Upendra Kumar Mohanty
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Upendra Kumar Mohanty has a total of 10 co-authors. Here are the top co-authors by number of shared publications:
- Ananta Prasad Chakraverty
School of Physics, Gangadhar Meher University, Sambalpur, India
3 shared publications - Ajit Behera
Department of Metallurgical & Materials Engineering National Institute of Technology Rourkela India
1 shared publication - Anil Kumar Chaubey
CSIR-IMMT
1 shared publication - Aravind Tripathy
ITER, SOA Deemed to be University
1 shared publication - Bharat Bhusan Biswal
Department of Biomedical Engineering, New Jersey Institute of Technology, Newark, NJ, 07102, USA
1 shared publication Dibyajyoti D. Pradhan
School of Physics, Gangadhar Meher University, Sambalpur, India
1 shared publication
Latest Publications
- 2 February 2024
- Published by SAGE Publications in Journal of Reinforced Plastics and Composites
Mechanothermal assessment of outdoors aged hybrid glass fibre reinforced polymer composite filled with fly ash as industrial waste
Industrial fly ash impregnated glass fibre reinforced polymer (GFRP) composites were examined to assess their overall characteristics in adverse ambient conditions, keeping in mind that use of filler materials in FRP composites was expected to enhance the strength properties of the material. GFRP composite specimens with 2–10 wt % industrial fly ash were fabricated in the laboratory. These were exposed to open ambient ageing for 120 days. The samples impregnated with 8 wt % fly ash and aged for 120 days were seen to absorb the minimum moisture and exhibited the maximum ILSS of 35.19 MPa and flexural strength of 690 MPa, respectively. These samples also exhibited the highest Tg of 101.53°C as revealed through low temperature DSC. It was also observed that the 8 wt% fly ash containing samples aged in the open for 120 days showed the ILSS to be 5.83% higher and Tg to be 21.95% higher as compared to the unaged GFRP samples without fly ash. FTIR spectra confirm the trend of thermo-mechanical properties. Both optical and scanning electron microscopy of the fractured surfaces of the test samples revealed the modes of mechanical failure of the hybrid GFRP composite with their indicative properties at optimized extent of fly ash dispersion.
- 2 February 2024
- Published by SAGE Publications in Journal of Reinforced Plastics and Composites
Mechanothermal assessment of outdoors aged hybrid glass fibre reinforced polymer composite filled with fly ash as industrial waste
Industrial fly ash impregnated glass fibre reinforced polymer (GFRP) composites were examined to assess their overall characteristics in adverse ambient conditions, keeping in mind that use of filler materials in FRP composites was expected to enhance the strength properties of the material. GFRP composite specimens with 2–10 wt % industrial fly ash were fabricated in the laboratory. These were exposed to open ambient ageing for 120 days. The samples impregnated with 8 wt % fly ash and aged for 120 days were seen to absorb the minimum moisture and exhibited the maximum ILSS of 35.19 MPa and flexural strength of 690 MPa, respectively. These samples also exhibited the highest Tg of 101.53°C as revealed through low temperature DSC. It was also observed that the 8 wt% fly ash containing samples aged in the open for 120 days showed the ILSS to be 5.83% higher and Tg to be 21.95% higher as compared to the unaged GFRP samples without fly ash. FTIR spectra confirm the trend of thermo-mechanical properties. Both optical and scanning electron microscopy of the fractured surfaces of the test samples revealed the modes of mechanical failure of the hybrid GFRP composite with their indicative properties at optimized extent of fly ash dispersion.
- 4 September 2019
- Published by Springer Nature
- p. 377-387
Fabrication of Al/Al2o3 Functionally Graded Material Using Powder Metallurgy Route
- 4 September 2019
- Published by Springer Nature
- p. 377-387
Fabrication of Al/Al2o3 Functionally Graded Material Using Powder Metallurgy Route
- 6 February 2018
- Published by SAGE Publications in Journal of Reinforced Plastics and Composites
- Vol. 37 (8) , 533-547
Impact of the ambiance on GFRP composites and role of some inherent factors: A review report
A composite material scores over its metallic counter parts in many aspects and can be tailor-made to suit the specific purpose for which it is conceived. However, during functioning the composite is exposed to the severities of the surrounding ambiance and is damaged and degraded by the atmospheric deterrent-reagents like moisture and heat fluctuations. In order to ensure a safe, extended service life-span of the composite material, it is, therefore, pertinent that the behaviour of the material related to its physical, chemical and mechanical characteristics must be analysed and established under different fluctuating ambient conditions. The present report aims at analysing and presenting the degradation/damages caused to the glass-fibre reinforced plastic (GFRP) composites under different ambient conditions and the role played by some inherent factors like the constituent components of the GFRP composites, its pre-existing flaws created during manufacturing/service-life, volume fraction fibres, length and distribution of the fibres in the matrix phase and the curing processes adopted for strengthening and stabilising the matrix structure.
- 6 February 2018
- Published by SAGE Publications in Journal of Reinforced Plastics and Composites
- Vol. 37 (8) , 533-547
Impact of the ambiance on GFRP composites and role of some inherent factors: A review report
A composite material scores over its metallic counter parts in many aspects and can be tailor-made to suit the specific purpose for which it is conceived. However, during functioning the composite is exposed to the severities of the surrounding ambiance and is damaged and degraded by the atmospheric deterrent-reagents like moisture and heat fluctuations. In order to ensure a safe, extended service life-span of the composite material, it is, therefore, pertinent that the behaviour of the material related to its physical, chemical and mechanical characteristics must be analysed and established under different fluctuating ambient conditions. The present report aims at analysing and presenting the degradation/damages caused to the glass-fibre reinforced plastic (GFRP) composites under different ambient conditions and the role played by some inherent factors like the constituent components of the GFRP composites, its pre-existing flaws created during manufacturing/service-life, volume fraction fibres, length and distribution of the fibres in the matrix phase and the curing processes adopted for strengthening and stabilising the matrix structure.
- 1 October 2012
- Published by Emerald Publishing in Emerging Materials Research
- Vol. 1 (5) , 263-270
Thermal shock behavior of hydrothermally conditioned e-glass fiber/epoxy composites
The glass fiber-reinforced polymer composites suffer from significant moisture absorption properties, moisture due to both the ambience and direct immersion in ordinary water during the course of their practical applications. The quantity of moisture absorbed and its effect on the composite component in any engineering application is also severely influenced by the temperature fluctuations. Hence the present work aims at evaluating the glass fiber/epoxy composite under hydrothermal exposure coupled with up and down-thermal shocks for various lengths of time. Inter-laminar shear strength (ILSS) values of shocked and non-shocked composite specimens were determined using INSTRON-1195 testing system. Low-temperature differential scanning calorimetry was used to monitor the glass transition temperature (Tg). A longer hydrothermal exposure showed an increase in the ILSS value after an initial low value. The ILSS seemed to vary with up and down-thermal shock differently for hydrothermally treated sample. Despite little variation in Tg value, the depression in the same was observed under up-thermal shock compared to down-thermal shock conditions. The fractographs of shocked and non-shocked specimen, as obtained from scanning electron microscope, divulged the chief mode of failure viz. fiber fragmentation and delamination.
- 1 October 2012
- Published by Emerald Publishing in Emerging Materials Research
- Vol. 1 (5) , 263-270
Thermal shock behavior of hydrothermally conditioned e-glass fiber/epoxy composites
The glass fiber-reinforced polymer composites suffer from significant moisture absorption properties, moisture due to both the ambience and direct immersion in ordinary water during the course of their practical applications. The quantity of moisture absorbed and its effect on the composite component in any engineering application is also severely influenced by the temperature fluctuations. Hence the present work aims at evaluating the glass fiber/epoxy composite under hydrothermal exposure coupled with up and down-thermal shocks for various lengths of time. Inter-laminar shear strength (ILSS) values of shocked and non-shocked composite specimens were determined using INSTRON-1195 testing system. Low-temperature differential scanning calorimetry was used to monitor the glass transition temperature (Tg). A longer hydrothermal exposure showed an increase in the ILSS value after an initial low value. The ILSS seemed to vary with up and down-thermal shock differently for hydrothermally treated sample. Despite little variation in Tg value, the depression in the same was observed under up-thermal shock compared to down-thermal shock conditions. The fractographs of shocked and non-shocked specimen, as obtained from scanning electron microscope, divulged the chief mode of failure viz. fiber fragmentation and delamination.