James T. Burns
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
James T. Burns has a total of 34 co-authors. Here are the top co-authors by number of shared publications:
- Zachary D. Harris
Department of Mechanical Engineering and Materials Science, University of Pittsburgh, Pittsburgh, PA, USA
7 shared publications - John Robert Scully
University of Virginia
4 shared publications - Matthew E. McMahon
Center for Electrochemical Science and Engineering, Department of Materials Science and Engineering, University of Virginia, Charlottesville, VA 22904
4 shared publications - Robert G. Kelly
Center for Electrochemical Science and Engineering, Department of Materials Science and Engineering, University of Virginia, Charlottesville, Virginia 22904, United States of America
4 shared publications Richard P. Gangloff
University of Virginia
2 shared publications- A. Pandaleon
**Department of Materials Science and Engineering, University of Virginia, Charlottesville, Virginia 22904
1 shared publication
Latest Publications
- 1 October 2025
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 81  (11) , 1062-1075
Mitigation of Environmental-Assisted Cracking in Martensitic Stainless Steel via ZnNi Plating in Sodium Chloride Solution
The impact of galvanic coupling on the environmental-assisted cracking (EAC) resistance of a martensitic stainless steel (P675) was evaluated by the introduction of a ZnNi electrodeposit during fracture mechanics testing. The influence of ZnNi galvanic coupling on EAC behavior was studied under both constant stress intensity K (dK/dt = 0 MPa√m/h) and rising K (dK/dt = 4 MPa√m/h) conditions in 0.6 M NaCl. For constant K, the ZnNi anode was galvanically coupled to the steel via a zero-resistance ammeter, and both small and large area ratios of ZnNi to P675 steel were examined across different exposure durations. The results showed that even a small anode-to-cathode area ratio (∼1:1,000) was effective in reducing the crack growth rate, depending on exposure time. Shorter exposure durations (e.g., 90 min) led to reduced crack propagation, whereas longer exposures (up to 800 min) further mitigated EAC under small-area galvanic coupling conditions. This improvement was attributed to the electrochemical potential generated by the galvanic coupling, which remained within the immunity well throughout the immersion time. In contrast, the large area ratio (∼6:1) did not initiate EAC, even when the potential was outside the immunity well. This unexpected suppression of cracking is attributed to Zn2+ ions released from ZnNi, which appear to counteract the electrochemical driving force for crack initiation and propagation. To validate this, ZnNi coatings with small area ratios (∼1:1,000) were directly applied to the P675 steel surface, and fracture mechanics testing was conducted under rising K conditions. The results demonstrated that ZnNi continued to suppress EAC even under increasing crack-driving force, confirming that controlled galvanic coupling can effectively enhance crack resistance in martensitic stainless steel.
- 1 October 2025
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 81  (11) , 1062-1075
Mitigation of Environmental-Assisted Cracking in Martensitic Stainless Steel via ZnNi Plating in Sodium Chloride Solution
The impact of galvanic coupling on the environmental-assisted cracking (EAC) resistance of a martensitic stainless steel (P675) was evaluated by the introduction of a ZnNi electrodeposit during fracture mechanics testing. The influence of ZnNi galvanic coupling on EAC behavior was studied under both constant stress intensity K (dK/dt = 0 MPa√m/h) and rising K (dK/dt = 4 MPa√m/h) conditions in 0.6 M NaCl. For constant K, the ZnNi anode was galvanically coupled to the steel via a zero-resistance ammeter, and both small and large area ratios of ZnNi to P675 steel were examined across different exposure durations. The results showed that even a small anode-to-cathode area ratio (∼1:1,000) was effective in reducing the crack growth rate, depending on exposure time. Shorter exposure durations (e.g., 90 min) led to reduced crack propagation, whereas longer exposures (up to 800 min) further mitigated EAC under small-area galvanic coupling conditions. This improvement was attributed to the electrochemical potential generated by the galvanic coupling, which remained within the immunity well throughout the immersion time. In contrast, the large area ratio (∼6:1) did not initiate EAC, even when the potential was outside the immunity well. This unexpected suppression of cracking is attributed to Zn2+ ions released from ZnNi, which appear to counteract the electrochemical driving force for crack initiation and propagation. To validate this, ZnNi coatings with small area ratios (∼1:1,000) were directly applied to the P675 steel surface, and fracture mechanics testing was conducted under rising K conditions. The results demonstrated that ZnNi continued to suppress EAC even under increasing crack-driving force, confirming that controlled galvanic coupling can effectively enhance crack resistance in martensitic stainless steel.
- 1 May 2025
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 81  (6) , 609-621
Methods for Regulating Depth of Corrosion Fissures in Simulated Fastener Holes of 7050-T7451 Aluminum Alloy
This study presents a new test method for inducing controlled corrosion damage within simulated fastener holes of aluminum alloys, aimed at pretreating fatigue test specimens. The method involves insulating the outer surfaces while exposing the fastener hole surface to electrolytes containing 0.66 M NaCl + 0.1 M AlCl3 with varying concentrations of K2S2O8. The evolution of corrosion damage within the fastener hole was examined as a function of exposure duration, electrolyte composition, and volume, as well as the effect of galvanic coupling with an SS316 cathode. Results indicate that fissure depth increases with an increase in K2S2O8 concentration, but does not progress further after 24 h to 48 h of exposure in the chemical, or freely-corroding, exposure test. In contrast, galvanic coupling with an SS316 plate significantly accelerates corrosion, leading to much deeper fissures in a shorter time. The importance of electrolyte replenishment has been explored using electrochemical measurements, revealing the impact of evolving electrolyte chemistry. Beyond its application in specimen pretreatment to study environmentally assisted cracking, this method provides a simple yet effective approach for studying localized corrosion and potentially evaluating mitigation strategies for fastener holes in aerospace structures.
- 1 May 2025
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 81  (6) , 609-621
Methods for Regulating Depth of Corrosion Fissures in Simulated Fastener Holes of 7050-T7451 Aluminum Alloy
This study presents a new test method for inducing controlled corrosion damage within simulated fastener holes of aluminum alloys, aimed at pretreating fatigue test specimens. The method involves insulating the outer surfaces while exposing the fastener hole surface to electrolytes containing 0.66 M NaCl + 0.1 M AlCl3 with varying concentrations of K2S2O8. The evolution of corrosion damage within the fastener hole was examined as a function of exposure duration, electrolyte composition, and volume, as well as the effect of galvanic coupling with an SS316 cathode. Results indicate that fissure depth increases with an increase in K2S2O8 concentration, but does not progress further after 24 h to 48 h of exposure in the chemical, or freely-corroding, exposure test. In contrast, galvanic coupling with an SS316 plate significantly accelerates corrosion, leading to much deeper fissures in a shorter time. The importance of electrolyte replenishment has been explored using electrochemical measurements, revealing the impact of evolving electrolyte chemistry. Beyond its application in specimen pretreatment to study environmentally assisted cracking, this method provides a simple yet effective approach for studying localized corrosion and potentially evaluating mitigation strategies for fastener holes in aerospace structures.
- 20 September 2023
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 79  (10) , 1223-1233
Effect of Chloride Concentration on the Environment-Assisted Cracking Behavior of an Al-Mg Alloy in Atmospheric Environments
The effect of chloride concentration on the environment-assisted cracking (EAC) behavior of AA5083-H131 in atmospheric environments was investigated using high-fidelity fracture mechanics-based testing and concurrent electrochemical potential measurements. EAC susceptibility was found to increase across all environments as chloride concentration increased, denoted by a decrease in the threshold stress intensity and faster stage II crack growth rates. However, EAC susceptibility for a given chloride concentration decreased across all chloride concentrations as cathodic limitation due to solution geometry effects increased. These results are analyzed in the context of the proposed anodic dissolution-enabled hydrogen embrittlement mechanism for EAC in Al-Mg alloys. Specifically, the increase in EAC susceptibility noted at higher chloride concentrations is postulated to arise from an increased overpotential for hydrogen production at the crack tip. Conversely, the decrease in EAC susceptibility observed as the solution geometry becomes more restrictive is attributed to cathodic limitation at the bulk surface decreasing dissolution at the crack tip, resulting in a concomitant less aggressive crack chemistry, and thus lower levels of hydrogen production and uptake at the crack tip. A close correlation between the open-circuit potential on the bulk specimen surface and the crack growth kinetics was also observed across all environments and chloride concentrations, with higher chloride concentrations and cathodic limitations resulting in larger changes in electrochemical potential. This correlates well with known electrochemical potential-dependent EAC observations for these alloys.
- 20 September 2023
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 79  (10) , 1223-1233
Effect of Chloride Concentration on the Environment-Assisted Cracking Behavior of an Al-Mg Alloy in Atmospheric Environments
The effect of chloride concentration on the environment-assisted cracking (EAC) behavior of AA5083-H131 in atmospheric environments was investigated using high-fidelity fracture mechanics-based testing and concurrent electrochemical potential measurements. EAC susceptibility was found to increase across all environments as chloride concentration increased, denoted by a decrease in the threshold stress intensity and faster stage II crack growth rates. However, EAC susceptibility for a given chloride concentration decreased across all chloride concentrations as cathodic limitation due to solution geometry effects increased. These results are analyzed in the context of the proposed anodic dissolution-enabled hydrogen embrittlement mechanism for EAC in Al-Mg alloys. Specifically, the increase in EAC susceptibility noted at higher chloride concentrations is postulated to arise from an increased overpotential for hydrogen production at the crack tip. Conversely, the decrease in EAC susceptibility observed as the solution geometry becomes more restrictive is attributed to cathodic limitation at the bulk surface decreasing dissolution at the crack tip, resulting in a concomitant less aggressive crack chemistry, and thus lower levels of hydrogen production and uptake at the crack tip. A close correlation between the open-circuit potential on the bulk specimen surface and the crack growth kinetics was also observed across all environments and chloride concentrations, with higher chloride concentrations and cathodic limitations resulting in larger changes in electrochemical potential. This correlates well with known electrochemical potential-dependent EAC observations for these alloys.
- 10 July 2023
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 79  (8) , 868-880
The Effect of Crack-Initiating Feature on the Environment-Assisted Cracking Behavior of Sensitized AA5456-H116 in Marine Environments
The influence of crack-initiating feature on the environment-assisted cracking (EAC) behavior of sensitized AA5456-H116 exposed to marine environments is assessed via fracture mechanics-based testing. Specimens that contained either a traditional fatigue precrack or purposefully introduced intergranular corrosion fissures were immersed in 0.6 M NaCl and polarized to select electrochemical potentials while held at a constant force. The measured crack length versus time relationships from these experiments reveal that the two specimen geometries yield similar crack growth rates at -900 mVSCE and after the onset of accelerated crack propagation at -800 mVSCE. However, precorroded specimens exhibit significantly shorter times to failure than the precracked specimens at -800 mVSCE due to increased crack growth rates at the start of the experiment. The mechanical, environmental, and material factors that could contribute to the initially increased EAC susceptibility of the precorroded specimens are identified using a generalized model for EAC. Analysis of these possible causal factors suggests that the increased susceptibility is due to a residual, initially more deleterious crack chemistry at the occluded corrosion fissure tip from the aggressive galvanostatic polarizations used to accelerate fissure growth. The implications of these results on the efficacy of traditional fracture mechanics-based methods for quantifying EAC susceptibility are discussed.
- 10 July 2023
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 79  (8) , 868-880
The Effect of Crack-Initiating Feature on the Environment-Assisted Cracking Behavior of Sensitized AA5456-H116 in Marine Environments
The influence of crack-initiating feature on the environment-assisted cracking (EAC) behavior of sensitized AA5456-H116 exposed to marine environments is assessed via fracture mechanics-based testing. Specimens that contained either a traditional fatigue precrack or purposefully introduced intergranular corrosion fissures were immersed in 0.6 M NaCl and polarized to select electrochemical potentials while held at a constant force. The measured crack length versus time relationships from these experiments reveal that the two specimen geometries yield similar crack growth rates at -900 mVSCE and after the onset of accelerated crack propagation at -800 mVSCE. However, precorroded specimens exhibit significantly shorter times to failure than the precracked specimens at -800 mVSCE due to increased crack growth rates at the start of the experiment. The mechanical, environmental, and material factors that could contribute to the initially increased EAC susceptibility of the precorroded specimens are identified using a generalized model for EAC. Analysis of these possible causal factors suggests that the increased susceptibility is due to a residual, initially more deleterious crack chemistry at the occluded corrosion fissure tip from the aggressive galvanostatic polarizations used to accelerate fissure growth. The implications of these results on the efficacy of traditional fracture mechanics-based methods for quantifying EAC susceptibility are discussed.
- 21 March 2023
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 79  (6) , 647-664
Mechanistic Insight into Al-Zn, Mg, and Al-Mg-Rich Primer Design for Enhanced Cathodic Prevention on Sensitized Al-Mg Alloys
Three Al-Zn, Mg, and Mg/Al-rich primers (RPs) were evaluated for their ability to suppress intergranular corrosion (IGC) and intergranular stress corrosion cracking (IG-SCC) on highly sensitized aluminum alloy 5456-H116 by sacrificial anode-based cathodic prevention and chemical deposition effects. Tests were conducted in a 0.6 M NaCl solution under full immersion. These evaluations considered the ability of the primer to attain an intermediate open-circuit potential (OCP) such that the galvanic couple potential with bare 5456 resided outside a range of potentials where IGC prevention is observed. The ability of the primer to achieve OCP’s negative enough so that the 5456-H116 could be protected by sacrificial anode-based cathodic prevention and the ability to sustain this function over time were evaluated. The primers consisted of epoxy resins embedded with either (1) spherical Al-5 wt% Zn, (2) spherical Al-5 wt% Zn and spherical Mg, or (3) Mg flake pigments. A variety of electrochemical techniques evaluated the performance specified including OCP, electrochemical impedance spectroscopy, diagnostic cycle testing, as well as zero resistance ammeter tests with simultaneous pH measurement. Electrochemical cycle testing demonstrated that Al-5%Zn did not activate or provide cathodic prevention. Mg-RP had a suitable OCP for cathodic protection of 5456 but the time to primer activation as well as the activated potential both decreased upon utilization of Mg flake content in the primer. The pure Mg-RP activated quickly but ceased to achieve protective potentials after 1 to 11 cycles of DC/AC/OCP cycle testing. Cross-sectional analysis demonstrated that some flakes dissolved while uniform surface oxidation occurred on the remaining Mg flakes, which in combination led to impaired activation. The composite Mg plus Al/Zn-RP mixed primer maintained a suitably negative OCP over time, remained activated, dispensed high anodic charge, and remained an anode in zero-resistance ammeter testing. Chemical stability modeling and zero-resistance ammeter testing suggest that Mg corrosion elevates the pH which activates the Al-5 wt% Zn pigments, thereby providing a secondary pathway for sacrificial anode-based cathodic protection which supports the long-lasting cathodic protection achieved by the Al-5 wt% Zn/Mg primer. These analyses set a baseline for the consideration of Al-Zn/Mg-based coatings to establish effective cathodic protection on highly sensitized 5456-H116 in an aggressive alternate immersion environment and illustrate the merit of using Al/Mg-RP.
- 21 March 2023
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 79  (6) , 647-664
Mechanistic Insight into Al-Zn, Mg, and Al-Mg-Rich Primer Design for Enhanced Cathodic Prevention on Sensitized Al-Mg Alloys
Three Al-Zn, Mg, and Mg/Al-rich primers (RPs) were evaluated for their ability to suppress intergranular corrosion (IGC) and intergranular stress corrosion cracking (IG-SCC) on highly sensitized aluminum alloy 5456-H116 by sacrificial anode-based cathodic prevention and chemical deposition effects. Tests were conducted in a 0.6 M NaCl solution under full immersion. These evaluations considered the ability of the primer to attain an intermediate open-circuit potential (OCP) such that the galvanic couple potential with bare 5456 resided outside a range of potentials where IGC prevention is observed. The ability of the primer to achieve OCP’s negative enough so that the 5456-H116 could be protected by sacrificial anode-based cathodic prevention and the ability to sustain this function over time were evaluated. The primers consisted of epoxy resins embedded with either (1) spherical Al-5 wt% Zn, (2) spherical Al-5 wt% Zn and spherical Mg, or (3) Mg flake pigments. A variety of electrochemical techniques evaluated the performance specified including OCP, electrochemical impedance spectroscopy, diagnostic cycle testing, as well as zero resistance ammeter tests with simultaneous pH measurement. Electrochemical cycle testing demonstrated that Al-5%Zn did not activate or provide cathodic prevention. Mg-RP had a suitable OCP for cathodic protection of 5456 but the time to primer activation as well as the activated potential both decreased upon utilization of Mg flake content in the primer. The pure Mg-RP activated quickly but ceased to achieve protective potentials after 1 to 11 cycles of DC/AC/OCP cycle testing. Cross-sectional analysis demonstrated that some flakes dissolved while uniform surface oxidation occurred on the remaining Mg flakes, which in combination led to impaired activation. The composite Mg plus Al/Zn-RP mixed primer maintained a suitably negative OCP over time, remained activated, dispensed high anodic charge, and remained an anode in zero-resistance ammeter testing. Chemical stability modeling and zero-resistance ammeter testing suggest that Mg corrosion elevates the pH which activates the Al-5 wt% Zn pigments, thereby providing a secondary pathway for sacrificial anode-based cathodic protection which supports the long-lasting cathodic protection achieved by the Al-5 wt% Zn/Mg primer. These analyses set a baseline for the consideration of Al-Zn/Mg-based coatings to establish effective cathodic protection on highly sensitized 5456-H116 in an aggressive alternate immersion environment and illustrate the merit of using Al/Mg-RP.
- 5 February 2023
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 79  (3) , 363-375
Coupling Fracture Mechanics Experiments and Electrochemical Modeling to Mitigate Environment-Assisted Cracking in Engineering Components
Environment-assisted cracking (EAC) is a pertinent failure mode for many applications and industries, but the design of robust EAC mitigation strategies can be challenging due to the number of material and environmental factors that affect EAC behavior. In this study, a coupled experimental-modeling approach for designing EAC mitigation strategies in a standard panel-and-fastener geometry is presented. Fracture mechanics-based testing is executed on a high-performance steel (Pyrowear 675) immersed in 0.6 M NaCl to assess the effect of electrode potential and loading rate on EAC susceptibility. Finite element modeling (FEM) is then used to calculate the electrode potential distribution across the panel for four realistic EAC mitigation strategies (anodized fastener, fully coated panel, selectively coated panel, and bare panel/fastener). The FEM and EAC susceptibility data are synthesized to inform the efficacy of each proposed mitigation strategy. Results demonstrate that the anodized fastener and fully coated panel approaches are likely to promote EAC, while the selectively coated panel and all-bare strategies mitigate EAC. The benefits and limitations of this coupled approach for mitigating EAC are then discussed.
- 5 February 2023
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 79  (3) , 363-375
Coupling Fracture Mechanics Experiments and Electrochemical Modeling to Mitigate Environment-Assisted Cracking in Engineering Components
Environment-assisted cracking (EAC) is a pertinent failure mode for many applications and industries, but the design of robust EAC mitigation strategies can be challenging due to the number of material and environmental factors that affect EAC behavior. In this study, a coupled experimental-modeling approach for designing EAC mitigation strategies in a standard panel-and-fastener geometry is presented. Fracture mechanics-based testing is executed on a high-performance steel (Pyrowear 675) immersed in 0.6 M NaCl to assess the effect of electrode potential and loading rate on EAC susceptibility. Finite element modeling (FEM) is then used to calculate the electrode potential distribution across the panel for four realistic EAC mitigation strategies (anodized fastener, fully coated panel, selectively coated panel, and bare panel/fastener). The FEM and EAC susceptibility data are synthesized to inform the efficacy of each proposed mitigation strategy. Results demonstrate that the anodized fastener and fully coated panel approaches are likely to promote EAC, while the selectively coated panel and all-bare strategies mitigate EAC. The benefits and limitations of this coupled approach for mitigating EAC are then discussed.
- Open Access
- 16 April 2022
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 78  (6) , 528-546
Comparing Stress Corrosion Cracking Behavior of Additively Manufactured and Wrought 17-4PH Stainless Steel
As a high-strength corrosion-resistant alloy, stress corrosion cracking (SCC) behavior is a key consideration for the conventional, wrought form of 17-4PH stainless steel. With the increasing popularity of the additively manufactured (AM) form of 17-4PH, understanding the SCC behavior of AM 17-4PH will be similarly critical for its presumed, future applications. The current study quantifies and compares the SCC behavior of both the wrought form, as a baseline, and AM form of 17-4PH at peak-aged (∼1,200 MPa) and overaged (∼1,050 MPa) strength levels. The laser powder bed fusion technique followed by post-process hot isostatic press (HIP), solution annealing, and aging heat treatments is used to produce AM 17-4PH with similar microstructures and strength levels to wrought 17-4PH and facilitate the comparison. SCC behavior is quantified using fracture mechanics-based rising (dK/dt = 2 MPa√m/h) and constant (dK/dt = 0 MPa√m/h) stress intensity tests in neutral 0.6 M NaCl at various applied potentials. Limited SCC susceptibility was observed at open-circuit and anodic potentials for both forms of 17-4PH. At cathodic applied potentials, AM consistently underperforms wrought with up to 5-fold faster crack growth rates and 200 mV to 400 mV wider SCC susceptibility ranges. These results are interrogated through microstructural and fractographic analysis and interpreted through a decohesion-based hydrogen-assisted crack model. Initial analyses show that (1) increased oxygen content, (2) porosity induced by argon processing, and (3) slow cooling (310°C/h) during conventional HIP processing might contribute to degraded SCC performance in AM 17-4PH.
- 16 April 2022
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 78  (6) , 528-546
Open AccessComparing Stress Corrosion Cracking Behavior of Additively Manufactured and Wrought 17-4PH Stainless Steel
As a high-strength corrosion-resistant alloy, stress corrosion cracking (SCC) behavior is a key consideration for the conventional, wrought form of 17-4PH stainless steel. With the increasing popularity of the additively manufactured (AM) form of 17-4PH, understanding the SCC behavior of AM 17-4PH will be similarly critical for its presumed, future applications. The current study quantifies and compares the SCC behavior of both the wrought form, as a baseline, and AM form of 17-4PH at peak-aged (∼1,200 MPa) and overaged (∼1,050 MPa) strength levels. The laser powder bed fusion technique followed by post-process hot isostatic press (HIP), solution annealing, and aging heat treatments is used to produce AM 17-4PH with similar microstructures and strength levels to wrought 17-4PH and facilitate the comparison. SCC behavior is quantified using fracture mechanics-based rising (dK/dt = 2 MPa√m/h) and constant (dK/dt = 0 MPa√m/h) stress intensity tests in neutral 0.6 M NaCl at various applied potentials. Limited SCC susceptibility was observed at open-circuit and anodic potentials for both forms of 17-4PH. At cathodic applied potentials, AM consistently underperforms wrought with up to 5-fold faster crack growth rates and 200 mV to 400 mV wider SCC susceptibility ranges. These results are interrogated through microstructural and fractographic analysis and interpreted through a decohesion-based hydrogen-assisted crack model. Initial analyses show that (1) increased oxygen content, (2) porosity induced by argon processing, and (3) slow cooling (310°C/h) during conventional HIP processing might contribute to degraded SCC performance in AM 17-4PH.
- 26 March 2022
- Published by Elsevier in Corrosion Science
- Vol. 201, 110267
On the loading rate dependence of environment-assisted cracking in sensitized AA5456-H116 exposed to marine environments
- 26 March 2022
- Published by Elsevier in Corrosion Science
- Vol. 201, 110267
On the loading rate dependence of environment-assisted cracking in sensitized AA5456-H116 exposed to marine environments
- Open Access
- 1 July 2021
- Published by MDPI AG in Corrosion and Materials Degradation
- Vol. 2  (3) , 360-375
The Effect of Loading Rate on the Environment-Assisted Cracking Behavior of AA7075-T651 in Aqueous NaCl Solution
The influence of loading rate on the environment-assisted cracking (EAC) behavior of AA7075-T651 immersed in 0.6 and 1.0 M NaCl solution was assessed at applied potentials ranging from −800 to −1200 mVSCE via a slow-rising stress intensity (K) testing methodology. Measured crack growth rates under rising K loading are compared to those obtained using a fixed K protocol, which revealed that rising K-based testing consistently yields increased crack growth rates relative to static K approaches across all tested conditions. However, relative to other alloy systems, EAC in AA7075-T651 is only modestly loading rate-dependent, as demonstrated by testing conducted at fixed dK/dt ranging from 0.25 to 2.0 MPa√m/h. The implications of the observed results are considered in the context of current EAC testing specifications, with specific focus on the conservatism and efficiency of rising K-based approaches.
- 1 July 2021
- Published by MDPI AG in Corrosion and Materials Degradation
- Vol. 2  (3) , 360-375
Open AccessThe Effect of Loading Rate on the Environment-Assisted Cracking Behavior of AA7075-T651 in Aqueous NaCl Solution
The influence of loading rate on the environment-assisted cracking (EAC) behavior of AA7075-T651 immersed in 0.6 and 1.0 M NaCl solution was assessed at applied potentials ranging from −800 to −1200 mVSCE via a slow-rising stress intensity (K) testing methodology. Measured crack growth rates under rising K loading are compared to those obtained using a fixed K protocol, which revealed that rising K-based testing consistently yields increased crack growth rates relative to static K approaches across all tested conditions. However, relative to other alloy systems, EAC in AA7075-T651 is only modestly loading rate-dependent, as demonstrated by testing conducted at fixed dK/dt ranging from 0.25 to 2.0 MPa√m/h. The implications of the observed results are considered in the context of current EAC testing specifications, with specific focus on the conservatism and efficiency of rising K-based approaches.
- 6 February 2020
- Published by ASME International in Journal of Engineering Materials and Technology
- Vol. 142  (3) , 1-27
Validation of Hot Corrosion and Fatigue Models in HOTPITS
HOTPITS is a set of physics-based modeling tools for treating Type II hot corrosion in Ni-based superalloys. The methodology includes modeling the nucleation, growth, and coalescence of pits and microcracks as a random process, as well as the transition of pits to micrcracks and the propagation of the resulting large crack to failure. In this investigation, critical experiments were performed on coupon and low-cycle fatigue (LCF) specimens in order to validate the hot corrosion and the fatigue models in HOTPITS. The pit nucleation, growth, and coalescence models in HOTPITS including the assumption of a random process are validated by the hot corrosion critical experiments performed at two salt contents. The LCF critical experiments, performed using a marker band protocol, validated the stress concentration factor-based models used to predict the pit-to-crack transition in the HOTPITS tool.
- 6 February 2020
- Published by ASME International in Journal of Engineering Materials and Technology
- Vol. 142  (3) , 1-27
Validation of Hot Corrosion and Fatigue Models in HOTPITS
HOTPITS is a set of physics-based modeling tools for treating Type II hot corrosion in Ni-based superalloys. The methodology includes modeling the nucleation, growth, and coalescence of pits and microcracks as a random process, as well as the transition of pits to micrcracks and the propagation of the resulting large crack to failure. In this investigation, critical experiments were performed on coupon and low-cycle fatigue (LCF) specimens in order to validate the hot corrosion and the fatigue models in HOTPITS. The pit nucleation, growth, and coalescence models in HOTPITS including the assumption of a random process are validated by the hot corrosion critical experiments performed at two salt contents. The LCF critical experiments, performed using a marker band protocol, validated the stress concentration factor-based models used to predict the pit-to-crack transition in the HOTPITS tool.