Xiaochen Xie
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Xiaochen Xie has a total of 20 co-authors. Here are the top co-authors by number of shared publications:
- Xiuchen Zhao
School of Materials Science & Engineering, Beijing Institute of Technology, Beijing 100081, China
3 shared publications - Shuyuan Shi
National Key Laboratory of Spintronics, Hangzhou International Innovation Institute, Beihang University 1 , Hangzhou 311115
2 shared publications - Binhao Lian
Beijing Microelectronics Technology Institute, Beijing 100076, China
1 shared publication - Changhao Chen
Package R&D Center, Beijing Microelectroniscs Technology Institute, Beijing 100076, China
1 shared publication Jiahui Chang
Beijing Inst Technol, Sch Mat Sci & Engn, Beijing 100081, Peoples R China
1 shared publication- Jiahui Chang
School of Materials Science and Engineering, Beijing Institute of Technology, Beijing 100081, China
1 shared publication
Latest Publications
- Open Access
Microstructure and Mechanical Properties of In-Doped Low-Temperature SnPb Solders
In this paper, In was introduced into SnPb eutectic solder to develop a new low-temperature solder for three-dimensional packaging technology. SnPbIn solders containing 5, 10, 13, 15 and 17 wt.% In were prepared through vacuum induction melting. The effect of the addition of In on the microstructure and thermal and mechanical properties of the SnPbIn solders was investigated. The results showed that the SnPb eutectic solder consisted of Sn(ss) and Pb(ss), but when the In content was higher than 5 wt.%, the SnPbIn solder included Sn(ss) and Pb(ss) and a new InSn4 phase. Solid dissolution of the In element into Sn(ss) and Pb(ss) preferentially occurred. The melting points of the SnPbIn solders gradually decreased with the increasing addition of the In element. The melting point of the Sn-Pb-13In solder decreased to 150.5 °C, which met the requirements of 2.5D packaging. But the cast Sn-Pb-5In solder reached the best tensile strength of 48.8 MPa and elongation of 27.3%. Super-plasticity occurred in the cold-rolled SnPbIn, while the 59.9Sn35.1 Pb5In solder achieved elongation of 382.0% and 408.6%, respectively, at deformation of 70% and 90%. The super-plasticity originated from the recrystallization behavior and soft orientation.
Open AccessMicrostructure and Mechanical Properties of In-Doped Low-Temperature SnPb Solders
In this paper, In was introduced into SnPb eutectic solder to develop a new low-temperature solder for three-dimensional packaging technology. SnPbIn solders containing 5, 10, 13, 15 and 17 wt.% In were prepared through vacuum induction melting. The effect of the addition of In on the microstructure and thermal and mechanical properties of the SnPbIn solders was investigated. The results showed that the SnPb eutectic solder consisted of Sn(ss) and Pb(ss), but when the In content was higher than 5 wt.%, the SnPbIn solder included Sn(ss) and Pb(ss) and a new InSn4 phase. Solid dissolution of the In element into Sn(ss) and Pb(ss) preferentially occurred. The melting points of the SnPbIn solders gradually decreased with the increasing addition of the In element. The melting point of the Sn-Pb-13In solder decreased to 150.5 °C, which met the requirements of 2.5D packaging. But the cast Sn-Pb-5In solder reached the best tensile strength of 48.8 MPa and elongation of 27.3%. Super-plasticity occurred in the cold-rolled SnPbIn, while the 59.9Sn35.1 Pb5In solder achieved elongation of 382.0% and 408.6%, respectively, at deformation of 70% and 90%. The super-plasticity originated from the recrystallization behavior and soft orientation.
- 31 August 2024
- Published by Elsevier in Materials Today Communications
- Vol. 41
High-reliability Sn37Pb/Sn58Bi composite solder joints by solid-liquid low-temperature soldering
- 31 August 2024
- Published by Elsevier in Materials Today Communications
- Vol. 41
High-reliability Sn37Pb/Sn58Bi composite solder joints by solid-liquid low-temperature soldering
- Open Access
Effect of Sb Content on the Microstructure and Mechanical Properties of Eutectic SnPb Solder
SnPb solder was widely used in electronic packaging for aerospace devices due to its high reliability. However, its creep resistance is poor and can be improved by adding alloying elements. The effects of Sb content on the microstructure, tensile, and creep properties of eutectic SnPb solder were investigated. Sb addition effectively improved the mechanical properties of the SnPb solder. When Sb content exceeds 1.7 wt.%, SbSn intermetallic compounds (IMCs) occurred. And increasing the Sb content increased the tensile strength. Furthermore, Sb addition decreased the steady-state creep rate and increased the stress exponent n, suggesting that the creep resistance had been enhanced, which may be attributed to the hindrance of dislocation movement by SbSn IMCs, as well as the reduction in phase boundaries, which consequently reduced grain boundary sliding.
Open AccessEffect of Sb Content on the Microstructure and Mechanical Properties of Eutectic SnPb Solder
SnPb solder was widely used in electronic packaging for aerospace devices due to its high reliability. However, its creep resistance is poor and can be improved by adding alloying elements. The effects of Sb content on the microstructure, tensile, and creep properties of eutectic SnPb solder were investigated. Sb addition effectively improved the mechanical properties of the SnPb solder. When Sb content exceeds 1.7 wt.%, SbSn intermetallic compounds (IMCs) occurred. And increasing the Sb content increased the tensile strength. Furthermore, Sb addition decreased the steady-state creep rate and increased the stress exponent n, suggesting that the creep resistance had been enhanced, which may be attributed to the hindrance of dislocation movement by SbSn IMCs, as well as the reduction in phase boundaries, which consequently reduced grain boundary sliding.
- Open Access
Improvement of PbSn Solder Reliability with Ge Microalloying-Induced Optimization of Intermetallic Compounds Growth
PbSn solders are used in semiconductor devices for aerospace or military purposes with high levels of reliability requirements. Microalloying has been widely adopted to improve the reliability for Pb-free solders, but its application in PbSn solders is scarce. In this article, the optimization of PbSn solder reliability with Ge microalloying was investigated using both experimental and calculation methods. Intermetallic compounds (IMC) growth and morphologies evolution during reliability tests were considered to be the main factors of device failure. Through first-principle calculation, the growth mechanism of interfacial Ni3Sn4 was discussed, including the formation of vacancies, the Ni-vacancies exchange diffusion and the dominant Ni diffusion along the [1 0 0] direction. The doping of Ge in the cell increased the exchange energy barrier and thus inhibited the IMC development and coarsening trend. In three reliability tests, only 0.013 wt% Ge microalloying in Pb60Sn40 was able to reduce IMC thickness by an increment of 22.6~38.7%. The proposed Ge microalloying method in traditional PbSn solder could yield a prospective candidate for highly reliable applications.
Open AccessImprovement of PbSn Solder Reliability with Ge Microalloying-Induced Optimization of Intermetallic Compounds Growth
PbSn solders are used in semiconductor devices for aerospace or military purposes with high levels of reliability requirements. Microalloying has been widely adopted to improve the reliability for Pb-free solders, but its application in PbSn solders is scarce. In this article, the optimization of PbSn solder reliability with Ge microalloying was investigated using both experimental and calculation methods. Intermetallic compounds (IMC) growth and morphologies evolution during reliability tests were considered to be the main factors of device failure. Through first-principle calculation, the growth mechanism of interfacial Ni3Sn4 was discussed, including the formation of vacancies, the Ni-vacancies exchange diffusion and the dominant Ni diffusion along the [1 0 0] direction. The doping of Ge in the cell increased the exchange energy barrier and thus inhibited the IMC development and coarsening trend. In three reliability tests, only 0.013 wt% Ge microalloying in Pb60Sn40 was able to reduce IMC thickness by an increment of 22.6~38.7%. The proposed Ge microalloying method in traditional PbSn solder could yield a prospective candidate for highly reliable applications.