Ashutosh Panchal
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Ashutosh Panchal has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
- Ashok Kumar Singh
Materials Science Division, Defence Metallurgical Research Laboratory, Hyderabad, India
2 shared publications - Tapash Kumar Nandy
DRDO-Defence Metallurgical Research Laboratory (DMRL), Kanchanbagh, Hyderabad - 500 058, India
2 shared publications A. K. Singh
Defence Metallurgical Research Laboratory, Hyderabad, India
1 shared publicationAshish Pathak
Defence Metallurgical Research Laboratory, Hyderabad, India
1 shared publication- Ch.R.V.S. Nagesh
DRDO-Defence Metallurgical Research Laboratory (DMRL), Kanchanbagh PO, Hyderabad - 500 058, India
1 shared publication - Devabrata Mishra
Metal Extraction and Recycling Division, National Metallurgical Laboratory, Jamshedpur, India
1 shared publication
Latest Publications
- Open Access
- 9 March 2023
- Published by Defence Scientific Information and Documentation Centre in Defence Science Journal
- Vol. 73 (No 2) , 241-251
Microstructure and Mechanical Properties of Tungsten Heavy Alloy Prepared Using Tungsten Metal Powder Produced from Heavy Alloy Scrap
Tungsten metal powder, using a hydrometallurgical route, was extracted from tungsten heavy alloy scrap that was generated during machining of penetrator cores for the manufacture of Fin Stabilised Armour Piercing Discarding Sabot (FSAPDS). The powder was subjected to extensive characterisation that included physical property evaluation and analysis of the alloy chemistry in order to assess its suitability for the preparation of tungsten heavy alloys with enhanced mechanical properties. Subsequently, a tungsten heavy alloy based on W-Ni-Co was consolidated using this powder through liquid phase sintering followed by heat treatment and swaging operations to realize long rods (~500 mm). This was followed by a detailed characterisation that included microstructure and mechanical property. The mechanical properties of these rods are promising, exhibiting a good balance of tensile and impact properties, which in turn underscores the potential of these recycled powders in the production of premium quality heavy alloy long rods for stringent applications such as kinetic energy penetrators.
- 9 March 2023
- Published by Defence Scientific Information and Documentation Centre in Defence Science Journal
- Vol. 73 (No 2) , 241-251
Open AccessMicrostructure and Mechanical Properties of Tungsten Heavy Alloy Prepared Using Tungsten Metal Powder Produced from Heavy Alloy Scrap
Tungsten metal powder, using a hydrometallurgical route, was extracted from tungsten heavy alloy scrap that was generated during machining of penetrator cores for the manufacture of Fin Stabilised Armour Piercing Discarding Sabot (FSAPDS). The powder was subjected to extensive characterisation that included physical property evaluation and analysis of the alloy chemistry in order to assess its suitability for the preparation of tungsten heavy alloys with enhanced mechanical properties. Subsequently, a tungsten heavy alloy based on W-Ni-Co was consolidated using this powder through liquid phase sintering followed by heat treatment and swaging operations to realize long rods (~500 mm). This was followed by a detailed characterisation that included microstructure and mechanical property. The mechanical properties of these rods are promising, exhibiting a good balance of tensile and impact properties, which in turn underscores the potential of these recycled powders in the production of premium quality heavy alloy long rods for stringent applications such as kinetic energy penetrators.
- 20 June 2022
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering
- Vol. 238 (2) , 576-584
On the development of gelcasting process for tungsten and its alloys
Gelcasting technique has been successfully used for the preparation of porous tungsten. Gel forming monomer (methacrylamide (MAM)) and Cross-linker (NN’-Methylenebisacrylamide (MBAM)) dissolved in water were used for gelcasting of green compacts of tungsten with 39% solid loading. Appropriate quantity of dispersant, initiator, and catalyst were used in order to obtain a uniform dispersion of tungsten particles and also control the polymerization process. Several issues related to dispersant selection, de-airing, de-bindering, sintering, and selection of mold material have been addressed in order to obtain a defect-free product. Theoretical density of the porous sintered tungsten pellets produced by gelcasting process is ∼85%. The average pore diameter and mean pore area are 3 µm and 16 µm 2 , respectively, which are specifically required for the cathode application. Complex shape components of pure tungsten have been successfully made using gelcasting technique for the first time.
- 20 June 2022
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering
- Vol. 238 (2) , 576-584
On the development of gelcasting process for tungsten and its alloys
Gelcasting technique has been successfully used for the preparation of porous tungsten. Gel forming monomer (methacrylamide (MAM)) and Cross-linker (NN’-Methylenebisacrylamide (MBAM)) dissolved in water were used for gelcasting of green compacts of tungsten with 39% solid loading. Appropriate quantity of dispersant, initiator, and catalyst were used in order to obtain a uniform dispersion of tungsten particles and also control the polymerization process. Several issues related to dispersant selection, de-airing, de-bindering, sintering, and selection of mold material have been addressed in order to obtain a defect-free product. Theoretical density of the porous sintered tungsten pellets produced by gelcasting process is ∼85%. The average pore diameter and mean pore area are 3 µm and 16 µm 2 , respectively, which are specifically required for the cathode application. Complex shape components of pure tungsten have been successfully made using gelcasting technique for the first time.
- 17 August 2021
- Published by SAGE Publications in Powder Metallurgy
- Vol. 65 (2) , 151-158
Effects of Co and Co + Mo additions on tensile properties of tungsten heavy alloys: first-principles study and experimental investigations
The present work illustrates the deformation behaviour of tungsten heavy alloys (WHAs) using first-principles calculation under tensile stress of three virtual alloy systems comprising the matrix phase and a W-grain along with two fcc–bcc interfaces. The energy values of the alloy systems decrease with the additions of Co and Co + Mo in the ternary alloy (W–Ni–Fe). The experimental lattice parameters of the matrix phase of alloys are in good agreement with those of the alloy systems calculated using the first-principles calculation. The lattice constants, yield strength and strength at 20% strain increase with the additions of Co and Co + Mo. The nature of theoretical stress–strain curves of systems is similar to those of the experimental stress–strain curves of typical alloys. The nitty-gritty of virtual alloy systems and the interrelated consequences resulting in closer to real alloys in terms of tensile flow curves have been discussed.
- 17 August 2021
- Published by SAGE Publications in Powder Metallurgy
- Vol. 65 (2) , 151-158
Effects of Co and Co + Mo additions on tensile properties of tungsten heavy alloys: first-principles study and experimental investigations
The present work illustrates the deformation behaviour of tungsten heavy alloys (WHAs) using first-principles calculation under tensile stress of three virtual alloy systems comprising the matrix phase and a W-grain along with two fcc–bcc interfaces. The energy values of the alloy systems decrease with the additions of Co and Co + Mo in the ternary alloy (W–Ni–Fe). The experimental lattice parameters of the matrix phase of alloys are in good agreement with those of the alloy systems calculated using the first-principles calculation. The lattice constants, yield strength and strength at 20% strain increase with the additions of Co and Co + Mo. The nature of theoretical stress–strain curves of systems is similar to those of the experimental stress–strain curves of typical alloys. The nitty-gritty of virtual alloy systems and the interrelated consequences resulting in closer to real alloys in terms of tensile flow curves have been discussed.
- 23 June 2021
- Published by Taylor & Francis in Advances in Materials and Processing Technologies
- Vol. 8 (sup2) , 992-1006
On the development of porous nickel through gelcasting technique
In this study, a slurry-based technique has been developed for the manufacturing of porous nickel structures for capillary pumping systems. The application of porous Ni structures to capillary pumping systems requires porosity levels higher than 40% and pore size diameter lower than 20 μm. Irregular type open pores are observed in the sintered blanks. The porosity level and volume shrinkage decreases and increases with increase in sintering temperature, respectively. The compressive flow stress-strain curves exhibit three distinct regions namely, (i) linear region characterised by elastic modulus, (ii) corresponds to plastic yield and buckling of pore ligaments and (iii) densification region characterised by increasing slope. As the sintering temperature increases, porosity level decreases and resulting in increase in the plateau and densification stress.
- 23 June 2021
- Published by Taylor & Francis in Advances in Materials and Processing Technologies
- Vol. 8 (sup2) , 992-1006
On the development of porous nickel through gelcasting technique
In this study, a slurry-based technique has been developed for the manufacturing of porous nickel structures for capillary pumping systems. The application of porous Ni structures to capillary pumping systems requires porosity levels higher than 40% and pore size diameter lower than 20 μm. Irregular type open pores are observed in the sintered blanks. The porosity level and volume shrinkage decreases and increases with increase in sintering temperature, respectively. The compressive flow stress-strain curves exhibit three distinct regions namely, (i) linear region characterised by elastic modulus, (ii) corresponds to plastic yield and buckling of pore ligaments and (iii) densification region characterised by increasing slope. As the sintering temperature increases, porosity level decreases and resulting in increase in the plateau and densification stress.