Mustafa Tekin
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Mustafa Tekin has a total of 16 co-authors. Here are the top co-authors by number of shared publications:
- Hasan Kotan
Bursa Technical University
6 shared publications - Gökhan Polat
İzmir Katip Çelebi University, Faculty of Engineering and Architecture, Department of Metallurgical and Materials Engineering
2 shared publications - Murat Baydoğan
Department of Metallurgical and Materials Engineering, Istanbul Technical University, Istanbul 34469, Türkiye
2 shared publications Aleyna Bayatlı
1 shared publication- Ali Rıza Baloğlu
Necmettin Erbakan Universitesi
1 shared publication - Erdem Balcı
Department of Metallurgical and Materials Engineering, Istanbul Technical University, Istanbul 34469, Türkiye
1 shared publication
Latest Publications
- Open Access
Microhardness and Abrasive Wear-Induced Material Loss in FDM-Printed PLA, PETG, ABS, ASA, and Fe-Filled PLA
This exploratory study comparatively evaluated the time-dependent abrasive wear-induced material loss, local microhardness, and worn-surface morphology of fused deposition modeling (FDM)-printed PLA, PETG, ABS, ASA, and PLA containing 1 wt.% Fe under controlled wet–abrasive grinding. Two physical cylindrical specimens from the same print build were tested concurrently in opposing holder positions against P180 SiC abrasive paper under continuous water lubrication for 60 min at a normal load of 5 N. After 60 min, cumulative mass losses were 11.1% for PLA, 13.0% for PETG, 22.6% for PLA–1 wt.% Fe, 39.3% for ABS, and 50.1% for ASA. Based on the two specimen-level means, Vickers microhardness (HV0.1) was highest for PLA–1 wt.% Fe (28.5), followed by PLA (22.4) and ABS (13.3), while ASA (11.9) and PETG (11.8) showed very similar values. Optical microscopy and selected SEM/EDS observations revealed material-dependent surface features and showed local Fe detectability in the analyzed regions of the filled PLA. The microhardness ranking did not follow the cumulative material-loss trend, most clearly for Fe-filled PLA and for PETG versus ASA. These results indicate that the local indentation-hardness ranking did not correspond directly to the cumulative mass-loss ranking of the investigated FDM-printed polymers under the selected conditions. For material selection in FDM components subjected to abrasive contact, these findings indicate that local microhardness should not be used alone as a proxy for condition-specific abrasive wear performance.
Open AccessMicrohardness and Abrasive Wear-Induced Material Loss in FDM-Printed PLA, PETG, ABS, ASA, and Fe-Filled PLA
This exploratory study comparatively evaluated the time-dependent abrasive wear-induced material loss, local microhardness, and worn-surface morphology of fused deposition modeling (FDM)-printed PLA, PETG, ABS, ASA, and PLA containing 1 wt.% Fe under controlled wet–abrasive grinding. Two physical cylindrical specimens from the same print build were tested concurrently in opposing holder positions against P180 SiC abrasive paper under continuous water lubrication for 60 min at a normal load of 5 N. After 60 min, cumulative mass losses were 11.1% for PLA, 13.0% for PETG, 22.6% for PLA–1 wt.% Fe, 39.3% for ABS, and 50.1% for ASA. Based on the two specimen-level means, Vickers microhardness (HV0.1) was highest for PLA–1 wt.% Fe (28.5), followed by PLA (22.4) and ABS (13.3), while ASA (11.9) and PETG (11.8) showed very similar values. Optical microscopy and selected SEM/EDS observations revealed material-dependent surface features and showed local Fe detectability in the analyzed regions of the filled PLA. The microhardness ranking did not follow the cumulative material-loss trend, most clearly for Fe-filled PLA and for PETG versus ASA. These results indicate that the local indentation-hardness ranking did not correspond directly to the cumulative mass-loss ranking of the investigated FDM-printed polymers under the selected conditions. For material selection in FDM components subjected to abrasive contact, these findings indicate that local microhardness should not be used alone as a proxy for condition-specific abrasive wear performance.
- Open Access
- 1 September 2026
- Published by IOP Publishing in Materials Research Express
- Vol. 13 (17) , 176503
Probing microstructural modification and hardness response in h-BN reinforced A356 aluminum matrix composites
A356 Al–Si–Mg alloys are widely used in lightweight structural applications; however, their as-cast mechanical performance is strongly influenced by the morphology of dendritic α -Al, the interconnected eutectic Si-rich network, and casting-induced microstructural heterogeneity. In this study, A356 aluminum matrix composites containing 1 and 4 wt.% hexagonal boron nitride (h-BN) were fabricated by induction melting to investigate the effect of h-BN addition on microstructural evolution and localized hardness. The composites were characterized using x-ray diffraction (XRD), FESEM, Energy-dispersive spectroscopy (EDS) mapping, semiquantitative image analysis, and Vickers microhardness testing. XRD analysis showed that α -Al and Si remained the dominant crystalline phases, with no distinct reaction products detected. SEM observations and image analysis indicated that h-BN addition reduced the apparent continuity of the interdendritic eutectic Si-rich network, with the median major-axis length of the segmented Si-rich features decreasing from 3.38 µ m in the unreinforced A356 alloy to 3.14 µ m and 2.72 µ m in the composites containing 1 and 4 wt.% h-BN, respectively. EDS mapping qualitatively confirmed the presence of B-containing regions in the reinforced composites. The mean Vickers hardness increased from 57.5 HV to 64.4 HV and 71 HV with increasing h-BN content, corresponding to improvements of approximately 12% and 23.5%, respectively. The hardness enhancement is primarily attributed to eutectic Si network modification, with possible additional contributions from localized restriction of plastic deformation. Overall, the results establish a processing-microstructure-hardness relationship in cast A356/h-BN composites and demonstrate that h-BN addition improves localized deformation resistance through modification of the as-cast eutectic Si-rich network.
- 1 September 2026
- Published by IOP Publishing in Materials Research Express
- Vol. 13 (17) , 176503
Open AccessProbing microstructural modification and hardness response in h-BN reinforced A356 aluminum matrix composites
A356 Al–Si–Mg alloys are widely used in lightweight structural applications; however, their as-cast mechanical performance is strongly influenced by the morphology of dendritic α -Al, the interconnected eutectic Si-rich network, and casting-induced microstructural heterogeneity. In this study, A356 aluminum matrix composites containing 1 and 4 wt.% hexagonal boron nitride (h-BN) were fabricated by induction melting to investigate the effect of h-BN addition on microstructural evolution and localized hardness. The composites were characterized using x-ray diffraction (XRD), FESEM, Energy-dispersive spectroscopy (EDS) mapping, semiquantitative image analysis, and Vickers microhardness testing. XRD analysis showed that α -Al and Si remained the dominant crystalline phases, with no distinct reaction products detected. SEM observations and image analysis indicated that h-BN addition reduced the apparent continuity of the interdendritic eutectic Si-rich network, with the median major-axis length of the segmented Si-rich features decreasing from 3.38 µ m in the unreinforced A356 alloy to 3.14 µ m and 2.72 µ m in the composites containing 1 and 4 wt.% h-BN, respectively. EDS mapping qualitatively confirmed the presence of B-containing regions in the reinforced composites. The mean Vickers hardness increased from 57.5 HV to 64.4 HV and 71 HV with increasing h-BN content, corresponding to improvements of approximately 12% and 23.5%, respectively. The hardness enhancement is primarily attributed to eutectic Si network modification, with possible additional contributions from localized restriction of plastic deformation. Overall, the results establish a processing-microstructure-hardness relationship in cast A356/h-BN composites and demonstrate that h-BN addition improves localized deformation resistance through modification of the as-cast eutectic Si-rich network.
- 7 July 2025
- Published by Walter de Gruyter GmbH in Materials Testing
- Vol. 67 (9) , 1495-1506
Unveiling the creep mechanisms of rare earth element yttrium added and SPS consolidated CoCrFeNi high entropy alloys
As high entropy alloys (HEAs) continue to be increasingly studied for next-generation structural materials, gaining a comprehensive understanding of their mechanical properties, including their creep behaviors, remains essential. In this work, rare earth element yttrium (Y) added CoCrFeNi HEAs are produced by mechanical alloying, followed by consolidation via spark plasma sintering (SPS) with ultrafine grain sizes. The microstructures after SPS consolidation are examined using X-ray diffraction (XRD) and transmission electron microscopy (TEM). The creep properties, including creep displacement, creep strain rate, creep stress, and stress exponent, are evaluated using a nanoindentation test with a Berkovich tip indenter. The results reveal that the average grain size of CoCrFeNi HEA is determined to be 385 ± 65 nm after SPS consolidation, which reduces to 190 ± 30 nm and 155 ± 55 nm with 1 and 4 at.% Y additions, respectively. Accordingly, HEA with the addition of 4 at.% Y exhibits increased hardness, attributed to the presence of additional Y-based oxides and the reduced grain size in its microstructure. Furthermore, the creep mechanisms for the investigated CoCrFeNi HEAs are primarily dominated by dislocation–precipitation interaction based on the calculated stress exponent values.
- 7 July 2025
- Published by Walter de Gruyter GmbH in Materials Testing
- Vol. 67 (9) , 1495-1506
Unveiling the creep mechanisms of rare earth element yttrium added and SPS consolidated CoCrFeNi high entropy alloys
As high entropy alloys (HEAs) continue to be increasingly studied for next-generation structural materials, gaining a comprehensive understanding of their mechanical properties, including their creep behaviors, remains essential. In this work, rare earth element yttrium (Y) added CoCrFeNi HEAs are produced by mechanical alloying, followed by consolidation via spark plasma sintering (SPS) with ultrafine grain sizes. The microstructures after SPS consolidation are examined using X-ray diffraction (XRD) and transmission electron microscopy (TEM). The creep properties, including creep displacement, creep strain rate, creep stress, and stress exponent, are evaluated using a nanoindentation test with a Berkovich tip indenter. The results reveal that the average grain size of CoCrFeNi HEA is determined to be 385 ± 65 nm after SPS consolidation, which reduces to 190 ± 30 nm and 155 ± 55 nm with 1 and 4 at.% Y additions, respectively. Accordingly, HEA with the addition of 4 at.% Y exhibits increased hardness, attributed to the presence of additional Y-based oxides and the reduced grain size in its microstructure. Furthermore, the creep mechanisms for the investigated CoCrFeNi HEAs are primarily dominated by dislocation–precipitation interaction based on the calculated stress exponent values.
- Open Access
- 20 May 2024
- Published by Journal of the Faculty of Engineering and Architecture of Gazi University in Gazi Üniversitesi Mühendislik-Mimarlık Fakültesi Dergisi
- Vol. 39 (4) , 2515-2524
Geleneksel sinterleme ve spark plazma sinterleme yöntemlerinin nanokristal yapılı CoCrFeNi yüksek entropili alaşımın mikroyapısal özellikleri ve sertliği üzerine etkilerinin araştırılması
CoCrFeNi YEA’ları mekanik alaşımlama yöntemiyle üretilerek geleneksel sinterleme ve spark plazma sinterleme yöntemleriyle konsolide edilmiştir. Sinterleme yöntemi ve sıcaklıklarının bir fonksiyonu olarak mikroyapıların incelenmesi için x-ışınları difraksiyonu (XRD), odaklanmış iyon demeti mikroskobu (FIB) ve geçirimli elektron mikroskobu (TEM) yöntemleri kullanılmıştır. Elde edilen sonuçlar, alaşımlanmış yapıların tek fazlı yüzey merkezli kübik (ymk) kristal yapıya sahip olduğunu göstermiştir. Bununla birlikte, aynı sıcaklıklarda uygulanan spark plazma sinterleme sonrasında alaşımların mikroyapılarında ymk kristal yapıya sahip matris fazına ilave olarak Cr7C3 fazının da oluştuğu tespit edilmiştir. Mekanik alaşımlanmış yapıların tane boyutu 10 nm civarında iken, 1000 ve 1100 °C’deki geleneksel sinterleme sonrasında tane boyutu sırasıyla 450 nm ve 1,5 µm değerlerine ulaşmış, bu da nanokristal yapılı CoCrFeNi alaşımının geleneksel sinterleme ile termal kararlığını koruyamadığını göstermektedir. Mekanik alaşımlanmış tozların spark plazma sinterleme ile 1100 °C’de konsolidasyonu sonrası YEA’nın tane boyutu yaklaşık 355 nm olarak elde edilmiş olup bu değer aynı sıcaklıkta geleneksel sinterleme ile elde edilmiş alaşımın tane boyutundan daha küçüktür. Buna göre, CoCrFeNi YEA’sının mekanik alaşımlama sonrası 4,6 GPa olarak tespit edilen sertliği, 1100 °C’deki geleneksel sinterleme sonrasında görülen tane büyümesi nedeniyle 2,1 GPa’ya düşmüş, ancak 1100 °C’de spark plazma sinterleme ile konsolidasyon sonucunda sertlik değeri 3,6 GPa olarak korunmuştur.
- 20 May 2024
- Published by Journal of the Faculty of Engineering and Architecture of Gazi University in Gazi Üniversitesi Mühendislik-Mimarlık Fakültesi Dergisi
- Vol. 39 (4) , 2515-2524
Open AccessGeleneksel sinterleme ve spark plazma sinterleme yöntemlerinin nanokristal yapılı CoCrFeNi yüksek entropili alaşımın mikroyapısal özellikleri ve sertliği üzerine etkilerinin araştırılması
CoCrFeNi YEA’ları mekanik alaşımlama yöntemiyle üretilerek geleneksel sinterleme ve spark plazma sinterleme yöntemleriyle konsolide edilmiştir. Sinterleme yöntemi ve sıcaklıklarının bir fonksiyonu olarak mikroyapıların incelenmesi için x-ışınları difraksiyonu (XRD), odaklanmış iyon demeti mikroskobu (FIB) ve geçirimli elektron mikroskobu (TEM) yöntemleri kullanılmıştır. Elde edilen sonuçlar, alaşımlanmış yapıların tek fazlı yüzey merkezli kübik (ymk) kristal yapıya sahip olduğunu göstermiştir. Bununla birlikte, aynı sıcaklıklarda uygulanan spark plazma sinterleme sonrasında alaşımların mikroyapılarında ymk kristal yapıya sahip matris fazına ilave olarak Cr7C3 fazının da oluştuğu tespit edilmiştir. Mekanik alaşımlanmış yapıların tane boyutu 10 nm civarında iken, 1000 ve 1100 °C’deki geleneksel sinterleme sonrasında tane boyutu sırasıyla 450 nm ve 1,5 µm değerlerine ulaşmış, bu da nanokristal yapılı CoCrFeNi alaşımının geleneksel sinterleme ile termal kararlığını koruyamadığını göstermektedir. Mekanik alaşımlanmış tozların spark plazma sinterleme ile 1100 °C’de konsolidasyonu sonrası YEA’nın tane boyutu yaklaşık 355 nm olarak elde edilmiş olup bu değer aynı sıcaklıkta geleneksel sinterleme ile elde edilmiş alaşımın tane boyutundan daha küçüktür. Buna göre, CoCrFeNi YEA’sının mekanik alaşımlama sonrası 4,6 GPa olarak tespit edilen sertliği, 1100 °C’deki geleneksel sinterleme sonrasında görülen tane büyümesi nedeniyle 2,1 GPa’ya düşmüş, ancak 1100 °C’de spark plazma sinterleme ile konsolidasyon sonucunda sertlik değeri 3,6 GPa olarak korunmuştur.
- 20 July 2023
- Published by Walter de Gruyter GmbH in Materials Testing
- Vol. 65 (9) , 1405-1415
Indentation creep behavior of Fe–8Ni–xZr oxide dispersion strengthened alloys
This study was conducted to understand the creep behavior of two oxide dispersion strengthened alloys containing Zr as the alloying addition by performing indentation creep tests at room temperature. The oxide dispersion strengthened alloys were Fe–8Ni–xZr (x = 1 and 4 at.%, i.e., Zr-1 and Zr-4 alloys, respectively), which had been previously fabricated by mechanical alloying; followed by consolidation via equal channel angular extrusion at 1000 °C. The indentation tests were conducted under a maximum load of 100 mN with the loading rates at 300 and 400 mN min−1. The hardness was calculated by the Oliver–Pharr method, and the creep properties, such as the creep displacement, creep strain rate, creep stress, and stress exponent n, were determined. The results showed that the Zr-4 alloy was harder than the Zr-1 alloy. However, the creep resistance of the Zr-1 alloy was better than that of the Zr-4 alloy. It was further demonstrated that both the hardness and creep resistance depended on the loading rate. Moreover, a possible creep mechanism was proposed. Although the tests were performed at room temperature, they can provide insight into the effect of an oxide dispersion strengthened alloys microstructure on creep at higher temperatures.
- 20 July 2023
- Published by Walter de Gruyter GmbH in Materials Testing
- Vol. 65 (9) , 1405-1415
Indentation creep behavior of Fe–8Ni–xZr oxide dispersion strengthened alloys
This study was conducted to understand the creep behavior of two oxide dispersion strengthened alloys containing Zr as the alloying addition by performing indentation creep tests at room temperature. The oxide dispersion strengthened alloys were Fe–8Ni–xZr (x = 1 and 4 at.%, i.e., Zr-1 and Zr-4 alloys, respectively), which had been previously fabricated by mechanical alloying; followed by consolidation via equal channel angular extrusion at 1000 °C. The indentation tests were conducted under a maximum load of 100 mN with the loading rates at 300 and 400 mN min−1. The hardness was calculated by the Oliver–Pharr method, and the creep properties, such as the creep displacement, creep strain rate, creep stress, and stress exponent n, were determined. The results showed that the Zr-4 alloy was harder than the Zr-1 alloy. However, the creep resistance of the Zr-1 alloy was better than that of the Zr-4 alloy. It was further demonstrated that both the hardness and creep resistance depended on the loading rate. Moreover, a possible creep mechanism was proposed. Although the tests were performed at room temperature, they can provide insight into the effect of an oxide dispersion strengthened alloys microstructure on creep at higher temperatures.
- 11 May 2022
- Published by Elsevier in Intermetallics
- Vol. 146
An investigation of abnormal grain growth in Zr doped CoCrFeNi HEAs through in-situ formed oxide phases
- 11 May 2022
- Published by Elsevier in Intermetallics
- Vol. 146
An investigation of abnormal grain growth in Zr doped CoCrFeNi HEAs through in-situ formed oxide phases
- Open Access
- 1 January 2021
- Published by Elsevier in SSRN Electronic Journal
Role of Yttrium Addition and Annealing Temperature on Thermal Stability and Hardness of Nanocrystalline CoCrFeNi High Entropy Alloy
CoCrFeNi high entropy alloys (HEAs) with yttrium (Y) additions (1 and 4 at. %) were nanostructured by mechanical alloying process and annealed at various temperatures between 500 °C and 1100 °C. The structure, grain growth, and hardness were studied as a function of solute addition and annealing temperature using X-ray diffraction (XRD), focused ion beam (FIB), and scanning transmission electron microscope (S/TEM) techniques, and hardness test. The thermo-physical calculations were utilized to discuss the phase evolution after mechanical alloying and annealing with respect to added solutes. The results showed that Y additions did not affect the main crystal structure of the base CoCrFeNi HEA as the solid solution with a single face-centered cubic (fcc) crystal structure was maintained even after 1 h annealing at 1100 °C. The as-milled nanocrystalline grain size of CoCrFeNi HEA yielded extensive grain growth with the temperature exposures reaching 291 nm and 1.4 µm after annealing at 900 °C and 1100 °C, respectively. However, Y additions retarded the grain growth and decreased the average grain size upon annealing as compared to the base HEA. That is, 1 and 4 at. % Y additions stabilized the grain size around 88 nm and 95 nm (both determined by TEM) after annealing at 900 °C and 1100 °C, respectively. Accordingly, the as-milled hardness of CoCrFeNi HEA dropped from 475 HV to 220 HV after annealing at 1100 °C, while the reduction in hardness was relatively gradual with Y additions and retained around 435 HV with 4 at. % Y addition even after annealing at 1100 °C. Such thermal stability may facilitate the use of HEAs at high temperatures and enable the consolidation routes of powders into dense nanocrystalline compact HEAs.
- 1 January 2021
- Published by Elsevier in SSRN Electronic Journal
Open AccessRole of Yttrium Addition and Annealing Temperature on Thermal Stability and Hardness of Nanocrystalline CoCrFeNi High Entropy Alloy
CoCrFeNi high entropy alloys (HEAs) with yttrium (Y) additions (1 and 4 at. %) were nanostructured by mechanical alloying process and annealed at various temperatures between 500 °C and 1100 °C. The structure, grain growth, and hardness were studied as a function of solute addition and annealing temperature using X-ray diffraction (XRD), focused ion beam (FIB), and scanning transmission electron microscope (S/TEM) techniques, and hardness test. The thermo-physical calculations were utilized to discuss the phase evolution after mechanical alloying and annealing with respect to added solutes. The results showed that Y additions did not affect the main crystal structure of the base CoCrFeNi HEA as the solid solution with a single face-centered cubic (fcc) crystal structure was maintained even after 1 h annealing at 1100 °C. The as-milled nanocrystalline grain size of CoCrFeNi HEA yielded extensive grain growth with the temperature exposures reaching 291 nm and 1.4 µm after annealing at 900 °C and 1100 °C, respectively. However, Y additions retarded the grain growth and decreased the average grain size upon annealing as compared to the base HEA. That is, 1 and 4 at. % Y additions stabilized the grain size around 88 nm and 95 nm (both determined by TEM) after annealing at 900 °C and 1100 °C, respectively. Accordingly, the as-milled hardness of CoCrFeNi HEA dropped from 475 HV to 220 HV after annealing at 1100 °C, while the reduction in hardness was relatively gradual with Y additions and retained around 435 HV with 4 at. % Y addition even after annealing at 1100 °C. Such thermal stability may facilitate the use of HEAs at high temperatures and enable the consolidation routes of powders into dense nanocrystalline compact HEAs.