SMSoumitra Maiti

Soumitra Maiti

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


Soumitra Maiti has a total of 5 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Heavy Metal Leachability Tendency of Ladle Furnace Steel Slags: Investigating Stable Slag Matrix for Construction Use

    by Jyoti Ahlawat, S. K. Singh, Soumitra Maiti

    The leachability potential of ladle furnace steel slag (LFSS) is critical for assessing environmental compatibility and sustainability in construction applications. This study systematically investigates the leaching behavior of different LFSS types, focusing on the mobilization of environmentally sensitive heavy metals. Three LFSS variants such as Al‐killed, Al‐Si‐killed, and Si‐killed, produced from different steelmaking routes were examined using standardized protocols: the Toxicity Characteristic Leaching Procedure (TCLP), the Single Batch Test (SBT), and the Long‐Term Leaching Test (LTLT). Experimental variables included leaching medium pH, slag particle size, liquid‐to‐solid (L/S) ratio, and duration. Results reveal variations in leachate composition, specifically in release of the heavy metals that is, Cr, As, Cd, Hg, Pb, Mn, Fe, Co, Ni, Zn, Cu, and Mo. Findings indicate that metal mobilization depends on both slag chemistry and leaching environment acidity, with enhanced leaching under acidic conditions. A comparative analysis shows that Al‐Si‐killed LFSS has the lowest leaching potential, indicating more stable immobilization and precipitation of heavy metals. In contrast, Al‐killed and Si‐killed LFSS show higher leaching, particularly increased manganese release under acidic and alkaline conditions. However, concentrations of other heavy metals remain negligible and within regulatory limits. Long‐term leaching assessments confirm the environmental safety of the tested LFSS variants. Al‐Si killed LFSS found to exhibit lowest or negligible leaching of toxic trace metals particularly in TCLP test. This behavior is attributed to the formation of stable alumino‐silicate network and surface passivation layer which binds the metallic species within the matrix and reduces the mobility. The results support the safe and sustainable use of LFSS in construction. Incorporating suitable binders further reduces leachability by encapsulation and masking effects, enhancing performance.

  • Solidification/stabilisation of Pb (II) and Cu (II) containing wastewater in cement matrix

    by Soumitra Maiti, Jaideep Malik, Basheshwer Prasad, Ashwani Kumar Minocha

    This study reported solidification/stabilization of lead and copper-laden fly ash (adsorbent) utilizing cement as binder for their ultimate disposal. The Pb (II) and Cu (II) loaded fly ash was successfully immobilized within the cement matrix without presence of any chemical agents. A retardation of 80-100 minutes in the setting time of cement paste was noticed on the addition of metal-laden fly ash attributed to the presence of metal ions. However, a gradual decrease in mechanical strength of the mortars was observed with higher amounts of Pb (II) and Cu (II)-loaded fly ash in the mix composition. This gradual decrease is ascribed to the breakdown of calcium silicate hydrate (CSH) gel network in the presence of metal crystallites, as confirmed by scanning electron microscopy (SEM) and energy-dispersive x-ray (EDX) analyses. TG-DTG studies also reveal a decrease in CSH (%) from 4.77% (for fly ash cement mortar) to 4.14% and 3.86% for Pb (II) and Cu (II)-loaded fly ash mortars, respectively. X-ray diffraction (XRD) analysis of metal-laden fly ash cement mortars substantiate the immobilization of Pb (II) and Cu (II) metal ions in the cement matrix as peaks for Ca[Pb(OH)3]2 and Ca[CuH2O5Si] are visible in their patterns, respectively. TCLP tests conducted on 56 day cured metal-laden fly ash mortars show leachate concentration not exceeding the discharge standards. Overall, these results indicate that this integrated adsorption- solidification/stabilization process is efficient for safe disposal and utilization of heavy metal-laden fly ash for building and construction related work as a secondary material. GRAPHICAL ABSTRACT