Latest Publications

  • THE EFFECT OF THE COMPOSITION OF DESULFURIZATION SLAG FROM CAST IRON ON ADHESION TO REFRACTORY MATERIALS

    by Yevgen Siharov, Denis Eskov, Hennadii Kriachko, Mykola Rudenko, Igor Matina

    The influence of changes in the chemical composition of slag formed during cast iron desulfurization by blowing a mixture of lime and magnesium on the adhesion conditions to the refractories of the cast iron ladle was investigated. A statistically adequate linear regression model of refractory wetting by CaO-SiO2-MgO-Al2O3 slag was constructed. It was shown that the wetting of Al2O3- and SiC-based refractories by slag has a significantly nonlinear nature and is accompanied by a complex of interphase reactions. According to the results of the analysis of isolines in the MgO–Al2O3 plane at a fixed CaO content in the slag, an increase in the content of MgO is accompanied by a decrease in the contact angle, while an increase in (Al2O3) content is accompanied by an increase in the contact angle and a deterioration in the wetting of the refractory surface by slag, which is due to the high thermodynamic stability of alumina and the effect on the reactivity of slag to Al2O3-SiC refractories. A thermodynamic interpretation of the stability of ladle slag oxides and possible reactions in the temperature range of cast iron treatment is presented. Calculations were performed to optimize the composition of ladle slag for cast iron desulfurization in order to reduce the intensity of corrosion on the working layer of refractories in the cast iron ladle. The rational composition of slag for the conditions of the UDC of Kamet-Stal PJSC was determined: 42—46 % (CaO), 5—8 % (MgO), 6—9 % (Al2O3). The use of a three-layer lining for 230-ton iron-pouring ladles at Kamet-Steel PJSC is proposed: a working layer (8—20 mm thick) made of refractories containing 78—80 % MgO, 10—12 % Al2O3 and 5—7 % MgAl2O4; a middle layer (10—30 mm thick) of refractories containing 65 % Al2O3, 15—20 % SiC, 5—7 % C, and up to 3 % MgAl2O4; an inner layer of refractories containing 70 % Al2O3 and 8—10 % SiC.

  • Open Access

    АНАЛІЗ ПРИЧИН ТА НАСЛІДКІВ РЕЗОНАНСНИХ АВАРІЙ ДОМЕННИХ ПЕЧЕЙ

    by G. Kryachko, Є. Сігарьов, А. Похвалітий, М. Руденко, Д. Єськов, Ye. Sigarev, A. Pokhvalityi, D. Yeskov

    Вступ. Доменна піч, разом з повітронагрівальною і газоочисною технікою, залишається однією з найнебезпечних металургійних систем. Особливої уваги потребують аварії з катастрофічними наслідками якдля обладнання, так і для техперсоналу. Вони не мають терміну давності й повинні ретельно вивчатисязадля усунення причин їх виникнення та безпечного функціонування.Проблематика. Недостатнє, а іноді й протирічне, висвітлення у технічній літературі інформації про особливо важкі аварії, зокрема вибухи печей, є перепоною для подальшого удосконалення та розробки безпечної технології ведення доменного процесу, тому пошук засобів запобігання та уникнення аварійних ситуацій є актуальним.Мета. Встановити дійсний механізм вибухового руйнування доменної печі №7 Дніпровського металургійного комбінату (ДМК) 07.09.1993 р. з розглядом факторів об’єктивного та суб’єктивного впливів.Матеріали й методи. Для аналізу використано архівні матеріали візуалізації параметрів роботи печі напаперових носіях, фотодокументи, акти й висновки експертних комісій, а також публікації з досліджуваного питання.Результати. Відтворено механізм вибухового руйнування ДП №7 ДМК (Україна). Систематизовано фактори, що спричинили аварійну ситуацію. Виконано порівняння причин і наслідків аварій на досліджуванійпечі і ДП №5 заводу в Port Talbot (Великобританія), що мали однаковий механізм катастрофічного руйнування агрегатів через неконтрольоване потрапляння критичної маси води в робочий простір печі.Висновки. Встановлено, що на ДП №7 ДМК значний масштаб руйнувань з численними людськими жертвами був обумовлений не одним, як вважалося раніше, а двома вибухами різної потужності. Показано динаміку зміни газодуттьового режиму задувального періоду, що призвело при відсутності сходу шихти на колошнику до вибухової аварії. Охарактеризовано важливість дотримання рекомендацій для недопущенняпарових вибухів у доменних печах. Результати дослідження є важливим доповненням до створення нормативних документів для забезпечення безаварійної експлуатації доменних печей.

  • Impact of capillary moisture uptake on the formation of iron ore sinter mix granules

    by R. M. Rudenko, Ye. M. Sigarev, M. R. Rudenko, M. A. Kashcheev

    The research focuses on determining main factors that affect quality granulation of iron ore sinter mix. Granulation is a crucial stage in sintering technology, since strength, size distribution, and gas permeability of granules directly influence bed resistance, flame front stability, and overall productivity the sintering machine. Based on both experimental studies and theoretical analysis, role of moisture content, drum operating parameters, and pore structure characteristics has been clarified. It has been demonstrated that preliminary granulation of fine fractions (dust, sludges, lime, and other secondary raw materials) significantly improves the uniformity granule structure. Capillary absorption tests showed that concentrates, ores, and waste products differ considerably in water uptake, which is mainly due to variations in pore radius. According to the Washburn equation, smaller pores limit penetration depth and reduce moisture distribution, whereas larger pores accelerate water movement and ensure better wetting of the charge. Calculated data indicate that at pore sizes of 5 μm the penetration depth does not exceed 2 mm within 10 s, while at 20 – 40 μm moisture spreads several millimeters during the same period. These results confirm the necessity of pre-granulating fine wastes with poor wettability in order to stabilize the structure of the sinter mix. Optimization of granulation parameters has been carried out. The most favorable regime corresponds to a moisture content of 7.5 – 9.0%, drum speed of 12 – 14 rpm, and fill degree of 22 – 26 %. Under these conditions, strong and uniform granules with a dominant fraction of 3 – 6 mm are formed. The fraction below 1 mm decreases from more than 40% to approximately 24%, which considerably lowers dust generation during sintering. The obtained results also prove that the use of preliminary granulation makes it possible to introduce up to 25 – 30% of secondary materials without deterioration of granule stability. At the same time, dust emissions are reduced by 5 – 10% and the environmental performance of sintering is improved. The novelty of this work consists in establishing the relationship between moisture absorption mechanisms and the stability of granules, and in proving the possibility of increasing the share of secondary raw materials in the charge while simultaneously reducing the ecological footprint of agglomeration.

  • Open Access

    Technology for Purification of Sulphur-Containing Flue Gases with Obtaining Commodity Products

    by M.A. Kashcheev, S.V. Manzenko, Ukraine) Vav Design Bureau Llc (Kamianske, Ye.M. Siharov, M.R. Rudenko, V.A. Kvashyn, R.M. Rudenko, Є.м. Сігарьов

    Agglomerate is one of the main types of raw material for blast furnace production. During the processes of agglomeration, cooling, and processing of agglomerate, a significant amount of harmful technological emissions is generated, including dust, carbon oxides, sulfur oxides, nitrogen oxides, and others. The agglomeration charge contains solid fuel such as coke fines and anthracite fines, as well as a significant amount of iron-containing waste, which is the primary source of sulfur in the metallurgical process. To address the issue of comprehensive flue gas treatment, a technology based on the use of a plasma-catalytic reactor (PCR) has been developed. The proposed solution optimizes the process of cleaning gaseous emissions, enhances economic efficiency, and reduces the environmental impact of the agglomeration process. Additionally, the technology opens up the possibility for further processing of iron-containing and sulfur-containing materials. The operating principle of the reactor is based on ozone generation in a corona discharge. Ozone ensures the complete oxidation of sulfur dioxide (SO2) into sulfur trioxide (SO3). The apparatus consists of a PCR unit, which generates the required amount of ozone by passing air through the corona discharge, and a power supply unit (transformer). The integration of the “MV-2JS” apparatus into traditional desulfurization technology allows for the complete elimination of the third stage of the process — the oxidation of calcium sulfite in special vessels. By installing the PCR directly before the reactor-adsorber in the flow path of the flue gases, instead of sulfur dioxide (SO2), sulfur trioxide (SO3) is obtained. This, in turn, allows the synthesis of high-quality commercial gypsum that does not contain harmful toxic impurities and does not require additional oxidation. Агломерат є одним із основних видів сировини для доменного виробництва. У процесі агломерації, охолодження та обробки агломерату утворюється значна кількість шкідливих технологічних викидів, зокрема пил, оксиди вуглецю, сірки, азоту та інші. До складу агломераційної шихти входить тверде паливо, таке як коксовий дріб’язок та антрацитовий штиб, а також значна кількість залізовмісних відходів, які є основним джерелом надходження сірки в метал на технологічному маршруті виплавки сталі. З метою вирішення проблеми комплексної обробки димових газів розроблено технологію, що базується на використанні плазмово-каталітичного реактора (ПКР). Запропоноване рішення дозволяє оптимізувати процес очищення газоподібних викидів, підвищити економічну ефективність та зменшити екологічне навантаження процесу агломерації. Крім того, технологія відкриває можливість додаткової переробки залізовмісних та сірковмісних матеріалів. Принцип дії реактора полягає у генерації озону в коронному розряді. Озон забезпечує повне доокислення діоксиду сірки (SO2) до триоксиду сірки (SO3). Апарат складається з блоку ПКР, що забезпечує утворення необхідної кількості озону шляхом пропускання повітря через коронний розряд, та блоку живлення (трансформатора). Інтеграція апарата типу «MV-2JS» у традиційну технологію десульфурації дозволяє повністю відмовитися від третьої стадії процесу — окислення сульфіту кальцію у спеціальних ємностях. Установлення ПКР безпосередньо перед реактором-адсорбером, на шляху потоку димових газів, забезпечує замість сірчистого ангідриду (SO2) отримання сірчаного ангідриду (SO3). Це, у свою чергу, дозволяє синтезувати товарний високоякісний гіпс, що не містить шкідливих токсичних домішок і не потребує додаткового доокислення.

  • STUDY OF THE EFFICIENCY OF USE OF CONVERTER SLAG IN THE AGGLOMERATION CHARGE

    by Roman Rudenko, Yevhen Sigarev, Mykola Rudenko, Mykhailo Kashcheev, Olena Chubina, Kateryna Bozhko, Є.м. Сігарьов, М.а. Кащеєв, О.а. Чубіна

    The article raises a question related to the need to increase the use of secondary raw materials — final converter slags as a substitute for part of the fluxes and iron-containing materials (iron ore and concentrates), which will contribute to reducing the ecological burden on the environment, the volume of their accumulation as part of man-made deposits and implementation of the concept of a closed-cycle economy within the framework of the decisions of the UN climate summit (2019) and the European Commission on ensuring carbon neutrality of Europe by 2050 (Green Deal or "green course") in the direction of reducing the use of fossil coal. For the raw material conditions of agglomerate production, a technology of agglomerate production is proposed, which includes the uniform laying of carbonate flux on the "bed" before loading the charge, while loading the charge onto the grate grates is carried out simultaneously with the formation of the "bed". The "bed" formed in this way is a layer of fluxes with a fractional composition of materials between 0.050 m and a value exceeding the cross section between the grates of the spical carts. The results of research on the use of converter slag as components of agglomeration charge are presented. There is a well-founded possibility of returning its main components СаО, FeO, Fe2O3, MgO, Al2O3, MnO in the cycle of metallurgical production. The peculiarities of the formation of interlayers of the sintering charge with different modulus of basicity due to the introduction of converter slag with the dimensions of the specified range into the charge without using an additional tract of preparation of the charge have been established; dependence of the specific consumption of solid fuel, the output of the reverse fraction of agglomerate and the productivity of the sintering machine on the fractional composition of the converter slag particles loaded on the sintering carts of the sintering machine according to the proposed technology with a rational vertical distribution of materials along the section of the charge. Transferring part of the CaO-containing materials to the lower part of the charge layer can ensure a more rational use of heat from the combustion of solid fuel in the upper part of the charge layer on the sintering cart of the sintering machine.

  • Open Access

    DETERMINATION OF FACTORS AFFECTING THE STABILITY OF WELDED TIPS OF OXYGEN LANCE

    by Yevhen Sigarev, Artem Pokhvalityi, Mykola Rudenko, Dmytro Kondrashenkov, Artur Krut, Є.м. Сігарьов, А.а. Похвалітий

    It has been established that the most likely cause of crack formation is differences in the chemical composition of the welding wire, the material of the Laval nozzle and the outer cage of the lance tip. For example, the difference in copper content is 6.79%. The microstructures of the weld, Laval nozzle metal, and outer lance tip rim were analyzed and compared along the cross section of the weld location. Microcracks located along the grain boundaries were detected, which is probably due to the appearance of weak compounds with low ductility and non-propagation at the grain boundaries. In the structure of welds, accumulations of oxygen inclusions along the boundaries of crystallites were found, which leads to copper embrittlement and can contribute to weld failure. Freezing a layer of converter slag with low thermal conductivity on the tip surface reduces the thermal conductivity of the formed slag metal layer and heat transfer to the cooling water. Even if there is a 1 mm layer of slag on the surface of the weld, thermal conductivity decreases by 79-95%, depending on the thickness of the slag and its properties, respectively. If there is a layer of slag on the surface of the weld, the heat transfer decreases by 51-56% (at 1 mm of slag) and by 72-88% at 20 mm, respectively.In order to prevent the formation of cracks between the Laval nozzle and the outer cage of thehandpiece, it is advisable to follow the following recommendations when performing welding operations. In the simplest case, the first welded layer should be performed using a non-consumable electrode (tungsten or graphite) in an argon or helium atmosphere, which will ensure the formation of a reliable, tight weld around the entire circumference of the nozzle. To reduce stresses in the weld, subsequent welded layers should be performed in alternating directions. A more effective option is the technology according to which, after the first weld is applied, the nozzle is connected to the tip from the inside with a partial (discrete) or continuous weld, which minimizes the likelihood of failures and can ensure the sealing of the tip when the initial cross-section of the Laval nozzles increases to the critical ignition diameter. The implementation of an internal weld will reduce mechanical loads on the external weld, especially when using metal hose expansion joints, and increase the strength of the welded joint as a whole.

  • Open Access

    COMPLEX TECHNOLOGY OF THE CLEANING OF AGGLOMERATION GASES FROM DUST AND HARMFUL GASES WITH OBTAINING A GOOD PRODUCT

    by Mikhail Kashcheev, Serhij Manzenko, Mykola Rudenko, Volodymyr Kvashin, Rodion Rudenko, М.а. Кащеєв

    The purpose of the work is to improve the design of the dust-catching device of the sintering machine, to increase the efficiency of catching charged dust particles in laminar layers near the precipitating elements, the configuration and location of the elements of the precipitating elements, to establish the dependence of the effective (calculated) drift speed of charged dispersed particles on the speed of the medium being cleaned, with classical the process of electrogas purification and the combined flow of gases in electrofilters. It was established that the combined movement of gases in a modular unit ensures the charging of the entire population of dust particles to the limit values ​​by organizing a highly turbulent flow and keeping dust particles in the zones with the greatest tension in the corona charge covers, as well as effective trapping of charged dust particles in laminar layers near the precipitating elements . Mathematical modeling of the deposition block was carried out in order to optimize the configuration. The main dependences of the number and mutual location of precipitating elements to ensure maximum dust deposition were established. Studies of gas medium velocity spectra in models of new electrostatic precipitators have been carried out. The optimal live cross-sections of the aerodynamic partitions are determined to ensure favorable conditions for charging suspended particles and uniform distribution of the cleaned flow through the catching holes. The MV-2 modular type electric gas purification device with a capacity of 30 thousand nm3/h has been developed, based on innovative developments in the field of KEIT (combined electro-ion gas purification technology) in the field of conversion and control of cascade energy and aerodynamics of turbulent and laminar flows during inertial deposition dispersed suspension of flue gases. An apparatus for cleaning gases from a sinter machine with a capacity of up to 400,000 nm3/h is proposed. with an efficiency of 99 %, for replacing existing equipment (multicyclones). "MV-2JS" electric device was developed. This is a plasma-catalytic reactor, which allows you to produce the necessary amount of ozone in a low-cost way to oxidize the harmful components (SO2, NOx, CO) of the outgoing gases. The use of this device allows, in addition to the cleaning of flue gases from harmful gas impurities, to obtain commercial products (fertilizers, gypsum, sulfuric acid, etc.) at the output and to completely get rid of solid and liquid waste during gas desulfurization.

  • Open Access

    REDUCTION OF IRON CONSUMPTION IN STEEL PRODUCTION IN CONVERTER SHOPS: MODERN APPROACHES AND SOLUTIONS

    by Olena Chubina, Artem Pokhvalityy, Mykola Rudenko, Volodymyr Kislyakov, Dmytro Kondrashenkov, О.а. Чубіна, А.а. Похвалітий, В.г. Кисляков

    The article examines modern approaches and technological solutions aimed at reducing the cost of iron in the production of steel in converter shops. One of the key issues in the metallurgical industry is the optimization of raw material costs while simultaneously improving the quality of final products. In the conditions of growing competition on the market and increasing the cost of raw materials, the issue of reducing iron consumption in the steel production process becomes especially important. The purpose of the study is to substantiate effective technological methods of reducing the cost of cast iron while maintaining high technical and operational characteristics of steel. The work considers several directions for achieving this goal, in particular: improvement of the quality of raw materials through preliminary processing of scrap metal, modernization of converter equipment, optimization of oxygen purging modes, use of technologies of secondary processing of scrap metal, as well as the use of various technological additives and slag-forming materials. Special attention is paid to the possibilities of reducing energy consumption and increasing production efficiency through the use of scrap metal heating technologies.During the study, examples of the introduction of modern technologies at leading metallurgical enterprises, such as ArcelorMittal, ThyssenKrupp, Voestalpine and others, were considered. These technologies help to reduce the costs of raw materials and energy resources, which has a positive effect on the environmental indicators of production and the overall sustainability of metallurgical enterprises. An analysis of the use of carbon-containing materials, both in lump and powder forms, was also carried out to reduce the consumption of cast iron and increase the proportion of metal scrap in the metal charge. The question of the influence of such additives on the chemical composition of steel is considered. It was determined that the use of carbon-containing materials allows to significantly reduce the consumption of cast iron, however, it is necessary to take into account the influence of such factors as the composition of raw materials, the temperature in the converter and the parameters of adding carbon-containing materials during oxygen purging.The given results can be useful for enterprises of the metallurgical industry seeking to increase the efficiency of their production processes. The study demonstrates that the introduction of new technologies and approaches can provide a significant reduction in pig iron costs, increase the quality of steel and reduce the negative impact on the environment. The described methods have the potential for wide use in metallurgy, which will increase the competitiveness of Ukrainian enterprises on the international market.

  • Open Access

    НОВІ ТЕХНІЧНІ РІШЕННЯ З ПІДВИЩЕННЯ ПЛОЩІ АКТИВНОГО ПЕРЕТИНУ КОЛОСНИКОВИХ ГРАТ АГЛОМЕРАЦІЙНОЇ МАШИНИ

    by Є Сігарьов, Р Руденко, К Чубін, М Кащеєв, М Руденко, О Чубіна

    Вступ. Одним із визначальних елементів конструкції агломераційних машин є рухома конвеєрна стрічка, що складається зі спікальних візків, з комплектом колосників, на які безперервно завантажується шихта для виробництва агломерату.Проблематика. Наявність залишків сирої шихти та частинок агломерату у просторі між колосниками і елементами спікального візку призводить до збільшення маси конвеєрної стрічки, негативних змін у тепловому навантаженні корпусів візку та підвищення температури металоконструкцій й перевитрат енергії на процес. Мета. Дослідження особливостей використання колосникових ґрат агломераційної машини зі збільшеною площею активного перетину й зниженим за рахунок удосконалення конструкції колосників газодинамічним опором.Матеріали та методи. Особливості змін газодинамічного опору колосникових ґрат, виготовлених з використанням удосконалених колосників, теплового навантаження на спікальний візок та умов очищення колосникового поля відзалишків сирої шихти і частинок агломерату встановлювали шляхом дослідно-промислових випробувань на агломашинах типу АКМ-75 й моделюванням з використанням SOLIDWORKS.Результати. Встановлено, що колосники зі змінним перетином і кутом контактних граней зівів замка до підколосникової балки більше 90 забезпечують зменшення теплового навантаження на спікальний візок за рахунок мінімізації площі їх контакту з балкою. За результатами математичного моделювання встановлено характер впливу активного перетину на обсяг газів, що просмоктуються. Через збільшення вільного доступу газових потоків для охолодження колосників і підколосникових балок зростає ступень самоочищення їхніх контактних поверхонь.Висновки. Розробка дозволить збільшити площу активного перетину колосникових грат, забезпечить зменшення газодинамічного опору проходженню газових потоків і теплового навантаження системи, підвищення ефективності видалення залишків шихти із міжконтактного простору і виключення зі штатної схеми спікання агломерату механізм примусового струшування колосників. Introduction. One of the defi ning elements of the design of sintering machines is a moving conveyor belt consisting of sintering trucks, with a set of grates, on which the charge for the production of agglomerate is continuously loaded.Problem Statement. The presence of the remains of raw charge and agglomerate particles in the space between the grates and the elements of the sintering truck leads to an increase in the mass of the conveyor belt, negative changes in the thermal load of the truck bodies and an increase in the temperature of metal structures and excessive energy consumption for the process.Purpose. Studying the peculiarities of the use of fi re grates of the sintering machine with an increased active cross-sectional area and reduced gas dynamic resistance due to improving the grate design.Material and Methods. The features of changes in the gas-dynamic resistance of fi re grates made with the use of improved grates, the heat load on the sintering truck, and the conditions for cleaning the grate fi eld from the remains of the raw charge and agglomerate particles have been established by experimental and industrial tests on sintering machines of the AKM-75 type and by modeling with the use of SOLIDWORKS.Results. It has been established that the grates with a variable cross-section and the angle of the contact faces of the hinges of the lock to the under-rail beam, which exceeds 90 degrees, ensure a reduction in the heat load on the sintering truck due to the minimization of the area of their contact with the beam. According to the results of mathematical modeling, the nature of the infl uence of the active cross section on the volume of absorbed gases has been determined. As a result of the increase in the free access of gas fl ows for cooling the grates and under-grate beams, the degree of self-cleaning of their contact surfaces increases.Conclusions. The proposed design allows increasing the area of active cross-section of fi re grates, providing a reduction in the gas-dynamic resistance to the passage of gas fl ows and the thermal load of the system, raising the effi ciency of removing charge residues from the inter-contact space, and excluding the mechanism of forced grate...