier. The purpose of this study is to find the effect of ultrasonic waves heating (sonochemistry) to thermal decomposition of magnesium bicarbonate. In this work, the author conducted ultrasonic heating with the amplitude of the waves varied around 20 µm and 30 µm for 35 minutes. Conventional heating using heat plate was also conducted and compared with ultrasonic heating. Higher decomposition ratio was reached on samples heated using ultrasonic waves with the value of 85.70% compared to conventional heating with decomposition ratio of only 50.08%. Amplitude effect on decomposition ratio were also observed. Higher amplitude made decomposition rate faster.
- Open Access
- 1 June 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 858 (1)
The Degree of Lithium (Li) Stability Compared To Calcium (Ca) and Magnesium (Mg) From Low Lithium Grade Brine Water with Addition of Limestone and Oxalic Acid
The purpose of this study was to investigate whether lithium was precipitated along with the removal of Ca and Mg elements from brine water using limestone and oxalic acid. The first stage was Mg removal by adding CaO at room temperature for 3 hours. The second stage was the Ca removal by adding oxalic acid at a ratio of 2; 3; 4; 5; 10; 15; 20; 30; and 40 ml / 100 ml brine water and pH : 0, 1, and 4 at room temperature for 3 hours. The results showed the most optimal addition of CaO was 20 gr/1 l of brine water with the Mg element can be removed above 99 %, while Li was only reduced by about 1 ppm, and the Ca content only increased by around 28 ppm. The use of oxalic acid will also reduce the amount of lithium besides the Ca removal in the form a precipitate of calcium oxalate. The use of oxalic acid at pH 0 and 4 would reduce the Li content more than at pH 1. At the use of oxalic acid up to 40 ml at pH 1, brine water still contained about 78% Li element.
- 1 June 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 858 (1)
Open AccessThe Degree of Lithium (Li) Stability Compared To Calcium (Ca) and Magnesium (Mg) From Low Lithium Grade Brine Water with Addition of Limestone and Oxalic Acid
The purpose of this study was to investigate whether lithium was precipitated along with the removal of Ca and Mg elements from brine water using limestone and oxalic acid. The first stage was Mg removal by adding CaO at room temperature for 3 hours. The second stage was the Ca removal by adding oxalic acid at a ratio of 2; 3; 4; 5; 10; 15; 20; 30; and 40 ml / 100 ml brine water and pH : 0, 1, and 4 at room temperature for 3 hours. The results showed the most optimal addition of CaO was 20 gr/1 l of brine water with the Mg element can be removed above 99 %, while Li was only reduced by about 1 ppm, and the Ca content only increased by around 28 ppm. The use of oxalic acid will also reduce the amount of lithium besides the Ca removal in the form a precipitate of calcium oxalate. The use of oxalic acid at pH 0 and 4 would reduce the Li content more than at pH 1. At the use of oxalic acid up to 40 ml at pH 1, brine water still contained about 78% Li element.
- Open Access
- 1 June 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 858 (1)
Time and Amplitude Effect on Nano Magnesium Oxide Synthesis from Bittern using Sonochemical Process
Magnesium in nature can be found in the form of minerals and seawater. Bittern is a sea-salt industry by-product that contains magnesium and potassium salts. Usually, bittern is discharged back to the sea, even though bittern can be further processed to obtain magnesium contained in it. Magnesium oxide (MgO) nanoparticles can be used in a variety of applications because of their good surface recreation properties. In this study, precipitation of Mg2 + ions from bitterns was carried out using sodium hydroxide to produce magnesium hydroxide. Then, it was calcined and went through sonochemical process to produce nano magnesium oxide. Sonication time and amplitude were used as variables. Sample with sonication time of 16 minutes and amplitude of 30% has the smallest particles with an average diameter of 195.7 nanometers.
- 1 June 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 858 (1)
Open AccessTime and Amplitude Effect on Nano Magnesium Oxide Synthesis from Bittern using Sonochemical Process
Magnesium in nature can be found in the form of minerals and seawater. Bittern is a sea-salt industry by-product that contains magnesium and potassium salts. Usually, bittern is discharged back to the sea, even though bittern can be further processed to obtain magnesium contained in it. Magnesium oxide (MgO) nanoparticles can be used in a variety of applications because of their good surface recreation properties. In this study, precipitation of Mg2 + ions from bitterns was carried out using sodium hydroxide to produce magnesium hydroxide. Then, it was calcined and went through sonochemical process to produce nano magnesium oxide. Sonication time and amplitude were used as variables. Sample with sonication time of 16 minutes and amplitude of 30% has the smallest particles with an average diameter of 195.7 nanometers.