Tiancheng An
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Tiancheng An has a total of 19 co-authors. Here are the top co-authors by number of shared publications:
- Ziqiao Zhong
E.O. Paton Electric Welding Institute, National Academy of Sciences of Ukraine, Kyiv, Ukraine
3 shared publications - Olena M. Berdnikova
E.O. Paton Electric Welding Institute of the National Academy of Sciences of Ukraine
2 shared publications Xitong Li
Aerospace Engineering Equipment (Suzhou) Co. Ltd., Suzhou
2 shared publicationsBaihui Sun
Harbin Turbine Company Ltd
1 shared publicationBerdnikova Olena
E.O. Paton Electric Welding Institute, National Academy of Sciences of Ukraine, Kyiv, Ukraine
1 shared publicationChang Yiyun
Igor Sikorsky Kyiv Polytechnic Institute, National Technical University of Ukraine, Kyiv, Ukraine
1 shared publication
Latest Publications
- Open Access
- 7 September 2026
- Published by Elsevier in Materials Today Advances
- Vol. 31
Cooperative multi-phase precipitation and strengthening mechanisms in directed energy deposited XM-25 martensitic stainless steel
- 7 September 2026
- Published by Elsevier in Materials Today Advances
- Vol. 31
Open AccessCooperative multi-phase precipitation and strengthening mechanisms in directed energy deposited XM-25 martensitic stainless steel
- Open Access
- 20 May 2026
- Published by IOP Publishing in Materials Research Express
- Vol. 13 (10) , 106503
Study on the influence of tool rotational speeds/welding traverse speeds on the quality and surface formation of 6 mm copper friction stir welding
This paper describes a study on the formation and process parameters of friction stir welding joints on 6 mm thick copper plates. Numerous experiments were conducted at lower rotational speeds and moderate welding traverse speeds to obtain optimal process parameters for high-quality friction stir welding joints with good surface formation and no internal defects. Simultaneously, considering the thickness tolerance fluctuations in the large-scale engineering application of Copper FSW, tests were conducted with pin lengths and shoulder plunge depths less than the plate thickness. Additionally, a unique modular stirring tool was designed by ourselves to reduce costs in large-scale engineering applications. The experimental results demonstrate that under the parameters of a rotational speed of 275 r min −1 and a traverse speed of 120 mm min −1 , welding joints with both surface and internal integrity can be achieved, with the joint strength level exceeding 80% of the base material. The mechanical weak point of the joint is located in the TMAZ region just below the pin as revealed by SEM testing, which shows both plastic and brittle fractures. EDS results indicate no inclusions or second-phase precipitates at the surface and port locations.
- 20 May 2026
- Published by IOP Publishing in Materials Research Express
- Vol. 13 (10) , 106503
Open AccessStudy on the influence of tool rotational speeds/welding traverse speeds on the quality and surface formation of 6 mm copper friction stir welding
This paper describes a study on the formation and process parameters of friction stir welding joints on 6 mm thick copper plates. Numerous experiments were conducted at lower rotational speeds and moderate welding traverse speeds to obtain optimal process parameters for high-quality friction stir welding joints with good surface formation and no internal defects. Simultaneously, considering the thickness tolerance fluctuations in the large-scale engineering application of Copper FSW, tests were conducted with pin lengths and shoulder plunge depths less than the plate thickness. Additionally, a unique modular stirring tool was designed by ourselves to reduce costs in large-scale engineering applications. The experimental results demonstrate that under the parameters of a rotational speed of 275 r min −1 and a traverse speed of 120 mm min −1 , welding joints with both surface and internal integrity can be achieved, with the joint strength level exceeding 80% of the base material. The mechanical weak point of the joint is located in the TMAZ region just below the pin as revealed by SEM testing, which shows both plastic and brittle fractures. EDS results indicate no inclusions or second-phase precipitates at the surface and port locations.
- 22 September 2025
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 35 (8) , 8105-8117
Study on the Performance of Low-Temperature Long-Time Post-Weld Heat Treatment for Welding 9Cr-3W-3Co-1Cu-VNbBN Steel with Same Composition Welding Consumables
- 22 September 2025
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 35 (8) , 8105-8117
Study on the Performance of Low-Temperature Long-Time Post-Weld Heat Treatment for Welding 9Cr-3W-3Co-1Cu-VNbBN Steel with Same Composition Welding Consumables
- 20 January 2025
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 39 (10) , 1559-1578
Research and engineering application of DED laser cladding repair for steam turbine XM-25 alloy LP blades
- 20 January 2025
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 39 (10) , 1559-1578
Research and engineering application of DED laser cladding repair for steam turbine XM-25 alloy LP blades
- Open Access
- 1 September 2023
- Published by IOP Publishing in Materials Research Express
- Vol. 10 (9) , 096504
Study on mechanical properties of 2219 aluminum alloy bobbin tool friction stir welding
The Bobbin tool friction stir welding (BT-FSW) process experiment was performed on 2219 aluminum alloy with different butt clearances and misalignments. The maximum allowable clearance and misalignment amount for BT-FSW were obtained, and the weld formation, mechanical properties and microstructure under different parameters were compared and analysed. The results show that the face and back sides of the weld joint surface are perfect and there are no defect inside with the butt clearance under 2 mm and the misalignment under 1.5 mm. During the increase of butt clearance and misalignment, the tensile strength of the weld will be decreased gradually. In comparison, the impact of misalignment on weld strength is lower than that of the butt clearance. The tensile strength from both of them will reach more than 60% of the base metal strength. The lowest hardness value occurs in the thermal-mechanical influence zone, which is 79.1HV, about 70% of the base metal hardness value. The microstructure characteristics are similar to those of conventional friction stir welding. The macroscopic morphology of the welded joint is typical ‘dumbbell type’, and there are many ‘dimples’ in the tensile fracture, which is a typical ductile fracture. A large number of dispersed phase particles (Al2Cu) were found in the dimples, which is the main reason for the decrease in mechanical strength and hardness compared with the substrate.
- 1 September 2023
- Published by IOP Publishing in Materials Research Express
- Vol. 10 (9) , 096504
Open AccessStudy on mechanical properties of 2219 aluminum alloy bobbin tool friction stir welding
The Bobbin tool friction stir welding (BT-FSW) process experiment was performed on 2219 aluminum alloy with different butt clearances and misalignments. The maximum allowable clearance and misalignment amount for BT-FSW were obtained, and the weld formation, mechanical properties and microstructure under different parameters were compared and analysed. The results show that the face and back sides of the weld joint surface are perfect and there are no defect inside with the butt clearance under 2 mm and the misalignment under 1.5 mm. During the increase of butt clearance and misalignment, the tensile strength of the weld will be decreased gradually. In comparison, the impact of misalignment on weld strength is lower than that of the butt clearance. The tensile strength from both of them will reach more than 60% of the base metal strength. The lowest hardness value occurs in the thermal-mechanical influence zone, which is 79.1HV, about 70% of the base metal hardness value. The microstructure characteristics are similar to those of conventional friction stir welding. The macroscopic morphology of the welded joint is typical ‘dumbbell type’, and there are many ‘dimples’ in the tensile fracture, which is a typical ductile fracture. A large number of dispersed phase particles (Al2Cu) were found in the dimples, which is the main reason for the decrease in mechanical strength and hardness compared with the substrate.