Zhiqiang Wu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Zhiqiang Wu has a total of 33 co-authors. Here are the top co-authors by number of shared publications:
- Xiaowei Cheng
School of New Energy and Materials, Southwest Petroleum University
3 shared publications - Chengwen Wang
School of Petroleum Engineering, China University of Petroleum (East China), Qingdao 266580, China
2 shared publications Ni Xiucheng
CNOOC Research Institute Co. Ltd., Beijing, China
2 shared publications- Zehua Chen
Key Laboratory of Unconventional Oil & Gas Development, Ministry of Education, Colloge of Petroleum Engineering, China University of Petroleum (East China), Qingdao 266580, China
2 shared publications - Chao Xiong
Key Laboratory of Unconventional Oil & Gas Development, Ministry of Education, College of Petroleum Engineering, China University of Petroleum (East China), Qingdao 266580, China
1 shared publication - Daohang Wang
College of Materials Science and Engineering, Zhejiang University of Technology, Hangzhou 310014, China
1 shared publication
Latest Publications
- Open Access
Supercritical CO2-Stable Cementing Materials Based on Vinyl Ester Resin for Maintaining Wellbore Integrity
Ensuring long-term wellbore integrity is critical for carbon dioxide geological storage. Ordinary Portland cement (PC) is usually used for wellbore primary cementing and plug operation, and set cement is easily corroded by acidic fluids, such as carbon dioxide, in underground high-temperature and high-pressure (HTHP) environments, resulting in a decrease in the mechanical properties and an increase in permeability. In order to achieve long-term wellbore integrity in a CO2-rich environment This study introduces materials such as thermosetting vinyl ester resin (TSR), filler composite resin (FCR), and low-cost resin cement (RC). Corrosion experiments were conducted using four materials in 28 days under supercritical carbon dioxide gas and water phase conditions of 60 °C and 10 MPa. The samples were characterized through mechanical property testing machines, core permeability measuring instruments, FTIR, XRD, and SEM. The results proved that after corrosion, PC mechanical properties decreased, the permeability increased, and the microscopic composition and morphology changed greatly. Penetrating corrosion occurs in the sample in the gas phase environment, and propulsive corrosion from outside to inside occurs in the water phase environment. However, TSR, FCR, and RC materials all maintain excellent resistance to carbon dioxide corrosion in gas and water environments. They have higher compressive strength and extremely low permeability compared to ordinary Portland cement. These three materials’ compressive strengths can be maintained around 131, 99, and 58 MPa, and permeability can be stabilized at −7, −7, and 0.16 mD levels. In summary, the above three materials all show better performance than ordinary Portland cement and are promising alternative materials that can be used in primary cementing and plug operations of carbon dioxide geological storage wells.
Open AccessSupercritical CO2-Stable Cementing Materials Based on Vinyl Ester Resin for Maintaining Wellbore Integrity
Ensuring long-term wellbore integrity is critical for carbon dioxide geological storage. Ordinary Portland cement (PC) is usually used for wellbore primary cementing and plug operation, and set cement is easily corroded by acidic fluids, such as carbon dioxide, in underground high-temperature and high-pressure (HTHP) environments, resulting in a decrease in the mechanical properties and an increase in permeability. In order to achieve long-term wellbore integrity in a CO2-rich environment This study introduces materials such as thermosetting vinyl ester resin (TSR), filler composite resin (FCR), and low-cost resin cement (RC). Corrosion experiments were conducted using four materials in 28 days under supercritical carbon dioxide gas and water phase conditions of 60 °C and 10 MPa. The samples were characterized through mechanical property testing machines, core permeability measuring instruments, FTIR, XRD, and SEM. The results proved that after corrosion, PC mechanical properties decreased, the permeability increased, and the microscopic composition and morphology changed greatly. Penetrating corrosion occurs in the sample in the gas phase environment, and propulsive corrosion from outside to inside occurs in the water phase environment. However, TSR, FCR, and RC materials all maintain excellent resistance to carbon dioxide corrosion in gas and water environments. They have higher compressive strength and extremely low permeability compared to ordinary Portland cement. These three materials’ compressive strengths can be maintained around 131, 99, and 58 MPa, and permeability can be stabilized at −7, −7, and 0.16 mD levels. In summary, the above three materials all show better performance than ordinary Portland cement and are promising alternative materials that can be used in primary cementing and plug operations of carbon dioxide geological storage wells.
- Open Access
An Investigation into PVA Fiber Modified with SiO2 for Improving Mechanical Properties of Oil-Well Cements
In this paper, we conduct a comprehensive investigation into PVA fiber modified with SiO2 to improve the mechanical properties of oil-well cements. Specifically, SiO2 was coated onto the surface of polyvinyl alcohol fiber (PVAF) as its silicon source via a sol-gel process by using tetraethyl orthosilicate (TEOS), while hydrochloric acid and ammonia were respectively used as the catalyst in the sol (hydrolysis) and the gel (condensation) processes. The PVAF microstructure was then characterized with the scanning electron microscope (SEM), while the effects of the modified PVAF on both mechanical and rheological properties of oil-well cements were examined. Due to the fact that SiO2 can be uniformly coated onto the PVAF surface, such modified PVAF can slightly improve the rheology of the cement slurry, while the raw PVAF exhibits poor dispersion at a high dosage. Compared with those of cement stone without PVAF after curing for 28 days at 60 °C, the flexural strength, compressive strength, and elastic modulus of the cement stone incorporated with the modified PVAFs were enhanced by 37.7%, 66.1%, and 50.0%, respectively. The SEM test (EDX) test, XRD test, and thermogravimetric test prove that the SiO2 coating on the PVAF surface can promote the hydration of cement clinker and can react with Ca(OH)2 to generate CSH gel. The SiO2 grafted onto the surface of PVAFs can improve the bond strength at the fiber/cement matrix interface, thus improving the mechanical properties of cement stone.
Open AccessAn Investigation into PVA Fiber Modified with SiO2 for Improving Mechanical Properties of Oil-Well Cements
In this paper, we conduct a comprehensive investigation into PVA fiber modified with SiO2 to improve the mechanical properties of oil-well cements. Specifically, SiO2 was coated onto the surface of polyvinyl alcohol fiber (PVAF) as its silicon source via a sol-gel process by using tetraethyl orthosilicate (TEOS), while hydrochloric acid and ammonia were respectively used as the catalyst in the sol (hydrolysis) and the gel (condensation) processes. The PVAF microstructure was then characterized with the scanning electron microscope (SEM), while the effects of the modified PVAF on both mechanical and rheological properties of oil-well cements were examined. Due to the fact that SiO2 can be uniformly coated onto the PVAF surface, such modified PVAF can slightly improve the rheology of the cement slurry, while the raw PVAF exhibits poor dispersion at a high dosage. Compared with those of cement stone without PVAF after curing for 28 days at 60 °C, the flexural strength, compressive strength, and elastic modulus of the cement stone incorporated with the modified PVAFs were enhanced by 37.7%, 66.1%, and 50.0%, respectively. The SEM test (EDX) test, XRD test, and thermogravimetric test prove that the SiO2 coating on the PVAF surface can promote the hydration of cement clinker and can react with Ca(OH)2 to generate CSH gel. The SiO2 grafted onto the surface of PVAFs can improve the bond strength at the fiber/cement matrix interface, thus improving the mechanical properties of cement stone.
- Open Access
Theoretical and Experimental Study on Cementing Displacement Interface for Highly Deviated Wells
An effective drilling fluid removal is necessary to achieve an efficient cementing in oil and gas industry, i.e., it is ideal that all the drilling fluid is displaced by the cement slurry. The displacement efficiency is closely related to the stability and development of the displacing interface between the cementing slurry and drilling fluid. Thus, an effective cementing requires a validated theoretical model to describe the displacing interface to guide cementing applications, especially for highly deviated wells. The current studies suffer from a lack of experimental validation for proposed models. In this study, a theoretical model of cementing interfacial displacement in eccentric annulus is established. An experimental study is conducted to examine effects of well inclination, eccentricity and fluid properties on the stability of displacement interface to verify the theoretical model. The model is found to well describe the interface in the eccentric annulus, and it is applicable to the wellbore annulus with different inclination angles. The results show that: the displacement interface gradually extends (i.e., length is increased) with the increase of well inclination; the cement displacement effect became worse with deviation angle under the same injection and replacement conditions. Increasing the apparent viscosity of cement slurry is beneficial to improve the stability of displacement interface. In highly deviated wells, a certain casing eccentricity can inhibit the penetration of cement slurry in the wide gap of the low side of the annulus, which is conducive to maintaining the stability of the displacement interface.
Open AccessTheoretical and Experimental Study on Cementing Displacement Interface for Highly Deviated Wells
An effective drilling fluid removal is necessary to achieve an efficient cementing in oil and gas industry, i.e., it is ideal that all the drilling fluid is displaced by the cement slurry. The displacement efficiency is closely related to the stability and development of the displacing interface between the cementing slurry and drilling fluid. Thus, an effective cementing requires a validated theoretical model to describe the displacing interface to guide cementing applications, especially for highly deviated wells. The current studies suffer from a lack of experimental validation for proposed models. In this study, a theoretical model of cementing interfacial displacement in eccentric annulus is established. An experimental study is conducted to examine effects of well inclination, eccentricity and fluid properties on the stability of displacement interface to verify the theoretical model. The model is found to well describe the interface in the eccentric annulus, and it is applicable to the wellbore annulus with different inclination angles. The results show that: the displacement interface gradually extends (i.e., length is increased) with the increase of well inclination; the cement displacement effect became worse with deviation angle under the same injection and replacement conditions. Increasing the apparent viscosity of cement slurry is beneficial to improve the stability of displacement interface. In highly deviated wells, a certain casing eccentricity can inhibit the penetration of cement slurry in the wide gap of the low side of the annulus, which is conducive to maintaining the stability of the displacement interface.
- Open Access
Resource Utilization of Red Mud from the Solid Waste of Aluminum Industry Used in Geothermal Wells
It is difficult for the commonly used Class G oil well cement to withstand the high-temperature environment of geothermal wells, and it is easy to deteriorate the mechanical properties and damage the integrity of the cement sheath. Industrial solid waste red mud can be used as supplementary cementing materials (SCMs) to improve its mechanical properties at high temperatures. In addition, compared to Class G oil well cement, high belite cement (HBC) has lower energy consumption and better mechanical properties at high temperatures. In this study, the mechanical properties of HBC as a gel material and quartz sand and red mud as SCMs were studied at high temperatures. The ratio of HBC to SCMs and the ratio of quartz sand to red mud in SCMs were optimized using the response surface method (RSM). The response surface was established using the three-level factorial design model, which fit well with the experimental data. The optimization results show that the best mass ratio of SCMs/HBC is 37.5% and that the best quality ratio of quartz sand/red mud is 9 under the curing conditions of 180 °C. However, the best mass ratio of SCMs/HBC is 49.3%, and the best quality ratio of quartz sand/red mud is 7 under 220 °C. With the addition of SCMs, the silicon-to-calcium ratio of HBC hydration products decreases, and high-temperature-stable xonotlite and tobermorite can be formed. After adding SCMs, the cement sample is denser without obvious cracks.
Open AccessResource Utilization of Red Mud from the Solid Waste of Aluminum Industry Used in Geothermal Wells
It is difficult for the commonly used Class G oil well cement to withstand the high-temperature environment of geothermal wells, and it is easy to deteriorate the mechanical properties and damage the integrity of the cement sheath. Industrial solid waste red mud can be used as supplementary cementing materials (SCMs) to improve its mechanical properties at high temperatures. In addition, compared to Class G oil well cement, high belite cement (HBC) has lower energy consumption and better mechanical properties at high temperatures. In this study, the mechanical properties of HBC as a gel material and quartz sand and red mud as SCMs were studied at high temperatures. The ratio of HBC to SCMs and the ratio of quartz sand to red mud in SCMs were optimized using the response surface method (RSM). The response surface was established using the three-level factorial design model, which fit well with the experimental data. The optimization results show that the best mass ratio of SCMs/HBC is 37.5% and that the best quality ratio of quartz sand/red mud is 9 under the curing conditions of 180 °C. However, the best mass ratio of SCMs/HBC is 49.3%, and the best quality ratio of quartz sand/red mud is 7 under 220 °C. With the addition of SCMs, the silicon-to-calcium ratio of HBC hydration products decreases, and high-temperature-stable xonotlite and tobermorite can be formed. After adding SCMs, the cement sample is denser without obvious cracks.
- Open Access
A Study on the Integrity Evaluation of Cement Sheaths for Deep Wells in Deep Water
The complex temperature and pressure conditions of deepwater wells have a serious impact on cementing quality. Therefore, the integrity of the cement seal becomes a critical factor that can restrict the safety of the wellbore, especially for wells ranging from the conventional deep water to deep water with more prominent deep stratum problems. The operating conditions of deep wells in deep water (referred as the dual-deep well) are complex and harsh. For the conventional evaluation device, it is difficult to accurately simulate the alternating HTHP conditions and to clarify the location and situation of the cement sheath leakage, which directly leads to the deviation of the evaluation results from the engineering reality. To solve this defect, based on the condition and structure characteristics of dual-deep wells, a device and method for casing/cement sheath/formation seal integrity evaluation for dual-deep wells at HTHP has been developed and established. Combined with the analysis of microstructure and micromorphology, the sealing ability and integrity of different cement slurry systems were evaluated. Through this study, a set of cement slurry systems suitable for dual-deep wells is selected that can satisfy the requirements of dual-deep wells with excellent isolation ability and seal integrity under temperature and stress changes. The research results provide a reference for deepwater wells’ wellbore integrity evaluation and research.
Open AccessA Study on the Integrity Evaluation of Cement Sheaths for Deep Wells in Deep Water
The complex temperature and pressure conditions of deepwater wells have a serious impact on cementing quality. Therefore, the integrity of the cement seal becomes a critical factor that can restrict the safety of the wellbore, especially for wells ranging from the conventional deep water to deep water with more prominent deep stratum problems. The operating conditions of deep wells in deep water (referred as the dual-deep well) are complex and harsh. For the conventional evaluation device, it is difficult to accurately simulate the alternating HTHP conditions and to clarify the location and situation of the cement sheath leakage, which directly leads to the deviation of the evaluation results from the engineering reality. To solve this defect, based on the condition and structure characteristics of dual-deep wells, a device and method for casing/cement sheath/formation seal integrity evaluation for dual-deep wells at HTHP has been developed and established. Combined with the analysis of microstructure and micromorphology, the sealing ability and integrity of different cement slurry systems were evaluated. Through this study, a set of cement slurry systems suitable for dual-deep wells is selected that can satisfy the requirements of dual-deep wells with excellent isolation ability and seal integrity under temperature and stress changes. The research results provide a reference for deepwater wells’ wellbore integrity evaluation and research.
- Open Access
- 28 January 2022
- Published by Frontiers Media SA in Frontiers in Materials
- Vol. 8
Research on the Mechanical Integrity of Low-Density Cement Mortar
Poor mechanical integrity of cement sheaths during the production of oil and gas wells may cause air channeling and water channeling issues in the wells, leading to severe safety problems, and adversely affecting the safety and efficiency of the oil and gas resources production. This article focuses on a low-density cement slurry system with added floating beads. The compressive strength and flexural strength of cement stones, the mechanical integrity of cement rings, and triaxial mechanical properties were assessed. The optimal dosage of floating beads and the evolution of the cement stone’s mechanical properties and deformation ability were discussed. Bonding strengths of the first and the second interfaces were evaluated using the shrinkage test results of the cement mortar. Finally, the microscopic mechanism of the change in mechanical properties was analyzed by scanning electron microscopy. The results showed that the cement mortar exhibited the best compressive strength, mechanical integrity, and deformability after blending with 15% floating beads. At the same time, the volume shrinkage of the cement mortar mixed with 15% floating beads was the smallest, only 0.00667%, plausibly indicating good bonding with a casing and the formation to reduce the occurrence of gas channeling. Finally, the microscopic test of the cement mortar showed that the bonding between floating beads and cement was not tight, so internal cracks in the cement easily developed along the bonding part of cement and floating beads. The more floating beads were mixed, the more likely was cement mortar destroyed.
- 28 January 2022
- Published by Frontiers Media SA in Frontiers in Materials
- Vol. 8
Open AccessResearch on the Mechanical Integrity of Low-Density Cement Mortar
Poor mechanical integrity of cement sheaths during the production of oil and gas wells may cause air channeling and water channeling issues in the wells, leading to severe safety problems, and adversely affecting the safety and efficiency of the oil and gas resources production. This article focuses on a low-density cement slurry system with added floating beads. The compressive strength and flexural strength of cement stones, the mechanical integrity of cement rings, and triaxial mechanical properties were assessed. The optimal dosage of floating beads and the evolution of the cement stone’s mechanical properties and deformation ability were discussed. Bonding strengths of the first and the second interfaces were evaluated using the shrinkage test results of the cement mortar. Finally, the microscopic mechanism of the change in mechanical properties was analyzed by scanning electron microscopy. The results showed that the cement mortar exhibited the best compressive strength, mechanical integrity, and deformability after blending with 15% floating beads. At the same time, the volume shrinkage of the cement mortar mixed with 15% floating beads was the smallest, only 0.00667%, plausibly indicating good bonding with a casing and the formation to reduce the occurrence of gas channeling. Finally, the microscopic test of the cement mortar showed that the bonding between floating beads and cement was not tight, so internal cracks in the cement easily developed along the bonding part of cement and floating beads. The more floating beads were mixed, the more likely was cement mortar destroyed.
- Open Access
- 5 January 2022
- Published by Frontiers Media SA in Frontiers in Materials
- Vol. 8
Improvement of Calcium Aluminate Cement Containing Blast Furnace Slag at 50°C and 315°C
During the thermal recovery of heavy oil thermal recovery wells, improving the mechanical properties and integrity of the cement ring is of great significance for the safe and efficient exploitation of heavy oil resources. This paper studies the relative properties of calcium aluminate cement and three kinds of slags under the conditions of 50°C × 1.01 MPa and 315°C × 20.7 MPa. CAC-slag composite material performance was evaluated using the cement paste compressive strength and permeability tests to study the physical properties of CAC with blast furnace slag. X-ray diffraction analysis, scanning electron microscopy (SEM), and thermal analysis (DSC/TG) were carried out to investigate the mineralogical composition of CAC with blast furnace slag. Results show that adding blast furnace slag did not affect the performance of cement slurry. Moreover, C2ASH8 curing occurred at low temperature, the microstructure of CAC paste was compact, and the permeability resistance was improved, thus improving the low-temperature properties of neat CAC. When cured at a high temperature, the CAC paste was mainly hydrated with C3ASH4 and AlO(OH), which had a well-developed crystal structure. Adding blast furnace slag can improve the CAC resistance to high temperature.
- 5 January 2022
- Published by Frontiers Media SA in Frontiers in Materials
- Vol. 8
Open AccessImprovement of Calcium Aluminate Cement Containing Blast Furnace Slag at 50°C and 315°C
During the thermal recovery of heavy oil thermal recovery wells, improving the mechanical properties and integrity of the cement ring is of great significance for the safe and efficient exploitation of heavy oil resources. This paper studies the relative properties of calcium aluminate cement and three kinds of slags under the conditions of 50°C × 1.01 MPa and 315°C × 20.7 MPa. CAC-slag composite material performance was evaluated using the cement paste compressive strength and permeability tests to study the physical properties of CAC with blast furnace slag. X-ray diffraction analysis, scanning electron microscopy (SEM), and thermal analysis (DSC/TG) were carried out to investigate the mineralogical composition of CAC with blast furnace slag. Results show that adding blast furnace slag did not affect the performance of cement slurry. Moreover, C2ASH8 curing occurred at low temperature, the microstructure of CAC paste was compact, and the permeability resistance was improved, thus improving the low-temperature properties of neat CAC. When cured at a high temperature, the CAC paste was mainly hydrated with C3ASH4 and AlO(OH), which had a well-developed crystal structure. Adding blast furnace slag can improve the CAC resistance to high temperature.