Dorian P. Luccioni
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Dorian P. Luccioni has a total of 59 co-authors. Here are the top co-authors by number of shared publications:
- Kenny Huynh
University of California, Los Angeles
3 shared publications - Mark S. Goorsky
University of California, Los Angeles
3 shared publications - Michael E. Liao
University of California, Los Angeles
3 shared publications - Leora Dresselhaus-Marais
Department of Materials Science and Engineering, Stanford University, Stanford, CA 94305, USA
2 shared publications - Michael Wojcik
Advanced Photon Source, Argonne National Laboratory, Lemont, IL 60439, USA
2 shared publications - Xianrong Huang
Advanced Photon Source, Argonne National Laboratory, Lemont, IL 60439, USA
2 shared publications
Latest Publications
- Open Access
- 18 September 2026
- Published by American Association for the Advancement of Science (AAAS) in Science Advances
- Vol. 12 (38)
Ultrahigh flow strength in shocked nanopolycrystalline diamond
Extreme pressures and temperatures create conditions that allow even hard and brittle materials to flow plastically. Despite extensive research, the limits of flow strength under such conditions remain uncertain, and the mechanisms driving deformation at the relevant stresses are a subject of debate. Using femtosecond in situ x-ray diffraction experiments and large-scale molecular dynamics simulations, we demonstrate that stacking fault-mediated strengthening enables shock-compressed nanopolycrystalline diamond to achieve a peak flow strength of 92 ± 3 GPa at a stress of 212 ± 6 GPa. Our findings show that extreme conditions can unlock ultrahigh strength via a complex array of competing deformation mechanisms and thermodynamic effects.
- 18 September 2026
- Published by American Association for the Advancement of Science (AAAS) in Science Advances
- Vol. 12 (38)
Open AccessUltrahigh flow strength in shocked nanopolycrystalline diamond
Extreme pressures and temperatures create conditions that allow even hard and brittle materials to flow plastically. Despite extensive research, the limits of flow strength under such conditions remain uncertain, and the mechanisms driving deformation at the relevant stresses are a subject of debate. Using femtosecond in situ x-ray diffraction experiments and large-scale molecular dynamics simulations, we demonstrate that stacking fault-mediated strengthening enables shock-compressed nanopolycrystalline diamond to achieve a peak flow strength of 92 ± 3 GPa at a stress of 212 ± 6 GPa. Our findings show that extreme conditions can unlock ultrahigh strength via a complex array of competing deformation mechanisms and thermodynamic effects.
- Open Access
- 21 November 2025
- Published by American Chemical Society (ACS) in ChemRxiv
Imaging Hydrogen’s Effect on Single Crystal Austenitic Stainless Steel Microstructure using Dark-Field X-Ray Microscopy
Hydrogen embrittlement severely degrades mechanical properties of austenitic stainless steels (γ-SS), yet the bulk deformation microstructures responsible for this phenomenon have not been directly observed. While the internal microstructure is essential to define metal plasticity, deformation, and fracture, no technique has been able to image the deep subsurface structure. In this work, we use dark-field X-ray microscopy (DFXM) to compare the structure of an annealed single crystal γ-SS sample to one with the same annealing conditions and subsequently hydrogen pre-charged in a high pressure and temperature environment. While the non-charged sample exhibited features characteristic of dislocations packed into boundaries, the pre-charged sample showed diffuse features with a distinctly broader rocking curve characteristic of a higher geometrically necessary dislocation (GND) density. Our results demonstrate the utility of DFXM to characterize the unique subsurface microstructures, offering opportunities for future studies to resolve how these features cause fracture or embrittlement.
- 21 November 2025
- Published by American Chemical Society (ACS) in ChemRxiv
Open AccessImaging Hydrogen’s Effect on Single Crystal Austenitic Stainless Steel Microstructure using Dark-Field X-Ray Microscopy
Hydrogen embrittlement severely degrades mechanical properties of austenitic stainless steels (γ-SS), yet the bulk deformation microstructures responsible for this phenomenon have not been directly observed. While the internal microstructure is essential to define metal plasticity, deformation, and fracture, no technique has been able to image the deep subsurface structure. In this work, we use dark-field X-ray microscopy (DFXM) to compare the structure of an annealed single crystal γ-SS sample to one with the same annealing conditions and subsequently hydrogen pre-charged in a high pressure and temperature environment. While the non-charged sample exhibited features characteristic of dislocations packed into boundaries, the pre-charged sample showed diffuse features with a distinctly broader rocking curve characteristic of a higher geometrically necessary dislocation (GND) density. Our results demonstrate the utility of DFXM to characterize the unique subsurface microstructures, offering opportunities for future studies to resolve how these features cause fracture or embrittlement.
- Open Access
- 1 November 2025
- Published by AIP Publishing in APL Materials
- Vol. 13 (11)
Crack formation in strained β-(AlxGa1−x)2O3 films grown on (010) β-Ga2O3 substrates
The cracking and local strain relaxation in (010) (AlxGa1−x)2O3 films grown on Ga2O3 substrates are assessed in terms of film composition and thickness. We utilize x-ray diffraction and electron microscopy techniques combined with simulation and modeling to investigate that film cracking on curvature (flatness) has a directly proportional relationship with film thickness and/or aluminum content. Cross section transmission electron microscopy reveals that cracks along both the (001) and (100) cleavage planes penetrate into the substrate. The diffuse scattered intensity observed in reciprocal space maps (RSMs) is directly correlated with the tilt that is introduced due to the change in the deformation conditions near the cracks. While asymmetric RSMs show that the layers are fully strained, the diffuse scattering distribution in reciprocal space can be interpreted to show that the cracking relaxes and locally tilts the lattice ∼350 nm from the crack edges, which is consistent with the larger radius of curvature associated with the films with higher crack densities. For example, a 200 nm (Al0.13Ga0.87)2O3 thick film has an average inter-crack spacing of 3.3 µm, so most of the epitaxial layer is fully strained except near the cracks where it deforms elastically and is consistent with the gallium oxide Poisson ratio. A reciprocal space model was developed, which imports the strain and tilt distributions (based on finite element modeling) to match the features observed in the experimental maps. We also note that previous studies involving (AlxGa1−x)2O3 films may show evidence of cracking as observed in their symmetric and asymmetric RSMs.
- 1 November 2025
- Published by AIP Publishing in APL Materials
- Vol. 13 (11)
Open AccessCrack formation in strained β-(AlxGa1−x)2O3 films grown on (010) β-Ga2O3 substrates
The cracking and local strain relaxation in (010) (AlxGa1−x)2O3 films grown on Ga2O3 substrates are assessed in terms of film composition and thickness. We utilize x-ray diffraction and electron microscopy techniques combined with simulation and modeling to investigate that film cracking on curvature (flatness) has a directly proportional relationship with film thickness and/or aluminum content. Cross section transmission electron microscopy reveals that cracks along both the (001) and (100) cleavage planes penetrate into the substrate. The diffuse scattered intensity observed in reciprocal space maps (RSMs) is directly correlated with the tilt that is introduced due to the change in the deformation conditions near the cracks. While asymmetric RSMs show that the layers are fully strained, the diffuse scattering distribution in reciprocal space can be interpreted to show that the cracking relaxes and locally tilts the lattice ∼350 nm from the crack edges, which is consistent with the larger radius of curvature associated with the films with higher crack densities. For example, a 200 nm (Al0.13Ga0.87)2O3 thick film has an average inter-crack spacing of 3.3 µm, so most of the epitaxial layer is fully strained except near the cracks where it deforms elastically and is consistent with the gallium oxide Poisson ratio. A reciprocal space model was developed, which imports the strain and tilt distributions (based on finite element modeling) to match the features observed in the experimental maps. We also note that previous studies involving (AlxGa1−x)2O3 films may show evidence of cracking as observed in their symmetric and asymmetric RSMs.
- Open Access
- 8 May 2023
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 133 (18)
Origins of epitaxial macro-terraces and macro-steps on GaN substrates
Localized lattice distortions in GaN substrates can serve as nucleation sites for epitaxial macro-steps and macro-terraces. These detrimental macro-scale features give rise to optically hazy homoepitaxial GaN surfaces. After nucleating, these macro-features grow laterally along the surface and coalesce, leading to significant coverage of the wafer surface. Dot-core GaN substrates consisting of a periodic array of cores were used as a defect-engineered system, where dislocations are intentionally concentrated at the cores. The high density of threading dislocations at the cores induced localized lattice distortions. These distortions are associated predominantly with lattice tilt on the order of hundreds of arcsec across ∼0.5 mm laterally along the wafer surface. The resulting macro-features that nucleated at these localized distorted sites were made up of macro-terraces with lengths ranging ∼30–∼150 μm and macro-step heights ranging ∼200–∼400 nm. Another source of localized distortion was threading screw dislocations or GaN nanopipes that resulted in spiral growth and hillock formation. Based on x-ray topography and optical microscopy measurements, we speculate that the coalescence of hillocks evolves into macro-terraces and macro-steps. While previous studies focused on the substrate miscut as a means to control macro-feature formation, we show that localized lattice tilt from defects is another important contributor to macro-feature formation.
- 8 May 2023
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 133 (18)
Open AccessOrigins of epitaxial macro-terraces and macro-steps on GaN substrates
Localized lattice distortions in GaN substrates can serve as nucleation sites for epitaxial macro-steps and macro-terraces. These detrimental macro-scale features give rise to optically hazy homoepitaxial GaN surfaces. After nucleating, these macro-features grow laterally along the surface and coalesce, leading to significant coverage of the wafer surface. Dot-core GaN substrates consisting of a periodic array of cores were used as a defect-engineered system, where dislocations are intentionally concentrated at the cores. The high density of threading dislocations at the cores induced localized lattice distortions. These distortions are associated predominantly with lattice tilt on the order of hundreds of arcsec across ∼0.5 mm laterally along the wafer surface. The resulting macro-features that nucleated at these localized distorted sites were made up of macro-terraces with lengths ranging ∼30–∼150 μm and macro-step heights ranging ∼200–∼400 nm. Another source of localized distortion was threading screw dislocations or GaN nanopipes that resulted in spiral growth and hillock formation. Based on x-ray topography and optical microscopy measurements, we speculate that the coalescence of hillocks evolves into macro-terraces and macro-steps. While previous studies focused on the substrate miscut as a means to control macro-feature formation, we show that localized lattice tilt from defects is another important contributor to macro-feature formation.
- Open Access
- 1 January 2023
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 41 (1)
Optimization of chemical mechanical polishing of (010) β-Ga2O3
Smooth (< 0.5 nm rms) and subsurface damage-free (010) β-Ga2O3 was achieved with low-pressure chemical mechanical polishing. An applied pressure of 1 kPa along with colloidal silica and poromeric polyurethane polishing pads rotating at 30 rpm was found to be the optimal polishing parameters for (010) β-Ga2O3. Using higher pressures typically employed in the current literature induced subsurface damage in the substrates. Diffuse scatter intensity of triple-axis x-ray rocking curves was used to determine the presence of subsurface lattice damage, which was quantified by measuring peak widths below the half maximum (i.e., FWXM where X < 0.5). The initially rough surfaces of (010) β-Ga2O3 substrates due to wafer slicing and grinding were lapped and polished. A 5 μm Al2O3 slurry followed by a 0.3 μm Al2O3 slurry was used as the primary lap material removal step. The material removal rates were ∼20 and ∼9 μm/h, respectively. Then, chemical mechanical polishing was performed using colloidal alumina followed by colloidal silica. The removal rates were ∼1.3 and ∼0.4 μm/h, respectively. Only colloidal silica showed the complete removal of subsurface damage. The final (020) β-Ga2O3 rocking curve FWHM was ∼13″ and FW(0.001)M was ∼120″, which matches the widths of commercially available pristine (010) β-Ga2O3. A final cleaning step using dilute bleach and dilute citric acid to remove residual silica slurry particles from the surface was demonstrated.
- 1 January 2023
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 41 (1)
Open AccessOptimization of chemical mechanical polishing of (010) β-Ga2O3
Smooth (< 0.5 nm rms) and subsurface damage-free (010) β-Ga2O3 was achieved with low-pressure chemical mechanical polishing. An applied pressure of 1 kPa along with colloidal silica and poromeric polyurethane polishing pads rotating at 30 rpm was found to be the optimal polishing parameters for (010) β-Ga2O3. Using higher pressures typically employed in the current literature induced subsurface damage in the substrates. Diffuse scatter intensity of triple-axis x-ray rocking curves was used to determine the presence of subsurface lattice damage, which was quantified by measuring peak widths below the half maximum (i.e., FWXM where X < 0.5). The initially rough surfaces of (010) β-Ga2O3 substrates due to wafer slicing and grinding were lapped and polished. A 5 μm Al2O3 slurry followed by a 0.3 μm Al2O3 slurry was used as the primary lap material removal step. The material removal rates were ∼20 and ∼9 μm/h, respectively. Then, chemical mechanical polishing was performed using colloidal alumina followed by colloidal silica. The removal rates were ∼1.3 and ∼0.4 μm/h, respectively. Only colloidal silica showed the complete removal of subsurface damage. The final (020) β-Ga2O3 rocking curve FWHM was ∼13″ and FW(0.001)M was ∼120″, which matches the widths of commercially available pristine (010) β-Ga2O3. A final cleaning step using dilute bleach and dilute citric acid to remove residual silica slurry particles from the surface was demonstrated.