ASAshok Kumar Singh

Ashok Kumar Singh

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


Ashok Kumar Singh has a total of 76 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Studies on the Structural, Optical, Photocatalytic and Luminescence Properties of Monodispersed CdS Nanoparticles Capped with Moringa oleifera L. Leaf Extract

    by B. Srinivasa Goud, Y. Suresh, G. Odelu, S. Annapurna, G. Bhikshamaiah, A.K. Singh

    This study reports the structural, optical, photocatalytic and luminescence properties of monodispersed cadmium sulphide nanoparticles (CdS NPs) synthesised via an eco-friendly green synthesis approach using Moringa oleifera leaf extract as a natural stabilizing and capping agent. Cadmium nitrate, cadmium sulphate and cadmium chloride are used as cadmium precursors, while sodium sulphide served as the sulphur source. X-ray diffraction (XRD) analysis confirmed the formation of cubic-phase CdS NPs with high crystalline nature. The optical properties are evaluated through UV-Vis absorption spectroscopy, revealing a band gap energy range of 3.08 to 4.92 eV. FTIR confirmed the presence of functional groups responsible for stabilisation of CdS NPs. The morphological characteristics, elemental composition and purity are assessed using FESEM and EDS. Small-angle X-ray scattering (SAXS) and transmission electron microscopy (TEM) determined the nanoparticle size to be below 5 nm, confirming their nanoscale dimensions. Photoluminescence (PL) spectra indicate strong emission properties, enhancing their potential use in optoelectronic applications. The photocatalytic activity of CdS NPs is evaluated by degrading methylene blue (MB) and rhodamine B (RhB) dyes under visible light irradiation, demonstrating their efficiency in environmental remediation and wastewater treatment. The results highlight the superior optical, structural and catalytic performance of M. oleifera-capped CdS NPs, making them promising candidates for advanced nanomaterial applications in solar cells, photocatalysis and biomedical fields.

  • Structure, processing, property correlation of metastable β titanium Ti-5Al-5Mo-5V-3Cr alloy

    by Premkumar Manda, Jawed Quamar, Chila Vanitha, Ashok Kumar Singh

    This work reports the evolution of “Structure, Processing, Property Correlation of Metastable β Titanium Ti-5Al-5Mo-5V-3Cr alloy” as a function of different aging temperatures (625,725 and 775 °C) for 4 h subsequent to solution heat treatment. The hot-rolled sheet was heat treated in β phase field and then water quenched. The solution heat treated in β phase field and then water quenched samples were aged at 625, 725 and 775 °C for 4 h. The hot-rolled sample shows the presence of α and β phases. The β-solution heat treated in β phase field and then water quenched sample of the alloy exhibits single β phase. The intensities of X-ray peaks are varying and β (211) peak shows the maximum intensity. The maximum intensity can be ascribed to β (211) texture. The solution heat treated in β phase field and then water quenched sample aged at 625 °C for 4 h shows the very fine hexagonal α phase precipitates as compared to the samples aged at 725 and 775 °C for 4 h. The samples aged at 725 and 775 °C for 4 h has resulted in precipitate-free zones as a result of the rejection of Mo, V, and Cr (β stabilizing elements) during nucleation and growth of α precipitates along the β grain boundaries. The Vickers hardness values of the alloy increase from solution heat treated in β phase field and then water quenched to all aging temperatures. The sample aged at 625 °C for 4 h shows the maximum hardness which is due to the presence of fine α phase precipitates. This can be ascribed to typical precipitation hardening.


  • On the development of gelcasting process for tungsten and its alloys

    by Ashutosh Panchal, Tk Nandy, Ak Singh

    Gelcasting technique has been successfully used for the preparation of porous tungsten. Gel forming monomer (methacrylamide (MAM)) and Cross-linker (NN’-Methylenebisacrylamide (MBAM)) dissolved in water were used for gelcasting of green compacts of tungsten with 39% solid loading. Appropriate quantity of dispersant, initiator, and catalyst were used in order to obtain a uniform dispersion of tungsten particles and also control the polymerization process. Several issues related to dispersant selection, de-airing, de-bindering, sintering, and selection of mold material have been addressed in order to obtain a defect-free product. Theoretical density of the porous sintered tungsten pellets produced by gelcasting process is ∼85%. The average pore diameter and mean pore area are 3 µm and 16 µm 2 , respectively, which are specifically required for the cathode application. Complex shape components of pure tungsten have been successfully made using gelcasting technique for the first time.

  • STRUCTURE - PROPERTY - PROCESSING CORRELATIONS IN METASTABLE BETA TITANIUM ALLOYS Ti-10V-2Fe-3Al AND Ti-5Al-5Mo-5V-3Cr

    by Premkumar Manda, Antim Rewapati, C. Vanitha, A.K. Singh

    This paper describes the microstructure, texture and tensile properties of the two metastable β titanium alloys (Ti-10V-2Fe-3Al and Ti-5Al-5Mo-5V-3Cr). Both the alloys exhibit the single β (body centered cubic) phase in β solution treated and water quenched (β ST WQ) condition. The β ST WQ samples were aged at two different temperatures (550 and 750 °C) and different aging times (2, 4 and 6 hrs). The aging has resulted in different α phase morphologies of a phase precipitates. The sizes and volume fractions of the a phase increase and decrease with increase in aging temperature, respectively. The higher aging temperature (750 °C) results in precipitation free zones (PFZ) within the vicinity of prior β grain boundaries. The a phase texture is basal and it changes to non-basal with increase in aging time. The sharp a phase texture consists of {0001} || ND fibre with high intensity. The Vickers hardness values of both the alloys increase from β ST WQ to all aging temperatures due to precipitation hardening. The specimens aged at 550 °C have resulted in high strength in alloy Ti-1023. In contrast, 750 °C aged samples of both the alloys result in lower strength and moderate elongation values.

  • On the development of porous nickel through gelcasting technique

    by Ashutosh Panchal, T. K. Nandy, A. K. Singh

    In this study, a slurry-based technique has been developed for the manufacturing of porous nickel structures for capillary pumping systems. The application of porous Ni structures to capillary pumping systems requires porosity levels higher than 40% and pore size diameter lower than 20 μm. Irregular type open pores are observed in the sintered blanks. The porosity level and volume shrinkage decreases and increases with increase in sintering temperature, respectively. The compressive flow stress-strain curves exhibit three distinct regions namely, (i) linear region characterised by elastic modulus, (ii) corresponds to plastic yield and buckling of pore ligaments and (iii) densification region characterised by increasing slope. As the sintering temperature increases, porosity level decreases and resulting in increase in the plateau and densification stress.

  • Microstructure, texture and mechanical properties of metastable beta titanium alloy Ti-5Al-5Mo-5V-3Cr

    by Premkumar Manda, Shaik Saleem, K. Srinivasa Rao, A.K. Singh

    Present work describes the evolution of microstructure, texture and mechanical properties of the alloy Ti-5Al-5Mo-5 V-3Cr as a function of ageing temperatures and time intervals. The hot-rolled sheet of the pancake was solution treated in β phase field and water quenched (β ST WQ) and aged. The β ST WQ sample of the alloy exhibits single β phase. The β ST WQ samples were initially aged at 300°C for 30, 60 and 90 min and again aged at 550 and 750°C for different ageing times. The ageing has resulted in different morphologies of the α phase precipitates. These are grain boundary α, sub boundary α, islands α and uniform distribution of α within prior β grains. The sizes and volume fractions of the α phase increase and decrease with increase in ageing temperature, respectively. The higher ageing temperature (750°C) results in precipitation-free zone within the vicinity of prior β grain boundaries. . The basal texture observed in α phase of the aged samples exhibits moderate to high intensity along with {0001}||ND fibre. Non-basal textures in α phase have always weak/moderate intensity. The Vickers hardness values of the alloy increase from βSTWQ to all ageing temperatures due to precipitation hardening. The A2-550-4h sample exhibits no yielding due to fine α phase precipitates. On the other hand, A2-750-4h sample displays moderate elongation with high strength values. .

  • Effect of Ni/Fe ratio on microstructure, tensile flow and work hardening behaviour of tungsten heavy alloys in heat treated and swaged conditions

    by Ashutosh Panchal, K. Venugopal Reddy, P. A. Azeem, Rajdeep Sarkar, Archana Paradkar, T. K. Nandy, A. K. Singh

    The present work describes the effect of Ni/Fe ratio on microstructure, tensile flow and work hardening behaviour of tungsten heavy alloys (WHAs) based on 92 wt. % W with varying Ni/Fe ratios in heat treated and swaged conditions. Evaluation of properties in the heat treated and swaged conditions reflect that the increasing Ni/Fe ratio has resulted in the enhancement of tensile as well as impact properties. Quantitative metallography and fractography have been conducted to identify the role of microstructural attributes on the failure behaviour in both the tensile and impact energy tests. The properties improvements at higher Ni/Fe ratios are due to the realisation of microstructure comprising relatively higher dissolved W in the matrix phase, higher volume fraction of matrix and reduced contiguity of W particles. True stress–true plastic strain curves of present alloys on log–log scale display two- and single-slopes in heat treated and swaged conditions, respectively. The instantaneous work hardening curves reveal the presence of three distinctive regimes (I, II and III) in heat treated and swaged conditions. The second derivatives of true stress–true plastic strain curves are parabola.


  • Instantaneous work hardening behaviour of two-phase tungsten heavy alloys: a phenomenological approach

    by Ashutosh Panchal, K. Venugopal Reddy, P. A. Azeem, T. K. Nandy, A. K. Singh

    The present work describes a phenomenological approach to explain the instantaneous behaviour of tungsten heavy alloys (WHAs) in heat-treated and swaged conditions. The strengths and elongation values of heat-treated materials are lower and higher than those of the swaged samples respectively. The heat-treated materials exhibit two slopes in true stress–true plastic strain curves and follow the Ludwigson constitutive equation. On the other hand, swaged materials display a single slope and adhere to typical Swift constitutive equation. The latter reflect the presence of pre-strain in the materials due to swaging deformation. The fracture surfaces in heat-treated materials consist of W-W decohesion along with matrix rupture and W-cleavage, while swaged samples consist of mainly W-cleavage. Both the materials display three typical stages (I, II and III) of work hardening. The second derivatives of true stress–true plastic strain curves of these alloys exhibit a perfect parabola although the nature of true stress–true strain as well as true stress–true plastic strain curves is quite different in heat-treated and swaged materials. This has been observed for the first time in WHAs consisting of matrix and W-grains. The shape of the parabola is simple and easy to fit. The fitting parameters of parabolas have been successfully employed to explain the flow behaviour of a large number of tungsten heavy alloys having two-phase microstructure in different processing conditions.