LHLukas Hennerici

Lukas Hennerici

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Lukas Hennerici has a total of 24 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Powder Aerosol Deposition and Electrochemical Characterization of 30 µm thick LLZO Solid Electrolyte as a Separator Layer for Solid-State Batteries

    by Lukas Hennerici, Till Fuchs, Sabrina Lang, Daniel Paulus, Mario Linz, Dominik Kramer, Reiner Mönig, Jürgen Janek, Daniela Schönauer-Kamin, Ralf Moos

    Garnet-type Li 7 La 3 Zr 2 O 12 (LLZO) is a promising solid electrolyte (SE) for solid-state batteries (SSBs). However, identifying a suitable processing method to allow dense film fabrication without high sintering temperatures remains challenging. Powder aerosol deposition method (PAD, a.k.a. ADM) enables the fabrication of dense LLZO films at room temperature. To date, studies on PAD-LLZO films primarily addressed the electrical properties in terms of conductivity, while their cycling performance remains largely unexplored. In this study, we show that PAD-LLZO films can be used for the reversible transport of lithium with current densities up to 0.41 mA cm −2 with no thermal post-treatment of pristine films after deposition, albeit at high overvoltage. A mild annealing at 400 °C is performed to reduce microstrain, which is known to lead to high overvoltage during cycling in the as-deposited state. Higher ionic conductivities are achieved after annealing, while the cycling stability deteriorates. These phenomena are attributed to reduced compressive stress as well as microstrain after annealing of the PAD-LLZO films with a nanocrystalline microstructure. Based on these assumptions, we propose a possible strategy to improve cycling stability by adapting a post-treatment process to reduce the volume fraction of grain boundaries by controlled grain growth.

  • Open Access

    Progress in the Cycling Performance of Oxidic Solid-State Batteries Fabricated at Room Temperature by Powder Aerosol Deposition

    by Lukas Hennerici, Dominik Bröse, Maximilian Schamel, Sabrina Lang, Paula Ficht, Dominik Kramer, Reiner Mönig, Michael A. Danzer, Ralf Moos

    The fabrication of solid-state batteries (SSBs) without the need for high-temperature sintering significantly requires less energy. The powder aerosol deposition (PAD) method enables direct film formation at room temperature, bypassing the conventional thermal densification step. This study presents an overview of recent advancements in the cycling properties of SSBs fabricated via PAD. Employing LiNi 0.82 Mn 0.07 Co 0.11 O 2 (NMC) as cathode active material (CAM) and Li 7 La 3 Zr 2 O 12 (LLZO) as solid electrolyte, a capacity of 141 mAh g −1 with 90 % capacity retention over 25 cycles is demonstrated with no thermal post-treatment applied after film fabrication. Based on these results, the role of LLZO as catholyte in the cathode layer is investigated. The findings suggest an electrochemical instability between nickel-rich NMC and LLZO during cycling. To enhance the capacity, the aggregated results are used to discuss various strategies for optimizing cathode layer design, particularly with respect to the composition and choice of the CAM.

  • Open Access

    Formation, Growth, and Shrinkage of Voids in Lithium Metal in Contact With an LLZO Electrolyte

    by Sabrina Lang, Lukas Hennerici, Dominik Kramer, Diana Avadanii, Stefan Mück, Mario Linz, Jaroslaw Kita, Ralf Moos, Reiner Mönig

    A leap forward in the energy density of solid-state batteries necessitates the successful implementation of metal electrodes. A serious problem of metal electrodes is their non-uniform deposition and dissolution, which can lead to dendrites and voids. Here, we report on formation, growth, and shrinkage of voids based on operando SEM observations of lithium metal in contact with a Li7La3Zr2O12 (LLZO) electrolyte. Our observations reveal a general tendency for the replenishment of voids upon redeposition of lithium. We explain this by gradients in the mechanical stress that act as driving forces for atom motion inside the electrode and thus feed lithium away from the interface back into existing voids, which restores the original shape of the electrode. During operation, lithium atoms are inserted or extracted at the interface, creating stresses in the electrode. In electrodes with smaller lithium grains we observe that the shape of voids is strongly influenced by the microstructure of the lithium metal and that grain boundaries can obstruct void growth. We consider diffusion along lithium grain boundaries and the inner surface of voids as important pathways for metal transport. We suggest that the local balance of the diffusional metal fluxes is responsible for the evolution of the shape of the metal electrode.

  • Open Access

    Lithium All‐Solid‐State Batteries Fabricated at Room Temperature by the Powder Aerosol Deposition Method with Garnet‐Type Electrolyte and Graded Composite Cathode

    by Lukas Hennerici, Paula Ficht, Maximilian Schamel, Ulrich Mansfeld, Mario Linz, Daniel Paulus, Jaroslaw Kita, Michael A. Danzer, Ralf Moos

    Lithium‐based all‐solid‐state batteries (ASSBs) are attracting worldwide attention as the next step in the evolution of Li‐ion batteries (LIBs). They have the potential to address safety concerns and limited energy densities, which are key challenges for LIBs. The current focus is on enhancing the electrochemical properties of ASSBs. However, a suitable economic method for fabricating them remains to be established, especially when ceramic materials are used as solid electrolytes. The powder aerosol deposition method (PAD or ADM) is a ceramic processing method that uses raw ceramic powders to fabricate dense, several micrometer thick ceramic films. The entire process takes place at room temperature and in the absence of additional binders. Therefore, PAD is used in this study to fabricate ASSBs with LiNi 0.83 Mn 0.11 Co 0.06 O 2 (NMC) as the cathode active material and Al 0.2 Li 6.025 La 3 Zr 1.625 Ta 0.375 O 12 (LLZO) as the solid electrolyte. The cathode is fabricated as a composite with a gradient in the electrolyte concentration. The successful fabrication is confirmed through scanning electron microscopy and energy‐dispersive X‐ray spectroscopy analysis. Electrochemical characterization shows that a PAD‐ASSB can be cycled. Furthermore, it can be shown that 145 µm thick NMC films can be fabricated by PAD. The electrochemical results are compared with the theoretical potential of PAD‐ASSBs, and methods to further improve the achieved state are discussed.


  • Open Access

    Revealing the Deposition Mechanism of the Powder Aerosol Deposition Method Using Ceramic Oxide Core–Shell Particles

    by Mario Linz, Florian Bühner, Daniel Paulus, Lukas Hennerici, Yiran Guo, Valeriu Mereacre, Ulrich Mansfeld, Martin Seipenbusch, Jaroslaw Kita, Ralf Moos

    The powder aerosol deposition (PAD) method is a process to manufacture ceramic films completely at room temperature. Since the first reports by Akedo in the late 1990s, much research has been conducted to reveal the exact mechanism of the deposition process. However, it is still not fully understood. This work tackles this challenge using core–shell particles. Two coated oxides, Al2O3 core with a SiO2 shell and LiNi0.6Mn0.2Co0.2O2 core with a LiNbO3 shell, are investigated. Initially, the element ratios Al:Si and Ni:Nb of the powder are determined by energy‐dispersive X‐ray spectroscopy (EDX). In a second step, the change in the element ratios of Al:Si and Ni:Nb after deposition is investigated. The element ratios from powder to film strongly shift toward the shell elements, indicating that the particles fracture and only the outer parts of the particles are deposited. In the last step, this work investigates cross‐sections of the deposited films with scanning transmission electron microscopy (STEM combined with EDX and an energy‐selective back‐scattered electron (EsB) detector to unveil the element distribution within the film itself. Therefore, the following overall picture emerges: particles impact on the substrate or on previously deposited particle, fracture, and only a small part of the impacting particles that originate from the outer part of the impacting particle gets deposited.