Galih Senopati
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Galih Senopati has a total of 69 co-authors. Here are the top co-authors by number of shared publications:
- Cahya Sutowo
Research Center for Metallurgy, National Research and Innovation Agency (BRIN), Kawasan Sains dan Teknologi B J Habibie, Tangerang Selatan, Banten 15314, Indonesia
5 shared publications Cahya Sutowo
Research Center for Metallurgy, National Research and Innovation Agency, Puspiptek, South Tangerang, Indonesia
4 shared publications- Albertus Deny Setyawan
Research Center for Metallurgy, National Research and Innovation Agency (BRIN), KST B.J. Habibie, Tangerang Selatan, Banten 15314, Indonesia
3 shared publications - Alfirano Alfirano
Department of Metallurgy Engineering, Sultan Ageng Tirtayasa University, Jl. Jenderal Sudirman Km. 3 Cilegon, Banten 42435, Indonesia
2 shared publications - Aprilia Erryani
Research Center for Metallurgy, National Research and Innovation Agency (BRIN), Kawasan Sains dan Teknologi B J Habibie, Tangerang Selatan, Banten 15314, Indonesia
2 shared publications Dhyah Annur
Research Center for Metallurgy, National Research and Innovation Agency, Puspiptek, South Tangerang, Indonesia
2 shared publications
Latest Publications
- 31 July 2026
- Published by IOP Publishing in Physica Scripta
- Vol. 101 (31) , 315901
Effect of annealing temperature on the microstructure and thermoelectric properties of TiNiSn 0.9 Al 0.1 half-Heusler alloys
The growing demand for efficient energy-conversion technologies has intensified research into thermoelectric materials capable of harvesting waste heat. This study investigates the effect of annealing temperature on the microstructure and thermoelectric performance of aluminum-doped TiNiSn half-Heusler alloys. TiNiSn 0.9 Al 0.1 samples were synthesized via vacuum arc remelting and annealed at 700 °C, 800 °C, and 900 °C for 168 h. Structural analysis reveals improved phase homogeneity and grain growth with increasing annealing temperature, with near single-phase formation at 800 °C. Transport measurements indicate n-type conduction for all samples, with semiconducting behavior observed at higher annealing temperatures. The sample annealed at 700 °C exhibits the highest Seebeck coefficient and the highest power factor among all investigated samples. Consequently, the highest thermoelectric performance is achieved at 700 °C, with a ZT value of ∼0.27 at 650 K. The present work provides an effective annealing strategy for enhancing the thermoelectric performance of TiNiSn-based materials for medium-temperature energy harvesting applications.
- 31 July 2026
- Published by IOP Publishing in Physica Scripta
- Vol. 101 (31) , 315901
Effect of annealing temperature on the microstructure and thermoelectric properties of TiNiSn 0.9 Al 0.1 half-Heusler alloys
The growing demand for efficient energy-conversion technologies has intensified research into thermoelectric materials capable of harvesting waste heat. This study investigates the effect of annealing temperature on the microstructure and thermoelectric performance of aluminum-doped TiNiSn half-Heusler alloys. TiNiSn 0.9 Al 0.1 samples were synthesized via vacuum arc remelting and annealed at 700 °C, 800 °C, and 900 °C for 168 h. Structural analysis reveals improved phase homogeneity and grain growth with increasing annealing temperature, with near single-phase formation at 800 °C. Transport measurements indicate n-type conduction for all samples, with semiconducting behavior observed at higher annealing temperatures. The sample annealed at 700 °C exhibits the highest Seebeck coefficient and the highest power factor among all investigated samples. Consequently, the highest thermoelectric performance is achieved at 700 °C, with a ZT value of ∼0.27 at 650 K. The present work provides an effective annealing strategy for enhancing the thermoelectric performance of TiNiSn-based materials for medium-temperature energy harvesting applications.
- 20 May 2026
- Published by Trans Tech Publications, Ltd. in Journal of Biomimetics, Biomaterials and Biomedical Engineering
- Vol. 72, 77-83
Optimization of Mechanical Properties and Corrosion Resistance of β-Ti-18Mo-7Cr Alloy through Heat Treatment for Orthopedic Implant Applications
β Ti-18Mo-xCr alloy has been widely used as an orthopedic implant material because this alloy has the advantage of high strength a lower modulus of elasticity than commercial alloys Ti-6Al-4V, good corrosion resistance. and formability. This research aims to find alloys with high corrosion resistance and low modulus of elasticity and identify the presence of phase β after heat treatment. Ti-18Mo-7Cr is obtained from the melting process using an arc melting furnace followed by heat treatment (solution and aging treatment). To determine the modulus of elasticity using a sonelastic tool and hardness test using Microhardness Vickers. The EIS method was used to determine the corrosion resistance using a 0.9% NaCl solution as a simulated body fluid. The modulus of elasticity owned by the solution treatment alloy tends to be lower than that of the aging alloy. The lowest elastic modulus value and the highest hardness value are found in the Ti-18Mo-7Cr ST850 alloy, which is 91 GPa and 471.42 HV. For corrosion resistance, the aging treatment alloy shows a lower corrosion rate than the solution treatment alloy and is much lower than that of the Ti-6Al-4V alloy. On the other hand, the solution treatment can stabilize the β phase and reduce the corrosion rate due to heating below transus temperature, but aging with a longer holding time can also reduce corrosion resistance more than the corrosion resistance of the solution treatment. The alloy Ti-18Mo-7Cr AT500 has the lowest corrosion rate among the samples in this study, which is 0,0004225 mmpy.
- 20 May 2026
- Published by Trans Tech Publications, Ltd. in Journal of Biomimetics, Biomaterials and Biomedical Engineering
- Vol. 72, 77-83
Optimization of Mechanical Properties and Corrosion Resistance of β-Ti-18Mo-7Cr Alloy through Heat Treatment for Orthopedic Implant Applications
β Ti-18Mo-xCr alloy has been widely used as an orthopedic implant material because this alloy has the advantage of high strength a lower modulus of elasticity than commercial alloys Ti-6Al-4V, good corrosion resistance. and formability. This research aims to find alloys with high corrosion resistance and low modulus of elasticity and identify the presence of phase β after heat treatment. Ti-18Mo-7Cr is obtained from the melting process using an arc melting furnace followed by heat treatment (solution and aging treatment). To determine the modulus of elasticity using a sonelastic tool and hardness test using Microhardness Vickers. The EIS method was used to determine the corrosion resistance using a 0.9% NaCl solution as a simulated body fluid. The modulus of elasticity owned by the solution treatment alloy tends to be lower than that of the aging alloy. The lowest elastic modulus value and the highest hardness value are found in the Ti-18Mo-7Cr ST850 alloy, which is 91 GPa and 471.42 HV. For corrosion resistance, the aging treatment alloy shows a lower corrosion rate than the solution treatment alloy and is much lower than that of the Ti-6Al-4V alloy. On the other hand, the solution treatment can stabilize the β phase and reduce the corrosion rate due to heating below transus temperature, but aging with a longer holding time can also reduce corrosion resistance more than the corrosion resistance of the solution treatment. The alloy Ti-18Mo-7Cr AT500 has the lowest corrosion rate among the samples in this study, which is 0,0004225 mmpy.
- 27 August 2025
- Published by IOP Publishing in Physica Scripta
- Vol. 100 (9)
Enhanced multi-environment corrosion resistance of HVOF-sprayed hydroxyapatite coatings on Ti-6Al-6Mo alloy for dental implants
Titanium dental implants require exceptional corrosion resistance in aggressive oral environments, where fluoride and antibiotics compromise long-term integrity. This study investigates a vanadium-free Ti-6Al-6Mo alloy coated with hydroxyapatite (HA) using high-velocity oxygen fuel (HVOF) spraying. Surface characterization using scanning electron microscopy and X-ray diffractometry confirmed a dense and adherent HA layer (Ca/P = 1.79) with favorable crystallinity. Electrochemical performance was evaluated in three different environments, namely artificial saliva (AS), AS with gentamicin (2 g/L), and AS with NaF (225 ppm F⁻) at 37 °C using potentiodynamic polarization and electrochemical impedance spectroscopy (EIS). The HA-coated Ti-6Al-6Mo samples show a lower contact angle than the base Ti-6Al-6Mo, which indicates the hydrophilic properties in AS, AS+gentamicin, and AS+NaF solutions. The HA-coated specimens exhibit significant enhanced corrosion resistance compared to the uncoated alloy: the corrosion current density (icorr) decreased from 3.68 to 0.18 µA/cm², while polarization resistance (Rp) increased from 41.7 to 2660 kΩ in the AS+gentamicin solution. Corrosion rates dropped by 70% across all media, with the lowest rate of 0.003 mm/year and highest Rp of 2660 kΩ observed for the HA-coated alloy in gentamicin-containing AS solution, indicating a synergistic protection. The HVOF-sprayed HA coating in Ti-6Al-6Mo alloy markedly improves electrochemical stability in diverse oral environments, supporting its application for long-lasting dental implants.
- 27 August 2025
- Published by IOP Publishing in Physica Scripta
- Vol. 100 (9)
Enhanced multi-environment corrosion resistance of HVOF-sprayed hydroxyapatite coatings on Ti-6Al-6Mo alloy for dental implants
Titanium dental implants require exceptional corrosion resistance in aggressive oral environments, where fluoride and antibiotics compromise long-term integrity. This study investigates a vanadium-free Ti-6Al-6Mo alloy coated with hydroxyapatite (HA) using high-velocity oxygen fuel (HVOF) spraying. Surface characterization using scanning electron microscopy and X-ray diffractometry confirmed a dense and adherent HA layer (Ca/P = 1.79) with favorable crystallinity. Electrochemical performance was evaluated in three different environments, namely artificial saliva (AS), AS with gentamicin (2 g/L), and AS with NaF (225 ppm F⁻) at 37 °C using potentiodynamic polarization and electrochemical impedance spectroscopy (EIS). The HA-coated Ti-6Al-6Mo samples show a lower contact angle than the base Ti-6Al-6Mo, which indicates the hydrophilic properties in AS, AS+gentamicin, and AS+NaF solutions. The HA-coated specimens exhibit significant enhanced corrosion resistance compared to the uncoated alloy: the corrosion current density (icorr) decreased from 3.68 to 0.18 µA/cm², while polarization resistance (Rp) increased from 41.7 to 2660 kΩ in the AS+gentamicin solution. Corrosion rates dropped by 70% across all media, with the lowest rate of 0.003 mm/year and highest Rp of 2660 kΩ observed for the HA-coated alloy in gentamicin-containing AS solution, indicating a synergistic protection. The HVOF-sprayed HA coating in Ti-6Al-6Mo alloy markedly improves electrochemical stability in diverse oral environments, supporting its application for long-lasting dental implants.
- 24 February 2025
- Published by IOP Publishing in Physica Scripta
- Vol. 100 (3) , 035026
Microstructure, mechanical properties, and corrosion behavior of novel antibacterial Ti-25Nb-xCu for dental implant
The growing demand for innovative metallic biomaterials for replacing and repairing dental tissue has increased due to the increasing number of people in the aging population and the expectation for an improved quality of life. In this study, a series of novel Ti-25Nb-xCu (25 and x = 3, 6, and 9, are in wt%) alloys were fabricated by powder metallurgy processing in an argon atmosphere. The Nb content was fixed at 25 wt%, while the Cu content was varied. The sintering temperature was 1300 °C, and the holding time was 4 h. Physical characterization, microstructure, mechanical (hardness) properties, and corrosion behavior were observed. The microstructure of the Ti-25Nb-xCu alloys consists of α-Ti, β-Ti phases, and the precipitation of Ti2Cu. The lower content of Cu (Ti-25Nb-3Cu) would have a lamellar structure, while the higher content of Cu (Ti-25Nb-6Cu and Ti-25Nb-9Cu) would have a more equiaxed structure. The increasing percentage of Cu would increase the mechanical properties. As for the corrosion behavior, adding Cu did not significantly affect the corrosion resistance, but Ti-25Nb-6Cu was shown to have the highest corrosion resistance. Furthermore, Ti-25Nb-6Cu exhibited higher antibacterial performance. Therefore, Ti-25Nb-6Cu was shown to be a promising material for dental implants.
- 24 February 2025
- Published by IOP Publishing in Physica Scripta
- Vol. 100 (3) , 035026
Microstructure, mechanical properties, and corrosion behavior of novel antibacterial Ti-25Nb-xCu for dental implant
The growing demand for innovative metallic biomaterials for replacing and repairing dental tissue has increased due to the increasing number of people in the aging population and the expectation for an improved quality of life. In this study, a series of novel Ti-25Nb-xCu (25 and x = 3, 6, and 9, are in wt%) alloys were fabricated by powder metallurgy processing in an argon atmosphere. The Nb content was fixed at 25 wt%, while the Cu content was varied. The sintering temperature was 1300 °C, and the holding time was 4 h. Physical characterization, microstructure, mechanical (hardness) properties, and corrosion behavior were observed. The microstructure of the Ti-25Nb-xCu alloys consists of α-Ti, β-Ti phases, and the precipitation of Ti2Cu. The lower content of Cu (Ti-25Nb-3Cu) would have a lamellar structure, while the higher content of Cu (Ti-25Nb-6Cu and Ti-25Nb-9Cu) would have a more equiaxed structure. The increasing percentage of Cu would increase the mechanical properties. As for the corrosion behavior, adding Cu did not significantly affect the corrosion resistance, but Ti-25Nb-6Cu was shown to have the highest corrosion resistance. Furthermore, Ti-25Nb-6Cu exhibited higher antibacterial performance. Therefore, Ti-25Nb-6Cu was shown to be a promising material for dental implants.
- 30 September 2024
- Published by IOP Publishing in Physica Scripta
- Vol. 99 (10) , 1059e7
Optimizing biomimetic hydroxyapatite coating on Ti-6Al-6Mo alloy: influence of immersion time
This study investigates the formation and characteristics of hydroxyapatite (HAp) coating on Ti-6Al-6Mo alloy through immersion in a supersaturated calcification solution (SCS) for 3, 7, and 14 days. X-ray diffraction (XRD) and secondary electron microscopy (SEM) with electron dispersive spectroscopy (EDS) were used to identify the phases and characterize the morphology and composition of the HAp layer. Atomic force microscopy (AFM) and contact angle tests were used to evaluate the surface properties, while potentiodynamic corrosion testing in Hanks’ solution was used to assess corrosion behavior. It is confirmed that the sample immersed for 14 days formed an HAp layer on the Ti-6Al-6Mo substrate with a Ca/P ratio of 2.5, approaching the ideal value of 1.67. This HAp film exhibits a smooth and homogeneous crystal structure, with a surface roughness of 31.47 nm and an appreciable corrosion rate of 0.0005 mm y−1. This study signifies the impact of immersion time on the microstructural properties and biocompatibility of biomimetic HAp coatings applied to Ti-6Al-6Mo alloy, contributing to the progress of HAp coatings in biomedical engineering.
- 30 September 2024
- Published by IOP Publishing in Physica Scripta
- Vol. 99 (10) , 1059e7
Optimizing biomimetic hydroxyapatite coating on Ti-6Al-6Mo alloy: influence of immersion time
This study investigates the formation and characteristics of hydroxyapatite (HAp) coating on Ti-6Al-6Mo alloy through immersion in a supersaturated calcification solution (SCS) for 3, 7, and 14 days. X-ray diffraction (XRD) and secondary electron microscopy (SEM) with electron dispersive spectroscopy (EDS) were used to identify the phases and characterize the morphology and composition of the HAp layer. Atomic force microscopy (AFM) and contact angle tests were used to evaluate the surface properties, while potentiodynamic corrosion testing in Hanks’ solution was used to assess corrosion behavior. It is confirmed that the sample immersed for 14 days formed an HAp layer on the Ti-6Al-6Mo substrate with a Ca/P ratio of 2.5, approaching the ideal value of 1.67. This HAp film exhibits a smooth and homogeneous crystal structure, with a surface roughness of 31.47 nm and an appreciable corrosion rate of 0.0005 mm y−1. This study signifies the impact of immersion time on the microstructural properties and biocompatibility of biomimetic HAp coatings applied to Ti-6Al-6Mo alloy, contributing to the progress of HAp coatings in biomedical engineering.
- 1 January 2024
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 3003 (1)
The influence of iron addition on microstructure and mechanical behavior Ti-6Mo-4Cr alloy
The effect of iron addition on microstructure and mechanical properties of Ti-6Mo-4Cr system were investigated in this work. The alloy was produced by a vacuum
- 1 January 2024
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 3003 (1)
The influence of iron addition on microstructure and mechanical behavior Ti-6Mo-4Cr alloy
The effect of iron addition on microstructure and mechanical properties of Ti-6Mo-4Cr system were investigated in this work. The alloy was produced by a vacuum
- Top Cited PapersOpen Access
Recent Development of Low-Cost β-Ti Alloys for Biomedical Applications: A Review
The necessity for biomedical components is increasing every year. However, Ti6Al4V, the most widely utilized titanium alloy for biomedical implants are very costly owing to the high price of V alloying element. Furthermore, both alloying elements Al and V, have adverse effects in human body which is not desirable. This review paper highlights significant findings on alloy design using low-cost alloying elements, their processing routes, and their relationship to microstructural, mechanical, and biological properties. Mo, Fe, Mn, Zr, and Cu were identified as low-cost alloying elements and fabrication of titanium alloys with these elements are usually carried out using arc melting, investment casting, powder metallurgy, additive manufacturing, diffusion couple, and thermomechanical processing. Several processing routes can be chosen to obtain optimum properties such as β-phase titanium alloy structure, low elastic modulus, and high strength. Alloy design, post-heat treatment process, and fatigue test for newly developed alloys are research that can be carried out in the future for the development of new titanium materials that are safe for human use and at a more affordable price.
Top Cited PapersOpen AccessRecent Development of Low-Cost β-Ti Alloys for Biomedical Applications: A Review
The necessity for biomedical components is increasing every year. However, Ti6Al4V, the most widely utilized titanium alloy for biomedical implants are very costly owing to the high price of V alloying element. Furthermore, both alloying elements Al and V, have adverse effects in human body which is not desirable. This review paper highlights significant findings on alloy design using low-cost alloying elements, their processing routes, and their relationship to microstructural, mechanical, and biological properties. Mo, Fe, Mn, Zr, and Cu were identified as low-cost alloying elements and fabrication of titanium alloys with these elements are usually carried out using arc melting, investment casting, powder metallurgy, additive manufacturing, diffusion couple, and thermomechanical processing. Several processing routes can be chosen to obtain optimum properties such as β-phase titanium alloy structure, low elastic modulus, and high strength. Alloy design, post-heat treatment process, and fatigue test for newly developed alloys are research that can be carried out in the future for the development of new titanium materials that are safe for human use and at a more affordable price.
- Open Access
- 1 January 2023
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 2630 (1)
Effect of hot rolling on structure and hardness of α/β Ti-6Al-6Nb alloy for orthopedic application
Ti-6Al-4V is the most common titanium alloy for implant application. However, Ti-6Al-4V has disadvantages that this alloy’s vanadium element. Vanadium is a toxic element and may cause potentially serious health problems. In this study, Vanadium was substituted with Niobium to obtain an alpha/beta titanium alloy which is safe for use in the human body as an orthopedic material. The Hot Rolling process carried out Ti-6Al-6Nb to improve its mechanical properties. Hot rolling is carried out at 900, 1000, and 1100 °C temperatures. Microstructural observations with optical microscopy (OM), scanning electron microscope (SEM), and hard tests were carried out to observe changes in microstructure and hardness after melting, homogenization, and hot rolling processes. The study revealed that hot rolling at 1000 °C has the lowest hardness, and rolling at 900 °C has the highest hardness value. The finer grain size most influenced to the increasing hardness value of hot rolled Ti-6Al-6Nb.
- 1 January 2023
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 2630 (1)
Open AccessEffect of hot rolling on structure and hardness of α/β Ti-6Al-6Nb alloy for orthopedic application
Ti-6Al-4V is the most common titanium alloy for implant application. However, Ti-6Al-4V has disadvantages that this alloy’s vanadium element. Vanadium is a toxic element and may cause potentially serious health problems. In this study, Vanadium was substituted with Niobium to obtain an alpha/beta titanium alloy which is safe for use in the human body as an orthopedic material. The Hot Rolling process carried out Ti-6Al-6Nb to improve its mechanical properties. Hot rolling is carried out at 900, 1000, and 1100 °C temperatures. Microstructural observations with optical microscopy (OM), scanning electron microscope (SEM), and hard tests were carried out to observe changes in microstructure and hardness after melting, homogenization, and hot rolling processes. The study revealed that hot rolling at 1000 °C has the lowest hardness, and rolling at 900 °C has the highest hardness value. The finer grain size most influenced to the increasing hardness value of hot rolled Ti-6Al-6Nb.