Volkan Karakurt
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Volkan Karakurt has a total of 11 co-authors. Here are the top co-authors by number of shared publications:
- Esma Keskin
BUMA Engineering and Consulting Inc
2 shared publications - Feyzanur Öztürk
Sağlam Metal San. ve Tic. A.Ş.
2 shared publications - Hayrettin Ahlatci
Karabuk University
2 shared publications - Ismail Esen
Karabuk University
2 shared publications - Orçun Zığındere
Sağlam Metal San. ve Tic. A.Ş.
2 shared publications - Talip Çitrak
Sağlam Metal San. ve Tic. A.Ş.
2 shared publications
Latest Publications
- Open Access
- 25 February 2026
- Published by Kaunas University of Technology (KTU) in Materials Science
- Vol. 32 (1) , 42-56
Effect of 0.40 % and 0.20 % Titanium Addition on Microstructure Properties and Corrosion Behavior of CuAl10Ni5Fe4 Alloy
This study examined how post-casting heat treatment (solution treatment and tempering) and forging affected the corrosion and microstructural properties of the nickel aluminium bronze (CuAl10Ni5Fe4) with 0.20 % and 0.40% titanium addition. Heat-treated CuAl10Ni5Fe4 alloy microstructures showed copper-rich α-solid solution, martensitic β-phase, and intermetallic κ-phases, such as flake-shaped κI, fine κIII, and black globular κIV. Adding 0.20 % and 0.40 % titanium to CuAl10Ni5Fe4 alloys reduced dendritic arm thickness and increased κ phase abundance. Additionally, significant κIV and κII precipitations were observed in the tempered β phase. Tempering β may cause martensitic β to split into tiny α and κIII phases. The grain refinement of the CuAl10Ni5Fe4, CuAl10Ni5Fe4-0.20 % Ti, and CuAl10Ni5Fe4-0.40 % Ti alloys was significantly noticeable after forging. The alloys retained the same α, β, and κ phases seen in the heat-treated alloys after forging. Titanium's refining effect increased the hardness of the alloy into which it was incorporated. Increased stiff phases, such as tempered β and fine κIV, contribute to increased hardness. The forging process enhanced the hardness of all three alloys. Forged and heat treated CuAl10Ni5Fe4-0.40 % Ti alloy had the highest hardness with 243.50 HB and 256.18 HB, respectively. The microstructural phases α, β, and κ significantly impact the corrosion behaviour of CuAl10Ni5Fe4 alloy. The CuAl10Ni5Fe4-0.40 % Ti alloy after forging had the lowest 24-hour weight loss of 0.003326 mg/dm2. The CuAl10Ni5Fe4 alloy loses the most weight (0.013659 mg/dm²) following heat treatment (S.T.+T) after 24 hours. The minimal corrosion rate for the CuAl10Ni5Fe4-0.40 % Ti alloy after forging was 0.003916 mg/(dm2·day) after 72 hours. Due to stratification, corrosion creates craters. Pitted or porous structures and craters are common. All alloys show a decrease in these structures after forging. The formation of the CuCl2 phase is believed to occur in regions experiencing pitting corrosion.
- 25 February 2026
- Published by Kaunas University of Technology (KTU) in Materials Science
- Vol. 32 (1) , 42-56
Open AccessEffect of 0.40 % and 0.20 % Titanium Addition on Microstructure Properties and Corrosion Behavior of CuAl10Ni5Fe4 Alloy
This study examined how post-casting heat treatment (solution treatment and tempering) and forging affected the corrosion and microstructural properties of the nickel aluminium bronze (CuAl10Ni5Fe4) with 0.20 % and 0.40% titanium addition. Heat-treated CuAl10Ni5Fe4 alloy microstructures showed copper-rich α-solid solution, martensitic β-phase, and intermetallic κ-phases, such as flake-shaped κI, fine κIII, and black globular κIV. Adding 0.20 % and 0.40 % titanium to CuAl10Ni5Fe4 alloys reduced dendritic arm thickness and increased κ phase abundance. Additionally, significant κIV and κII precipitations were observed in the tempered β phase. Tempering β may cause martensitic β to split into tiny α and κIII phases. The grain refinement of the CuAl10Ni5Fe4, CuAl10Ni5Fe4-0.20 % Ti, and CuAl10Ni5Fe4-0.40 % Ti alloys was significantly noticeable after forging. The alloys retained the same α, β, and κ phases seen in the heat-treated alloys after forging. Titanium's refining effect increased the hardness of the alloy into which it was incorporated. Increased stiff phases, such as tempered β and fine κIV, contribute to increased hardness. The forging process enhanced the hardness of all three alloys. Forged and heat treated CuAl10Ni5Fe4-0.40 % Ti alloy had the highest hardness with 243.50 HB and 256.18 HB, respectively. The microstructural phases α, β, and κ significantly impact the corrosion behaviour of CuAl10Ni5Fe4 alloy. The CuAl10Ni5Fe4-0.40 % Ti alloy after forging had the lowest 24-hour weight loss of 0.003326 mg/dm2. The CuAl10Ni5Fe4 alloy loses the most weight (0.013659 mg/dm²) following heat treatment (S.T.+T) after 24 hours. The minimal corrosion rate for the CuAl10Ni5Fe4-0.40 % Ti alloy after forging was 0.003916 mg/(dm2·day) after 72 hours. Due to stratification, corrosion creates craters. Pitted or porous structures and craters are common. All alloys show a decrease in these structures after forging. The formation of the CuCl2 phase is believed to occur in regions experiencing pitting corrosion.
- 29 November 2025
- Published by Kaunas University of Technology (KTU) in Materials Science
- Vol. 31 (4) , 510-520
Tribological Effects of 0.30% Titanium in NAB Alloy Post-Casting, Heat Treatment and Forging
This study explores the effects of solution treatment, tempering, and forging on the microstructure and tribological properties of 0.30 % Ti-alloyed nickel–aluminum bronze. The modified NAB alloy exhibited a refined microstructure comprising a copper-rich α-phase, martensitic β-phase, and various intermetallic κ (kappa) phases. Titanium addition enhanced nucleation during solidification, reduced dendritic arm spacing, and promoted the formation of discrete κ phases, thereby improving grain refinement and phase uniformity. Notably, tempering the β-phase facilitated its partial decomposition into α and κIII, with further precipitation of κIV and κII phases. Forging significantly altered the alloy's morphology, fragmenting dendritic arms into near-spherical forms and increasing the formation of secondary κIV phases while preserving the fundamental α, β, and κ phases. Hardness analysis revealed that Ti addition markedly improved hardness, with NAB-0.30 %Ti achieving 239.53 HB and 254.06 HB after heat treatment and forging, respectively. Enhanced hardness and improved wear resistance have been attributed to the presence of intermetallic κ phases, increased dislocation density, and grain refinement. Tribological testing confirmed that the forged NAB-0.30 %Ti alloy demonstrated the lowest friction coefficient (0.097), minimal weight loss (0.0035 g), and the best wear rate (1.17 × 10⁻⁸ g/N·m) over 10,000 meters of sliding distance. The findings highlight titanium’s role in refining microstructure and enhancing both hardness and tribological performance of NAB, making it a promising candidate for applications demanding superior wear resistance.
- 29 November 2025
- Published by Kaunas University of Technology (KTU) in Materials Science
- Vol. 31 (4) , 510-520
Tribological Effects of 0.30% Titanium in NAB Alloy Post-Casting, Heat Treatment and Forging
This study explores the effects of solution treatment, tempering, and forging on the microstructure and tribological properties of 0.30 % Ti-alloyed nickel–aluminum bronze. The modified NAB alloy exhibited a refined microstructure comprising a copper-rich α-phase, martensitic β-phase, and various intermetallic κ (kappa) phases. Titanium addition enhanced nucleation during solidification, reduced dendritic arm spacing, and promoted the formation of discrete κ phases, thereby improving grain refinement and phase uniformity. Notably, tempering the β-phase facilitated its partial decomposition into α and κIII, with further precipitation of κIV and κII phases. Forging significantly altered the alloy's morphology, fragmenting dendritic arms into near-spherical forms and increasing the formation of secondary κIV phases while preserving the fundamental α, β, and κ phases. Hardness analysis revealed that Ti addition markedly improved hardness, with NAB-0.30 %Ti achieving 239.53 HB and 254.06 HB after heat treatment and forging, respectively. Enhanced hardness and improved wear resistance have been attributed to the presence of intermetallic κ phases, increased dislocation density, and grain refinement. Tribological testing confirmed that the forged NAB-0.30 %Ti alloy demonstrated the lowest friction coefficient (0.097), minimal weight loss (0.0035 g), and the best wear rate (1.17 × 10⁻⁸ g/N·m) over 10,000 meters of sliding distance. The findings highlight titanium’s role in refining microstructure and enhancing both hardness and tribological performance of NAB, making it a promising candidate for applications demanding superior wear resistance.
- 31 July 2025
- Published by Namik Kemal University in European Journal of Engineering and Applied Sciences
- Vol. 8 (1) , 1-6
The Effect Of Vacuum Heat Treatment On Microstructural And Corrosion Properties Of CuAl10Ni5Fe3Mn Alloy
Nickel aluminum bronzes (NAB) are copper alloys widely used in critical applications in the defense, aerospace and marine industries. These alloys exhibit excellent properties such as wear resistance, corrosion resistance, impact strength, hardness and ductility, which are highly dependent on their composition and production conditions. Despite the relatively low formation of oxide layers on the surface of nickel aluminum bronze components under heat treatment conditions due to the high nickel content, there are special applications where the formation of oxide layers on the surface is undesirable. For this reason, the heat treatment of CuAl10Ni5Fe3Mn alloy was carried out in a vacuum furnace and the heat treatment process conditions in a non-vacuum muffle furnace were compared. For comparison purposes, the microstructure of the materials was examined and hardness and tensile tests and potentiodynamic corrosion tests were performed. It was determined that heat treatment in the muffle furnace led to a decrease in the proportion of the α phase and a higher formation of the β and κ phases compared to the heat treatment in a vacuum atmosphere. The material heat treated in the muffle furnace exhibited higher hardness and strength values as well as improved corrosion resistance compared to the material treated in the vacuum furnace.
- 31 July 2025
- Published by Namik Kemal University in European Journal of Engineering and Applied Sciences
- Vol. 8 (1) , 1-6
The Effect Of Vacuum Heat Treatment On Microstructural And Corrosion Properties Of CuAl10Ni5Fe3Mn Alloy
Nickel aluminum bronzes (NAB) are copper alloys widely used in critical applications in the defense, aerospace and marine industries. These alloys exhibit excellent properties such as wear resistance, corrosion resistance, impact strength, hardness and ductility, which are highly dependent on their composition and production conditions. Despite the relatively low formation of oxide layers on the surface of nickel aluminum bronze components under heat treatment conditions due to the high nickel content, there are special applications where the formation of oxide layers on the surface is undesirable. For this reason, the heat treatment of CuAl10Ni5Fe3Mn alloy was carried out in a vacuum furnace and the heat treatment process conditions in a non-vacuum muffle furnace were compared. For comparison purposes, the microstructure of the materials was examined and hardness and tensile tests and potentiodynamic corrosion tests were performed. It was determined that heat treatment in the muffle furnace led to a decrease in the proportion of the α phase and a higher formation of the β and κ phases compared to the heat treatment in a vacuum atmosphere. The material heat treated in the muffle furnace exhibited higher hardness and strength values as well as improved corrosion resistance compared to the material treated in the vacuum furnace.
- Open Access
- 31 December 2024
- Published by The International Journal of Materials and Engineering Technology in The International Journal of Materials and Engineering Technology
- Vol. 7 (2) , 77-84
EFFECT OF DEEP CRYOGENIC TREATMENT ON MICROSTRUCTURAL AND MECHANICAL PROPERTIES OF HIGH-PERFORMANCE CPOH AND WP7V TOOL STEELS
In recent years, deep cryogenic treatment (DCT) has been applied to steel materials as an additional heat treatment to improve various material properties that include wear resistance, impact resistance and hardness. In this study, the mechanical properties of CPOH cold work tool steel with high wear and impact resistance and Dörrenberg Edelstahl patented WP7V cold work tool steel used in applications requiring high hardness were improved by deep cryogenic heat treatment. The material subjected to deep cryogenic heat treatment was subjected to deep cryogenic heat treatment and tempering after a conventional austenitizing and quenching process. The microstructure, hardness, wear and impact properties of the cryogenic heat treated materials were investigated in comparison with those obtained after conventional heat treatment. It was found that deep cryogenic heat treatment of tool steels in addition to conventional heat treatment can improve performance and provide high performance tool steels required by the industry.
- 31 December 2024
- Published by The International Journal of Materials and Engineering Technology in The International Journal of Materials and Engineering Technology
- Vol. 7 (2) , 77-84
Open AccessEFFECT OF DEEP CRYOGENIC TREATMENT ON MICROSTRUCTURAL AND MECHANICAL PROPERTIES OF HIGH-PERFORMANCE CPOH AND WP7V TOOL STEELS
In recent years, deep cryogenic treatment (DCT) has been applied to steel materials as an additional heat treatment to improve various material properties that include wear resistance, impact resistance and hardness. In this study, the mechanical properties of CPOH cold work tool steel with high wear and impact resistance and Dörrenberg Edelstahl patented WP7V cold work tool steel used in applications requiring high hardness were improved by deep cryogenic heat treatment. The material subjected to deep cryogenic heat treatment was subjected to deep cryogenic heat treatment and tempering after a conventional austenitizing and quenching process. The microstructure, hardness, wear and impact properties of the cryogenic heat treated materials were investigated in comparison with those obtained after conventional heat treatment. It was found that deep cryogenic heat treatment of tool steels in addition to conventional heat treatment can improve performance and provide high performance tool steels required by the industry.