Yinan Xiao
Research Subjects
Yinan Xiao has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
- Liyuan Sheng
Shenzhen Institute, Peking University, Shenzhen 518057, China
2 shared publications - Di Wu
PKU-HKUST Shenzhen-HongKong Institution, Shenzhen 518057, China
1 shared publication - Fang Yang
Shenzhen AirlinesShenzhen Bao’an International Airport, Shenzhen 518128, China
1 shared publication - Hongyang Lin
Department of Mechanical and Aerospace Engineering, The Hong Kong University of Science and Technology, Hong Kong, China
1 shared publication - Peng Hua
School of Science, Harbin Institute of Technology, Shenzhen, China
1 shared publication - Qiaoli Wang
PKU-HKUST Shenzhen-HongKong Institution, Shenzhen 518057, China
1 shared publication
Latest Publications
- 11 April 2024
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- Vol. 69 (1) , 181-187
Microstructure, Compressive Properties and Oxidation Behaviors of the Nb-Si-Ti-Cr-Al-Ta-Hf Alloy with Minor Holmium Addition
In the present research, the Nb-Si-Ti-Cr-Al-Ta-Hf alloys with different Ho addition were prepared. Their microstructure, compressive properties and oxidation behaviors were investigated preliminarily. The results exhibit that the Nb-Si-Ti-Cr-Al-Ta-Hf alloy has coarse microstructure which is mainly composed of Nb solid solution, Nb5Si3 and Ti5Si3 phases. The minor Ho addition could refine the microstructure and suppress the precipitation of Ti5Si3 phase. Moreover, the Ho addition also leads to the formation of Ho2Hf2O7, which prefers to precipitate along the Nbss/Nb5Si3 phase interface. Compared with the Nb-Si-Ti-Cr-Al-Ta-Hf alloy, the minor Ho addition improves the room-temperature and high-temperature compressive properties of the alloy. Its room-temperature compressive strength and ductility obtain the maximum value of 1825 MPa and 16.5% when the Ho content is 0.1 at.%. Moreover, its best compressive strength at 873 K, 1273 K and 1473 K is 1495 MPa, 765 MPa and 380 MPa, respectively, when the Ho addition is 0.1 at.%. The oxidation behavior of the Nb-Si-Ti-Cr-Al-Ta-Hf alloy is diversified with the Ho addition. The oxidation rate of the alloy with 0.1 at.% Ho addition is the lowest while the alloy with 0.2 at.% Ho addition is the highest. Therefore, the 0.1 at.% Ho would be the appropriate content for the Nb-Si-Ti-Cr-Al-Ta-Hf alloy.
- 11 April 2024
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- Vol. 69 (1) , 181-187
Microstructure, Compressive Properties and Oxidation Behaviors of the Nb-Si-Ti-Cr-Al-Ta-Hf Alloy with Minor Holmium Addition
In the present research, the Nb-Si-Ti-Cr-Al-Ta-Hf alloys with different Ho addition were prepared. Their microstructure, compressive properties and oxidation behaviors were investigated preliminarily. The results exhibit that the Nb-Si-Ti-Cr-Al-Ta-Hf alloy has coarse microstructure which is mainly composed of Nb solid solution, Nb5Si3 and Ti5Si3 phases. The minor Ho addition could refine the microstructure and suppress the precipitation of Ti5Si3 phase. Moreover, the Ho addition also leads to the formation of Ho2Hf2O7, which prefers to precipitate along the Nbss/Nb5Si3 phase interface. Compared with the Nb-Si-Ti-Cr-Al-Ta-Hf alloy, the minor Ho addition improves the room-temperature and high-temperature compressive properties of the alloy. Its room-temperature compressive strength and ductility obtain the maximum value of 1825 MPa and 16.5% when the Ho content is 0.1 at.%. Moreover, its best compressive strength at 873 K, 1273 K and 1473 K is 1495 MPa, 765 MPa and 380 MPa, respectively, when the Ho addition is 0.1 at.%. The oxidation behavior of the Nb-Si-Ti-Cr-Al-Ta-Hf alloy is diversified with the Ho addition. The oxidation rate of the alloy with 0.1 at.% Ho addition is the lowest while the alloy with 0.2 at.% Ho addition is the highest. Therefore, the 0.1 at.% Ho would be the appropriate content for the Nb-Si-Ti-Cr-Al-Ta-Hf alloy.
- Open Access
- 1 December 2022
- Published by AIP Publishing in AIP Advances
- Vol. 12 (12) , 125202
Elastocaloric effect characterization of a NiTi tube to be applied in a compressive cooler
In this article, the elastocaloric effect of a commercial superelastic NiTi shape memory alloy (SMA) tube (with an outer diameter of 5 mm and wall thickness of 1 mm) to be applied in a compressive cooler was measured and analyzed. The elastocaloric effect of the tube was measured vs the applied strain and strain rate. The largest temperature changes of 21 K during loading and 16 K during unloading were measured at an applied strain of 3.30% and strain rate of 0.33 s−1. In the fatigue testing of the sample, only 0.20% of the residual strain accumulated after a runout of 1 × 106 sinusoidal force-controlled loading–unloading cycles at a maximum compressive stress of 1100 MPa and frequency of 20 Hz. Numerical results of the cooling characteristics of a compressive device using a single NiTi tube with the above-mentioned cross section and an aspect ratio of 60:1 as the refrigerant showed that the device could produce a total cooling power of up to 20 W and a coefficient of performance of up to 6.5. The results of this article demonstrate that superelastic NiTi SMA tubes of suitable wall thickness and aspect ratios are good candidates to be applied in a compressive elastocaloric cooler.
- 1 December 2022
- Published by AIP Publishing in AIP Advances
- Vol. 12 (12) , 125202
Open AccessElastocaloric effect characterization of a NiTi tube to be applied in a compressive cooler
In this article, the elastocaloric effect of a commercial superelastic NiTi shape memory alloy (SMA) tube (with an outer diameter of 5 mm and wall thickness of 1 mm) to be applied in a compressive cooler was measured and analyzed. The elastocaloric effect of the tube was measured vs the applied strain and strain rate. The largest temperature changes of 21 K during loading and 16 K during unloading were measured at an applied strain of 3.30% and strain rate of 0.33 s−1. In the fatigue testing of the sample, only 0.20% of the residual strain accumulated after a runout of 1 × 106 sinusoidal force-controlled loading–unloading cycles at a maximum compressive stress of 1100 MPa and frequency of 20 Hz. Numerical results of the cooling characteristics of a compressive device using a single NiTi tube with the above-mentioned cross section and an aspect ratio of 60:1 as the refrigerant showed that the device could produce a total cooling power of up to 20 W and a coefficient of performance of up to 6.5. The results of this article demonstrate that superelastic NiTi SMA tubes of suitable wall thickness and aspect ratios are good candidates to be applied in a compressive elastocaloric cooler.