Mateus de Sousa Zanzi
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Mateus de Sousa Zanzi has a total of 18 co-authors. Here are the top co-authors by number of shared publications:
Jorge Luiz Goes Oliveira
4 shared publicationsGabriel Benedet Dutra
Department of Mobility Engineering, Federal University of Santa Catarina, Joinville, Brazil
3 shared publications- Gabriel Benedet Dutra
Federal University of Santa Catarina
3 shared publications Guilherme Mariz de Oliveira Barra
3 shared publicationsKleber Vieira Paiva
Department of Mobility Engineering, Federal University of Santa Catarina, Joinville, Brazil
3 shared publications- Elias Luiz de Souza
Department of Mechanical Engineering Federal University of Santa Catarina Florianópolis Brazil
2 shared publications
Latest Publications
- Open Access
- 21 August 2026
- Published by American Chemical Society (ACS) in ACS Omega
- Vol. 11 (35) , 52980-52993
Effect of Reactive Gas Composition and Duty Cycle in Low-Pressure DC-Pulsed Plasmas on the Surface Oxidation of Nitrile Rubber
Nitrile rubber (NBR) is widely used in components across several industrial sectors due to its properties that are suitable for engineering applications. Surface-environment interactions often limit performance, which depends critically on surface characteristics, especially barrier properties for sealing and membrane applications. This study investigates the effects of low-pressure direct-current pulsed plasma treatment in O2/Ar atmospheres on NBR surfaces to generate oxidized layers. Samples were treated at duty cycles of 30% and 70% with oxygen contents of 20% (low) and 80% (high). Nanoindentation post-treatment revealed increased surface contact stiffness, while differential scanning calorimetry (DSC) confirmed unchanged bulk properties. Attenuated total reflectance Fourier transform infrared (ATR-FTIR) spectroscopy indicated the incorporation of oxidized groups and reduced C–H signals. The highest duty cycles (70%) improved sputtering species production, and the highest oxygen content (80%) enhanced O ion creation and surface oxidation, as evidenced by optical emission spectroscopy (OES) and X-ray photoelectron spectroscopy (XPS). XPS depth profiling showed a rising oxidation profile (oxygen implantation) at the treated surface. Based on a plasma-surface interaction mechanism, the condition with 80% oxygen and 30% duty cycle yields the highest surface oxidation level. It potentially enhances barrier properties, contributing to plasma-parameter optimization for tailored NBR surface modifications.
- 21 August 2026
- Published by American Chemical Society (ACS) in ACS Omega
- Vol. 11 (35) , 52980-52993
Open AccessEffect of Reactive Gas Composition and Duty Cycle in Low-Pressure DC-Pulsed Plasmas on the Surface Oxidation of Nitrile Rubber
Nitrile rubber (NBR) is widely used in components across several industrial sectors due to its properties that are suitable for engineering applications. Surface-environment interactions often limit performance, which depends critically on surface characteristics, especially barrier properties for sealing and membrane applications. This study investigates the effects of low-pressure direct-current pulsed plasma treatment in O2/Ar atmospheres on NBR surfaces to generate oxidized layers. Samples were treated at duty cycles of 30% and 70% with oxygen contents of 20% (low) and 80% (high). Nanoindentation post-treatment revealed increased surface contact stiffness, while differential scanning calorimetry (DSC) confirmed unchanged bulk properties. Attenuated total reflectance Fourier transform infrared (ATR-FTIR) spectroscopy indicated the incorporation of oxidized groups and reduced C–H signals. The highest duty cycles (70%) improved sputtering species production, and the highest oxygen content (80%) enhanced O ion creation and surface oxidation, as evidenced by optical emission spectroscopy (OES) and X-ray photoelectron spectroscopy (XPS). XPS depth profiling showed a rising oxidation profile (oxygen implantation) at the treated surface. Based on a plasma-surface interaction mechanism, the condition with 80% oxygen and 30% duty cycle yields the highest surface oxidation level. It potentially enhances barrier properties, contributing to plasma-parameter optimization for tailored NBR surface modifications.
- 11 September 2024
- Published by Springer Nature in Journal of the Brazilian Society of Mechanical Sciences and Engineering
- Vol. 46 (10) , 1-11
Structural analysis and sealing capacity of gasketed plate heat exchangers with HNBR and EPDM rubbers
- 11 September 2024
- Published by Springer Nature in Journal of the Brazilian Society of Mechanical Sciences and Engineering
- Vol. 46 (10) , 1-11
Structural analysis and sealing capacity of gasketed plate heat exchangers with HNBR and EPDM rubbers
- Open Access
- 31 January 2024
- Published by Springer Nature in Research Square
Structural Analysis and Sealing Capacity of Gasketed Plate Heat Exchangers with HNBR and EPDM Rubbers
Rubber is an engineering polymer of interest in most industrial sectors. In gasketed plate heat exchangers (GPHEs), these elements comprise gaskets that are responsible for sealing the system under high levels of compression, temperature and pressure. Therefore, it is a necessity to understand how operating conditions affect GPHE structural behavior and sealing performance, regarding rubber materials and features. This work aims at determining GPHE integrity and mechanical characteristics with the aid of sealing performance experiments and strain gauge measurements at critical plate locations in a real equipment and in prototypes consisting of GPHE components. Hydrogenated Nitrile Butadiene Rubber (HNBR) and Ethylene-Propylene-Diene Rubber (EPDM) gasket materials were evaluated. Based on compression strength experiments, the effects of the number of plates and the compression level on the system stiffness in the direction where the quasi-static compression load is applied have been determined. Stable compression strength behavior was attained with prototypes containing six gaskets or more. The combined effects of pressure load and compression levels, and rubber material on sealing performance were obtained with prototypes comprising six gaskets. Stress analysis was possible with plate deformation measurements in a heat exchanger comprising twenty plates. Highest stress levels were obtained with EPDM gaskets during tightening. It is conjectured that higher operation loads can occur with the latter material. Empirical correlations relate sealing capacity and compression level for EPDM and HNBR gaskets.
- 31 January 2024
- Published by Springer Nature in Research Square
Open AccessStructural Analysis and Sealing Capacity of Gasketed Plate Heat Exchangers with HNBR and EPDM Rubbers
Rubber is an engineering polymer of interest in most industrial sectors. In gasketed plate heat exchangers (GPHEs), these elements comprise gaskets that are responsible for sealing the system under high levels of compression, temperature and pressure. Therefore, it is a necessity to understand how operating conditions affect GPHE structural behavior and sealing performance, regarding rubber materials and features. This work aims at determining GPHE integrity and mechanical characteristics with the aid of sealing performance experiments and strain gauge measurements at critical plate locations in a real equipment and in prototypes consisting of GPHE components. Hydrogenated Nitrile Butadiene Rubber (HNBR) and Ethylene-Propylene-Diene Rubber (EPDM) gasket materials were evaluated. Based on compression strength experiments, the effects of the number of plates and the compression level on the system stiffness in the direction where the quasi-static compression load is applied have been determined. Stable compression strength behavior was attained with prototypes containing six gaskets or more. The combined effects of pressure load and compression levels, and rubber material on sealing performance were obtained with prototypes comprising six gaskets. Stress analysis was possible with plate deformation measurements in a heat exchanger comprising twenty plates. Highest stress levels were obtained with EPDM gaskets during tightening. It is conjectured that higher operation loads can occur with the latter material. Empirical correlations relate sealing capacity and compression level for EPDM and HNBR gaskets.
- 22 December 2023
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 141 (10)
HNBR and NBR gasket rubbers for plate heat exchangers: Thermo‐oxidative aging and service lifetime prediction
Among several available rubbers used in gaskets for plate heat exchangers, the selection of the appropriate material for each operation window is crucial. This work evaluated nitrile butadiene rubber (NBR) and hydrogenated butadiene rubber (HNBR) gaskets aged at high temperatures for up to 60 days. The properties assessed of compression set (CS), hardness, and cross‐link density demonstrated superior degradation rates for the NBR specimens. Fourier transform infrared analysis showed that the hydrogenation process predominantly affected CC double bonds. Compress stress relaxation highlighted the impact of aging on the counterforce of rubber over time. Furthermore, indentation modulus profile analysis showed heterogeneous degradation for both materials at 140°C for NBR and 170°C for HNBR. The end‐of‐life criteria of 79% CS for both materials were determined through sealing tests of the aged samples. The service lifetime prediction, using the time–temperature superposition and Arrhenius methods through the CS evolution curves, demonstrated a higher degradation resistance of HNBR gaskets, that have a superior service lifetime of at least 3.5 times at 80°C concerning those of NBR, proving a superior behavior for the hydrogenated elastomer. In addition, the evaluation of the lifetime prediction enables the verification of which rubber gasket is recommended for each operational condition in terms of material cost, service lifetime, and maintenance costs.
- 22 December 2023
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 141 (10)
HNBR and NBR gasket rubbers for plate heat exchangers: Thermo‐oxidative aging and service lifetime prediction
Among several available rubbers used in gaskets for plate heat exchangers, the selection of the appropriate material for each operation window is crucial. This work evaluated nitrile butadiene rubber (NBR) and hydrogenated butadiene rubber (HNBR) gaskets aged at high temperatures for up to 60 days. The properties assessed of compression set (CS), hardness, and cross‐link density demonstrated superior degradation rates for the NBR specimens. Fourier transform infrared analysis showed that the hydrogenation process predominantly affected CC double bonds. Compress stress relaxation highlighted the impact of aging on the counterforce of rubber over time. Furthermore, indentation modulus profile analysis showed heterogeneous degradation for both materials at 140°C for NBR and 170°C for HNBR. The end‐of‐life criteria of 79% CS for both materials were determined through sealing tests of the aged samples. The service lifetime prediction, using the time–temperature superposition and Arrhenius methods through the CS evolution curves, demonstrated a higher degradation resistance of HNBR gaskets, that have a superior service lifetime of at least 3.5 times at 80°C concerning those of NBR, proving a superior behavior for the hydrogenated elastomer. In addition, the evaluation of the lifetime prediction enables the verification of which rubber gasket is recommended for each operational condition in terms of material cost, service lifetime, and maintenance costs.
- 6 May 2022
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 139 (28)
Service lifetime prediction of nitrile butadiene rubber gaskets used in plate heat exchangers
Gasketed plate heat exchangers are characterized in a usual heat exchanger class. These systems employ elastomeric gaskets as the sealing element. Several conditions lead to oxidation and deterioration of these materials and their properties. In addition, the complex geometry of the gaskets and operation conditions may cause divergence in the expected aging behavior of the rubber. In light of this, this study aims to predict the service lifetime for nitrile butadiene rubber gaskets used in plate heat exchangers based on their geometry under thermo‐oxidative aging. These gaskets were evaluated by means of Shore A hardness, compression set (CS), and indentation modulus profile. Through aging‐sealing tests, an end‐of‐life criteria was determined concerning CS measurements and the service lifetime prediction was obtained by time–temperature superposition and WLF method. Diffusion‐limited oxidation effects were observed at high temperatures in postaging analysis and a non‐Arrhenius behavior was observed at 170°C. The value of 79% CS was obtained as end‐of‐life criteria from 60 to 140°C, ranged from 731 to 80 days, respectively, revealing an activation energy equivalent to 32.3 kJ mol−1. These results might support the maintenance planning control of gasketed plate heat exchangers.
- 6 May 2022
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 139 (28)
Service lifetime prediction of nitrile butadiene rubber gaskets used in plate heat exchangers
Gasketed plate heat exchangers are characterized in a usual heat exchanger class. These systems employ elastomeric gaskets as the sealing element. Several conditions lead to oxidation and deterioration of these materials and their properties. In addition, the complex geometry of the gaskets and operation conditions may cause divergence in the expected aging behavior of the rubber. In light of this, this study aims to predict the service lifetime for nitrile butadiene rubber gaskets used in plate heat exchangers based on their geometry under thermo‐oxidative aging. These gaskets were evaluated by means of Shore A hardness, compression set (CS), and indentation modulus profile. Through aging‐sealing tests, an end‐of‐life criteria was determined concerning CS measurements and the service lifetime prediction was obtained by time–temperature superposition and WLF method. Diffusion‐limited oxidation effects were observed at high temperatures in postaging analysis and a non‐Arrhenius behavior was observed at 170°C. The value of 79% CS was obtained as end‐of‐life criteria from 60 to 140°C, ranged from 731 to 80 days, respectively, revealing an activation energy equivalent to 32.3 kJ mol−1. These results might support the maintenance planning control of gasketed plate heat exchangers.